45 SCD 6 Steel

Steel name: 45 SCD 6
Diagram No.: 1747
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.8062
DIN designation: 46SiCrMo6
AFNOR designation: 45 SCD 6
Chemical composition in weight %: 0.45% C, 0.55% Mn, 1.31% Si, 0.005% S, 0.013% P 0.21% Ni, 0.60% Cr, 0.22% Mo, 0.27% Cu, <0.05% V, trace Ti
Steel group: Structural and constructional steels
Note: Austenitizing temperature: 900oC (1652oF) for 30 min. Grain size: 11.
Ac1: 770oC, Ac3: 860oC, Ms: 310oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.














Copyright © 2019 by Steel Data. All Rights Reserved.