1.5732 Steel

Steel name: 1.5732
Steel name of producers:
14NiCr10 Dirostahl Germany
TEW14NiCr10 Thyssen Edelstahl Service GmbH Germany
14NiCr10 Zapp Germany
14NiCr14 Zapp Germany
14NiCr10 Stahl Eisen List: 2000 Germany
14NiCr10 Krupp Germany
RAE2 Röchling Germany
Diagram No.: 4501
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.5732
Chemical composition in weight %: 0.13% C, 0.39% Si, 0.42% Mn, 0.013% P, 0.008% S, 0.78% Cr, 3.53% Ni
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 840oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.










Copyright © 2019 by Steel Data. All Rights Reserved.