Chemical Composition of Steels in Weight %

0.00% C, 0.00% Mn, 0.00% Si, 0.00% P, 0.00% S, 0.00% Ni, 0.00% Cr, 0.00% Mo, 0.00% Cu
0.00% C, 0.00% Si, 0.00% Mn, 0.00% P, 0.00% S, 0.00% Cr, 0.00% Cu, 0.00% Mo, 0.00% Ni, 0.00% V
0.00% C, 0.00% Si, 0.00% Mn, 0.00% S, 0.00% P, 0.00% Ni, 0.00% Cr, 0.00% Mo, 0.00% Cu
0.00% C, max. 0.00% Si, 0.00% Mn, max. 0.00% P, max. 0.00% S, max. 0.00% Cr, max. 0.00% Mo, max. 0.00% Ni, max. 0.00% V, max. 0.00% Ti, max. 0.00% Cu, min. 0.00% Al, max. 0.00% Nb
0.001% C, 0.017% Si, 0.130% Mn, 0.005% P, 0.008% S, 0.004% N, 0.032% Al, 0.064% Ti, 0.002% Nb. Steel IF-TiNb: 0.002% C, 0.007% Si, 0.097% Mn, 0.010% P, 0.004% S, 0.003% N, 0.042% Al, 0.035% Ti, 0.028% Nb
0.002% C, 13.20% Cr, 0.011% N, 0.42% Ti
0.0021% C, 0.014% Si, 0.23% Mn, 0.0052% S, 0.010% P, 0.038% Al, 0.25% Nb, 0.0022% N
0.0021% C, 0.022% Si, 0.23% Mn, 0.0053% S, 0.010% P, 0.038% Al, 0.75% Nb, 0.0024% N
0.0023% C, 0.01% Mn, 0.106% Si, 0.018% P, 0.015% S, 0.072% Ni, 25.50% Cr, 0.01% Mo, 0.0083% N
0.0026% C, 0.14% Mn, 0.007% Si, 0.052% Al, 0.042% Ti, 0.012% Nb, 0.008% S, 0.031% P, 0.0021% N. MA steel: 0.15% C, 1.44% Mn, 0.344% Si, 0.01% Al, 0.028% Ti, 0.044% Nb, 0.003% S, 0.016% P, 0.01% N.
0.003% C, 0.47% Mn, 0.13% Si, 20.02% Mo, 15.00% Co
0.003% C, 4.78% Mn, 0.21% Si, 10.04% Mo, 15.33% Co
0.003-0.007% C, 9.60% Cr
0.003-0.007% C, 9.60% Cr
0.004% C, 0.164% O, 2.94% Cr, 0.29% Mo, 0.28% V
0.004% C, 0.04% Mn, 0.02% Si, 0.007% P, 0.012% S, 2.17% Ni, 29.50% Cr, 4.00% Mo, 0.0146% N, 0.06% Al, 0.0011% O
0.004% C, 0.10% Mn, 0.10% Si, 0.01% P, 0.015% S, 0.10% Ni, 29.00% Cr, 4.00% Mo, 0.012% N
0.004% C, 0.148% O, 0.97% Cr, 0.34% Mo, 0.25% V
0.004% C, 0.41% Mn, 0.15% Si, 9.99% Mo, 15.30% Co, 9.95% Ni
0.004% C, 0.42% Mn, 0.12% Si, 9.95% Mo, 15.20% Co
0.004% C, 0.43% Mn, 0.13% Si, 9.95% Ni, 20.02% Mo, 15.13% Co
0.004% C, 0.62% Si, 0.71% Mn, 0.052% P, 0.0104% S, 0.044% Al, 0.003% N, 0.078% Ti, 0.0027% B
0.005% C, 0.030% S, 9.50% Ni, 18.50% Cr, 0.01% N, Sulfur dopped
0.006% C, 12.66% Cr, 0.018% N, 0.40% Ti
0.006% C, 4.93% Mn, 0.23% Si, 20.17% Mo, 15.33% Co
0.007% C, 0.003% Si, 0.11% Mn, 0.010% S, 0.010% P, 0.043% Al, 12 ppm O, 50 ppm N
0.008% C, 0.55% Si, 22.00% Cr, 5.60% Ni, 2.93% Mo, 0.15% Ni. 3W Steel: 0.008% C, 0.42% Si, 21.70% Cr, 5.50% Ni, 3.08% W, 0.15% Ni
0.009% C, 1.00% Mn, 0.05% Si, 0.010% S, 0.020% P, 14.50-17.50% Cr, 10.00-17.00% Mo, 0.70% Ti, 2.00% Co, Ni is balance
0.009% C, 12.77% Cr, 0.002% N, 0.15% Ti
0.009% C, 12.77% Cr, 0.002% N, 0.15% Ti
0.01% C, 0.20% Mn, 0.007% P, 0.011% S, 0.01% Si, 0.01% Ni, 0.02% Cr, 0.001% V, 0.001% Ti, <0.0005% B, 0.004% N. Steel B: 0.059% C, 0.22% Mn, 0.008% P, 0.004% S, 0.01% Si, 0.03% Ni, 0.02% Cr, 0.001% V, 0.001% Ti, 0.002-0.004% B, 0.004% N
0.01% C, 3.00% Cr, 0.50% Mo, 0.20% O, balance is Fe
0.010 % C, 0.011 % N, 0.11 % Ti
0.010% C, 0.08% Mn, 0.08% Si, 24.90% Ni, 0.26% Al, 1.58% Ti, 0.15% Cb(Nb)
0.010% C, 0.50% Mn, 0.08% Si, 0.015% S, 0.025% P, 2.00-6.00% Fe, 20.00-22.50% Cr, 12.50-14.50% Mo, 2.50-3.50% W, 2.50% Co, 0.35% V, Ni is balance
0.010% C, 0.50% Mn, 0.10% Si, 0.005% S, 0.015% P, 22.00-24.00% Cr, 15.00-16.50% Mo, 1.50% Fe, 0.30% Co, 0.10-0.40% Al, Ni is balance
0.010% C, 1.00% Mn, 0.08% Si, 0.010% S, 0.025% P, 14.50-16.50% Cr, 15.00-17.00% Mo, 3.00-4.50% W, 4.00-7.00% Fe, 2.5% Co, 0.35% V, Ni is balance
0.010% C, 0.03% Si, 1.74% Mn, 0.007% P, 0.011% S
0.010% C, 0.03% Si, 1.74% Mn, 0.007% P, 0.011% S
0.012% C, <0.03% Mn, <0.05% Si, 17.60% Ni, 3.10% Mo, 0.10% Al, 8.30% Co, 0.08% Ti
0.012% C, 0.03% Si, 0.33% Mn, 0.007% P, 0.011% S
0.013% C, 0.29% Mn, 0.27% Si, 0.012% P, 0.009% S, 4.66% Ni, 24.41% Cr, 3.50% Mo, 0.012% Al, 0.32% Nb
0.013% C, 0.45% Mn, 0.27% Si, 0.020% P, 0.011% S, 17.40% Cr, 2.02% Mo, 0.0148% N, 0.24% Ti
0.013% C, 0.49% Mn, 0.27% Si, 0.019% P, 0.013% S, 17.40% Cr, 2.00% Mo, 0.0095% N, 0.35% Nb
0.013% C, 8.46% Ni, 17.30% Cr, 0.037% N, LCN2: 0.015% C, 8.77% Ni, 17.96% Cr, 0.097% N
0.013% C, 24% Cr, 21% Ni, 7% Mo, 0.5%N. S31254 steel: 0.012% C, 20% Cr, 18% Ni, 6% Mo, 0.2% N.
0.013% C, 0.03% Si, 0.87% Mn, 0.007% P, 0.011% S
0.013% C, 0.62% Si, 0.05% Mn, 0.005% P, 0.024% S
0.013% C, 0.95% Si, 0.05% Mn, 0.005% P, 0.024% S
0.014% C, 0.29% Mn, 0.27% Si, 0.019% P, 0.011% S, 3.90% Ni, 24.54% Cr, 3.54% Mo, 0.32% Al, 0.17% Nb
0.014% C, 0.02% Si, 0.50% Mn, 0.007% P, 0.011% S
0.015% C, 0.30-0.50% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 4.50-5.50% Cr, 0.45-0.65% Mo
0.015% C, 1.00% Mn, 1.00% Si, 21.50-23.50% Cr, 18.00-21.00% Fe, 6.00-8.00% Mo, 1.50-2.50% Cu, 5.00% Co, 0.20-0.50% Nb, 1.50% W, Ni is balance
0.015% C, 1.99% Mn, 0.31% Si, 0.006% P, 0.004% S, 1.00% Ni, <0.01% Cr, 0.29% Mo, 0.017% Al, 0.002% B
0.015% C, 2.00% Mn, 0.30% Si, 0.010% S, 0.020% P, 30.00-32.00% Ni, 26.00-28.00% Cr, 6.00-7.00% Mo, 1.00-1.40% Cu, 0.15-0.25% N, Fe is balance
0.015% C, 2.00% Mn, 0.50% Si, 0.010% S, 0.020% P, 30.00-33.0% Ni, 31.00-35.00% Cr, 0.50-2.00% Mo, 0.30-1.20% Cu, 0.35-0.60% N, Fe is balance
0.016% C, 0.32% Si, 1.58% Mn, 0.003% S, 0.014% P, 0.029% Al, others: Cu, Ni, Nb, B, Ti, Ceq=0.30, Pcm=0.144
0.016% C, 0.72% Mn, 0.80% Si, 11.09% Ni, 19.28% Cr, <0.01% Mo, ferrite content=0.7%
0.016% C, 3.62% Mn, 0.04% Si, 23.20% Ni, 0.001% N, 0.0015% O
0.016% C, 1.58% Mn
0.018% C, 2.00% Mn, 0.010% P, 0.005% S, 0.042% Al, 0.15% Mo
0.018% C, max. 0.50% Si, 0.90-1.65% Mn, max. 0.03% P, max. 0.025% S, max. 0.30% Cr, max. 0.10% Mo, max. 0.50% Ni, max. 0.35% Cu, max. 0.05% Nb, max. 0.12% V, max. 0.02% Al, max. 0.03% Ti, max. 0.015% N
0.019% C, 0.37% Si, 0.087% Mn, 24.80% Cr, 3.82% Mo, 6.77% Ni, 0.20% Cu, 0.281% N
0.019% C, 1.21% Mn, 0.49% Si, 33.50% Ni, 20.60% Cr, 0.01% Cu, 0.51% Al, 0.46% Ti, 0.027% N
0.019% C, 1.21% Mn, 0.49% Si, 33.50% Ni, 20.60% Cr, 0.01% Cu, 0.51% Al, 0.46% Ti, 0.027% N
0.019% C, 1.21% Mn, 0.49% Si, 33.50% Ni, 20.60% Cr, 0.01% Cu, 0.51% Al, 0.46% Ti, 0.027% N
0.019% C, 1.21% Mn, 0.49% Si, 33.50% Ni, 20.60% Cr, 0.01% Cu, 0.51% Al, 0.46% Ti, 0.027% N
0.019% C, 1.21% Mn, 0.49% Si, 33.50% Ni, 20.60% Cr, 0.01% Cu, 0.51% Al, 0.46% Ti, 0.027% N
0.02% C, 0.003% Al, 0.0034% N
0.02% C, 0.07% Mn, 0.07% Si, 18.40% Ni, 4.90% Mo, 0.09% Al, 8.80% Co, 0.66% Ti, 0.003% B
0.02% C, 0.09% Mn, 0.09% Si, 17.80% Ni, 0.0021% B, 0.12% Al, 7.90% Cr, 0.42% Ti
0.02% C, 0.20% Si, 0.03% Mn, max. 0.008% P, 0.014% S, 4.80% Mo, 17.60% Ni, 10.08% Co, 0.390% Ti, 0.090% Al
0.02% C, 0.37% Mn, 0.0186% N
0.02% C, 0.45% Si, 1.11% Mn, 11.06% Cr, 0.41% Ni, 0.030% V, 0.05% Cu, 0.009% Al, 0.014% N
0.02% C, 0.85% Mn, 0.14% Si, 20.6% Cr, 14.5% Ni, 6.5% Mo, 0.02% S, 0.001% S, 0.8% Cu, 0.19% N
0.02% C, 0.94% Mn, 0.48% Si, 0.02% P, 0.009% S, 6.64% Ni, 25.30% Cr, 2.96% Mo, 0.49% Cu, 0.11% N, 0.32% W
0.02% C, 1.00% Mn, 0.50% Si, 0.010% S, 0.030% P, 24.00-26.00% Ni, 20.00-21.00% Cr, 6.00-7.00% Mo, 0.50-1.50% Cu, 0.15-0.25% N, Fe is balance
0.02% C, 1.00% Ni, 0.015% Al, 0.0010% N
0.02% C, 1.50% Mn, 0.40% Si, 0.02% P, 0.02% S, 24.50% Ni, 20.50% Cr, 6.30% Mo
0.02% C, 1.60% Mn, 0.16% Si, 0.043% Nb, 0.017% Ti, 0.0018% B, 0.0020% N
0.02% C, max. 0.5% Si, max. 0.020% P, max. 0.015% S, 30.0% Cr, 60.0% Ni
0.020% C, 1.40% Mn, 0.41% Si, 0.032% P, 0.013% S, 10.30% Ni, 18.10% Cr, 0.32% Mo, 0.24% Cu, 0.039% N
0.020% C, 22.50% Cr, 5.80% Ni, 3.10% Mo, 0.17% N, <0.002% S
0.02% C, 0.35% Si, 18.3% Cr, 3.8% Ni, 2.3% Mo, 0.05% Cu
0.02% C, 0.02% Si, 0.13% Mn, 0.013% P, 0.019% S
0.021% C, 1.74% Mn, 0.41% Si, 0.030% P, 0.007% S, 12.30% Ni, 17.20% Cr, 2.40% Mo, 0.080% N, 0.0032% B, 0.21% Co, 0.15% Cu
0.022% C, 0.01% Si, 0.004% P, 0.006% S, 9.20% Ni, 18.50% Cr, 0.01% N, High purity
0.022% C, 0.01% Si, 0.060% P, 0.006% S, 9.20% Ni, 18.20% Cr, 0.01% N, Phosphorus dopped
0.022% C, 0.015% S, 0.020% P, 0.35% Si, 1.74% Mn, 13.4% Ni, 17.3% Cr, 2.13% Mo, 0.005% Ti, 0.005% Nb, 0.04% Cu, 0.035% N, 14 ppm B
0.022% C, 1.04% Mn, 0.34% Si, 0.021% P, 0.018% S, 9.39% Ni, 19.31% Cr, 0.053% N
0.023% C, 0.33% Mn, 0.16% Si, 0.019% P, 0.012% S, 0.33% Ni, 17.15% Cr, 2.23% Mo, 0.04% Cu, 0.05% Co, 0.61% Ti
0.023% C, 0.33% Mn, 0.16% Si, 0.019% P, 0.012% S, 0.33% Ni, 17.15% Cr, 2.23% Mo, 0.04% Cu, 0.05% Co, 0.61% Ti
0.023% C, 0.70% Mn, 0.74% Si, 10.62% Ni, 19.09% Cr, <0.01% Mo, ferrite content=1.1%
0.023% C, 1.40% Mn, 0.32% Si, 0.018% P, 0.013% S, 12.62% Ni, 18.42% Cr, 3.00% Mo, 0.020% N
0.023% C, 1.74% Mn, 0.73% Si, 13.10% Ni, 17.30% Cr, 2.66% Mo
0.023% C, 1.74% Mn, 0.73% Si, 13.10% Ni, 17.30% Cr, 2.66% Mo
0.023% C, 1.74% Mn, 0.73% Si, 13.10% Ni, 17.30% Cr, 2.66% Mo
0.023% C, 0.48% Si, 1.07% Mn, 0.005% S, 8.47% Ni, 18.20% Cr
0.024% C, 0.22% Si, 1.47% Mn, 0.003% S, 0.002% P, 3.35% Ni, 0.23% Cr, 0.061% Mo, 0.006% Ti, 0.011% Al, 0.010% N, 0.006% O
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.002% P, 0.039% Nb, 0.019% V, 0.32% Mo, 0.0043% O, 0.0062% N
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.002% P, 0.039% Nb, 0.019% V, 0.32% Mo, 0.0043% O, 0.0062% N
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.002% P, 0.04% Nb, 0.02% V, 0.32% Mo, 0.0043% O, 0.0062% N
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.002% P, 0.04% Nb, 0.02% V, 0.32% Mo, 0.0043% O, 0.0062% N
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.0020% P, 0.32% Mo, 0.039% Nb, 0.019% V, 0.0062% N, 0.0043% O
