Steel name of producers:
X19CrMoNbVN11-1 DIN EN 10088-1:2005-09 Germany
X19CrMoNbVN11-1 DIN EN 10269:2006-07 Germany
X19CrMoNbVN11-1 DIN EN 10302:2008-06 Germany
X19CrMoNbVN11-1 Stahl Eisen List: 2004 Germany
T560 Bohler Uddeholm Austria
4913 Hover&Sohn Germany
THERMON4913 Thyssen Edelstahl Service GmbH Germany
X19CrMoNbVN11-1 DIN EN 10269:1999-11 Germany
X19CrMoNbVN11-1 DIN EN 10302:2002-09 Germany
X19CrMoNbVN11-1 AFNOR EN 10269:1999-11 France
CRONIDUR4913 Krupp Germany
Diagram No.: 4440
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.4913
Chemical composition in weight %: 0.17% C, 0.22% Si, 0.57% Mn, 0.027% P, 0.025% S, 12.00% Cr, 0.51% Mo, 0.81% Ni, 0.25% V, 0.20% Nb
Steel group: Steels
Note: Materials with elevated temperature properties. Austenitizing temperature: 1100oC, time: 10 min.
Reference: HTDG, 2008.

Transformation Diagram


Click the image to enlarge the diagram.

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.