1.2109 Steel

Steel name: 1.2109
Steel name of producers:
GWS4 Dorrenberg Germany
Spezial12 Hagener Gussstahlwerke Remy Germany
2109 Hover&Sohn Germany
FGS Kind & Co. Germany
KLS Ossenberg Germany
SC12 Zapp Germany
125 CrSi 5 Stahl Eisen List: 2000 Germany
125CrSi5 DDR-TGL Germany
1.2109 Hoverstahl Germany
125CrSi5 Klockner Stahl Bremen Germany
2109 Krupp Germany
Diagram No.: 4215
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.2109
Chemical composition in weight %: 1.29% C, 1.21% Si, 0.70% Mn, 0.017% P, 0.009% S, 1.20% Cr
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 850oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.






Copyright © 2019 by Steel Data. All Rights Reserved.