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.0020% P, 0.32% Mo, 0.039% Nb, 0.019% V, 0.0062% N, 0.0043% O
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.0020% P, 0.32% Mo, 0.039% Nb, 0.019% V, 0.0062% N, 0.0043% O
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.0020% P, 0.32% Mo, 0.039% Nb, 0.019% V, 0.0062% N, 0.0043% O
0.025% C, 0.24% Si, 1.56% Mn, 0.0006% S, 0.0020% P, 0.32% Mo, 0.039% Nb, 0.019% V, 0.0062% N, 0.0043% O
0.025% C, 0.26% Mn, 0.10% Si, 0.012% P, 0.015% S, 7.38% Ni, 24.49% Cr, 4.99% Mo, 0.36% N. 6Mo composition: 0.018% C, 0.28% Mn, 0.14% Si, 0.011% P, 0.012% S, 9.18% Ni, 23.82% Cr, 5.98% Mo, 0.20% N
0.025% C, 0.31% Si, 1.61% Mn, 22.4% Cr, 5.6% Ni, 0.14% N
0.025% C, 0.31% Si, 1.61% Mn, 22.4% Cr, 5.6% Ni, 0.14% N
0.025% C, 0.69% Mn, 0.72% Si, 12.48% Ni, 18.44% Cr, 2.75% Mo, ferrite content=0.3%
0.025% C, 1.00% Mn, 0.50% Si, 0.010% S, 0.020% P, 38.00-46.00% Ni, 19.50-23.50% Cr, 2.50-3.50% Mo, 1.15-3.0% Cu, 0.60-1.20% Ti, 0.20% Al, Fe is balance
0.025% C, 14.90% Ni, 34.75% Co, 3.55% Cu, 7.00% Al, 0.00% Ti. b.) 0.017% C, 14.92% Ni, 34.25% Co, 3.20% Cu, 7.00% Al, 2.10% Ti. c.) 0.005% C, 14.92% Ni, 34.50% Co, 2.88% Cu, 7.07% Al, 3.85% Ti. d.) 0.014% C, 14.76% Ni, 34.50% Co, 3.05% Cu, 7.10% Al, 6.25% Ti
0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
0.025% C, 18.00% Cr, 2.70% Mo, 1.00% W, 9.00% Co, 10.00% Fe, 5.40% Nb, 1.45% Al, 0.007% P, 0.004% B, balance is Ni
0.025% C, 18.1% Cr, 2.90% Mo, 18.0% Fe, 5.40% Nb, 1.00% Ti, 0.45% Al, 0.007% P, 0.004% B. Alloy 718 Plues: 0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
0.025% C, 18.1% Cr, 2.90% Mo, 18.0% Fe, 5.40% Nb, 1.00% Ti, 0.45% Al, 0.007% P, 0.004% B. Alloy 718 Plues: 0.025% C, 18.0% Cr, 2.70% Mo, 1.0% W, 9.0% Co, 10.0% Fe, 5.40% Nb, 0.70% Ti, 1.45% Al, 0.007% P, 0.004% B
0.025% C, 9.00% Ni, 18.00% Cr
0.025-0.01% C, 0.10-0.46% Si, 0.15-0.30% Mn, 0.001-0.009% S, 0.010-0.030% P, 0.009-0.010% Al, 8.80-9.96% Cr, 0.30-0.50% Cu, 0.20-0.30% Ni, 0.0095-0.0126% C+N
0.026% C, 0.66% Si, 2.90% Mn, 0.006% S, 0.014% P, 5.40% Ni, 22.10% Cr, 2.90% Mo, 0.15% Cu, 0.17% N
0.026% C, 0.66% Si, 2.90% Mn, 0.006% S, 0.014% P, 5.40% Ni, 22.10% Cr, 2.90% Mo, 0.15% Cu, 0.17% N
0.026% C, 14.97% Ni, 18.02% Cr, 0.027% N
0.027% C, 0.722% Si, 0.70% Mn, 0.006% S, 0.014% P, 5.30% Ni, 21.905% Cr, 0.041% Co, 0.136% Cu, 0.169% N
0.028% C, 0.75% Si, 0.80% Mn, 0.011% S, 0.03% P, 7.38% Ni, 24.68% Cr, 3.54% Mo, 0.918% Cu, 0.29% N, 0.752% W
0.028% C, 0.75% Si, 0.80% Mn, 0.011% S, 0.03% P, 7.38% Ni, 24.68% Cr, 3.54% Mo, 0.918% Cu, 0.29% N, 0.752% W
0.028% C, 1.63% Mn, 0.45% Si, 0.031% P, 0.012% S, 5.00% Ni, 21.80% Cr, 3.12% Mo, 0.113% N, 0.05% Cu
0.028% C, 1.64% Mn, 0.34% Si, 0.03% P, 9.78% Ni, 16.29% Cr, 2.53% Mo, 0.078% N
0.028% C, 17.42% Cr, 2.72% Mo, 9.66% Fe, 5.48% Nb, 1.46% Al, 0.71% Ti, 1.04 W, 9.13% Co, Ni is balance
0.028% C, 17.42% Cr, 2.72% Mo, 9.66% Fe, 5.48% Nb, 1.46% Al, 0.71% Ti, 1.04 W, 9.13% Co, Ni is balance
0.028% C, 21.65% Ni, 25.29% Cr, 0.041% N
0.03% C, 0.10% Si, 1.60% Mn, 0.003% S, 0.007% P, 0.30% Ni, 0.60% Cr, 0.015% Nb, 0.015% Ti, 0.001% l, 0.004% O, 0.0023% N, 0.0009% B
0.03% C, 0.23% Si, 1.62% Mn, 0.014% P, 0.002% S, 0.05% Nb, Others V,Ti,Cu,Ni,Mo, 0.15% Pcm, Pcm=C+Si/30+(Mn+Cu+Cr)/20+Ni/60+Mo/15+V/10+5B
0.03% C, 0.40% Mn, 0.014% P, 0.018% S, 0.07% Cr, 9.00% Ni
0.03% C, 0.70% Mn, 0.60% Si, 5.00% Ni, 26.00% Cr, 1.30% Mo
0.03% C, 1.00% Mn, 0.50% Si, 0.03% S, 0.03% P, 42.00-46.00% Ni, 19.50-22.50% Cr, 22.0% Fe, 2.50-3.50% Mo, 1.50-3.0% Cu, 1.90-2.40% Ti, 0.10-0.50% Al, 0.50% Nb
0.03% C, 1.75% Mn, 0.09-0.10% Nb
0.03% C, 18.0-20.0% Cr, 8.0-12.0% Ni, 0.10% N
0.03% C, 23% Cr, 13% Ni, 2.5% Mo
0.03% C, 25.00% Cr, 6.50% Ni, 3.50% Mo, 0.25% Ni, >1.50% Cu
0.03% C, 4.23% Cr
0.03% C, 58-71% Ni, 21-23% Cr, 5% Fe, 0.5% Mn, 0.4% Si, 1% Co, 0.4% Al, 0.4% Ti, 0.01% P, 0.01% S, 8-10% Mo, 3.2-3.8% Nb+Ta
0.03% C, max. 1.0% Si, max. 2.0% Mn, max. 0.030% P, max. 0.015% S, 22% Cr, 5.5% Ni, 3.2% Mo, 0.18% N
0.03% C, max. 1.00% Si, max. 1.00% Mn, 0.01% S, 0.03% P, 6.00-8.00% Ni, 24.00-26.00% Cr, 3.00-4.00% Mo, 0.50-1.00% Cu, 0.20-0.30% N
0.03% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, max. 0.015% S, 10.50-12.50% Cr, 0.30-1.00% Ni
0.03% C, max. 1.00% Si, mqx. 2.00% Mn, max. 0.030% P, max. 0.015% S, 22% Cr, 2.5% Ni, 3.2% Mo, 0.18% N
0.03% C, 16.018.0% Cr, 10.014.0% Ni, 2.003.00% Mo, 0.10% N
0.030% C, 0.08% Mn, 3.30% Si, 0.006% P, 0.012% S
0.030% C, 1.29% Mn, 0.78% Si, 0.022% P, 0.014% S, 5.14% Ni, 24.75% Cr, 1.80% Mo, 0.071% N. Steel 2: 0.020% C, 1.19% Mn, 0.31% Si, 0.027% P, 0.009% S, 5.52% Ni, 21.90% Cr, 2.97% Mo, 0.151% N
0.030% C, 1.60% Mn, 0.38% Si, 0.03% P, 7.88% Ni, 18.58% Cr, 0.108% N, 304LN: 0.038% C, 1.59% Mn, 0.49% Si, 0.03% P, 9.52% Ni, 20.22% Cr, 0.083% N
0.030% C, 14.37% Ni, 17.78% Cr, 2.04% Mo, 0.024% N
0.030% C, 25.00% Cr, 6.50% Ni, 3.60% Mo, 0.26% N
0.030% C, max. 1.00% Si, max. 2.00% Mn, max. 0.030% P, max. 0.020% S, 22.0-23.0% Cr, 4.50-6.50% Ni, 3.00-3.50% Mo
0.03% C, 16.018.0% Cr, 10.014.0% Ni, 2.003.00% Mo, 0.10% N
0.03% C, max. 1.00% Si, max. 2.00% Mn, max. 0.035% P, max. 0.015% S, 21.00-23.00% Cr, 4.50-6.50% Ni, 2.50-3.50% Mo, 0.10-0.22% N
0.03% C, 22.51% Cr, 5.6% Ni, 3.03% Mo, 0.60% Si, l.64% Mn, 0.134% N
0.03% C, 0.57% Mn, 0.15% Si, 0.003% P, 0.001% S, 9.13% Ni, 0.02% Cr, 0.06% Mo, 0.027% Al, 0.01% Nb, 0.01% V, 0.01% Ti
0.03% C, 11.50-13.50% Cr, 4.50-6.50% Ni, 1.50-3.50% Mo, max. 0.50% Mn, max. 0.50% Si, max. 0.02% P, max. 0.005% S, 0.01-0.50% Ti, max. 0.05% V
0.03% C, 0.01% Si, 0.13% Mn, 0.003% P, 0.019% S
0.032% C, 0.25% Si, 2.02% Mn, 0.008% S, 0.011% P, 7.23% Ni, 0.47% Cr, 0.63% Mo, 0.03% Cu, 380 ppm O, 250 ppm N
0.032% C, 0.25% Si, 2.02% Mn, 0.008% S, 0.011% P, 7.23% Ni, 0.63% Mo, 0.003% Cu, 380 ppm O, 250 ppm N
0.032% C, 0.25% Si, 2.02% Mn, 0.011% P, 0.008% S, 0.47% Cr, 7.23% Ni, 0.63% Mo, 0.03% Cu, 380 ppm O, 250 ppm N
0.032% C, 0.62% Mn, 0.45% Si, 0.022% P, 0.021% S, 7.38% Ni, 21.08% Cr, 2.39% Mo, 1.33% Cu, 0.003% B, 0.071% N, <0.01% Ti (33% ferrite)
0.032% C, 0.62% Mn, 0.45% Si, 0.022% P, 0.021% S, 7.38% Ni, 21.08% Cr, 2.39% Mo, 1.33% Cu, 0.071% N, 0.003% B, <0.01% Ti (33% ferrite)
0.033% C, 0.29% Si, 1.93% Mn, 0.011% S, 0.007% P, 0.39% Ni, 0.35% Mo, 1.12% Cu, 0.006% Al, 0.062% Nb, 0.029% Ti, 0.0016% B, 0.0030% N
0.033% C, 0.42% Si, 1.98% Mn, 0.008% P, 0.003% S, 0.76% Cu, 0.77% Ni, 0.029% Al
0.033% C, 0.57% Mn, 0.22% Si, 0.006% P, 0.007% S, 8.63% Ni, 0.13% Cr, 0.02% Mo, 0.032% Al, 0.0083% N2
0.033% C, 1.55% Mn, 0.44% Si, 0.022% P, 0.022% S, 13.60% Ni, 16.40% Cr, 2.12% Mo, 0.025% N, 0.0012% B, 0.18% Co, 0.07% Cu
0.034% C, 1.51% Mn, 0.64% Si, 0.04% P, 8.83% Ni, 18.02% Cr, 0.002% N, 304LN: 0.029% C, 1.54% Mn, 0.52% Si, 0.03% P, 11.88% Ni, 18.13% Cr, 0.13% N
0.035% C, 18.42% Cr, 2.96% Mo, 19.35% Fe, 5.05% Nb, 0.55% Al, 0.95% Ti, Ni is balance
0.035% C, 18.42% Cr, 2.96% Mo, 19.35% Fe, 5.05% Nb, 0.55% Al, 0.95% Ti, Ni is balance
0.036% C, 0.23% Mn, 0.38% Si, 0.020% P, 0.004% S, 33.70% Ni, 19.76% Cr, 2.25% Mo, 3.14% Cu, 0.79% Nb
0.036% C, 0.23% Mn, 0.38% Si, 0.020% P, 0.004% S, 33.70% Ni, 19.76% Cr, 2.25% Mo, 3.14% Cu, 0.79% Nb
0.036% C, 1.33% Mn, 0.049% Nb, 0.0029% B
0.037% C, 0.61% Si, 0.68% Nb
0.037% C, 2.90% Mn, 0.73% Si, 0.009% P, 0.016% S, 0.02% Ni, 0.04% Cr, <0.005% Mo, 0.03% Cu, 0.033% Al, <0.005% Nb, <0.005% Ti
0.038% C, 0.25% Si, 1.43% Mn, 0.018% P, 0.012% S, 17.50% Cr, 12.81% Ni, 4.60% Mo, 0.55% Nb
0.038% C, 1.60% Mn, 0.45% Si, 0.021% P, 0.019% S, 9.20% Ni, 18.40% Cr, <0.03% Ti, <0.03% Nb+Ta, 0.027% Al+Ta
0.038% C, 1.60% Mn, 0.45% Si, 0.021% P, 0.019% S, 9.20% Ni, 18.40% Cr, <0.03% Ti, <0.03% Nb+Ta, 0.027% Al+Ta
0.038% C, 3.83% Mn, 0.72% Si, 0.005% P, 0.019% S, 0.04% Ni, 0.02% Cr, <0.005% Mo, 0.04% Cu, 0.080% Al, <0.005% Nb, <0.005% Ti
0.038% C, 9.00% Ni, 18.00% Cr
0.039% C, 0.69% Mn, 0.72% Si, 10.57% Ni, 18.63% Cr, 0.01% Mo, ferrite content=0.5%
0.04% C, 0.22% Si, 1.24% Mn, 0.010% P, 0.007% S, 0.36% Mo, 5.21% Ni, 0.034% Al
0.04% C, 0.29% Si, 1.54% Mn, 0.013% P, 0.001% S, 0.04% Cr, 0.014% Mo, 0.253% Ni, 0.238% Cu, 0.037% Nb, 0.0048% N, 0.03% Al, 0.0003% B
0.04% C, 0.30% Si, 1.50% Mn, 0.01% Al, 0.02% Cr, 0.01% Mo, 0.041% V, 0.035% Al, 0.012% Ti, 0.035% Nb
0.04% C, 0.30% Si, 1.50% Mn, 0.01% Ni, 0.02% Cr, 0.01% Mo, 0.041% V, 0.035% Al, 0.012% Ti, 0.035% Nb
0.04% C, 0.33% Si, 0.48% Mn, 0.014% P, 0.007% S, 17.55% Cr, 1.19% Mo, 0.18% Ni, 0.0290% N
0.04% C, 0.37% Si, 1.74% Mn, 0.004% S, 0.008% P, 0.32% Ni, 0.02% Cr, 0.31% Mo, 0.26% Cu, 0.075% Nb, 0.013% Ti, 0.005% N
0.04% C, 0.39% Si, 0.46% Mn, 0.022% P, 0.015% S, 17.40% Cr, 0.10% Mo, 0.26% Ni, 0.003% Al
0.04% C, 0.52% Si, 0.49% Mn, 0.015% P, 0.013% S, 14.57% Cr, 4.45% Ni, 3.59% Cu, 0.22% Mo
0.04% C, 1.19% Mn, 0.30% Si, 0.001% S, 0.002% P, 0.02% Cr, 0.02% Ni, 0.33% Mo, 0.09% V, 0.01% Nb, 0.057% Al
0.04% C, 1.20% Mn, 0.41% Si, 0.024% P, 0.014% S, 1.10% Ni, 0.07% Mo, 120 ppm N, 430 ppm O
0.04% C, 1.20% Mn, 0.41% Si, 0.024% P, 0.014% S, 1.10% Ni, 0.07% Mo, 120 ppm N, 430 ppm O
0.04% C, 1.29% Mn, 0.38% Si, 0.030% P, 0.017% S, 3.58% Ni, 0.08% Mo, 141 ppm N, 432 ppm O
0.04% C, 1.4% Mn, 0.10% Nb, 0.30% Mo. 0.05% C, 1.7% Mn, 0.10% Nb, 0.10% Mo, 0.25% Cr. 0.05% C, 1.6% Mn, 0.10% Nb, 0.20% Ni, 0.25% Cu, 0.25% Cr.
