1.1181 Steel

Steel name: 1.1181
Steel name of producers:
Diagram No.: 4120
C35E DIN EN 10083-2:2006-10 Germany
C35E DIN EN 10132-3:2000-05 Germany
C35E DIN EN 10250-2:1999-12 Germany
C35E DIN EN 10269:2006-07 Germany
C35E DIN EN 10277-5:2008-06 Germany
C35E DIN EN 10297-1:2003-06 Germany
C35E DIN EN 10305-1:2003-02 Germany
C35E Stahl Eisen List: 2004 Germany
C35E SEW 550:1976-08 Germany
Ck 35 SEW 550:1976-08 Germany
W3-1572 BOFORS Sweden
Ck35 Buderus Germany
C35E Dillinger Hüttenwerke Germany
Ck35 Dirostahl Germany
CK35 Grimm Edelstahl Germany
Ck35 HKM Krupp Mannesmann Germany
Ck35 Hover&Sohn Germany
Ck35 Platestahl Germany
Ck35 Saarstahl Germany
TEWCk35 Thyssen Edelstahl Service GmbH Germany
Ck35 Zapp Germany
C35E DIN EN 10083-1:1996-10 Germany
Ck 35 DIN EN 10083-1:1996-10 Germany
C35E DIN EN 10269:1999-11 Germany
C35E DIN EN 10277-5:1999-10 Germany
C35E DIN 1652-4:1990-11 Germany
Ck 35 DIN 1652-4:1990-11 Germany
C35E DIN 17204:1990-11 Germany
Ck 35 DIN 17204:1990-11 Germany
C35E DIN 17240:1976-07 Germany
Ck 35 DIN 17240:1976-07 Germany
Ck 35 SEL Germany
C35E AFNOR EN 10083-1:1997-02 France
XC38H1 AFNOR EN 10083-1:1997-02 France
C35E AFNOR EN 10269:1999-11 France
C35E BS EN 10083-1:1991 Great Britain
C35E UNE EN 10083-1:1997 Spain
C35E UNI EN 10083-1:1998 Italy
Ck35 DDR-TGL Germany
B7 BOFORS Sweden
V935 Bohler Uddeholm Austria
UB60 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
Ck35 Hoverstahl Germany
Ck35 Krupp Germany
V935 Bohler Uddeholm Germany
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.1181
Chemical composition in weight %: 0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
Steel group: Structural steels
Note: Austenitizing temperature: 850oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.