Alphabetical Index
Chemical Composition of Steels
Keyword Search
Steel Names
Alloyed Steels
Carbon Steels
Cast Irons
Chromium Steels
Cold Work Tool Steels
Creep Resistant Steels
Hot Work Tool Steels
Molybdenum Steels
PM steels
Stainless Steels
Structural Steels
Tool Steels
Vanadium Steels
White Cast Irons
M2C Carbides
M3C Carbides
M7C3 Carbides
M23C6 Carbides
MC Carbides
Light Microscopy
EDS/WDS Microanalysis
Scanning Electron Microscopy
Transmission Electron Microscopy
X-Ray Diffraction
Help
Contact Us
Home
Carbides in 1.2080 steel

Figure 1: Carbides, scale bar: 500 µm.

Figure 2: Carbides, scale bar: 50 µm.
Carbide name: No data
Record No.: 420
Carbide formula: No data
Carbide type: No data
Carbide composition in weight %: No data
Image type: LM
Steel name: 1.2080
Mat.No. (Wr.Nr.) designation: 1.2080
DIN designation: X210Cr12
AISI/SAE/ASTM designation: D3
Other designation: No data
Steel group: No data
Steel composition in weight %: 2.06% C, 0.19% Si, 0.25% Mn, 0.023% P, 0.001% S, 11.4% Cr, 0.12% Ni, 0.05% V, 0.06% Mo, 0.05% Cu.
Heat treatment/condition: QT, sample diameter: 232 mm, hardness: 63 HRC.
Note: No data
Links: No data
Reference: Not shown in this demo version.