Scratch Through a Polyimide PI 2562 and Cr/Au Film
Material Name: Polyimide
Record No.: 163
Primary Chemical Element in Material: No data
Sample Type: Layer
Uses: Etching
Etchant Name: None
Etching Method: Dry etching
Etchant (Electrolyte) Composition: No data
Procedure (Condition): No data
Note: No data
Reference: Owen Cherry, Fabrication of an Atom Chip for Rydberg Atom-Metal SurfaceInteraction Studies, MSc Thesis, University of Waterloo, Ontario, 2007, p. 111.

Figure 1: SEM image of a scratch through a polyimide PI 2562 and Cr/Au film.