1.7149 Steel

Steel name: 1.7149
Steel name of producers:
20MnCrS5 DIN EN 10084:2008-06 Germany
20MnCrS5 DIN EN 10263-3:2002-02 Germany
20MnCrS5 DIN EN 10277-4:2008-06 Germany
20MnCrS5 Stahl Eisen List: 2004 Germany
20MnCrS5 AFNOR EN 10084:1999-03 France
20MnCrS5 UNE EN 10084:1998 Spain
20MnCrS5 Dirostahl Germany
20MnCrS5 HKM Krupp Mannesmann Germany
20MnCrS5 Saarstahl Germany
20MnCrS5 Thyssen Edelstahl Service GmbH Germany
TEW20MnCrS5 Thyssen Edelstahl Service GmbH Germany
20MnCrS5 DIN EN 10084:1998-06 Germany
20MnCrS5 DIN EN 10277-4:1999-10 Germany
20MnCrS5 DIN 1652-3:1990-11 Germany
20MnCrS5 Krupp Germany
Diagram No.: 4633
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.7149
Chemical composition in weight %: 0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 850oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.