Alphabetical Index
Chemical Composition of Steels
Keyword Search
Steel Names
Alloyed Steels
Carbon Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
Creep Resistant Steels
Hot Work Tool Steels
Molybdenum Steels
PM steels
Stainless Steels
Structural Steels
Tool Steels
Vanadium Steels
White Cast Irons
M2C Carbides
M3C Carbides
M7C3 Carbides
M23C6 Carbides
MC Carbides
Light Microscopy
EDS/WDS Microanalysis
Scanning Electron Microscopy
Transmission Electron Microscopy
X-Ray Diffraction
Help
Contact Us
Home
M23C6 carbides in austenitic stainless steel

Figure 1: M23C6 carbides, Mag. 6,000x.

Figure 2: M23C6 carbides, Mag. 6,000x.
Carbide name: M23C6
Record No.: 350
Carbide formula: M23C6
Carbide type: M23C6
Carbide composition in weight %: No data
Image type: TEM
Steel name: Austenitic stainless steel
Mat.No. (Wr.Nr.) designation: No data
DIN designation: No data
AISI/SAE/ASTM designation: No data
Other designation: No data
Steel group: Stainless steels
Steel composition in weight %: No data
Heat treatment/condition: Solution treated, quenched and tempered at 750 C, 4 hours.
Note: Intergranular impact ruptures at -196 C. Influence of boron on the size and distribution of M23C6 carbides.
Links: No data
Reference: Not shown in this demo version.