1.2365 Steel

Steel name: 1.2365
Steel name of producers:
32CrMoV12-28 DIN EN ISO 4957:2001-02 Germany
32CrMoV12-28 Stahl Eisen List: 2004 Germany
32CrMoV12-28 SE 201:1992-10 Germany
X 32 CrMoV 3 3 SE 201:1992-10 Germany
X32CrMoV33 SE 201:1992-10 Germany
W320 ISODISC Bohler Uddeholm Austria
2365 ISO-B Buderus Germany
X32CrMoV33 Dirostahl Germany
DM3 Dorrenberg Germany
THYROTHERM2365EFS Edelstahl Witten-Krefeld Germany
THYROTHERM2365EFSSup Edelstahl Witten-Krefeld Germany
225W Eschmann-Stahl Germany
WPR Grimm Edelstahl Germany
WP3 Hagener Gussstahlwerke Remy Germany
2365 Hover&Sohn Germany
RP Kind & Co. Germany
Kobalt10 Lohmann Germany
WMo Lohmann Germany
EPS33 Ossenberg Germany
USMo Platestahl Germany
1.2365 Saarstahl Germany
WM28 Schmidt+Clemens Germany
MoforsSpezialT Stahlwerk Stahlschmidt Germany
THYROTHERM2365 Thyssen Edelstahl Service GmbH Germany
WAS65 WSM Werkzeugstahl Germany
CVL30 Zapp Germany
X 32 CrMoV 3 3 Stahl Eisen List: 2000 Germany
32CrMoV11.28 DDR-TGL Germany
DuraxMo3 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2365 Hoverstahl Germany
X32CrMoV33 Klockner Stahl Bremen Germany
2365 Krupp Germany
RPG3 Röchling Germany
W320 Bohler Uddeholm Germany
Diagram No.: 4253
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2365
Chemical composition in weight %: 0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, max. 0.030% P, max. 0.020% S, 2.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1030oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.