Hardness of Various Carbide Types in HiCr Cast Steel Rolls

Figure 1: Hardness of various carbide types.
Reference: K. H. Schröder, B. Feistritzer, M. Windhager, K. H. Ziehenberger: "Progress of
Carbide Enhanced ICDP (and Remarks on Coefficient of Friction of HSS
Work Rolls in Hot Strip Mills"; 37. Rolling Seminar - Process and Rolled and
Coated Product, ABM, September 2000, Curitiba, Brasil.