Electrolytes Used for Carbides Extraction

Figure 1: Electrolytes used for particle extraction, along with experimental conditions and steels investigated.
Reference: A.L. Rivas, E. Vidal, D.K. Matlock and J.G. Speer, Electrochemical extraction of microalloy carbides in Nb-steel, REV. METAL. MADRID, 44 (5), SEPTIEMBRE-OCTUBRE, pp. 447-456.