1.3536 Steel

Steel name: 1.3536
Steel name of producers:
100CrMo7-3 DIN EN ISO 683-17:2000-04 Germany
100CrMo7-3 Stahl Eisen List: 2004 Germany
100CrMo73 Dirostahl Germany
ExtraMo Kind & Co. Germany
W5 Platestahl Germany
TEW100CrMo73 Thyssen Edelstahl Service GmbH Germany
100CrMo7-3 DIN 17230:1980-09 Germany
100CrMo7-3 Stahl Eisen List: 2000 Germany
100CrMo6 Krupp Germany
Diagram No.: 4375
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.3536
Chemical composition in weight %: 0.93-1.05% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, max. 0.30% Cu, max. 0.050% Al
Steel group: Bearing steels
Note: Austenitizing temperature: 860oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.







Copyright © 2019 by Steel Data. All Rights Reserved.