1.2999 Steel

Steel name: 1.2999
Diagram No.: 97
Chemical composition in weight %: 0.45% C, 0.30% Si, 0.50% Mn, 3.10% Cr, 5.00% Mo, 1.00% V
Steel group: Hot work tool steels
Applications: No data
Comment: No data
Reference: D. Duh and I. Schruff, OPTIMIZEDHEATTREATMENTANDNITRIDING PARAMETERS FOR A NEWHOT-WORK TOOL STEEL, Proceedings of the 6th International Tooling Conference Karlstad, Sweden, 10-13 September 2002.

Heat Treatment

Tempering Diagram

Price: 20.00 US $
Buy Online Tempering Diagram

Other steel data links
Carbides in Steel
CCT and TTT Diagrams of Steels
CCT and TTT Diagram Calculating Service
Hardenability Diagrams of Steels
Hardenability Calculating Service
Macro Defects in Steel
Metal Etchants
Non-Metallic Inclusions in Steel
Semiconductor Etchants

Disclaimer: The information and data presented herein are typical or average values and are not a guarantee of maximum or minimum values. Applications specifically suggested for material described herein are made solely for the purpose of illustration to enable the reader to make his own evaluation and are not intended as warranties, either express or implied, of fitness for these or other purposes. There is no representation that the recipient of this literature will receive updated editions as the become available.

Copyright © 2017 by Steel Data. All Rights Reserved.