1.8918 Steel

Steel name: 1.8918
Steel name of producers:
P460NL2 DIN EN 10028-3:2003-09 Germany
P460NL2 DIN EN 10216-3:2004-07 Germany
P460NL2 DIN EN 10217-3:2005-04 Germany
P460NL2 Stahl Eisen List: 2004 Germany
EStE 460 SEW 081-2:1998-09 Germany
P460NL2 SEW 081-2:1998-09 Germany
DILLINAL58/47E Dillinger Hüttenwerke Germany
KStE460 Dirostahl Germany
P460NL2 DIN EN 10028-3:1993-04 Germany
P460NL2 DIN EN 10216-3:2002-08 Germany
P460NL2 DIN EN 10217-3:2002-08 Germany
EStE 460 DIN 17142 Germany
P460NL2 DIN 17142 Germany
EStE 460 DIN 17178:1986-05 Germany
P460NL2 DIN 17178:1986-05 Germany
EStE 460 DIN 17179:1986-05 Germany
P460NL2 DIN 17179:1986-05 Germany
EStE 460 Stahl Eisen List: 2000 Germany
P460NL2 AFNOR EN 10028-3:1992-12 France
P460NL2 BS EN 10028-3:1993 Great Britain
P460NL2 UNE EN 10028-3:1996 Spain
P460NL2 UNI EN 10028-3:1993 Italy
Diagram No.: 4730
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.8918
Chemical composition in weight %: 0.18% C, 0.32% Si, 1.32% Mn, 0.33% Ni, 0.168% V, 0.020% Al
Steel group: High strength weldable structural steels
Note: Austenitizing temperature: 900oC, time: 15 min.
Reference: Not shown in this demo version.

Transformation Diagram

Price: 30.00 US $
Buy Online Transformation Diagram

Other Steel Data links
Carbides in Steel
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel
Tempering Diagrams of Steels
CCT and TTT Diagram Calculating Service

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other puposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2019 by Steel Data. All Rights Reserved.