1.5919 Steel

Steel name: 1.5919
Steel name of producers:
15CrNi6 Stahl Eisen List: 2004 Germany
E230 Bohler Uddeholm Austria
15CrNi6 Dirostahl Germany
15CrNi6 Grimm Edelstahl Germany
15CrNi6 Hover&Sohn Germany
15CrNi6 Saarstahl Germany
15CrNi6 Thyssen Edelstahl Service GmbH Germany
TEW15 CrNi6 Thyssen Edelstahl Service GmbH Germany
TEW15CrNi6 Thyssen Edelstahl Service GmbH Germany
15CrNi6 Zapp Germany
15CrNi6 DIN 1652-3:1990-11 Germany
15CrNi6 DIN 1654-3:1989-10 Germany
15CrNi6 DIN 17210:1986-09 Germany
15CrNi6 DDR-TGL Germany
E15Z Deutsche Edelstahlwerke (Witten-Krefeld) Germany
15CrNi6 Krupp Germany
RECNW Röchling Germany
E230 Bohler Uddeholm Germany
Diagram No.: 4528
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.5919
Chemical composition in weight %: 0.14% C, 0.25% Si, 0.56% Mn, 0.019% P, 0.020% S, 1.59% Cr, 1.46% Ni
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 870oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.