0.04% C, 1.90% Mn, 0.11% Si, 0.021% S, 0.019% P, 0.09% V, 0.02% Al, 0.009% N
0.04% C, 1.90% Mn, 0.11% Si, 0.021% S, 0.019% P, 0.19% Mo, 0.09% V, 0.02% Al, 0.009% N
0.04% C, 1.90% Mn, 0.11% Si, 0.021% S, 0.019% P, 0.19% Mo, 0.09% V, 0.02% Al, 0.009% N
0.04% C, 1.90% Mn, 0.11% Si, 0.021% S, 0.019% P, 0.34% Mo, 0.09% V, 0.02% Al, 0.009% N
0.04% C, 12.00% Cr, 5.20% Ni, 0.30% Mo
0.04% C, 3.70% Ni, 1.56% Mn, 0.89% Mo, 0.08% Cu, 0.06% Cr, 0.30% Si, 0.013% Ti, 0.005% V, 0.0014% Nb
0.04-0.06% C, 0.40% Si, 0.75-1.05% Mn, 0.006% S, 0.020% P, 3.35-3.65% Ni, 0.45-0.75% Cr, 0.55-0.65% Mo, 1.45-1.75% Cu, 0.02-0.06% Nb
0.04-0.08% C, 0.60% Mn, 0.40% Si, 0.007% S, 0.015% P, 19.00-21.00% Cr, 5.60-6.10% Mo, 19.00-21.00% Co, 0.20% Cu, 0.70% Fe, 0.30-0.60% Al, 1.90-2.40% Ti, 2.40-2.60% Al+Ti, 0.002% Pb, 0.0005% Ag, 0.02% Zr, Ni is balance
0.04-0.10% C, <2.00% Mn, <1.00% Si, <0.045% P, <0.030% S, 10.6-14.00% Ni, 16.00-18.50% Cr, 2.00-3.00% Mo. Weld metal: <0.08% C, 0.50-2.50% Mn, <1.00% Si, <0.040% P, <0.035% S, 10.00-14.00% Ni, 17.00-20.00% Cr, 2.50-3.50% Mo
0.040% C, 0.20% Si, 2.94% Mn, 0.0004% S, 0.001% P, 0.028% Nb, 0.023% Ti, 0.017% Al, 0.0002% B, 0.0018% N
0.040% C, 0.20% Si, 2.94% Mn, 0.0004% S, 0.001% P, 0.028% Nb, 0.023% Ti, 0.017% Al, 0.0002% B, 0.0018% N
0.040% C, 0.20% Si, 2.95% Mn, 0.0004% S, 0.001% P, 0.022% Ti, 0.017% Al, 0.0003% B, 0.0019% N
0.040% C, 0.62% Si, 0.71% Mn, 0.0104% S, 0.052% P, 0.044% Al, 0.00% Cr, 0.0030% N, 0.078% Ti, 0.0027% B
0.040% C, 0.64% Si, 1.20% Mn, 0.030% P, 0.001% S, 10.59% Ni, 17.22% Cr, 2.00% Mo. AISI 316L: 0.016% C, 0.67% Si, 1.20% Mn, 0.028% P, 0.001% S, 12.02% Ni, 17.20% Cr, 2.07% Mo
0.040% C, 3.97% Mn, 0.37% Si, 0.01% Cr, 0.17% Ni, 0.02% Cu, 0.02% Mo, 0.02% Nb, 0.017% Ti
0.042% C, 1.50% Mn, 0.45% Si, 14.34% Ni, 17.76% Cr, 4.72% Mo, 0.025% N
0.042% C, 1.50% Mn, 0.45% Si, 14.34% Ni, 17.76% Cr, 4.72% Mo, 0.025% N
0.043% C, 0.086% N, 18.39% Cr, 9.7% Ni, 0.03% Mo, 1.68% Mn, 0.31% Si, 0.026% P, 0.014% S
0.043% C, 0.24% Si, 1.57% Mn, 0.014% P, 0.010% S, 17.44% Cr, 12.89% Ni, 4.55% Mo, 2.05% Nb
0.043% C, 1.96% Mn, 0.62% Si, 0.011% P, 0.015% S, 9.98% Ni, 19.96% Cr, <0.01% Mo, 0.04% V, 0.57% Ti, 0.002% B, 0.03% Cu, 0.011% N
0.043% C, 0.03% Si, 2.03% Mn, 0.007% P, 0.011% S
0.044% C, 0.18% Si, 1.66% Mn, 0.018% P, 0.008% S, 16.67% Cr, 12.67% Ni, 2.50% Mo, max. 0.025% Nb
0.044% C, 0.24% Si, 0.06% Mn, 0.59% Cr, 5.21% Ni, 0.40% Mo, <0.005% S, <0.01% P
0.044% C, 0.32% Si, 0.65% Mn, 0.011% S, 0.005% P, 0.87% Ni, 0.77% Cr, 0.23% Mo, 1.12% Cu, 0.013% Al, 0.077% Nb, 0.0030% N
0.044% C, 0.38% Si, 1.65% Mn, 0.014% P, 0.007% S, 16.55% Cr, 12.86% Ni, 2.00% Mo, 0.86% Nb
0.045% C, 0.16% Si, 0.80% Mn, 1.09% Ni, 0.11% Mo, 0.057% Cr, 0.0007% N
0.045% C, 0.16% Si, 0.80% Mn, 1.09% Ni, 0.11% Mo, 0.057% Cr, 0.0007% N
0.045% C, 0.21% Si, 1.07% Mn, 0.001% S, <0.015% P, 2.36% Ni, 0.069% Cr, 0.22% Mo, 0.69% Cu, 0.015% Al, 0.013% Ti, 0.001% V, 0.019% Nb, 0.0010% B, 0.032% O, 0.015% N, 1.00 ppm H2
0.045% C, 0.21% Si, 1.07% Mn, 0.001% S, <0.015% P, 2.36% Ni, 0.069% Cr, 0.22% Mo, 0.69% Cu, 0.015% Al, 0.013% Ti, 0.001% V, 0.019% Nb, 0.0010% B, 0.032% O, 0.015% N, 1.00 ppm H2
0.045% C, 0.30% Si, 1.94% Mn, 0.0008% S, 0.0009% P, 0.0011% O, 0.003% N
0.045% C, 0.30% Si, 1.94% Mn, 0.0008% S, 0.0009% P, 0.0011% O, 0.003% N
0.045% C, 0.425% Mn, 0.008% Si, 0.012% P, 0.021% Nb, 0.0041% N, 0.043% Al
0.046% C, 0.35% Mn, 0.020% P, 0.018% S, 0.03% sol. Al, 0.010% insol. Al, 0.006% N
0.046% C, 1.14% Mn, 0.36% Si, 25.50% Ni, 15.60% Cr, 4.10% Ti, 0.009% N
0.047% C, 0.022% Si, 1.19% Mn, 0.003% P, 0.002% S, 0.029% Al, 0.0017% N, 0.49% Cr
0.047% C 1.23% Mn
0.0475% C, 1.49% Mn, 0.006% P, 0.0046% S
0.048% C, 0.80% Mn, 0.64% Si, 0.017% P, 0.011% S, 13.55% Ni, 16.80% Cr, 4.80% Mo, 0.039% N
0.049% C, 0.795% Si, 1.235% Mn, 0.0121% P, 0.0108% S, 0.0211% Al, 0.0264% Cr, 0.0228% Ni, 0.0065% Cu, 0.06% Ti
0.05% C, 0.02% Si, 0.13% Mn, 0.012% P, 0.010% S, 3.98% Cr, 0.54% Mo
0.05% C, 0.04% Nb
0.05% C, 0.18% Si, 0.41% Mn, 0.02% Cr, 0.05% Mo, 5.18% Ni, 0.001% V, 0.03% Cu, 0.036% Al, 0.0020% Nb
0.05% C, 0.20% Si, 1.52% Mn, 0.40% Ni, 0.16% Cr, 0.19% Mo, 0.033% Al, 0.018% Ti, 0.042% Nb.
0.05% C, 0.20% Si, 1.52% Mn, 0.40% Ni, 0.16% Cr, 0.19% Mo, 0.033% Al, 0.018% Ti, 0.042% Nb
0.05% C, 0.21% Si, 0.49% Mn, 2.70% Cr, 0.11% Mo, 1.55% W, 0.23% V, 0.05% Nb, 0.0042% B
0.05% C, 0.25% Si, 1.14% Mn, 0.22% Mo, 0.055% Nb, 0.021% Ti, 0.065% Al, 17ppm O, 0.0027% N
0.05% C, 0.25% Si, 1.14% Mn, 0.22% Mo, 0.055% Nb, 0.021% Ti, 0.065% Al, 17ppm O, 0.0027% N
0.05% C, 0.25% Si, 1.40% Mn, 0.012% P, 0.003% S, 0.85% Ni, 1.10% Cu, 0.02% Nb, 0.013% Ti
0.05% C, 0.26% Si, 0.51% Mn, 2.42% Cr, 0.11% Mo, 1.56% W, 0.26% V, 0.05% Nb, 0.0045% B
0.05% C, 0.35% Mn, 0.008% Si, 0.013% P, 0.027% S, 0.03% Ni, 0.02% Cr, 0.03% Cu, 0.058% Al
0.05% C, 0.35% Mn, 0.008% Si, 0.013% P, 0.027% S, 0.03% Ni, 0.02% Cr, 0.03% Cu, 0.058% Al
0.05% C, 0.39% Si, 0.41% Mn, 0.024% P, 0.002% S, 16.50% Cr, 0.05% Mo, 0.26% Ni, 0.031% Al
0.05% C, 0.50% Mn, 0.28% Si, 0.88% Ni, 0.71% Cr, 0.20% Mo, 1.12% Cu, 0.035% Nb
0.05% C, 0.90% Mn, 1.20% Si, 0.40% Mo, 0.00% Cr
0.05% C, 0.90% Mn, 1.20% Si, 0.40% Mo, 0.16% Cr
0.05% C, 0.90% Mn, 1.20% Si, 0.40% Mo, 0.30% Cr
0.05% C, 0.90% Mn, 1.20% Si, 0.40% Mo, 0.48% Cr
0.05% C, 0.90% Mn, 1.20% Si, 0.50% Cr, 0.00% Mo
0.05% C, 0.90% Mn, 1.20% Si, 0.50% Cr, 0.15% Mo
0.05% C, 0.90% Mn, 1.20% Si, 0.50% Cr, 0.30% Mo
0.05% C, 0.90% Mn, 1.20% Si, 0.50% Cr, 0.38% Mo
0.05% C, 0.90% Mn, 1.20% Si, 0.50% Cr, 0.50% Mo
0.05% C, 0.98% Mn, 0.33% Si, 0.017% P, 0.011% S, 0.06% Ni, 0.06% Mo, 45 ppm N, 446 ppm O
0.05% C, 1.00% Mn, 0.34% Si, 1.77% Ni, 0.72% Cr, 0.50% Mo, 1.25% Cu, 0.040% Nb
0.05% C, 1.17% Mn, 0.26% Si, 0.015% S, 0.016% P, 0.04% V, 0.01% Ti
0.05% C, 1.18% Mn, 0.38% Si, 0.022% P, 0.010% S, 2.52% Ni, 0.08% Mo, 178 ppm N, 482 ppm O
0.05% C, 1.18% Mn, 0.38% Si, 0.022% P, 0.010% S, 2.52% Ni, 0.08% Mo, 178 ppm N, 482 ppm O
0.05% C, 1.40% Mn, 0.25% Si, 0.85% Ni, 1.10% Cu, 0.013% Ti, 0.012% P, 0.003% S
0.05% C, 1.5% Mn, 0.0% Mo, 0.1% Cr. 0.05% C, 1.5% Mn, 0.25% Mo, 0.1% Cr. 0.05% C, 1.5% Mn, 0.50% Mo, 0.1% Cr
0.05% C, 1.50% Al, 0.0019% N
0.05% C, 1.64% Mn, 0.59% Si, 0.019% P, 0.014% S, 10.40% Ni, 17.60% Cr, 0.87% Nb, 0.025% N
0.05% C, 1.68% Mn, 0.44% Si, 0.023% P, 0.012% S, 11.85% Ni, 16.81% Cr, 2.21% Mo, 0.16% Cu, 0.030% Al, 0.002% Pb, 0.002% B
0.05% C, 1.70% Mn, 1.00% Cr. 0.05% C, 1.00% Si, 1.00% Cr. 0.05% C, 1.50% Mn, 1.00% Si, 1.00% Cr.
