1.4104 Steel

Steel name: 1.4104
Steel name of producers:
X14CrMoS17 DIN EN 10088-1:2005-09 Germany
X14CrMoS17 DIN EN 10088-3:2005-09 Germany
X14CrMoS17 Stahl Eisen List: 2004 Germany
N310 Bohler Uddeholm Austria
DE4104 Dorrenberg Germany
R17WS Dorrenberg Germany
REMANIT4104 Edelstahl Witten-Krefeld Germany
RF17S Grimm Edelstahl Germany
PuroWS Hagener Gussstahlwerke Remy Germany
RS14 Hover&Sohn Germany
RM161A Kind & Co. Germany
RFS3 Ossenberg Germany
PFC171S Platestahl Germany
REMANIT4104 Thyssen Edelstahl Service GmbH Germany
1.4104 Zapp Germany
ARGESTE 1.4104 YU Zapp Germany
X14CrMoS17 DIN EN 10088-1:1995-08 Germany
X14CrMoS17 DIN EN 10088-3:1995-08 Germany
X14CrMoS17 DIN 17440:2001-03 Germany
X14CrMoS17 AFNOR EN 10088-3:1995-11 France
X14CrMoS17 BS EN 10088-3:1995 Great Britain
X14CrMoS17 UNE EN 10088-3:1996 Spain
X14CrMoS17 UNI EN 10088-1:1997 Italy
X14CrMoS17 UNI EN 10088-3:1997 Italy
X12CrMoS17 DDR-TGL Germany
Coracid4104 Hoverstahl Germany
1.4104 Klockner Stahl Bremen Germany
NIROSTA4104 ThyssenKrupp Nirosta Germany
Westig4104 Westig GmbH Germany
Diagram No.: 4412
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.4104
Chemical composition in weight %: 0.15% C, 0.26% Si, 0.79% Mn, 0.020% P, 0.240% S, 17.10% Cr, 0.34% Mo, 0.10% Ni
Steel group: Stainless steels
Note: Austenitizing temperature: 1030oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.