Tyrodur 2762 Steel

Steel name: Tyrodur 2762
Diagram No.: 2591
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2762
DIN designation: 75CrMoNiW67
Chemical composition in weight %: 0.72% C, 0.40% Mn, 0.89% Si, 0.003% S, 0.014% P, 0.88% Ni, 2.94% Cr, 0.97% Mo, 0.20% V, 0.02% W, 0.004% Al, 0.25% Co, 0.06% Cu, 0.007% N, 0.01% Ti
Steel group: Cold work tool steels
Note: Steel roll diameter of 580 mm. Zeit in min - Time in min, Temperatur inoC - Temperature inoC, Abstand v.d. Walzenoberflache - distance v.s. roll surface.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.















Copyright © 2019 by Steel Data. All Rights Reserved.