1.4005 Steel

Steel name: 1.4005
Steel name of producers:
X12CrS13 DIN EN 10088-1:2005-09 Germany
X12CrS13 DIN EN 10088-3:2005-09 Germany
X12CrS13 Stahl Eisen List: 2004 Germany
X12CrS13 NF S 94-090:2001-04 Germany
DE4005 Dorrenberg Germany
PuroWA Hagener Gussstahlwerke Remy Germany
X12CrS13 Platestahl Germany
REMANIT4005 Thyssen Edelstahl Service GmbH Germany
TS4005 ThyssenKrupp Schulte Germany
ARGESTE 1.4005 IA Zapp Germany
ARGESTE 1.4005 IU Zapp Germany
X12CrS13 DIN EN 10088-1:1995-08 Germany
X12CrS13 DIN EN 10088-3:1995-08 Germany
X12CrS13 AFNOR EN 10088-3:1995-11 France
X12CrS13 BS EN 10088-3:1995 Great Britain
X12CrS13 UNE EN 10088-3:1996 Spain
X12CrS13 UNI EN 10088-1:1997 Italy
X12CrS13 UNI EN 10088-3:1997 Italy
NIROSTA4005 ThyssenKrupp Nirosta Germany
Westig4005 Westig GmbH Germany
Diagram No.: 4393
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.4005
Chemical composition in weight %: 0.14% C, 0.31% Si, 0.97% Mn, 0.017% P, 0.137% S, 12.65% Cr, 0.07% Mo, 0.24% Ni, 0.003% Al, 0.0350% N
Steel group: Stainless steels
Note: Austenitizing temperature: 1100oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.