1.2581 Steel

Steel name: 1.2581
Steel name of producers:
X30WCrV9-3 DIN EN ISO 4957:2001-02 Germany
X30WCrV9-3 Stahl Eisen List: 2004 Germany
W100 Bohler Uddeholm Austria
X30WCrV93 Buderus Germany
X30WCrV93 Dirostahl Germany
W9 Dorrenberg Germany
2581 Eschmann-Stahl Germany
HWP Grimm Edelstahl Germany
WZK-Spezial Hagener Gussstahlwerke Remy Germany
2581 Hover&Sohn Germany
MA Kind & Co. Germany
EPS Ossenberg Germany
PW190 Platestahl Germany
PW190/So Platestahl Germany
PW190Ni Platestahl Germany
1.2581 Saarstahl Germany
W11 Schmidt+Clemens Germany
S.Z.P.80 Stahlwerk Stahlschmidt Germany
TES2581 Thyssen Edelstahl Service GmbH Germany
THYROTHERM2581 Thyssen Edelstahl Service GmbH Germany
CVW85 Zapp Germany
X30WCrV9-3 Stahl Eisen List: 2000 Germany
30WCrV34.11 DDR-TGL Germany
SpezialW Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2581 Hoverstahl Germany
2581 Krupp Germany
RCW2H Röchling Germany
W100 Bohler Uddeholm Germany
Diagram No.: 4284
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2581
Chemical composition in weight %: 0.30% C, 2.60% Cr, 8.50% W, 0.40% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1150oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.