0.038C-0.25Si-1.43Mn-17.50Cr-12.81Ni-4.60Mo-0.55Nb Steel
0.043C-0.24Si-1.57Mn-17.44Cr-12.89Ni-4.55Mo-2.05Nb Steel
0.044C-0.18Si-1.66Mn-16.67Cr-12.67Ni-2.50Mo Steel
0.044C-0.38Si-1.65Mn-16.55Cr-12.86Ni-2.00Mo-0.86Nb Steel
0.05C-0.90Mn-1.20Si-0.40Mo Steel
0.05C-17Cr-13Ni-5Mo-0.039N Steel
0.08% C, 2.9% Cr Steel
0.1% C - 13.0% Cr Steel
0.1% C - 13.0% Cr Steel
0.1% C - 13.0% Cr Steel
0.1% C - 13.0% Cr Steel
0.1% C - 13.0% Cr Steel
0.1% C - 13.0% Cr Steel
0.1% C - 13.0% Cr Steel
0.12C-0.6Cr-0.65Mo Steel
0.15C-2.9Cr Steel
0.15C-4Ni-1.5Cr Steel
0.1C-5.5Cr-0.4Mo Steel
0.26C-3Cr Steel
0.28C-1.0Cr-0.4Mo Steel
0.29C-1.5Cr-0.4Mo Steel
0.2C-3Cr Steel
0.33C-2Cr Steel
0.33C-3.26Ni-0.85Cr Steel
0.35C-4.23Ni-1.43Cr Steel
0.38C-0.6Cr Steel
0.3C-0.5Cr-0.4Mo Steel
0.3C-2.1Cr-0.48Mo Steel
0.3C-2.4Cr-0.34Mo Steel
0.3C-2Cr-0.33Mo Steel
0.4C-1Cr-0.42Mo Steel
0.4C-3Cr Steel
0.5C-0.65Cr-0.18Mo Steel
0.75C-0.5Cr Steel
0.76C-2Cr-0.25Mo Steel
0.7C-3Cr Steel
0.89Cr-4Ni-1.58Cr Steel
1% Cr Steel
1.0% C High-Chromium Steel
1.0% C High-Chromium Steel
1.0% C High-Chromium Steel
1.0% C High-Chromium Steel
1.0% C-0.7% Mn-0.5% Si-6.0% Cr-0.038% Mo Steel
1.19C-0.33Mo Steel
1.2316 Steel
1.35% C-0.7% Mn-0.5% Si-12.0% Cr-0.078% Mo Steel
1.35% C-0.7% Mn-0.5% Si-12.0% Cr-1.00% Mo Steel
1.35% C-0.7% Mn-0.5% Si-12.0% Cr-3.06% Mo Steel
1.3C-2.9Cr Steel
1.95% C, 10.80% Cr, 3.80% Mo Alloyed White Cast Iron
1.95% C, 10.80% Cr, 3.80% Mo Alloyed White Cast Iron
1.96% C, 15.40% Cr, 2.20% Mo Alloyed White Cast Iron
1.96% C, 15.40% Cr, 2.20% Mo Alloyed White Cast Iron
1.98% C, 20.25% Cr, 2.14% Mo Alloyed White Cast Iron
1.98% C, 20.25% Cr, 2.14% Mo Alloyed White Cast Iron
1021 + 1 Ni + 0.5 Cr Steel
1021 + 1 Ni + 1 Cr Steel
1021 + 1 Ni + 2 Cr Steel
10CrMo9-10 Steel
10CrMo9-10 Steel
11.20% Cr Cast Iron
12% Cr Ferritic Stainless Steel
12% Cr Ferritic Stainless Steel
12% Cr Ferritic Stainless Steel
12% Cr Ferritic Stainless Steel
12% Cr Martensitic Steel
12%Cr USC Rotor Steel
12Cr-1MoV Steel
12CrMo19-5 Steel
13CrMo4-4 Steel
13CrMo4-4 Steel
15-2-1 LC White Cast Iron
15Mo3 Steel
17CrMoV10 Steel
18% Cr-15% Ni Stainless Steel
18%Cr-8%Ni Austenitic Stainless Steel
1C-2.9Cr Steel
1C-4Cr Steel
1C-5.7Cr Steel
1C-8.8Cr Steel
2-1/4Cr-1Mo Steel
2.04% C, 20.55% Cr, 0.61% Mo Alloyed White Cast Iron
2.04% C, 20.55% Cr, 0.61% Mo Alloyed White Cast Iron
2.05% C, 15.60% Cr, 0.81% Mo Alloyed White Cast Iron
2.05% C, 15.60% Cr, 0.81% Mo Alloyed White Cast Iron
2.08% C, 15.85% Cr Alloyed White Cast Iron
2.08% C, 15.85% Cr Alloyed White Cast Iron
2.08% C, 20.55% Cr, <0.01% Mo Alloyed White Cast Iron
2.08% C, 20.55% Cr, <0.01% Mo Alloyed White Cast Iron
2.13% C, 11.30% Cr, 1.41% Mo Alloyed White Cast Iron
2.13% C, 11.30% Cr, 1.41% Mo Alloyed White Cast Iron
2.19% C, 11.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.19% C, 11.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.41% C, 12.15% Cr, 2.45% Mo Alloyed White Cast Iron
