Pits on polished face of AISI A2 tool steel mold - Polishing defects

Figure 1: Pits on polished face of AISI A2 tool steel mold.

Figure 2: Holes in region with carbide segregation, 100x.
Defect name: Pitting
Record No.: 1888
Type of defect (Internal/Surface): Internal, surface
Defect classification: Polishing defects
Steel name: AISI A2 tool steel
Steel composition in weight %: No data.
Note: Tool steel failure example.
Reference: Not shown in this demonstration version.