1.4122 Steel

Steel name: 1.4122
Steel name of producers:
X39CrMo17-1 DIN EN 10088-1:2005-09 Germany
X39CrMo17-1 DIN EN 10088-2:2005-09 Germany
X39CrMo17-1 DIN EN 10088-3:2005-09 Germany
GX35CrMo17 Stahl Eisen List: 2004 Germany
X39CrMo17-1 Stahl Eisen List: 2004 Germany
N335 Bohler Uddeholm Austria
X35CrMo17 Buderus Germany
GR17M;HC17M Dorrenberg Germany
REMANIT4122 Edelstahl Witten-Krefeld Germany
RF20C Grimm Edelstahl Germany
PuroHMo2 Hagener Gussstahlwerke Remy Germany
RS16 Hover&Sohn Germany
RM174 Kind & Co. Germany
RFMo Lohmann Germany
RFSh4 Ossenberg Germany
PMCo174 Platestahl Germany
MärkerIrrubigo. Schmidt+Clemens Germany
Corronon17Mo Stahlwerk Stahlschmidt Germany
REMANIT4122 Thyssen Edelstahl Service GmbH Germany
X35CrMo17 Thyssen Edelstahl Service GmbH Germany
ARGESTE 1.4122 YL Zapp Germany
K35L Zapp Germany
WESTIG 1.4122 YL Zapp Germany
X39CrMo17-1 DIN EN 10088-1:1995-08 Germany
X39CrMo17-1 DIN EN 10088-2:1995-08 Germany
X39CrMo17-1 DIN EN 10088-3:1995-08 Germany
X39CrMo17-1 AFNOR EN 10088-1:1995-11 France
X39CrMo17-1 BS EN 10088-2:1995 Great Britain
X39CrMo17-1 BS EN 10088-3:1995 Great Britain
X39CrMo17-1 UNE EN 10088-2:1996 Spain
X39CrMo17-1 UNE EN 10088-3:1996 Spain
X39CrMo17-1 UNI EN 10088-1:1997 Italy
X39CrMo17-1 UNI EN 10088-2:1997 Italy
X39CrMo17-1 UNI EN 10088-3:1997 Italy
X35CrMo17 DDR-TGL Germany
Remanit1740 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
Coracid4122 Hoverstahl Germany
1.4122 Klockner Stahl Bremen Germany
NOVONIT4122 Krupp Germany
NIROSTA4122 ThyssenKrupp Nirosta Germany
Westig4122 Westig GmbH Germany
Diagram No.: 4421
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.4122
Chemical composition in weight %: 0.33-0.45% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, max. 0.015% S, 15.50-17.50% Cr, 0.80-1.30% Mo, max. 1.00% Ni
Steel group: Stainless steels
Note: Austenitizing temperature: 1010oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.