1.1625 Steel

Steel name: 1.1625
Steel name of producers:
C 80 W2 Stahl Eisen List: 2004 Germany
C80W2 Buderus Germany
C80W2 Dirostahl Germany
Elefantzähhart Dorrenberg Germany
WE4 Grimm Edelstahl Germany
Extra80 Hagener Gussstahlwerke Remy Germany
1625 Hover&Sohn Germany
Extrazäh Kind & Co. Germany
WO9Prima Ossenberg Germany
K18 Platestahl Germany
1.1625 Saarstahl Germany
Extrazäh Schmidt+Clemens Germany
SGS5 Stahlwerk Stahlschmidt Germany
THYRODUR1625 Thyssen Edelstahl Service GmbH Germany
K6Prima Zapp Germany
C80W2 DDR-TGL Germany
K980 Bohler Uddeholm Austria
1.1625 Hoverstahl Germany
C80W2 Klockner Stahl Bremen Germany
1625 Krupp Germany
RB8 Röchling Germany
K980 Bohler Uddeholm Germany
Diagram No.: 4182
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.1625
Chemical composition in weight %: 0.75-0.85% C, 0.10-0.30% Si, 0.10-0.35% Mn, max. 0.030% P, max. 0.030% S
Steel group: Tool steels, unalloyed
Note: Austenitizing temperature: 800oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.