1.1525 Steel

Steel name: 1.1525
Steel name of producers:
C80U DIN EN ISO 4957:2001-02 Germany
C80U Stahl Eisen List: 2004 Germany
C80W1 Buderus Germany
C80W1 Dirostahl Germany
Januszähhart Dorrenberg Germany
WS4 Grimm Edelstahl Germany
Extra-Edel8 Hagener Gussstahlwerke Remy Germany
1525 Hover&Sohn Germany
Spezialzäh Kind & Co. Germany
WO9Extra Ossenberg Germany
KS9 Platestahl Germany
SpezialMzäh Schmidt+Clemens Germany
STS5 Stahlwerk Stahlschmidt Germany
THYRODUR1525 Thyssen Edelstahl Service GmbH Germany
K6Extra Zapp Germany
C 80 W1 DIN 17350:1980-10 Germany
C80U DIN 17350:1980-10 Germany
C 80 W1 Stahl Eisen List: 2000 Germany
K980 Bohler Uddeholm Austria
Hoverstahl Germany
C80W1 Klockner Stahl Bremen Germany
1525 Krupp Germany
K980 Bohler Uddeholm Germany
Diagram No.: 4177
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.1525
Chemical composition in weight %: 0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S
Steel group: Tool steels, unalloyed
Note: Austenitizing temperature: 800oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.