Hardness of M7C3 Carbides in Cr White Cast Iron

Table 1: Reported hardness values of M7C3 carbides.
Reference: G. D. Nelson, The Influence Of Microstructure On TheCorrosion And Wear Mechanisms Of High Chromium White Irons In Highly Caustic Solutions, The University of Adelaide, School of Mechanical Engineering, Australia, PhD Thesis, 2010.