1.2662 Steel

Steel name: 1.2662
Steel name of producers:
X30WCrCoV9-3 Stahl Eisen List: 2004 Germany
W11C Dorrenberg Germany
WP12 Hagener Gussstahlwerke Remy Germany
2662 Hover&Sohn Germany
MASupra Kind & Co. Germany
EPSK2 Ossenberg Germany
PZ190 Platestahl Germany
MärkerSPM Schmidt+Clemens Germany
S.Z.P.120 Stahlwerk Stahlschmidt Germany
BCVW85 Zapp Germany
WC2 Deutsche Edelstahlwerke (Witten-Krefeld) Germany In
2662 Krupp Germany
Diagram No.: 4295
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2662
Chemical composition in weight %: 0.27-0.32% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 2.20-2.50% Cr, 8.00-9.00% W, 0.20-0.30% V, 1.80-2.30% Co
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1080oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.