1.0540 Steel

Steel name: 1.0540
Steel name of producers:
C50 DIN EN 10250-2:1999-12 Germany
C50 Stahl Eisen List: 2004 Germany
C50 Dirostahl Germany
C50 DIN EN 10083-2:1996-10 Germany
C50 DIN EN 10277-2:1999-10 Germany
C50 AFNOR EN 10083-2:1997-02 France
C50 BS EN 10083-2:1991 Great Britain
C50 UNE EN 10083-2:1997 Spain
C50 UNI EN 10083-2:1998 Italy
Diagram No.: 4085
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.0540
Chemical composition in weight %: 0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
Steel group: Structural steels
Note: Austenitizing temperature: 880oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.