1.4935 Steel

Steel name: 1.4935
Steel name of producers:
X20CrMoWV12-1 DIN EN 10088-1:2005-09 Germany
X20CrMoWV12-1 DIN EN 10302:2008-06 Germany
X20CrMoWV12-1 Stahl Eisen List: 2004 Germany
X20CrMoWV12-1 DIN EN 10302:2002-09 Germany
T502 Bohler Uddeholm Austria
CRONIDUR4935 Krupp Germany
Diagram No.: 4437
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.4935
Chemical composition in weight %: 0.24% C, 0.28% Si, 0.43% Mn, 0.017% P, 0.009% S, 11.52% Cr, 0.93% Mo, 0.69% Ni, 0.30% V, 0.50% W
Steel group: Steels
Note: Materials with elevated temperature properties. Austenitizing temperature: 1050oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.










Copyright © 2019 by Steel Data. All Rights Reserved.