1.2714 Steel

Steel name: 1.2714
Steel name of producers:
55NiCrMoV7 DIN EN ISO 4957:2001-02 Germany
55NiCrMoV7 Stahl Eisen List: 2004 Germany
55NiCrMoV7 SE 201:1992-10 Germany
56 NiCrMoV 7 SE 201:1992-10 Germany
56NiCrMoV7 SE 201:1992-10 Germany
55NiCrMoV7 SE 202:1995-08 Germany
56 NiCrMoV 7 SE 202:1995-08 Germany
W500 Bohler Uddeholm Austria
2714 ISO-B Buderus Germany
2714 ISO-B MOD Buderus Germany
56NiCrMoV7 Dirostahl Germany
A50 Dorrenberg Germany
THYROTHERM2714 Edelstahl Witten-Krefeld Germany
370G Eschmann-Stahl Germany
GHM Grimm Edelstahl Germany
OmegaExtraV Hagener Gussstahlwerke Remy Germany
2714 Hover&Sohn Germany
PWM Kind & Co. Germany
GSNi Lohmann Germany
WPS1 Ossenberg Germany
PU37 Platestahl Germany
1.2714 Saarstahl Germany
SRSE Schmidt+Clemens Germany
H.W.G. Stahlwerk Stahlschmidt Germany
TES2714 Thyssen Edelstahl Service GmbH Germany
THYROTHERM2714 Thyssen Edelstahl Service GmbH Germany
WHG2 WSM Werkzeugstahl Germany
CNL5 Zapp Germany
55NiCrMoV7 DIN 17350:1980-10 Germany
56 NiCrMoV 7 DIN 17350:1980-10 Germany
56 NiCrMoV 7 Stahl Eisen List: 2000 Germany
56NiCrMoV7.4 DDR-TGL Germany
AMSextra Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2714 Hoverstahl Germany
56NiCrMoV7 Klockner Stahl Bremen Germany
2714 Krupp Germany
RGS4 Röchling Germany
W500 Bohler Uddeholm Germany
Diagram No.: 4303
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2714
Chemical composition in weight %: 0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 850oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.