1.7380 Steel

Steel name: 1.7380
Steel name of producers:
10CrMo9-10 DIN EN 10028-2:2003-09 Germany
10CrMo9-10 DIN EN 10216-2:2007-10 Germany
10CrMo9-10 DIN EN 10273:2008-02 Germany
10CrMo9-10 Stahl Eisen List: 2004 Germany
10CrMo910 Buderus Germany
10CrMo9-10 Dillinger Hüttenwerke Germany
10CrMo910 Dirostahl Germany
T1 Grimm Edelstahl Germany
10CrMo910 HKM Krupp Mannesmann Germany
10CrMo910 Hover&Sohn Germany
10CrMo910 Platestahl Germany
10CrMo910 Saarstahl Germany
10CrMo9-10 Thyssen Edelstahl Service GmbH Germany
TEW10CrMo910 Thyssen Edelstahl Service GmbH Germany
10CrMo910 Zapp Germany
10CrMo9-10 DIN EN 10028-2:1993-04 Germany
10CrMo9-10 DIN EN 10216-2:2002-08 Germany
10CrMo9-10 DIN EN 10216-2:2004-07 Germany
10CrMo9-10 DIN EN 10273:2000-04 Germany
10CrMo9-10 DIN 17175:1979-05 Germany
10CrMo9-10 DIN 17176:1990-11 Germany
10CrMo9-10 DIN 17243:1987-01 Germany
10CrMo9-10 AFNOR EN 10028-2:1992-12 France
10CrMo9-10 BS EN 10028-2:1993 Great Britain
GS12CrMo9-10 SEW 595:1976-08 Germany
10CrMo9-10 UNE EN 10028-2:1994 Spain
10CrMo9-10 UNI EN 10028-2:1993 Italy
10CrMo9.10 DDR-TGL Germany
D320 Bohler Uddeholm Austria
MC90 Deutsche Edelstahlwerke (Witten-Krefeld) Germany
1.7380 Hoverstahl Germany
10CrMo910 Krupp Germany
D320 Bohler Uddeholm Germany Diagram No.: 4684
Type of diagram: TTT
Mat. No. (Wr. Nr.) designation: 1.7380
Chemical composition in weight %: 0.11% C, 0.21% Si, 0.47% Mn, 0.010% P, 0.010% S, 2.29% Cr, 1.02% Mo, 0.14% Ni, 0.010% V, 0.18% Cu
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 980oC, time: 10 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.