0.05% C, 1.73% Mn, 0.60% Si, 0.028% P, 0.012% S, 9.00% Ni, 18.70% Cr, 0.026% N
0.05% C, 1.76% Mn, 0.59% Si, 0.024% P, 0.008% S, 10.50% Ni, 17.60% Cr, 0.35% Ti, 0.011% N
0.05% C, 1.81% Mn, 0.63% Si, 0.029% P, 0.010% S, 11.90% Ni, 16.60% Cr, 2.30% Mo, 0.024% N
0.05% C, 1.82% Mn, 0.39% Si, 0.012% S, 0.018% P, 0.06% V, 0.055% Nb, 0.011% Al, 0.011% N
0.05% C, 17% Cr, 13% Ni, 5% Mo, 0.039% N
0.05% C, 3.73% Mn, 22.94% Ni, 0.015% N
0.05% C, 5.00% Ni, 0.60% Cr, 0.45% Mo, <0.05% S, <0.01% P, 0.03% Al, 0.07% V, 0.05% Nb
0.05% C, 8.50% Cr
0.05% C, 9.00% Ni, 18.00% Cr
0.05% C, max. 0.70% Si, max. 1.50% Mn, max. 0.040% P, max. 0.015% S, 12.00-14.00% Cr, 0.30-0.70% Mo, 3.50-4.50% Ni
0.05-0.35% C, 0.2-1.0% Si, 0.5-2.0% Mn, 0.003-0.06% S, 0.5-1.75% Mo, 0.01-0.1% Nb, 0.003-0.015% Ni
0.050% C, 0.19% Si, 1.87% Mn, 0.030% Nb, 0.010% Ti, 0.0025% N, Ni+Mo+Cr=1.09, 0.001% S
0.050% C, 0.19% Si, 1.87% Mn, 0.030% Nb, 0.010% Ti, 0.0025% N, Ni+Mo+Cr=1.09, 0.001% S
0.050% C, 0.19% Si, 1.87% Mn, 0.030% Nb, 0.010% Ti, 0.004% V, 0.0030% N, Mo+Cr=0.65, 0.45% Cu, 0.44% Ni
0.050% C, 0.228% Si, 1.850% Mn, 0.016% Cr, 0.307% Mo, 0.285% Ni, 0.246% Cu, 0.065% Nb, 0.013% Ti
0.050% C, 0.29% Si, 1.49% Mn, 0.022% Al, 0.084% Cr, 0.006% Al, 0.25-0.50% Mo, 0.001% Ti, 32 ppm N
0.050% C, 0.67% Mn, 0.49% Si, 0.016% P, 0.011% S, 13.45% Ni, 17.05% Cr, 4.73% Mo, 0.145% N
0.05% C, 1.40% Mn, 0.25% Si, 0.85% Ni, 1.10% Cu, 0.03% Nb, 0.013% Ti, 0.012% P, 0.003% S
0.05-0.20% C, max. 0.20% Si, max. 0.30% Mn, 1.70-2.40% Ni, 13.00-16.20% Cr, 0.00-2.50% Mo, max. 0.006% B, 0.01-0.12% N
0.05-0.15% C, max. 0.50% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 1.90-2.60% Cr, 0.87-1.13% Mo
0.05% C, 0.43% Si, 1.44% Mn, 0.010% P, 0.008% S, 1.33% Cr, 0.53% Ni, 0.37% Mo, 0.05% Nb, 0.055% Al, 0.05% V
0.05% C, 0.45% Si, 1.03% Mn, 0.022% P, 0.019% S, 0.10% Cu, 0.02% Cr, 0.50% Ni, 0.01% Mo, 0.02% Ti, 0.01% Al, 0.01% V
0.05% C, 0.47% Si, 1.47% Mn, 0.018% P, 0.021% S, 0.18% Cu, 0.07% Cr, 0.07% Ni, 0.10% Mo, 0.01% Ti, 0.005% Al, 0.04% V
0.051% C, 0.21% Mn, 3.44% Si, 0.010% P, 0.011% S
0.051% C, 0.25% Si, 1.92% Mn, 0.067% Ti+Nb, 1.10% Mo+Ni+Cr, 40 ppm N, 15 ppm B
0.051% C, 0.25% Si, 1.92% Mn, 0.067% Ti+Nb, 1.10% Mo+Ni+Cr, 40 ppm N, 15 ppm B
0.053% C, 0.25% Si, 1.90% Mn, 0.067% Ti+Nb, 1.10% Mo+Ni+Cr, 37 ppm N, 0 ppm B
0.053% C, 0.25% Si, 1.90% Mn, 0.067% Ti+Nb, 1.10% Mo+Ni+Cr, 37 ppm N, 0 ppm B
0.054% C, 0.03% Si, 0.48% Mn, 0.007% P, 0.011% S
0.055% C, 0.25% Si, 1.40% Mn, 0.003% S, 0.012% P, 0.85% Ni, 0.02% Nb, 0.013% Ti, 1.10% Cu, 0.0075% N
0.055% C, 0.25% Si, 1.40% Mn, 0.012% P, 0.003% S, 0.85% Ni, 1.10% Cu, 0.02% Nb, 0.013% Ti, 0.0075% N
0.057% C, 1.41% Mn, 0.03% Si, 0.005% P, 0.004% S, 13.96% Ni, 17.52% Cr, 2.51% Mo, 0.29% Ti, 0.004% N
0.057% C, 1.65% Mn, <0.07% Si, <0.025% P, 0.007% S, 12.44% Ni, 16.62% Cr, 2.32% Mo, 0.135% Cu, <0.01% Ti, <0.01% Nb
0.057% C, 1.67% Mn, 0.54% Si, 0.035% P, 0.025% S, 12.77% Ni, 17.14% Cr, 0.31% Cu, 2.21% Mo
0.057% C, 0.284% Si, 1.550% Mn, 0.010% P, 0.006% S, 0.700% Cr, 0.275% Ni, 0.010% Mo, 0.013% Cu, 0.047% Al, 0.009% V, 0.078% Nb, 0.009% Co
0.058% C, 0.09% Si, 1.80% Mn, 0.046% Nb, 0.004% V, 0.010% Ti, 0.0060% N, Mo+Cr=0.46, 0.14% Ni, 0.25% Cu
0.059% C, 1.13% Mn, 0.34% Si, 25.15% Ni, 15.39% Cr, 0.86% Al, 4.30% Ti, 0.01% N
0.059% C, 1.70% Mn, 0.12% Si, 0.018% P, 0.011% S, 0.29% Mo, 0.080% Nb, 0.022% Al, 0.0062% N
0.059% C, 1.70% Mn, 0.12% Si, 0.018% P, 0.011% S, 0.29% Mo, 0.080% Nb, 0.022% Al, 0.0062% N
0.059% C, 1.96% Si, 2.88% Mn
0.059% C, 1.96% Si, 2.88% Mn
0.059% C, 0.382% Si, 1.10% Mn, 0.008% P, 0.009% S, 0.043% Cr, 1.018% Ni, 0.021% Cu, 0.23% Mo, 0.056% Ti, 0.028% V
0.059% C, 0.337% Si, 1.421% Mn, 0.013% P, 0.050% S, 0.020% Cr, 1.065% Ni, 0.028% Cu, 0.012% Ti, 0.031% V
0.06% C, 0.24% Si, 0.18% Mn, 0.017% P, 0.005% S, 2.18% Cr, 0.07% Mo, 1.50% W, 0.25% V, 0.0055% B, 0.007% N, 0.04% Nb, 0.003% Al
0.06% C, 0.24% Si, 0.77% Mn, 0.008% P, 0.006% S, 0.02% Cr, 0.02% Mo, 9.36% Ni
0.06% C, 0.24% Si, 1.12% Mn, 5.75% Ni, 0.58% Cr, 0.19% Mo
0.06% C, 0.24% Si, 1.12% Mn, 5.75% Ni, 0.58% Cr, 0.19% Mo
0.06% C, 0.30% Mn
0.06% C, 0.30% Si, 1.60% Mn, 0.35% Cr, 1.70% Ni, 0.40% Mo
0.06% C, 0.43% Mn, 0.01% Si, 0.012% P, 0.027% S
0.06% C, 0.43% Mn
0.06% C, 0.43% Mn
0.06% C, 0.48% Si, 0.45% Mn, 0.096% S, 0.014% P, 0.21% Ni, 0.51% Cr, 0.29% Cu
0.06% C, 0.50% Mn
0.06% C, 0.56% Mn, 0.41% Si, 0.023% P, 0.008% S, 0.05% Ni, 0.01% Mo, 71 ppm N, 411 ppm O
0.06% C, 0.82% Mn, 0.26% Si, 0.001% S, 0.015% P, 0.25% Mo, 0.08% V, 0.04% Nb, sol. 0.040% Al, 0.003% N
0.06% C, 0.83% Mn, 0.37% Si, 3.48% Ni, 0.58% Cr, 0.59% Mo, 1.66% Cu, 0.28% Nb
0.06% C, 1.19% Mn, 0.87% Si, 0.38% Mo, 0.064% Al
0.06% C, 1.21% Mn, 0.25% Si, 0.001% S, 0.014% P, 0.25% Mo, 0.08% V, 0.044% Nb, sol. 0.036% Al, 0.003% N
0.06% C, 1.21% Mn, 0.25% Si, 0.001% S, 0.015% P, 0.07% V, 0.043% Nb, 0.30% Cu, sol. 0.041% Al, 0.003% N
0.06% C, 1.25% Cu, 0.97% Ni, 0.72% Cr, 0.42% Mo
0.06% C, 1.27% Mn, 0.30% Si, 0.080% S, 0.009% P, 0.01% Cr, 0.01% Ni, 0.01% Mo, 0.04% V, 0.01% Cu, 0.045% Al
0.06% C, 1.45% Mn, 0.35% Si, 0.97% Ni, 0.72% Cr, 0.42% Mo, 1.25% Cu, 0.040% Nb
0.06% C, 1.46% Mn, 0.14% Si, 0.003% S, 0.018% P, 0.20% Cr, 0.02% Ni, 0.25% Mo, 0.03% V, 0.01% Cu, sol. 0.035% Al
0.06% C, 1.69% Mn, 0.25% Si, 0.001% S, 0.015% P, 0.31% Ni, 0.08% V, 0.043% Nb, 0.30% Cu, sol. 0.040% Al, 0.003% N
0.06% C, 1.69% Mn, 0.54% Si, 0.012% P, 0.006% S, 9.58% Ni, 17.48% Cr, 0.50% Ti, 0.011% N
0.06% C, 1.70% Mn, 0.50% Mo, 0.10% V, 0.020% N
0.06% C, 1.72% Mn, 0.27% Mo, 0.06% Nb
0.06% C, 1.72% Mn, 0.27% Mo, 0.06% Nb
0.06% C, 1.72% Mn, 0.40% Si, 0.012% P, 0.007% S, 13.30% Ni, 17.30% Cr, 2.33% Mo, 0.003% Ti
0.06% C, 1.95% Mn, 0.29% Si, 0.003% S, 0.010% P, 0.010% Mo, 0.25% V, 0.037% Al, 0.008% N
0.06% C, 1.96% Mn, 0.32% Si, 0.003% S, 0.006% P, 0.18% Mo, 0.22% V, 0.020% Al, 0.005% N
0.06% C, 1.97% Mn, 0.37% Si, 0.020% S, 0.006% P, 0.45% V, 0.029% Al, 0.009% N
0.06% C, 12.80% Cr
0.06% C, 18.0% Cr, 8.0% Ni. 18-8 steel with 0.1%C: 0.10% C, 18.0% Cr, 7.7% Ni
0.06% C, 18.0% Cr, 8.0% Ni. 18-8 steel with 0.1%C: 0.10% C, 18.0% Cr, 7.7% Ni
0.06% C, 2.00% Mn, 0.37% Si, 0.005% S, 0.006% P, 0.45% V, 0.029% Al, 0.009% N
0.06% C, 2.33% Mn, 0.38% Si, 0.008% S, 0.025% P, 0.40% Cr, 0.01% Ni, 0.01% Mo, 0.08% V, 0.048% Nb, 0.01% Cu, sol. 0.035% Al
0.06% C, max. 0.70% Si, max. 1.50% Mn, max. 0.040% P, max. 0.015% S, 15.00-17.00% Cr, 0.80-1.50% Mo, 4.00-6.00% Ni
0.06% C. Right diagram: 0.17% C
0.06%C, 1.45% Mn, 1.25%Cu, 0.97% Ni, 0.72%Cr, 0.42% Mo
0.06-0.12% C, 0.15-0.35% Si, 0.25-0.50% Mn, 0.045% P, 0.045% S
0.06-0.12% C, 0.15-0.35% Si, 0.25-0.50% Mn, 0.045% P, 0.045% S
0.06-0.12% C, 0.6-1.2% Si, 1.50-2.50% Mn, 0.05-1.20% Cr, 0.02% V
0.06-0.15% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, 0.15-0.35% S, 12.00-14.00% Cr, max. 0.60% Mo
0.060% C, 1.74% Mn, 0.12% Si, 0.017% P, 0.011% S, 0.29% Mo, 0.075% Nb, 0.022% Al, 0.0061% N
0.06% C, 0.27% Si, 1.84% Mn, 0.02% Mo
0.060% C, 0.40% Si, 0.80% Mn, 11.00% Cr, 0.80% Ni, 0.20% Ti, 0.020% Ni
0.061% C, 0.10% Si, 1.76% Mn, 0.029% Nb, 0.012% Ti, 0.004% V, 0.0025% N, Mo+Cr=0.239, 0.28% Cu, 0.50% Ni
0.061% C, 1.00% Mn, 1.00% Si
0.061% C, 1.13% Mn, 0.77% Si, 0.28% Cr, 0.30% Mo
0.061% C, 3.02% Mn, 0.23% Si, 0.008% Al, 0.0009% N, 0.0020% B
0.062% C, 1.71% Mn, 0.12% Si, 0.016% P, 0.011% S, 0.02% Mo, 0.074% Nb, 0.025% Al, 0.0060% N
0.062% C, 1.75% Mn, 0.12% Si, 0.018% P, 0.011% S, 0.03% Mo, 0.075% Nb, 0.029% Al, 0.0102% N
0.062% C, 13.37% Cr, 5.33% Ni, 1.44% Mo, 0.67% Mn, 0.29% Nb, 1.46% Cu, 0.44% Si
0.063% C, 0.01% Si, 0.060% P, 0.003% S, 9.40% Ni, 18.60% Cr, 0.001% N, Phosphorus dopped
0.063% C, 1.71% Mn, 0.11% Si, 0.018% P, 0.011% S, 0.03% Mo, 0.084% Nb, 0.024% Al, 0.0058% N
0.063% C, 0.26% Si, 1.38% Mn, 0.0081% P, 0.0016% S, 0.044% Nb, 0.65% Ni, 0.40% Cr, 0.22% Mo, 0.017% Ti, 0.35% Cu
