1.1740 Steel

Steel name: 1.1740
Steel name of producers:
C60U Stahl Eisen List: 2004 Germany
C60W Buderus Germany
C60W Dirostahl Germany
ExtraNr.12 Dorrenberg Germany
1740 Eschmann-Stahl Germany
Extra60 Hagener Gussstahlwerke Remy Germany
1740 Hover&Sohn Germany
Primasehrzäh Kind & Co. Germany
WO5 Ossenberg Germany
1.1740 Saarstahl Germany
W360 Schmidt+Clemens Germany
THYRODUR1740 Thyssen Edelstahl Service GmbH Germany
K60 Zapp Germany
C 60 W DIN 17350:1980-10 Germany
C60U DIN 17350:1980-10 Germany
C 60 W Stahl Eisen List: 2000 Germany
C60W3 DDR-TGL Germany
K960 Bohler Uddeholm Austria
W85 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.1740 Hoverstahl Germany
C60W3 Klockner Stahl Bremen Germany
1740 Krupp Germany
K960 Bohler Uddeholm Germany
Diagram No.: 4187
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.1740
Chemical composition in weight %: 0.55-0.65% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.035% P, max. 0.035% S
Steel group: Tool steels, unalloyed
Note: Austenitizing temperature: 810oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.