2.41% C, 12.15% Cr, 2.45% Mo Alloyed White Cast Iron
2.45% C, 19.82% Cr, 2.94% Mo Alloyed White Cast Iron
2.45% C, 19.82% Cr, 2.94% Mo Alloyed White Cast Iron
2.54% C, 20.22% Cr, 1.52% Mo Alloyed White Cast Iron
2.54% C, 20.22% Cr, 1.52% Mo Alloyed White Cast Iron
2.55% C, 12.40% Cr, 1.25% Mo Alloyed White Cast Iron
2.55% C, 12.40% Cr, 1.25% Mo Alloyed White Cast Iron
2.60% C, 15.20% Cr, 1.95% Mo Alloyed White Cast Iron
2.60% C, 15.20% Cr, 1.95% Mo Alloyed White Cast Iron
2.65% C, 12.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.65% C, 12.65% Cr, 0.02% Mo Alloyed White Cast Iron
2.67% C, 14.95% Cr Alloyed White Cast Iron
2.67% C, 14.95% Cr Alloyed White Cast Iron
2.67% C, 15.20% Cr, 1.09% Mo Alloyed White Cast Iron
2.67% C, 20.75% Cr, <0.01% Mo Alloyed White Cast Iron
2.67% C, 20.75% Cr, <0.01% Mo Alloyed White Cast Iron
2.67% C-15.20% Cr-1.09% Mo Alloyed White Cast Iron
2.72% C, 25.15% Cr, 2.52% Mo Alloyed White Cast Iron
2.72% C, 25.15% Cr, 2.52% Mo Alloyed White Cast Iron
2.87% C, 25.50% Cr, 1.22% Mo Alloyed White Cast Iron
2.87% C, 25.50% Cr, 1.22% Mo Alloyed White Cast Iron
2.93C-0.60Si-0.78Mn-17.4Cr-0.04% Mo White Cast Iron
2.95% C, 25.82% Cr, 0.02% Mo Alloyed White Cast Iron
2.95% C, 25.82% Cr, 0.02% Mo Alloyed White Cast Iron
2.96C-0.52Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
2.96C-0.93Si-0.79Mn-17.5Cr-0.98Cu-1.55Mo White Cast Iron
20-2-1 LC White Cast Iron
22.59% Cr Cast Iron
3.25% C, 11.80% Cr, 2.60% Mo Alloyed White Cast Iron
3.25% C, 11.80% Cr, 2.60% Mo Alloyed White Cast Iron
3.39% C, 11.95% Cr, 1.36% Mo Alloyed White Cast Iron
3.39% C, 11.95% Cr, 1.36% Mo Alloyed White Cast Iron
3.40% C, 19.85% Cr, 3.40% Mo Alloyed White Cast Iron
3.40% C, 19.85% Cr, 3.40% Mo Alloyed White Cast Iron
3.5% Chromium Magnet Steel
3.51% C, 12.20% Cr, 0.02% Mo Alloyed White Cast Iron
3.51% C, 12.20% Cr, 0.02% Mo Alloyed White Cast Iron
3.51% C, 20.10% Cr, 1.37% Mo Alloyed White Cast Iron
3.51% C, 20.10% Cr, 1.37% Mo Alloyed White Cast Iron
3.52% C, 24.65% Cr, 2.67% Mo Alloyed White Cast Iron
3.52% C, 24.65% Cr, 2.67% Mo Alloyed White Cast Iron
3.56% C, 14.60% Cr, 0.47% Mo Alloyed White Cast Iron
3.56% C, 14.60% Cr, 0.47% Mo Alloyed White Cast Iron
3.58% C, 14.45% Cr Alloyed White Cast Iron
3.58% C, 14.45% Cr Alloyed White Cast Iron
3.58% C, 14.65% Cr, 0.52% Mo Alloyed White Cast Iron
3.58% C, 14.65% Cr, 0.52% Mo Alloyed White Cast Iron
3.62% C, 20.35% Cr, <0.01% Mo Alloyed White Cast Iron
3.62% C, 20.35% Cr, <0.01% Mo Alloyed White Cast Iron
3.66% C, 24.95% Cr, 1.53% Mo Alloyed White Cast Iron
3.66% C, 24.95% Cr, 1.53% Mo Alloyed White Cast Iron
3.70% C, 25.32% Cr, 0.02% Mo Alloyed White Cast Iron
3.70% C, 25.32% Cr, 0.02% Mo Alloyed White Cast Iron
3.81% C, 14.75% Cr, 2.50% Mo Alloyed White Cast Iron
3.81% C, 14.75% Cr, 2.50% Mo Alloyed White Cast Iron
3.94% C, 23.45% Cr, 2.94% Mo Alloyed White Cast Iron
3.94% C, 23.45% Cr, 2.94% Mo Alloyed White Cast Iron
