1.2436 Steel

Steel name: 1.2436
Steel name of producers:
X210CrW12 DIN EN ISO 4957:2001-02 Germany
X210CrW12 Stahl Eisen List: 2004 Germany
K107 Bohler Uddeholm Austria
2436 ISO-B Buderus Germany
X210CrW12 Dirostahl Germany
CPW Dorrenberg Germany
50SW Eschmann-Stahl Germany
CWL Grimm Edelstahl Germany
IntensivWo Hagener Gussstahlwerke Remy Germany
2436 Hover&Sohn Germany
CHW Kind & Co. Germany
LC-Spezial Lohmann Germany
ESS Ossenberg Germany
NM240V Platestahl Germany
1.2436 Saarstahl Germany
476M Schmidt+Clemens Germany
S.N.S.Spezial Stahlwerk Stahlschmidt Germany
TES2436 Thyssen Edelstahl Service GmbH Germany
THYRODUR2436 Thyssen Edelstahl Service GmbH Germany
WCR36 WSM Werkzeugstahl Germany
WC120 Zapp Germany
X210CrW12 DIN 17350:1980-10 Germany
210CrW46 DDR-TGL Germany
Bora Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2436 Hoverstahl Germany
X210CrW12 Klockner Stahl Bremen Germany
2436 Krupp Germany
K107 Bohler Uddeholm Germany
Diagram No.: 4267
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2436
Chemical composition in weight %: 2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 950oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.