1.2767 Steel

Steel name: 1.2767
Steel name of producers:
45NiCrMo16 DIN EN ISO 4957:2001-02 Germany
45NiCrMo16 Stahl Eisen List: 2004 Germany
K600 Bohler Uddeholm Austria
2767 ISO-B Buderus Germany
VNC4 Dorrenberg Germany
VNC4M Dorrenberg Germany
275KM-Spezial Eschmann-Stahl Germany
KPH Grimm Edelstahl Germany
KPMo Hagener Gussstahlwerke Remy Germany
2767 Hover&Sohn Germany
N400 Kind & Co. Germany
CNi40 Lohmann Germany
ELBSpez. Ossenberg Germany
ELBSpezial Ossenberg Germany
KW83 Platestahl Germany
KW83/St Platestahl Germany
KW83Spez Platestahl Germany
KW83Spezial Platestahl Germany
1.2767 Saarstahl Germany
PSHB Schmidt+Clemens Germany
TES2767 Thyssen Edelstahl Service GmbH Germany
THYRODUR2767 Thyssen Edelstahl Service GmbH Germany
EP67 WSM Werkzeugstahl Germany
LCN45 Zapp Germany
X45NiCrMo4 DIN 17350:1980-10 Germany
X45NiCrMo4 Stahl Eisen List: 2000 Germany
CNK2 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.2767 Hoverstahl Germany
X45NiCrMo4 Klockner Stahl Bremen Germany
2767 Krupp Germany
K600 Bohler Uddeholm Germany
Diagram No.: 4321
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.2767
Chemical composition in weight %: 0.42% C, 0.39% Si, 0.38% Mn, 0.017% P, 0.010% S, 1.61% Cr, 0.23% Mo, 4.40% Ni, 0.060% V
Steel group: Tool steels, alloyed
Note: Austenitizing temperature: 1050oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.