AMS 6414, 6415 Steels

Steel name: AMS 6414, 6415
Diagram No.: 685
AMS designation: 6414, 6415 (Air Melt), AMS-S-5000 (Air Melt)
Chemical composition in weight %: 0.40% C, 0.30% Si, 0.75% Mn, 0.80% Cr, 0.25% Mo, 1.80% Ni
Steel group: High strength alloy steel
Applications: No data
Comment: The alloy has a good combination of ductility, toughness and strength along with high hardenability.
Reference: Not shown in this demo version.

Heat Treatment
Hardening: 802-857oC/oil
Tempering: See the diagram
Note: Diagram:
A: Normalize 899oC/1h, AC Austenitize 816oC/1/2h, OC temper 246oC/2 + 2h, AC
B: Normalize 899oC/1h, AC Austenitize 816oC/1/2h, OC temper 482oC/2 + 2h, AC
C: Normalize 899oC/1h, AC Austenitize 802oC/1/2h, OC temper 593oC/2 + 2h, AC

Diagram Tempering Temperature - Elevated Temperature Hardness Data

Price: 20.00 US $
Buy Online Tempering Diagram

Other steel data links
Carbides in Steel
CCT & TTT diagrams of Steels
Etchants Database
Hardenability Diagrams of Steels
Macro Defects in Steel
Non-Metallic Inclusions in Steel

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2017 by Steel Data. All Rights Reserved.