Nicrofer5716 hMoW - alloy C-276

Steel name: Nicrofer5716 hMoW - alloy C-276
Diagram No.: 3387
Type of diagram: TTS
Mat. No. (Wr. Nr.) designation: 2.4819
DIN designation: NiMo16Cr15W
UNS designation: N10276
Chemical composition in weight %: 0.010% C, 1.00% Mn, 0.08% Si, 0.010% S, 0.025% P, 14.50-16.50% Cr, 15.00-17.00% Mo, 3.00-4.50% W, 4.00-7.00% Fe, 2.5% Co, 0.35% V, Ni is balance
Steel group: Corrosion-resistant alloys
Note: Time-temperature-sensitization (TTS) diagram for Nicrofer 5716 hMoW and Nicrofer 5923 hMo according to the Streicher test (ASTM G-28, Method A).
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.














Copyright © 2019 by Steel Data. All Rights Reserved.