0.15C-0.5Mn Steel

Steel name: 0.15C-0.5Mn
Diagram No.: 1355
Type of diagram: CCT
Chemical composition in weight %: 0.13% C, 0.26% Si, 0.56% Mn, 0.019% P, 0.027% S, 0.07% Cr, <0.01% Mo, 0.05% Ni, <0.01% V, 0.20% Cu
Steel group: Structural steels
Note: Austenitizing temperature: 920oC. Holding time: 5 min, brought up to temperature in 3 min. Legend: Sthal-steel, Schmelze-heat, Temperatur-Temperature, Zeit-Time, Sekunden-Seconds, Minuten-Minutes, Studen-Hour, Tage-Day, Hartewerte-Hardness, Probennahme-Sample, Werksmarke-Grade, Austenitisierungstemperatur-Austenitizing temperature, Haltezeit-Holding time, Aufgehzeit-Rising time, Zw denotes intermediate structure or bainite, F denotes ferrite, M is martensite, and P is pearlite, Ms is the martensite start temperature, RA-Retained austenite, K-Carbide.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 10.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
CCT and TTT Diagram Calculating Service
CCT and TTT Diagrams Home
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
Semiconductor Etchants

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.










Copyright © 2022 by Steel Data. All Rights Reserved.