1.4113 Steel

Steel name: 1.4113
Steel name of producers:
X6CrMo17-1 DIN EN 10088-1:2005-09 Germany
X6CrMo17-1 DIN EN 10088-2:2005-09 Germany
X6CrMo17-1 DIN EN 10088-3:2005-09 Germany
X6CrMo17-1 DIN EN 10263-5:2002-02 Germany
X6CrMo17-1 Stahl Eisen List: 2004 Germany
DE4113 Dorrenberg Germany
REMANIT4113 Thyssen Edelstahl Service GmbH Germany
NIROSTA4113 ThyssenKrupp Nirosta Germany
ARGESTE 1.4113 IL Zapp Germany
ARGESTE 1.4113 IM Zapp Germany
X6CrMo17-1 DIN EN 10088-1:1995-08 Germany
X6CrMo17-1 DIN EN 10088-2:1995-08 Germany
X6CrMo17-1 DIN EN 10088-3:1995-08 Germany
X6CrMo17-1 AFNOR EN 10088-1:1995-11 France
X6CrMo17-1 BS EN 10088-2:1995 Great Britain
X6CrMo17-1 BS EN 10088-3:1995 Great Britain
X6CrMo17-1 UNE EN 10088-2:1996 Spain
X6CrMo17-1 UNE EN 10088-3:1996 Spain
X6CrMo17-1 UNI EN 10088-1:1997 Italy
X6CrMo17-1 UNI EN 10088-2:1997 Italy
X6CrMo17-1 UNI EN 10088-3:1997 Italy
1.4113 Klockner Stahl Bremen Germany
Diagram No.: 4418
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.4113
Chemical composition in weight %: 0.04% C, 0.33% Si, 0.48% Mn, 0.014% P, 0.007% S, 17.55% Cr, 1.19% Mo, 0.18% Ni, 0.0290% N
Steel group: Stainless steels
Note: Austenitizing temperature: 1100oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.