1.7735 Steel

Steel name: 1.7735
Steel name of producers:
14CrMoV6-9 Stahl Eisen List: 2004 Germany
14CrMoV69 Dirostahl Germany
14CrMoV6.9 Grimm Edelstahl Germany
Remy 1.7735 Hagener Gussstahlwerke Remy Germany
14CrMoV69 Saarstahl Germany
thermanit1m Thyssen Edelstahl Service GmbH Germany
Diagram No.: 4697
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.7735
Chemical composition in weight %: 0.11-0.17% C, max. 0.25% Si, 0.80-1.00% Mn, max. 0.020% P, max. 0.015% S, 1.25-1.50% Cr, 0.80-1.00% Mo, 0.20-0.300% V
Steel group: Structural steels
Note: Alloy special structural steels. Austenitizing temperature: 950oC.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.










Copyright © 2019 by Steel Data. All Rights Reserved.