1.7223 Steel

Steel name: 1.7223
Steel name of producers:
41CrMo4 Stahl Eisen List: 2004 Germany
41CrMo4 Dirostahl Germany
41CrMo4 HKM Krupp Mannesmann Germany
TEW41CrMo4 Thyssen Edelstahl Service GmbH Germany
41CrMo4 DIN 17212:1972-08 Germany
41CrMo4 Krupp Germany
V320 Bohler Uddeholm Germany
Diagram No.: 4648
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.7223
Chemical composition in weight %: 0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 850oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.









Copyright © 2019 by Steel Data. All Rights Reserved.