1.2367 Steel

Steel name: 1.2367
Steel name of producers:
X38CrMoV5-3 DIN EN ISO 4957:2001-02 Germany
X38CrMoV5-3 Stahl Eisen List: 2004 Germany
X38CrMoV5-3 SE 201:1992-10 Germany
X40CrMoV5-3 SE 201:1992-10 Germany
X38CrMoV5-3 SE 202:1995-08 Germany
W303 ISOBLOC/ISODISC Bohler Uddeholm Austria
2367 ISO-B Buderus Germany
DM3X Dorrenberg Germany
THYROTHERM2367EFS Edelstahl Witten-Krefeld Germany
THYROTHERM2367EFSSup Edelstahl Witten-Krefeld Germany
2367 Eschmann-Stahl Germany
WPR-Spezial Grimm Edelstahl Germany
WMCr Hagener Gussstahlwerke Remy Germany
RPU Kind & Co. Germany
LO67 Lohmann Germany
EPS53 Ossenberg Germany
HLDS Platestahl Germany
PM536 Platestahl Germany
PM536BLW Platestahl Germany
PM536St Platestahl Germany
1.2367 Saarstahl Germany
MärkerWM30 Schmidt+Clemens Germany
PD2 Stahlwerk Stahlschmidt Germany
TES2367 Thyssen Edelstahl Service GmbH Germany
THYROTHERM2367 Thyssen Edelstahl Service GmbH Germany
LC50 Zapp Germany
2367 Krupp Germany
RDC5 Röchling Germany
W303 Bohler Uddeholm Germany
Diagram No.: 4255
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2367
Chemical composition in weight %: 0.35-0.40% C, 0.30-0.50% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.020% S, 4.80-5.20% Cr, 2.70-3.20% Mo, 0.40-0.60% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1080oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.