1.2606 Steel

Steel name: 1.2606
Steel name of producers:
X37CrMoW5-1 Stahl Eisen List: 2004 Germany
2606 ISO-B Buderus Germany
WP5X Dorrenberg Germany
2606 Eschmann-Stahl Germany
PLP Grimm Edelstahl Germany
WM-SupraWo Hagener Gussstahlwerke Remy Germany
2606 Hover&Sohn Germany
US Kind & Co. Germany
WCr Lohmann Germany
EPSW51 Ossenberg Germany
PM512 Platestahl Germany
PM512C Platestahl Germany
PM512St Platestahl Germany
DCW Schmidt+Clemens Germany
MoforsExtraw Stahlwerk Stahlschmidt Germany
THYROTHERM2606 Thyssen Edelstahl Service GmbH Germany
CVL10Extra Zapp Germany
W304 Bohler Uddeholm Austria
E38W Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2606 Hoverstahl Germany
2606 Krupp Germany
RDC1 Röchling Germany
Diagram No.: 4291
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.2606
Chemical composition in weight %: 0.32-0.40% C, 0.90-1.20% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 5.00-5.60% Cr, 1.30-1.60% Mo, 1.20-1.40% W, 0.15-0.40% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1020oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.