1.3348 Steel

Steel name: 1.3348
Steel name of producers:
HS2-9-2 DIN EN ISO 4957:2001-02 Germany
HS2-9-2 Stahl Eisen List: 2004 Germany
S400 Bohler Uddeholm Austria
DMo5V Dorrenberg Germany
DMo9V Dorrenberg Germany
PrestoVaMoSu. Hagener Gussstahlwerke Remy Germany
B94 Kind & Co. Germany
SVX822 Platestahl Germany
1.3348 Saarstahl Germany
MO9V Schmidt+Clemens Germany
H.S.90V Stahlwerk Stahlschmidt Germany
THYRAPID3348 Thyssen Edelstahl Service GmbH Germany
HS2-9-2 DIN 17350:1980-10 Germany
S 2-9-2 DIN 17350:1980-10 Germany
S 2-9-2 Stahl Eisen List: 2000 Germany
Mo19 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
S2-9-2 Klockner Stahl Bremen Germany
3348 Krupp Germany
GigantM9V Röchling Germany
S400 Bohler Uddeholm Germany
Diagram No.: 4356
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.3348
Chemical composition in weight %: 1.00% C, 4.00% Cr, 9.00% Mo, 1.75% W, 2.00% V
Steel group: High speed steels
Note: Austenitizing temperature: 1210oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.