0.0637% C, 0.747% Si, 1.30% Mn, 0.0105% P, 0.0195% S, 0.022% Al, 0.0273% Cr, 0.0254% Ni, 0.0134% Cu, 0.0067% Mo, 0.0109% Ti
0.064% C, 8.53% Ni, 17.38% Cr, 0.124% N, MON2: 0.067% C, 8.80% Ni, 17.65% Cr, 2.03% Mo, 0.096% N, MN1: 0.068% C, 1.89% Mn, 8.67% Ni, 17.72% Cr, 0.091% N
0.064% C, 0.496% Si, 0.799% Mn, 0.015% P, 0.009% S, 0.025% Cr, 0.038% Ni
0.065% C, 0.29% Si, 1.55% Mn, 0.015%P, 0.003% S, 0.036% Al, 0.28% Mo, 0.076% Nb, 0.020% Ti
0.065% C, 0.559% Si, 1.144% Mn, 0.0188% P, 0.0162% S, 0.003% Al, 0.046% Cr, 0.029% Ni, 0.0575% Cu, 0.029% Ti
0.0657% C, 0.66% Si, 1.36% Mn, 0.0108% P, 0.0109% S, 0.0056% Al, 0.026% Cr, 0.019% Ni, 0.0124% Cu, 0.0008% Mo, 0.056% Ti
0.066% C, 0.26% Si, 1.583% Mn, 0.001% Mo, 0.037% Nb, 0.017% Ti, 0.037% Al, 12ppm O
0.066% C, 0.26% Si, 1.583% Mn, 0.001% Mo, 0.037% Nb, 0.017% Ti, 0.037% Al, 12ppm O
0.066% C, 1.75% Mn, 0.21% Si, 12.30% Ni, 17.40% Cr, 2.05% Mo
0.067% C, 8.76% Ni, 17.67% Cr, 2.00% Mo, 0.035% N, MON2: 0.067% C, 8.80% Ni, 17.65% Cr, 2.03% Mo, 0.096% N
0.068% C, 0.01% Si, 0.003% P, 0.033% S, 9.60% Ni, 18.60% Cr, 0.002% N, Sulfur dopped
0.068% C, 1.61% Mn, 0.49% Si, 0.018% P, 0.012% S, 10.28% Ni, 20.89% Cr, 0.05% Mo, 0.06% V, <0.01% Ti, <0.001% B, 0.10% Cu, 0.039% N
0.069% C, 0.01% Si, 0.003% P, 0.009% S, 9.40% Ni, 18.60% Cr, 0.002% N, High purity
0.069% C, 9.40% Ni, 18.60% Cr, 0.002% N, MO1: 0.077% C, 11.60% Ni, 18.08% Cr, 2.00% Mo, 0.097% N
0.069% C, 0.64% Si, 1.61% Mn, 0.016% P, 0.014% S, 0.018% Al, 0.04% Cr, 1.84% Ni, 0.024% Cu, 0.56% Mo
0.069% C, 0.64% Si, 1.61% Mn, 0.016% P, 0.014% S, 0.018% Al, 0.04% Cr, 1.84% Ni, 0.024% Cu, 0.56% Mo
0.07% C max, 0.55% Ni, 1.35% Cr, 0.20% Mo
0.07% C, 0.031% Nb. Fe-Nb-C-B: 0.09% C, 0.036% Nb, 0.003% B
0.07% C, 0.031% Nb
0.07% C, 0.031% Nb
0.07% C, 0.20% Si, 0.75% Mn, 0.43% Ni, 0.51% Cr, 0.11% Mo, 0.08% V, 0.01% Al
0.07% C, 0.20% Si, 0.75% Mn, 0.43% Ni, 0.51% Cr, 0.11% Mo, 0.08% V, 0.010% Al
0.07% C, 0.24% Si, 0.42% Mn, 9.33% Ni, 0.055% Al
0.07% C, 0.24% Si, 0.42% Mn, 9.33% Ni, 0.055% Al
0.07% C, 0.24% Si, 0.45% Mn, 0.020% P, 0.010% S, 17.35% Cr, 0.03% Mo, 0.15% Ni, 0.003% Al, 0.0280% N
0.07% C, 0.25% Si, 0.67% Mn, 3.96% Ni, 0.62% Cr, 0.46% Mo, 0.06% V
0.07% C, 0.25% Si, 0.67% Mn, 3.96% Ni, 0.62% Cr, 0.46% Mo, 0.060% V
0.07% C, 0.26% Si, 0.51% Mn, 0.007% P, 0.001% S, 0.018% Al, 0.13% Cu, 2.43% Cr, 0.11% Ni, 1.04% Mo, 0.23% V, 0.062% Ti, 0.004% Nb, 0.0041% Nb, 0.0100% N
0.07% C, 0.28% Si, 1.25% Mn
0.07% C, 0.28% Si, 1.25% Mn
0.07% C, 0.29% Si, 0.37% Mn, 3.12% Ni, 1.28% Cr, 0.005% Al
0.07% C, 0.29% Si, 0.37% Mn, 3.12% Ni, 1.28% Cr, 0.20% Mo
0.07% C, 0.29% Si, 0.37% Mn, 3.12% Ni, 1.28% Cr, 0.28% Mo, 0.005% Al
0.07% C, 0.39% Si, 1.53% Mn, 0.47% Ni, 0.34% Cr, 0.36% Mo, 0.052% Al, 0.18% Nb
0.07% C, 0.39% Si, 1.53% Mn, 0.47% Ni, 0.34% Cr, 0.36% Mo, 0.052% Al, 0.18% Nb
0.07% C, 0.43% Si, 0.24% Mn, 0.026% P, 0.022% S, 12.09% Cr, 0.06% Mo, 0.18% Ni
0.07% C, 0.43% Si, 0.24% Mn, 0.026% P, 0.022% S, 12.09% Cr, 0.06% Mo, 0.18% Ni
0.07% C, 0.49% Si, 0.40% Mn, 0.015% S, 0.10% P, 0.22% Ni, 0.56% Cr, 0.25% Cu, 0.33% Mo
0.07% C, 0.49% Si, 1.49% Mn, 0.57% Ni, 0.12% Cr, 0.28% Mo
0.07% C, 0.49% Si, 1.49% Mn, 0.57% Ni, 0.12% Cr, 0.28% Mo
0.07% C, 0.50% Mn, 0.38% Si, 0.020% P, 0.023% S, <0.10% Ni, 2.10% Cr, 1.00% Mo
0.07% C, 0.50% Mn, 0.40% Si, 0.020% P, 0.010% S, 13.00% Cr, 0.20% Ni
0.07% C, 0.50% Si, 0.43% Mn, 0.016% S, 0.098% P, 0.21% Ni, 0.55% Cr, 0.28% Cu, 0.41% Mo, 0.03% V
0.07% C, 0.50% Si, 1.49% Mn, 0.50% Ni, 0.12% Cr, 0.30% Mo
0.07% C, 0.50% Si, 1.49% Mn, 0.50% Ni, 0.12% Cr, 0.30% Mo
0.07% C, 0.53% Si, 0.35% Mn, 0.013% S, 0.063% P, 0.21% Ni, 0.53% Cr, 0.29% Cu, 0.41% Mo, 0.04% Ti
0.07% C, 0.53% Si, 0.49% Mn, 0.016% S, 0.11% P, 0.22% Ni, 0.53% Cr, 0.29% Cu, 0.42% Mo, 0.03% Nb
0.07% C, 0.53% Si, 0.49% Mn, 0.016% S, 0.11% P, 0.22% Ni, 0.53% Cr, 0.29% Cu, 0.42% Mo, 0.03% Nb
0.07% C, 0.55% Ni, 1.35% Cr, 0.20% Mo. -before carburizing
0.07% C, 0.55% Ni, 1.35% Cr, 0.20% Mo
0.07% C, 0.56% Si, 0.80% Mn, 0.010% P, 0.011% S, 25.95% Cr, 1.45% Mo, 5.50% Ni
0.07% C, 0.56% Si, 0.80% Mn, 0.010% P, 0.011% S, 25.95% Cr, 1.45% Mo, 5.50% Ni
0.07% C, 0.65% Mn, 0.40% Si, 13.00% Cr, 2.60% Ni, 1.80% Mo, 5.40% Co, 0.60% V
0.07% C, 0.65% Mn, 0.40% Si, 13.00% Cr, 2.60% Ni, 1.80% Mo, 5.40% Co, 0.60% V
0.07% C, 0.93% Mn, 0.99% Si, 0.27% Mo, 0.32% Cr
0.07% C, 0.93% Mn, 1.50% Si, 0.27% Mo, 0.32 % Cr
0.07% C, 0.93% Mn, 2.00% Si, 0.27% Mo, 0.32 % Cr
0.07% C, 1.0% Si, 2.0% Mn, 0.045% P, 0.015% S, 16.50-18.50% Cr, 2.0-2.50% Mo, 0.110% N, 10.00-13.00% Ni
0.07% C, 1.07% Mn, 0.033% Nb
0.07% C, 1.35% Mn, 0.29% Si, 0.004% S, 0.005% P, 0.08% V, 0.025% Nb, 0.036% Al, 0.006% N
0.07% C, 1.35% Mn, 0.52% Si, 0.022% P, 0.005% S, 0.05% Ni, 0.01% Mo, 94 ppm N, 352 ppm O
0.07% C, 1.35% Mn, 0.52% Si, 0.022% P, 0.005% S, 0.05% Ni, 0.01% Mo, 94 ppm N, 352 ppm O
0.07% C, 1.49% Mn, 0.26% Si, 0.001% S, 0.015% P, 0.25% Mo, 0.08% V, 0.042% Nb, sol. 0.036% Al, 0.003% N
0.07% C, 1.50% Mn, 0.38% Si, 0.031% P, 0.008% S, 11.75% Ni, 18.41% Cr, 0.81% Nb, 0.050% N
0.07% C, 1.50% Mn, 0.38% Si, 0.031% P, 0.008% S, 11.75% Ni, 18.41% Cr, 0.81% Nb, 0.050% N
0.07% C, 1.52% Mn, 0.47% Si, 0.008% S, 0.004% P, 0.01% Cr, 0.01% Ni, 0.27% Mo, 0.05% V, 0.01% Cu, sol. 0.064% Al
0.07% C, 1.57% Mn, 0.49% Si, 0.008% S, 0.004% P, 0.01% Cr, 0.01% Ni, 0.27% Mo, 0.05% V, 0.0005% B, sol. 0.066% Al
0.07% C, 1.71% Mn, 0.66% Si, 0.028% P, 0.005% S, 9.80% Ni, 18.00% Cr, 0.06% Ti, 0.033% N
0.07% C, 1.83% Mn. B added steel (X120): 0.05% C, 1.56% Mn 10 ppm B
0.07% C, 1.90% Mn, 0.24% Si, 0.006% S, 0.010% P, 0.08% Mo, 0.43% V, 0.06% Al, 0.009% N
0.07% C, 1.94% Mn, 0.30% Si, 0.003% S, 0.009% P, 0.010% Mo, 0.14% V, 0.038% Al, 0.007% N
0.07% C, 1.99% Mn, 0.25% Si, 0.004% S, 0.013% P, 0.48% V, 0.038% Al, 0.008% N
0.07% C, 2.12% Mn, 0.33% Si, 0.023% P, 0.008% S, 0.06% Ni, 0.01% Mo, 81 ppm N, 317 ppm O
0.07% C, 2.12% Mn, 0.33% Si, 0.023% P, 0.008% S, 0.06% Ni, 0.01% Mo, 81 ppm N, 317 ppm O
0.07% C, 2.79% Mn, 0.18% V, 0.046% Al, 0.005% N
0.07% C, max. 1.00% Si, max. 2.00% Mn, max. 0.045% P, max. 0.015% S, 17.00-19.50% Cr, 8.00-10.50% Ni, max. 0.11% N
0.07-0.12% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.07-0.12% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 1.20-1.50% Ni
0.07-0.13% C, <0.5% Si, 0.3-0.8% Mn, <0.02% P, <0.01% S, <0.4% Ni, 8.5-9.5% Cr, 0.3-0.6% Mo, 1.5-2.0% W, 0.15-0.25% V, 0.04-0.09% Nb, <0.04% Al, 0.001-0.006% B, 0.03-0.07% N.
0.07% C, 1.61% Mn, 0.32% Si, 0.025% Al, 0.22% Mo, 0.052% Nb, 0.012% Ti, Ti/N=1.48 (Grade 1.
0.07% C, 1.08% Mn, 0.09% Si, 0.032% Al, 0.19% Mo, 0.040% Nb, 0.014% Ti, 36 ppm N (Low-Mn+Si
0.07% C, 0.30% Si, 1.90% Mn, 0.20% Cu, 0.20% Mo, 0.25% Ni, 0.05% Nb
0.07% C, 1.42% Mn, 0.02% Si, 0.012% S, 0.011% P, 0.03% Al, 0.0046% N, 0.047% Nb, 0.0052% V, 0,073% Ti, 0.038% Cr, 0.035% Ni, 0.0055% Mo, 0.031% Cu
0.07% C, 0.21% Si, 1.00% Mn, 0.16% P, 0.022% S, 3.76% Cr, 0.42% Mo, 0.16% Ni
0.07% C, 0.65% Si, 1.42% Mn, 0.029% P, 0.031% S, 0.01% Al, 0.04% Cr, 0.02% Ni, 0.06% Cu, 0.004% N
0.07% C, 0.01% Si, 0.07% Mn, 0.003% P, 0.019% S
0.072% C, 0.21% Si, 0.42% Mn, 0.016% P, 0.001% S, 2.38% Cr, 0.12% Ni, 0.20% Mo, 1.50% W, 0.20% V, 0.038% Nb, 0.008% N, 0.0023% B, 0.022% Al, 0.031% Ti
0.072% C, 0.15% Si, 1.00% Mn, 0.40% Cr, 0.044% P, 0.029% Al, 0.006% N (Steel A.
0.074% C, 0.12% Si, 0.013% P, 0.002% S, 3.93% Ni, 24.80% Cr, 4.05% Mo, 0.0117% N, 0.51% Nb
0.074% C, 0.27% Si, 0.39% Mn, 0.034% P, 0.010% S, 0.30% Ni, 12.22% Cr, 0.52% Mo, 0.039% N
0.074% C, 0.57% Si, 1.35% Mn, 0.009% P, 0.003% S, 0.06% Ni, 0.12% Cu, 0.92% Cr, 0.52% Mo, 0.06% V, 0.026% Ti
0.074% C, 0.57% Si, 1.35% Mn, 0.009% P, 0.003% S, 0.06% Ni, 0.42% Cu, 0.92% Cr, 0.52% Mo, 0.06% V, 0.026% Al
0.074% C, 0.16% Si, 1.00% Mn, 0.40% Cr, 0.043% P, 0.85% Al, 0.003% N (Steel B.
