1.4016 Steel

Steel name: 1.4016
Steel name of producers:
X6Cr17 DIN EN 10088-1:2005-09 Germany
X6Cr17 DIN EN 10088-2:2005-09 Germany
X6Cr17 DIN EN 10088-3:2005-09 Germany
X6Cr17 DIN EN 10151:2003-02 Germany
X6Cr17 DIN EN 10250-4:2000-02 Germany
X6Cr17 DIN EN 10263-5:2002-02 Germany
X6Cr17 DIN EN 10296-2:2006-02 Germany
X6Cr17 DIN EN 10297-2:2006-02 Germany
X6Cr17 DIN 5512-3:2004-05 Germany
X6Cr17 Stahl Eisen List: 2004 Germany
N200 Bohler Uddeholm Austria
X8Cr17 Buderus Germany
DE4016 Dorrenberg Germany
PuroCr Hagener Gussstahlwerke Remy Germany
RS10 Hover&Sohn Germany
R17F Kind & Co. Germany
RFS1 Ossenberg Germany
PFC171 Platestahl Germany
1.4016Saarstahl Germany
Corronon16 Stahlwerk Stahlschmidt Germany
REMANIT4016 Thyssen Edelstahl Service GmbH Germany
NIROSTA4016 ThyssenKrupp Nirosta Germany
TS4016 ThyssenKrupp Schulte Germany
1.4016 Zapp Germany
ARGESTE 1.4016 IH Zapp Germany
ARGESTE 1.4016 IM Zapp Germany
X6Cr17 DIN EN 10088-1:1995-08 Germany
X6Cr17 DIN EN 10088-2:1995-08 Germany
X6Cr17 DIN EN 10088-3:1995-08 Germany
X6Cr17 DIN 1654-5:1989-10 Germany
X6Cr17 DIN 17440:2001-03 Germany
X6Cr17 DIN 17455:1999-02 Germany
X6Cr17 DIN 17456:1999-02 Germany
X6Cr17 DIN 5512-3:1991-01 Germany
X6Cr17 AFNOR EN 10088-1:1995-11 France
X6Cr17 BS EN 10088-2:1995 Great Britain
X6Cr17 BS EN 10088-3:1995 Great Britain
X6Cr17 UNE EN 10088-2:1996 Spain
E-430 UNE EN 10088-3:1996 Spain
X6Cr17 UNE EN 10088-3:1996 Spain
X6Cr17 UNI EN 10088-1:1997 Italy
X6Cr17 UNI EN 10088-2:1997 Italy
X6Cr17 UNI EN 10088-3:1997 Italy
X8Cr17 DDR-TGL Germany
Coracid4016 Hoverstahl Germany
1.4016 Klockner Stahl Bremen Germany
Westig4016 Westig GmbH Germany
Diagram No.: 4395
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.4016
Chemical composition in weight %: 0.07% C, 0.24% Si, 0.45% Mn, 0.020% P, 0.010% S, 17.35% Cr, 0.03% Mo, 0.15% Ni, 0.003% Al, 0.0280% N
Steel group: Stainless steels
Note: Austenitizing temperature: 1100oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.