1.5523 Steel

Steel name: 1.5523
Steel name of producers:
19MnB4 DIN EN 10269:2006-07 Germany
19MnB4 Stahl Eisen List: 2004 Germany
19MnB4 Saarstahl Germany
TEW19MnB4 Thyssen Edelstahl Service GmbH Germany
19MnB4 DIN EN 10269:1999-11 Germany
19MnB4 DIN 1654-4:1989-10 Germany
19MnB4 AFNOR EN 10269:1999-11 France
Diagram No.: 4479
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.5523
Chemical composition in weight %: 0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.0980% N
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 1150oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.









Copyright © 2019 by Steel Data. All Rights Reserved.