Alphabetical Index
Chemical Composition of Steels
Keyword Search
Steel Names
Alloyed Steels
Carbon Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
Creep Resistant Steels
Hot Work Tool Steels
Molybdenum Steels
PM steels
Stainless Steels
Structural Steels
Tool Steels
Vanadium Steels
White Cast Irons
M2C Carbides
M3C Carbides
M7C3 Carbides
M23C6 Carbides
MC Carbides
Light Microscopy
EDS/WDS Microanalysis
Scanning Electron Microscopy
Transmission Electron Microscopy
X-Ray Diffraction
Help
Contact Us
Home
Carbides in steel 1.2747


Table 1: Data for steel 1.2747.
Carbide name: See the table 1.
Record No.: 1279
Carbide formula: See the table 1
Carbide type: See the table 1.
Carbide composition in weight %: No data
Image type: No data
Steel name: 1.2747
Mat.No. (Wr.Nr.) designation: 1.2747
DIN designation: X210Cr12
AISI/SAE/ASTM designation: AISI D3
Other designation: No data
Steel group: Cold work tool steels
Steel composition in weight %: See the table 1.
Heat treatment/condition: No data
Note: XRD analysis. The legend: SA-soft annealing, Q-quenching, T-tempering, RA-retained austenite.
Links: No data
Reference: Not shown in this demo version.