1.1520 Steel

Steel name: 1.1520
Steel name of producers:
C70U DIN EN ISO 4957:2001-02 Germany
C70U Stahl Eisen List: 2004 Germany
C70W1 Buderus Germany
C70W1 Dirostahl Germany
Extra-Edel7 Hagener Gussstahlwerke Remy Germany
1520 Hover&Sohn Germany
KS7 Platestahl Germany
STS6 Stahlwerk Stahlschmidt Germany
C70W1 Zapp Germany
C 70 W1 Stahl Eisen List: 2000 Germany
1520 Krupp Germany
Diagram No.: 4175
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.1520
Chemical composition in weight %: 0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
Steel group: Tool steels, unalloyed
Note: Austenitizing temperature: 810oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.





Copyright © 2019 by Steel Data. All Rights Reserved.