3.96% C, 14.80% Cr, 1.45% Mo Alloyed White Cast Iron
3.96% C, 14.80% Cr, 1.45% Mo Alloyed White Cast Iron
3.96% C, 17.55% Cr, 2.53% Mo Alloyed White Cast Iron
3.96% C, 17.55% Cr, 2.53% Mo Alloyed White Cast Iron
304 Stainless Steel
310 Stainless Steel
3135 Steel
3140 Steel
316, 317 LMN, 254 SMO, 904L Steels
3310 Carburized to 0.4C Steel
3310 Carburized to 0.6C Steel
3310 Carburized to 0.8C Steel
3310 Carburized to 1.0C Steel
3310 Steel
3330 Steel
3330 Steel
3335 Steel
4.08% C, 18.00% Cr, 1.14% Mo Alloyed White Cast Iron
4.08% C, 18.00% Cr, 1.14% Mo Alloyed White Cast Iron
4.10% C, 15.10% Cr Alloyed White Cast Iron
4.10% C, 15.10% Cr Alloyed White Cast Iron
4.10% C, 23.67% Cr, 1.32% Mo Alloyed White Cast Iron
4.10% C, 23.67% Cr, 1.32% Mo Alloyed White Cast Iron
4.13% C, 18.22% Cr, 0.05% Mo Alloyed White Cast Iron
4.13% C, 18.22% Cr, 0.05% Mo Alloyed White Cast Iron
4.31% C, 24.80% Cr, 0.02% Mo Alloyed White Cast Iron
4.31% C, 24.80% Cr, 0.02% Mo Alloyed White Cast Iron
403/410 Stainless Steel
403/410 Stainless Steel
403/410 Stainless Steel
4130 Steel
4140 Steel
4140 Steel
4142 Steel
41x40 Steel
41x40 Steel
430 Stainless Steel
4340 Steel
442 Stainless Steel
446 Stainless Steel
5140 Steel
5150 Steel
5160 Steel
52100 Steel
52100 Steel
5Cr-0.5Mo Steel
6.27% Cr Cast Iron
8620 Steel
8630 Steel
8630 Steel
8660 Steel
8745 Steel
8Cr-2Mo Steel
9420 Steel
9440 Steel
9860 Steel
A 3120 Steel
AISI 1040, 5140, 45CrMoV67 Steels
AISI 304 Steel
AISI 316 Steel
AISI 316L Steel
AISI D2 (D2, D2F) Steel
AREA Steel
Astaloy CrM Steel
Austenitic Cr-Ni-Mo Steel X5CrNiMo17-13
Austenitic Steel
Austenitic Steel
Austenitic Steel
Austenitic Steel
Austenitic Steel
C110 Steel
CALMAX Steel
Carpenter No. 158 Steel
Carpenter No. 610 Steel
Ce Steel
ELMAX SUPERCLEAN 3 Steel
ES 4122 Steel
ES 50 S Steel
ES 50 SW Steel
ES 70 S Steel
EUROFER 97 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 18 Steel
En 19 Steel
En 19 Steel
En 20 Steel
En 20 Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Eutectoid Steel
Fe-10Cr Steel
Fe-10Cr Steel
Fe-30Cr (Alloy 90) Steel
Fe-C-Cr Steel
Fe-C-Cr Steel
Ferritic Stainless Steel
Four CCT Diagrams of Steels
High Chromium Cast Iron
High Nitrogen Stainless (HSN) Steels
Low Carbon 2.4-4.15% Steel
Ni-Cr Steel
Ni-Cr-Mo Steel
Nicrofer5621 hMoW - alloy 22
ROLTEC SF Steel
ROLTEC SF Steel
Rail Steel
SAE 3240 Steel
SAE 3312 Steel
SAE 3360 mod. Steel
SAE 3360 mod. Steel
SAE 4047 Steel
SAE 4130 Steel
SAE 4130 Steel
SAE 4147 Steel
SAE 5140 Steel
SLEIPNER Steel
SLEIPNER Steel
Sandvik 253 MA Steel
Sanicro 69 Steel
Steel with 0.16% Cr
Steel with 0.30% Cr
Steel with 0.48% Cr
Steel with about 8% Cr and 2% Mo
Thermit Steel
U.I.C 860 grade A and THS 11 Steels
UNIMAX Steel
VIDAR SUPERIOR Steel
VIDAR SUPREME Steel
X11CrMoWVNb9-1 Steel
X12CrMo7 Steel
X12CrMo9-1 Steel
X12CrMo9-1 Steel
X20CrMoV12-1 Steel
X210CrW12 Steel
X5CrNi18-9 Steel
X5CrNiMo17-13 Steel
Xl2CrMo7 Steel