0.074% C, 0.464% Si, 0.858% Mn, 0.015% P, 0.01% S, 0.042% Cr, 0.043% Ni
0.076% C, 0.26% Si, 1.47% Mn, 0.0006% S, 0.0010% P, 0.020% Ti, 0.049% Nb, 0.049% V, 0.0028% N, 0.0010% O
0.076% C, 0.30% Si, 1.41% Mn, 0.012% P, 0.010% S, 0.15% Cu, 1.13% Cr, 0.49% Ni, 0.37% Mo, 0.06% Nb, 0.026% Al
0.076% C, 1.17% Si, 1.86% Mn, 0.045% P, 0.012% S, 0.059% Cr, 0.004% Mo, 0.026% Ni, 0.019% Al, 0.065% Cu, 0.027% Ti
0.077% C, 0.25% Si, 1.28% Mn, 0.0006% S, 0.001% P, 0.045% Nb, 0.027% Ti, 0.0011% O, 0.0018% N
0.077% C, 0.25% Si, 1.28% Mn, 0.0006% S, 0.001% P, 0.045% Nb, 0.027% Ti, 0.0011% O, 0.0018% N
0.0774% C, 0.666% Si, 1.21% Mn, 0.0134% P, 0.0116% S, 0.0082% Al, 0.0377% Cr, 0.0233% Ni, 0.0155% Cu, 0.0013% Mo, 0.0024% Ti
0.078% C, 1.12% Mn, 0.41% Si, 0.025% P, 0.027% S, 8.49% Ni, 18.10% Cr, 0.21% Cu
0.079% C, 1.39% Mn, 0.20% Si, 0.0007% P, 0.0007% S, 0.002% Al, 0.012% Ti, 0.0015% N, 0.0017% O
0.079% C, 1.39% Mn, 0.20% Si, 0.0007% P, 0.0007% S, 0.002% Al, 0.012% Ti, 0.001595% N, 0.001796% O
0.079% C, 0.12% Si, 2.02% Mo, 0.0079% P, 0.0023% S, 0.061% Al, 0.33% Cr, 0.001% Nb, 0.0037% N
0.079% C, 0.49% Si, 0.774% Mn, 0.016% P, 0.007% S, 0.033% Cr, 0.004% Mo, 0.033% Ni, 0.029% V, 0.028% Cu, 0.003% Al, 0.012% Ti
0.08-0.14% C, max. 0.50% Si, 0.40-0.80% Mn, max. 0.020% P, max. 0.010% S, 2.00 - 2.50% Cr, 0.90-1.20% Mo, max. 0.012% N, max. 0.30% Cu
0.08% C, 0.03% Mn, 0.03% Si, 17.40% Ni, 3.70% Mo, 0.17% Al, 12.40% Co, 1.62% Ti
0.08% C, 0.13% Si, 0.26% Mn, 2.93% Cr
0.08% C, 0.17% Si, 0.61% Mn, 2.55% Ni, 0.70% Cr, 0.43% Mo
0.08% C, 0.17% Si, 0.61% Mn, 2.55% Ni, 0.70% Cr, 0.43% Mo
0.08% C, 0.17% Si, 0.61% Mn, 2.55% Ni, 0.70% Cr, 0.43% Mo
0.08% C, 0.21% Si, 0.37% Mn, 0.03% Cr, 0.06% Mo, 5.25% Ni, 0.001% V, 0.03% Cu, 0.048% Al, 0.0020% Nb
0.08% C, 0.21% Si, 0.53% Mn, 0.004% P, 0.004% S, 2.44% Cr, 0.18% Ni, 0.95% Mo, 0.26% V, 0.004% B, 0.002% Nb, 0.053% Ti, 0.0073% N, 0.004% Al, 0.09% Cu
0.08% C, 0.21% Si, 0.53% Mn, 0.004% S, 0.004% P, 0.18% Ni, 2.43% Cr, 0.95% Mo, 0.09% Cu, 0.004% Al, 0.26% V, 0.004% B, 0.002% Nb, 0.053% Ti, 0.0063% N
0.08% C, 0.21% Si, 1.74% Mn, 0.01% S, 0.01% P, 0.74% Ni, 3.46% Mo, 0.08% Ti, 0.05% Nb, 1.88% Cu, 0.03% Al, 0.01% N, 0.9 CE. CE = C + (Mn+Si)/6 + (Ni + Cu)/15 + (Cr +Mo + V)/5 = 0.9
0.08% C, 0.25% Si, 0.49% Mn, 3.48% Ni, 0.62% Cr, 0.30% Mo
0.08% C, 0.25% Si, 0.49% Mn, 3.48% Ni, 0.62% Cr, 0.30% Mo
0.08% C, 0.25% Si, 1.70% Mn, 0.002% S, 0.029% P, 0.17% Ni, 0.029% Al, 0.00% Mo, 0.033% Nb, 0.0024% B, 0.026% Ti, 0.0048% N
0.08% C, 0.28% Si, 1.44% Mn, 0.005% S, 2.31% Ni, 0.20% Mo, 0.040% Nb
0.08% C, 0.29% Mn, 0.16% Si, 0.035% S, 0.007% P 2.06% Ni, 0.08% Cr, 0.02% Mo, 0.13% Cu
0.08% C, 0.29% Si, 1.40% Mn, 0.007% S, 0.011% P, 0.019% Al, 0.019% Ti, 0.079% V, 0.0076% N
0.08% C, 0.30% Si, 1.40% Mn, 0.009% S, 0.006% P, 0.023% Al, 0.016% Ti, 0.12% V, 0.0082% N
0.08% C, 0.30% Si, 1.50% Mn, 0.05% Nb, 0.05% V
0.08% C, 0.34% Si, 1.43% Mn, 0.005% S, 0.008% P, 0.014% Al, 0.018% Ti, 0.077% V, 0.01% N
0.08% C, 0.35% Mn, 0.06% Si, 0.020% S, 0.010% P 4.06% Ni, 0.07% Cr, 0.88% Mo, 0.15% Cu
0.08% C, 0.40% Si, 0.61% Mn, 3.71% Ni, 1.46% Cr, 0.57% Mo, 0.05% Al
0.08% C, 0.40% Si, 0.61% Mn, 3.71% Ni, 1.46% Cr, 0.57% Mo, 0.050% Al
0.08% C, 0.40% Si, 0.80% Mn, 0.30% Cr, 0.20% Ni, 0.10% Ti, 0.20% Cu, 0.003% N
0.08% C, 0.40% Si, 1.50% Mn, 0.30% Cr, 0.20% Ni, 0.10% Ti, 0.20% Cu, 0.003% N
0.08% C, 0.40% Si, 1.50% Mn, 0.40% Mo
0.08% C, 0.41% Si, 1.45% Mn, 0.49% Ni, 0.29% Cr, 0.39% Mo, 0.15% Nb
0.08% C, 0.41% Si, 1.45% Mn, 0.49% Ni, 0.29% Cr, 0.39% Mo, 0.15% Nb
0.08% C, 0.49% Mn, 8.94% Ni
0.08% C, 0.49% Mn, 8.94% Ni
0.08% C, 0.58% Mn, 0.68% Si, 0.019% P, 0.007% S, 0.29% Ni, 6.31% Cr, 0.51% Mo, 0.04% V, 0.003% Al, 0.015% N
0.08% C, 0.62% Si, 0.47% Mn, 0.014% P, 0.013% S, 6.80% Cr, 0.23% Ni, 0.22% Cu, 0.05% Mo, 0.85% Al, 0.065% Co
0.08% C, 0.62% Si, 0.47% Mn, 0.014% P, 0.013% S, 6.80% Cr, 0.23% Ni, 0.22% Cu, 0.05% Mo, 0.85% Al, 0.065% Co
0.08% C, 1.0% Mn, 0.20% Si, 0.80% Al
0.08% C, 1.0% Mn, 0.80% Si, 0.80% Al
0.08% C, 1.0% Si, 1.7% Mn, 0.010% P, 0.005% S, 0.016% Cr
0.08% C, 1.00% Mn, 0.20% Si, 0.80% Al
0.08% C, 1.00% Ni, 12.00% Cr, 2.00% Mo, 0.30% V
0.08% C, 1.00% Ni, 12.00% Cr, 2.00% Mo, 0.30% V
0.08% C, 1.00% Si, 2.00% Mn, 0.045% P, 0.015% S, 17.00-19.00% Cr, 9.00-12.00% Cr, Nb (10 x C<=1,00)
0.08% C, 1.05% Mn, 0.014% P, 0.015% S, 0.45% Si, 2.00% Ni, 0.20% Cr, 0.75% Mo, 0.25% V
0.08% C, 1.05% Mn, 0.20% Cr, 2.00% Ni, 0.75% Mo, 0.25% V
0.08% C, 1.17% Mn, 0.70% Si, 0.62% Mo
0.08% C, 1.28% Mn, 0.41% Si, 0.020% P, 0.022% S, 10.72% Ni, 18.30% Cr, 0.77% Nb, 0.030% N
0.08% C, 1.28% Mn, 0.41% Si, 0.020% P, 0.022% S, 10.72% Ni, 18.30% Cr, 0.77% Nb, 0.030% N
0.08% C, 1.40% Mn, 0.25% Si, 0.008% P, 0.002% S, 0.04% Al, 0.008% Ti, 0.0030% N, 0.0014% B
0.08% C, 1.5% Mn, 0.35% Si, 0.045% Nb, 0.25% Mo and 0.0015% B
0.08% C, 1.5% Mn, 0.35% Si, 0.045% Nb, 0.25% Mo and 0.0015% B
0.08% C, 1.52% Mn, 0.37% Si, 0.007% S, 0.023% P, 0.21% Cr, 0.10% Ni, 0.10% V, 0.05% Nb, 0.34% Cu, 0.02% Al, 0.008% N
0.08% C, 1.57% Mn, 0.28% Si, 0.011% P, 0.002% S, 0.07% V, 0.03% Nb, 0.018% Ti, 0.0038% N
0.08% C, 1.6% Si, 0.8% Mn, 0.040% P, 0.030% S, 21.00% Cr, 11.00% Ni, 0.17% N, 0.05% Ce
0.08% C
0.08% C
0.08%, 1.0% Mn, 0.80% Si, 0.80% Al
0.08-0.12% C, <0.50% Si, 0.30-0.60% Mn, <0.020% P, <0.005% S, <0.040% Al, 8.00-9.50% Cr, <0.30% Cu, 0.85-1.05% Mo, 0.030-0.070% N, 0.060-0.10% Nb, <0.30% Ni, 0.18-0.25% V
0.08-0.12% C, <1.00% Si, <1.00% Mn, 12.00-14.00% Cr
0.08-0.12% C, 0.20-0.50% Si, 0.30-0.60% Mn, 0.020% P, 0.010% S, 8.00-9.50% Cr, 0.85-1.05% Mo, 0.40% Ni, 0.06-0.10% Nb, 0.18-0.25% V, 0.04% Al, 0.030-0.070% N
0.08-0.12% C, 0.25-0.45% Si, 1.60-2.0% Mn, 0.030% P, 0.015% S, 0.0030-0.0060% B, 14.50-15.50% Cr, 1.05-1.25% Mo, 15.0-16.0% Ni, 0.35-0.55% Ti
0.08-0.12% C, 0.25-0.45% Si, 1.60-2.0% Mn, 0.030% P, 0.015% S, 0.0030-0.0060% B, 14.50-15.50% Cr, 1.05-1.25% Mo, 15.0-16.0% Ni, 0.35-0.55% Ti
0.08-0.12% C, 0.30% Si, 0.30-0.60% Mn, 0.025% P, 0.025% S
0.08-0.12% C, 0.30% Si, 0.30-0.60% Mn, 0.025% P, 0.025% S
0.08-0.12% C, 0.37-0.50% Ti
0.08-0.12% C, max. 0.50% Si, 0.30-0.60% Mn, max. 0.020% P, max. 0.015% S, 8.00-9.50% Cr, 0.85-1.05% Mo, max. 0.30% Ni, 0.18-0.25% V, max. 0.30% Cu, max. 0.040% Al, 0.060-0.10% Nb
0.08-0.15% C, max. 0.50% Si, 0.40-0.70% Mn, max. 0.040% P, max. 0.040% S, 2.00-2.50% Cr, 0.90-1.20% Mo
0.08-0.15% C, max. 0.50% Si, 0.40-0.70% Mn, max. 0.040% P, max. 0.040% S, 2.00-2.50% Cr, 0.90-1.20% Mo
0.08-0.15% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, 0.15-0.35% S, 12.00-14.00% Cr, max. 0.60% Mo
0.08-0.15% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, max. 0.015% S, 11.50-13.50% Cr, max. 0.75% Ni
0.08-0.18% C, 0.10-0.35% Si, 0.40-1.00% Mn, max. 0.035% P, max. 0.030% S, 0.70-1.00% Cr, 0.40-0.60% Mo, max. 0.070% Al
0.08-0.20% C, max. 0.40% Si, 0.90-1.50% Mn, max. 0.025% P, max. 0.015% S, max. 0.30% Cr, max. 0.08% Mo, max. 0.30% Ni, max. 0.020% V, max. 0.30% Cu, max. 0.020% Nb, min. 0.02% Al
0.080% C, 2.0% Mn, 0.010% P, 0.005% S, 0.042% Al, 0.15% Mo
0.08% C, 0.21% Si, 0.53% Mn, 0.004% P, 0.004% S, 0.004% Al, 0.09% Cu, 2.44% Cr, 0.18% Ni, 0.95% Mo, 0.26% V, 0.004% B, 0.002% Nb, 0.053% Ti, 0.073% N
0.08% C, 1.55% Mn, 0.41% Si, 0.027% Al, 0.18% Mo, 0.031% Nb, 0.013% Ti, Ti/N=2.96 (Grade 1A.
