1.2344 Steel

Steel name: 1.2344
Steel name of producers:
X40CrMoV5-1 DIN EN ISO 4957:2001-02 Germany
X40CrMoV5-1 Stahl Eisen List: 2004 Germany
X40CrMoV5-1 SE 201:1992-10 Germany
X40CrMoV5-1 SE 202:1995-08 Germany
W3-2242 BOFORS Sweden
W302 ISOBLOC/ISODISC Bohler Uddeholm Austria
2344 ISO-B Buderus Germany
WP5V Dorrenberg Germany
THYROTHERM2344EFS Edelstahl Witten-Krefeld Germany
THYROTHERM2344EFSSup Edelstahl Witten-Krefeld Germany
245W Eschmann-Stahl Germany
CVM-Extra Grimm Edelstahl Germany
WM-SupraV Hagener Gussstahlwerke Remy Germany
2344 Hover&Sohn Germany
USD Kind & Co. Germany
Lo44 Lohmann Germany
EPS51V Ossenberg Germany
PM524V Platestahl Germany
1.2344 Saarstahl Germany
DCV Schmidt+Clemens Germany
MoforsextraV Stahlwerk Stahlschmidt Germany
TES2344EFS Thyssen Edelstahl Service GmbH Germany
TES2344ESU Thyssen Edelstahl Service GmbH Germany
THYROTHERM2344 Thyssen Edelstahl Service GmbH Germany
WAS44 WSM Werkzeugstahl Germany
CVL10V Zapp Germany
X 40CrMoV 5 1 DIN 17350:1980-10 Germany
X40CrMoV5-1 DIN 17350:1980-10 Germany
X40CrMoV5-1 Stahl Eisen List: 2000 Germany
40CrMoV21.14 DDR-TGL Germany
ROP19 BOFORS Sweden
E38V Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2344 Hoverstahl Germany
X40CrMoV51 Klockner Stahl Bremen Germany
2344 Krupp Germany
RDC2V Röchling Germany
W302 Bohler Uddeholm Germany
Diagram No.: 4243
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2344
Chemical composition in weight %: 0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, max. 0.030% P, max. 0.020% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1040oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.