0.08% C, 1.55% Mn, 0.41% Si, 0.027% Al, 0.18% Mo, 0.031% Nb, 0.013% Ti, 44 ppm N (Hi-Mn+Si
0.08% C, 0.38% Si, 1.62% Mn, 0.028% P, 0.003% S, 0.06% Cu, 0.05% Cr, 0.03% Ni, 0.046% Nb, 0.028% Al, 0.01% V
0.08% C, 0.26% Si, 0.05% Mn, 0.005% P, 0.024% S
0.08% C, 0.70% Si, 1.92% Mn, 0.017% P, 0.015% S, 0.018% Al, 0.034% Cr, 1.98% Ni, 0.020% Cu, 0.57% Mo
0.08% C, 0.65% Si, 1.93% Mn, 0.016% P, 0.013% S, 0.018% Al, 0.036% Cr, 2.05% Ni, 0.020% Cu, 0.58% Mo
0.08% C, 0.60% Si, 1.70% Mn, 0.013% P, 0.011% S, 0.018% Al, 0.031% Cr, 2.02% Ni, 0.016% Cu, 0.59% Mo
0.08% C, 0.60% Si, 1.70% Mn, 0.013% P, 0.011% S, 0.018% Al, 0.031% Cr, 2.02% Ni, 0.016% Cu, 0.59% Mo
0.080% C, 0.40% Si, 1.42% Mn, 0.031% P, 0.010% S, 0.008% Al, 0.043% Cr, 0.023% Ni, 0.060% Cu, 0.002% Mo, 0.001% Ti
0.081% C, 0.10% Si, 1.74 Mn, <0.015% P, <0.015% S, 0.18% Ti
0.081% C, 0.22% Si, 0.98% Mn, 0.022% P, 0.007% S, 0.011% Al, 0.040% Cr, 0.022% Ni, 0.062% Cu, 0.003% Mo, 0.002% Ti
0.082% C, 0.29% Si, 1.49% Mn, 0.02% Al, 0.085% Cr, 40 ppm N
0.082% C, 1.54% Mn, 0.01% P, 0.006% S, 0.36% Si, 0.033% Al, 0.055% Nb, 0.078% V, 0.005% N
0.083% C, 0.831% Si, 1.455% Mn, 0.006% P, 0.004% S, 0.015% Cr, 0.005% Ni
0.085% C, 0.72% Si, 1.219% Mn, 0.0129% P, 0.0095% S, 0.0056% Al, 0.0281% Cr, 0.0218% Ni, 0.0087% Cu
0.086% C, 0.22% Si, 1.01% Mn, 0.019% P, 0.006% S, 0.012% Al, 0.039% Cr, 0.023% Ni, 0.055% Cu, 0.003% Mo, 0.002% Ti
0.087% C, 0.10% Si, 0.21% Mn, 7.46% Cr, 0.15% V, 1.96% W, 0.0059% N, 0.023% Ta
0.087% C, 0.459% Si, 0.807% Mn, 0.017% P, 0.01% S, 0.038% Cr, 0.051% Ni, 0.02% V, 0.061% Cu, 0.002% Al, 0.01% Ti
0.088% C, 0.27% Si, 0.49% Mn, 0.028% P, 0.027% S, 0.77% Cr, 0.47% Mo
0.088% C, 0.27% Si, 0.49% Mn, 0.028% P, 0.027% S, 0.77% Cr, 0.47% Mo
0.088% C, 1.06% Mn, 0.42% Si, 8.00% Ni, 24.85% Cr, 0.0115% N
0.088% C, 1.40% Mn, 0.30% Si, 0.0055% B
0.088% C, 0.529% Si, 1.36% Mn, 0.014% P, 0.008% S, 0.025% Cr, 0.065% Ni, 0.008% V, 0.03% Cu, 0.002% Al, 0.001% Ti
0.089% C, 2.86% Mn, 0.21% Si, 0.014% Al, 0.00018% N, 0.0005% B
0.09% C, 0.016% Nb, 0.48% V, 40 ppm N, 59 ppm O. d.) 0.04% C, 0.020% Nb, 0.55% V, 0.02% Mn, 5 ppm N, 1 ppm O
0.09% C, 0.20% Si, 0.40% Mn, 3.41% Ni, 1.02% Cr, 0.27% Mo, 0.012% Al
0.09% C, 0.20% Si, 0.40% Mn, 3.41% Ni, 1.02% Cr, 0.27% Mo, 0.012% Al
0.09% C, 0.21% Si, 0.40% Mn, 2.46% Ni, 1.00% Cr, 0.01% Al
0.09% C, 0.21% Si, 0.40% Mn, 2.46% Ni, 1.00% Cr, 0.27% Mo, 0.010% Al
0.09% C, 0.22% Si, 0.37% Mn, 3.86% Cr
0.09% C, 0.22% Si, 0.37% Mn, 3.86% Cr
0.09% C, 0.22% Si, 0.45% Mn, 0.017% P, 0.002% S, 8.81% Cr, 0.45% Mo, 1.64% W, 0.23% V, 0.004% B, 0.042% N, 0.06% Nb, 0.017% Al
0.09% C, 0.22% Si, 1.35% Mn, 0.35% Cr, 0.24% Mo, 0.054% Al, 0.008% Nb
0.09% C, 0.22% Si, 1.35% Mn, 0.35% Cr, 0.24% Mo, 0.054% Al, 0.008% Nb
0.09% C, 0.24% Si, 0.41% Mn, 0.013% P, 0.009% S, 13.70% Cr, 0.03% Mo, 0.21% Ni
0.09% C, 0.24% Si, 1.15% Mn
0.09% C, 0.24% Si, 1.15% Mn
0.09% C, 0.27% Si, 0.44% Mn, 12.60% Cr
0.09% C, 0.28% Si, 0.83% Mn, 2.65% Ni, 0.01% Mo, 0.033% Al
0.09% C, 0.28% Si, 0.83% Mn, 2.65% Ni, 0.01% Mo, 0.033% Al
0.09% C, 0.29% Si, 0.53% Mn, 3.53% Ni, 0.90% Cr, 0.36% Mo
0.09% C, 0.29% Si, 0.53% Mn, 3.53% Ni, 0.90% Cr, 0.36% Mo
0.09% C, 0.29% Si, 1.40% Mn, 0.004% S, 0.011% P, 0.018% Al, 0.016% Ti, 0.041% V, 0.0074% N
0.09% C, 0.30% Mn, 0.62% Si, 0.022% P, 0.008% S, 0.14% Ni, 9.29% Cr, 1.01% Mo, 0.04% V, 0.009% Al, 0.018% N
0.09% C, 0.30% Si, 1.49% Mn, 0.004% S, 0.012% P, 0.02% Al, 0.016% Ti, 0.081% V, 0.014% N
0.09% C, 0.35% Si, 0.38% Mn, 2.46% Ni, 1.18% Cr, 0.29% Mo, 0.031% Al
0.09% C, 0.35% Si, 0.38% Mn, 2.46% Ni, 1.18% Cr, 0.29% Mo, 0.031% Al
0.09% C, 0.37% Si, 0.36% Mn, 0.031% P, 0.009% S, 13.17% Cr, 0.24% Ni, 0.13% Cu, 0.06% Mo, 0.015% Al, 0.010% Sn
0.09% C, 0.37% Si, 1.34% Mn, 0.02% Ni, 0.01% Mo, 0.06% V
0.09% C, 0.37% Si, 1.34% Mn, 0.02% Ni, 0.01% Mo, 0.060% V
0.09% C, 0.40% Mn, 0.33% Si, 0.34% Ni, 17.20% Cr, 0.06% Mo, 0.010% Al, 0.03% N
0.09% C, 0.41% Mn, 8.62% Cr, 0.23% Ni, 0.35% Mo, 0.10% V, 1.11% W, 0.0063% B, 0.050% Nb, 0.0345% N
0.09% C, 0.44% Mn, 0.26% Si, 0.008% P, 0.010% S, 2.25% Cr, 0.99% Mo
0.09% C, 0.45% Mn, 0.25% Si, 0.010% P, 0.012% S, 0.10% Cr, 9.00% Ni, 0.04% Mo, 0.030% Al
0.09% C, 0.45% Mn, 0.40% Si, 0.01% S, 0.02% P 0.18% Ni, 12.30% Cr
0.09% C, 0.51% Mn, 0.27% Si, 0.008% S, 0.010% P 9.00% Ni, 0.05% Cr, 0.03% Mo, 0.13% Cu, 0.012% Al
0.09% C, 0.51% Mn, 0.27% Si, 0.008% S, 0.010% P 9.00% Ni, 0.05% Cr, 0.03% Mo, 0.13% Cu, 0.012% Al
0.09% C, 0.54% Si, 1.34% Mn, 0.44% Ni, 0.96% Cr
0.09% C, 0.54% Si, 1.34% Mn, 0.96% Cr
0.09% C, 0.59% Mn, 0.47% Si, 0.010% S, 0.015% P, 2.00% Cr, 0.56% Mo, 0.37% V, O.18% Ti, 0.005% B, 0.41% W
0.09% C, 0.72% Mn, 0.29% Si, 0.28% Mo
0.09% C, 0.81% Mn, 0.11% Si, 0.017% P, 0.013% S, 0.11% Cu, 0.0050% N, 0.014% O
0.09% C, 0.82% Mn, 0.29% Si, 0.013% S, 0.019% P, 0.12% Cr, 1.85% Ni, 0.53% Mo, 0.04% V, 0.01% Cu, sol. 0.031% Al
0.09% C, 0.94% Mn, 0.28% Si, 0.008% S, 0.010% P, 0.10% Cr, 2.54% Ni, 0.64% Mo, 0.04% V, 0.07% Cu, sol. 0.029% Al
0.09% C, 1.01% Mn, 0.32% Si, 0.009% S, 0.011% P, 0.52% Cr, 1.49% Ni, 0.52% Mo, 0.05% V, 0.002% B, 0.25% Cu, sol. 0.053% Al
0.09% C, 1.03% Mn, 0.28% Si, 0.015% S, 0.010% P, 0.01% Cr, 0.01% Ni, 0.31% Mo, 0.10% V, 0.09% Nb, 0.021% Al
0.09% C, 1.10% Si, 1.30% Mn, 0.019% S, 0.025% P, 0.32% Mo
0.09% C, 1.10% Si, 1.30% Mn, 0.019% S, 0.025% P, 0.32% Mo
0.09% C, 1.17% Mn, 0.37% Si, 13.40% Ni, 18.10% Cr, 0.51% Ti, 0.017% N
0.09% C, 1.48% Mn, 0.25% Si, 0.060% S, 0.014% P, 0.010% Cr, 0.010% Ni, 0.010% Mo, 0.04% V, 0.010% Cu, 0.047% Al
0.09-0.12% C, max. 0.050% Si, 0.20-0.60% Mn, max. 0.005% P, max. 0.005% S, 8.50-9.50% Cr, 0.15-0.25% V, 1.00-1.20% W, 0.05-0.09% Ta, max. 0.005% Ni, max. 0.005% Mo, max. 0.095% Cu, As+Sn+Sb+Zr=max. 0.05
0.09-0.13% C, 0.10-0.50% Si, 0.30-0.60% Mn, 0.020% P, 0.010% S, 8.50-10.50% Cr, 0.90-1.10% Mo, 0.40% Ni, 0.06-0.10% Nb, 0.18-0.25% V, 0.040% Al, 0.90-1.10% W, 0.04-0.09% N, 0.0003-0.0060% B
0.09C?1.48Mn?0.25Si?0.06S?0.014P?0.01Cr?0.01Ni?0.01Mo?0.04V?0.01Cu?0.047Al
0.09% C, 0.10% Si, 1.42% Mn, 0.011% P, 0.010% S, 0.053% Al, 0.35% Cr, 0.01% Ni, 0.005% Mo, 0.020% V, 0.001% Nb, 0.001% Ti, 0.0050% N, 0.0002% B
0.09% C, 0.32% Si, 1.61% Mn, 0.017% P, 0.020% S, 0.07% Cu, 0.03% Cr, 0.03% Ni, 0.002% Al
0.09% C, 0.81% Si, 1.47% Mn, 0.018% P, 0.018% S, 0.20% Cu, 0.08% Cr, 0.07% Ni, 0.005% Al, 0.0045% N
0.09% C, 1.03% Si, 1.65% Mn, 0.026% P, 0.030% S, 0.20% Cu, 0.010% Ti, 0.03% As
0.09% C, 0.41% Si, 1.54% Mn, 0.022% P, 0.01% S, 0.17% Cu, 0.20% Cr, 0.09% Ni, 0.02% Nb, 0.019% Al
0.09% C, 0.43% Si, 1.74% Mn, 0.030% P, 0.006% S, 0.19% Cu, 0.15% Cr, 0.11% Ni, 0.049% Nb, 0.019% Al
0.09% C, 0.54% Si, 1.54% Mn, 0.017% P, 0.004% S, 0.12% Cu, 0.99% Cr, 0.50% Ni, 0.39% Mo, 0.052% Al
0.09% C, 0.54% Si, 1.60% Mn, 0.017% P, 0.004% S, 0.07% Cu, 1.17% Cr, 0.51% Ni, 0.38% Mo, 0.048% Al
0.09% C, 0.48% Si, 1.55% Mn, 0.014% P, 0.017% S, 0.20% Cu, 1.41% Cr, 1.01% Ni, 0.43% Mo, 0.047% Nb
0.09% C, 0.48% Si, 1.25% Mn, 0.012% P, 0.022% S, 0.048% Al, 1.45% Cr, 0.39% Mo, 0.07% Nb, 0.16% Cu, 0.50% Ni, 0.01% Ti
0.09% C, 0.56% Si, 0.93% Mn, 0.020% P, 0.021% S, 0.15% Cu, 0.05% Cr, 0.09% Ni, 0.37% Mo, 0.05% Ti, 0.01% V
0.09% C, 0.468% Si, 0.65% Mn, 0.01% P, 0.011% S, 0.034% Cr, 0.045% Ni
0.09% C, 0.68% Si, 1.90% Mn, 0.017% P, 0.015% S, 0.015% Al, 0.034% Cr, 2.00% Ni, 0.020% Cu, 0.58% Mo
0.09% C, 0.73% Si, 2.08% Mn, 0.018% P, 0.015% S, 0.035% Cr, 2.07% Ni, 0.020% Cu, 0.60% Mo
0.091% C, 0.40% Si, 1.36% Mn, 0.028% P, 0.011% S, 0.051% Cr, 0.004% Mo, 0.023% Ni, 0.009% Al, 0.068% Cu, 0.001% Ti
0.0915% C, 0.4320% Si, 1.2600% Mn, 0.0104% P, 0.0049% S, 0.0141% Cu, 0.0156% Cr, 0.0038% Mo, 0.0014% V, 0.0360% Ni, 0.0206% Nb, 0.0508% Al, 0.0037% Ti, 0.0079% W, 0.0066% Co, 0.0006% B
0.092% C, 1.42% Mn, 0.20% Si, 0.0010% P, 0.0008% S, 0.020% Al, 0.015% Ti, 0.0015% N, 0.0020% O
0.092% C, 0.34% Si, 0.05% Mn, 0.005% P, 0.024% S
0.092% C, 1.18% Si, 1.81% Mn, 0.040% P, 0.014% S, 0.063% Cr, 0.004% Mo, 0.028% Ni, 0.020% Al, 0.075% Cu, 0.032% Ti
0.093% C, 0.70% Mn, 0.36% Si, 0.51% Mo, 0.0054% B
0.093% C, 0.44% Mn, 8.39% Cr, 1.499% W, 0.196% V, 0.01% Ta
0.094% C, 0.30% Si, 1.32% Mn
0.094% C, 1.32% Mn, 0.30% Si
0.094% C, 0.94% Si, 0.05% Mn, 0.005% P, 0.024% S
0.095% C, 0.48% Mn, 0.27% Si, 0.008% P, 0.008% S, 9.30% Ni, 0.17% Cr, 0.51% Mo, 0.045% Al, 0.008% N2
0.096% C, 0.66% Mn, 0.32% Si, 0.0048% B
0.096% C, 0.66% Si, 1.90% Mn, 0.016% P, 0.013% S, 0.018% Al, 0.033% Cr, 2.04% Ni, 0.020% Cu, 0.61% Mo
0.097% C, 0.69% Mn, 0.31% Si, 1.45% Ni, 0.0048% B
0.097% C, 0.70% Mn, 0.36% Si, 0.26% Mo, 0.0050% B
0.098% C, 0.30% Si, 1.41% Mn, 0.014% P, 0.004% S, 0.023% Cr, 0.024% Ni, 0.055% V, 0.044% Nb, 0.102% Al, 0.001% Mo, 0.008% Ti, 0.009% Cu
0.099% C, 0.67% Mn, 0.32% Si, 1.46% Ni, 0.51% Mo, 0.0058% B
0.099% C, 0.221% Si, 1.940% Mn, 0.0166% S, 0.023% S, 0.829% Cr, 0.177% Mo, 0.050% Ni, 0.0359% Al, 0.056% Cu, 0.0023% Nb, 0.0299% Ti, 0.066% V, 0.0116% N
0.1-0.5% C, 0.01-0.5% Si, 0.3-1.5% Mn
0.10% C, 0.01% Si, 0.41% Mn, 0.02% Ni, 0.03% Cr, 0.005% Al
0.10% C, 0.01% Si, 0.41% Mn, 0.02% Ni, 0.03% Cr, 0.005% V
0.10% C, 0.02% Si, 0.51% Mn, 0.005% P, 0.005% S, 2.20% Cr, 0.94% Mo, 0.30% V, 0.022% Ti, 0.0020% B
0.10% C, 0.10% Mn, 0.05% Si, 10.00% Ni, 8.00% Co, 2.00% Cr, 1.00% Mo
0.10% C, 0.10% Mn, 0.05% Si, 10.00% Ni, 8.00% Co, 2.00% Cr, 1.00% Mo
0.10% C, 0.16% Si, 0.40% Mn, 0.017% S, 0.008% P, 0.22% Ni, 2.25% Cr, 0.91% Mo, 0.10% Cu, 0.017% Al, 0.009% Sn, 0.01% Pb, 0.002% Ti, 0.015% V
0.10% C, 0.16% Si, 1.38% Mn, 0.019% Ni, 0.017% Cr, 0.003% Mo, 0.013% Cu, 0.024% Al, 0.002% Sn, 0.005% Nb, 0.003% Ti, 0.003% V, 0.0003% B, 0.0005% Ca, 0.019% P, 0.011% S, 0.0056% N, 0.0042% O. High Si steel: 0.105% C, 1.40% Si, 1.35% Mn, 0.022% Ni, 0.017% Cr, 0.014% Mo, 0.026% Cu, 0.026% Al, 0.002% Sn, 0.005% Nb, 0.004% Ti, 0.003% V, 0.0003% B, 0.0005% Ca, 0.017% P, 0.011% S, 0.0038% N, 0.0041% O
0.10% C, 0.18% Si, 0.65% Mn, 3.58% Ni, 0.35% Cr, 0.44% Mo
0.10% C, 0.18% Si, 0.65% Mn, 3.58% Ni, 0.35% Cr, 0.44% Mo
0.10% C, 0.19% Si, 0.41% Mn, 2.50% Ni, 1.01% Cr, 0.29% Mo, 0.005% Al
0.10% C, 0.19% Si, 0.41% Mn, 2.50% Ni, 1.01% Cr, 0.29% Mo, 0.005% Al
0.10% C, 0.19% Si, 0.41% Mn, 2.50% Ni, 1.01% Cr, 0.29% Mo, 0.005% Al
0.10% C, 0.20% Si, 0.34% Mn, 3.51% Ni, 1.66% Cr
0.10% C, 0.20% Si, 0.42% Mn, 2.94% Ni, 1.45% Cr, 0.40% Mo
0.10% C, 0.20% Si, 0.42% Mn, 2.94% Ni, 1.45% Cr, 0.40% Mo
0.10% C, 0.21% Si, 0.52% Mn, 0.002% P, 0.005% S, 0.55% Mo, 0.0007% N, 0.050% Al, 0.0063% B
0.10% C, 0.23% Si, 0.35% Mn, 1.00% Cr
0.10% C, 0.23% Si, 0.35% Mn, 1.00% Cr
0.10% C, 0.23% Si, 0.35% Mn, 1.97% Cr
0.10% C, 0.23% Si, 0.35% Mn, 1.97% Cr
0.10% C, 0.23% Si, 0.41% Mn, 0.0016% B
0.10% C, 0.23% Si, 0.41% Mn, 0.0016% B
0.10% C, 0.23% Si, 0.60% Mn, 2.65% Ni, 0.47% Cr, 0.45% Mo
0.10% C, 0.23% Si, 0.60% Mn, 2.65% Ni, 0.47% Cr, 0.45% Mo
0.10% C, 0.24% Si, 0.60% Mn, 3.51% Cr
0.10% C, 0.24% Si, 0.60% Mn, 3.51% Ni
0.10% C, 0.25% Si, 0.60% Mn, 0.00% Cr, 9.00% Ni
0.10% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 1.45% Ni
0.10% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 1.45% Ni
0.10% C, 0.28% Si, 0.40% Mn, 0.022% P, 0.007% S, 5.39% Cr, 0.51% Mo, 0.08% Ni, 0.16% Cu, 0.0250% N
0.10% C, 0.28% Si, 0.57% Mn, 2.54% Ni, 0.79% Cr, 0.45% Mo
0.10% C, 0.28% Si, 0.57% Mn, 2.54% Ni, 0.79% Cr, 0.45% Mo
0.10% C, 0.32% Si, 0.38% Mn, 0.020% P, 0.019% S, 0.15% Cr, 0.05% Mo, 3.46% Ni, 0.08% Cu, 0.028% Al
0.10% C, 0.33% Mn, 0.026% Si, 0.005% S, 0.010% P 3.02% Ni, 0.68% Cr, 0.19% Mo, 0.14% Cu
0.10% C, 0.34% Mn, 0.20% Si, 3.51% Ni, 1.66% Cr, 0.06% Mo.
0.10% C, 0.34% Si, 0.47% Mn, 0.019% P, 0.025% S, 11.58% Cr, 0.60% Mo, 0.64% Ni
0.10% C, 0.35% Mn, 1.00% Si, 1.00% Cr, 2.00% Ni, 3.25% Mo, 2.00% Cu, 0.10% V
0.10% C, 0.35% Si, 0.50% Mn, 2.25% Cr, 1.00% Mo
0.10% C, 0.35% Si, 0.50% Mn, 2.25% Cr, 1.00% Mo
0.10% C, 0.35% Si, 0.78% Mn, 1.29% Ni, 0.44% Cr, 0.29% Mo, 0.022% Al
0.10% C, 0.35% Si, 0.78% Mn, 1.29% Ni, 0.44% Cr, 0.29% Mo, 0.022% Al
0.10% C, 0.38% Mn, 0.62% Si, 0.013% P, 0.012% S, 0.17% Ni, 1.15% Cr, 0.48% Mo, 0.10% Cu
0.10% C, 0.39% Si, 0.97% Mn, 0.14% Ni, 0.50% Cr, 0.33% Mo, 0.010% Al
0.10% C, 0.39% Si, 0.97% Mn, 0.14% Ni, 0.50% Cr
0.10% C, 0.40% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.20% Mo, 5.00% Ni
0.10% C, 0.40% Mn, 0.20% Si, 0.020% P, 0.020% S, 4.80% Ni
0.10% C, 0.40% Mn, 0.30% Si, <0.005% P, <0.015% S, 4.00% Ni, 17.00% Cr, 0.005% N
0.10% C, 0.42% Mn, 0.25% Si, 0.018% P, 0.013% S, 0.27% Ni, 2.16% Cr, 0.96% Mo, 0.10% Cu
0.10% C, 0.42% Mn, 0.25% Si, 0.018% P, 0.013% S, 0.27% Ni, 2.16% Cr, 0.96% Mo
0.10% C, 0.42% Si, 0.49% Mn, 4.73% Cr, 0.50% Mo, 0.16% Ni, 0.07% Cu, 0.010% Al, 0.0140% N
0.10% C, 0.46% Mn, 0.33% Si, 0.011% S, 0.025% P 5.00% Ni, 0.23% Cr, 0.04% Mo, 0.14% Cu
0.10% C, 0.46% Mn, 0.33% Si, 0.011% S, 0.025% P 5.00% Ni, 0.23% Cr, 0.04% Mo, 0.14% Cu
0.10% C, 0.48% Mn, 0.55% Si, 0.024% P, 0.011% S, 0.51% Ni, 13.30% Cr, 8.00% Co
0.10% C, 0.49% Mn, 0.24% Si, 0.013% P, 0.013% S, 2.43% Cr, 1.06% Mo, 0.01% V, 0.012% N
0.10% C, 0.49% Si, 0.46% Mn, 0.085% P, 8.36% Cr, 0.97% Mo
0.10% C, 0.50% Mn, 0.25% Si, 12.00% Cr, 1.00% Mo, 0.28% V, 0.06% Nb, 1.00% W
0.10% C, 0.50% Mn, 0.26% Si, 0.017% P, 0.025% S, 2.95% Mo
0.10% C, 0.50% Mn, 0.30% Si, 1.50% Cr, 3.50% Ni
0.10% C, 0.50% Mn, 0.30% Si, 1.50% Cr, 3.50% Ni
0.10% C, 0.50% Mn, 0.50% Si, 0.015% S, 0.015% P, 58.00% Ni, 20.00-23.00% Cr, 8.00-10.0% Mo, 5.00% Fe, 1.00% Co, 0.40% Ti, 0.40% Al, 3.15-4.14% Nb+Ta
0.10% C, 0.52% Mn, 0.007% P, 0.016% S, 0.28% Si, 5.00% Ni, 0.07% Cr, 0.03% Mo
0.10% C, 0.52% Mn, 0.21% Si, 0.002% P, 0.005% S 0.0063% B, 0.050% Al, 0.0007% N
0.10% C, 0.52% Mn, 5.00% Cr
0.10% C, 0.52% Mn, 5.00% Ni
0.10% C, 0.52% Si, 1.49% Mn, 0.01% P, 0.009% S, 0.04% Cr, 0.01% Mo, 0.02% Ni, 0.06% Al
0.10% C, 0.53% Mn, 0.26% Si, 0.007% P, 0.005% S, 0.05% Cr, 3.65% Ni, 0.045% Al, 0.07% Cu
0.10% C, 0.54% Si, 1.27% Mn, 0.12% Ni, 0.14% Cr, 0.018% Al
0.10% C, 0.68% Mn, 0.32% Si, 0.29% Cr, 0.0038% B
0.10% C, 0.68% Si, 1.24% Mn, 0.04% Ni, 0.01% Mo, 1.87% Cr, 0.007% Al, 0.015% Ti, 274 ppm O, 168 ppm N
0.10% C, 0.70% Mn, 0.29% Si, 0.76% Cr, 0.0036% B
0.10% C, 0.71% Mn, 0.28% Si, 0.33% Ni, 0.004% B
0.10% C, 0.71% Mn, 0.29% Si, 0.54% Mo
0.10% C, 0.71% Mn, 0.32% Si, 0.70% Cr, 0.0060% B, 0.51% Mo
0.10% C, 0.72% Mn, 0.29% Si, 1.43% Cr, 0.0059% B
0.10% C, 0.72% Mn, 0.33% Si, 1.43% Cr, 0.0064% B, 1.03% Mo
0.10% C, 0.72% Mn, 0.33% Si, 1.43% Ni, 0.26% Mo, 0.0053% B
0.10% C, 0.74% Mn, 0.29% Si
0.10% C, 0.75% Si, 0.77% Mn, 0.023% P, 0.024% S, 6.37% Cr, 0.12% Mo, 0.30% Ni, 0.92% Al
0.10% C, 0.76% Mn, 0.22% Si, 0.007% S, 0.012% P, 0.68% Cr, 0.85% Ni, 0.48% Mo, 0.07% V, 0.001% B, 0.21% Cu
0.10% C, 0.77% Mn, 0.010% P, 0.024% S, 0.28% Si, 8.56% Ni, 0.05% Cr, 0.02% Mo
0.10% C, 0.77% Mn, 0.28% Si, 0.56% Ni, 0.05% Cr 0.02% Mo
0.10% C, 0.87% Mn, 0.33% Si, 0.24% Mo, 0.002% B, 0.005% N, 0.048% Zr
0.10% C, 0.87% Mn, 0.33% Si, 0.24% Mo, 0.002% B, 0.005% N, 0.048% Zr
0.10% C, 0.88% Mn, 0.34% Si, 0.39% Mo, 0.003% B, 0.005% N, 0.046% Zr
0.10% C, 0.88% Mn, 0.34% Si, 0.39% Mo, 0.003% B, 0.005% N, 0.046% Zr
0.10% C, 0.88% Mn, 0.35% Si, 0.66% Mo, 0.003% B, 0.005% N, 0.044% Zr
0.10% C, 0.88% Mn, 0.35% Si, 0.66% Mo, 0.003% B, 0.005% N, 0.044% Zr
0.10% C, 1.00% Mn, 3.00% Cr, 1.50% Mo, 0.10% Ni, 0.10% V
0.10% C, 1.10% Mn, 0.20% Si, 0.020% P, 0.25% S
0.10% C, 1.2% Si, 1.6% Mn, <0.006% P
0.10% C, 1.46% Mn, 0.34% Si, 0.0051% B, 0.26% Mo
0.10% C, 1.48% Mn, 0.36% Si, 0.008% S, 0.014% P, 0.19% V, 0.003% Ti, 0.023% Nb, 0.046% Al
0.10% C, 1.50% Mn, 0.37% Si, 0.007% S, 0.011% P, 0.022% V, 0.023% Ti, 0.023% Nb, 0.044% Al
0.10% C, 1.51% Mn, 0.44% Si, 0.008% S, 0.033% P, 0.05% V, 0.013% Ti, 0.002% Nb, 0.033% Al
0.10% C, 1.53% Mn, 0.35% Si, 0.010% S, 0.013% P, 0.01% Mo, 0.07% V, 0.05% Nb, 0.045% Al, 0.007% N
0.10% C, 1.54% Mn, 0.0035% Si, 0.0015% P, 0.0012% S, 0.04% Nb, 0.0003% O
0.10% C, 1.54% Mn, 0.0035% Si, 0.0015% P, 0.0012% S, 0.04% Nb, 0.0003% O
0.10% C, 1.63% Mn, 0.41% Mo
0.10% C, 12.40% Cr
0.10% C, 13.00% Cr
0.10% C, 2.00% Mn, 1.09% Si, 0.005% S, 0.012% P, 1.80% Cr, 0.65% Mo, 0.15% V
0.10% C, 6.00% Mn, 0.50% Si, 9.60% Ni, 15.25% Cr, 1.02% Mo, 0.30% V, 1.10% Nb, 0.0066% B
0.10% C, 9.11% Ni
0.10% C, 9.11% Ni
0.10% C, max. 0.50% Si, max. 0.50% Mn, max. 0.015% P, max. 0.40% Al, 20.00-23.00% Cr, 8.00-10.00% Mo, max. 5.00% Fe, max. 0.40% Ti, 3.15-4.15% Nb/Ta, rest Ni.
0.10-0.11% C, 0.14-0.28% Si, 0.75-0.96% Mn, 0.004-0.005% S, 0.003-0.007% P, 10.3-10.37% Cr, 0.62-0.68% Ni, 0.56-0.61% Mo, 0.19-0.21% V, 0.14-0.16% Nb, 0.004-0.012% Al, 0.0072-0.0089% B, 0.027-0.032% N, 0.005-0.010% Co, 0.007-0.015% Cu, 0.007-0.028% Zr, 0.008-0.010% As, 0.0002-0.0004% Sb, 0.001% Sn. MANET-I: 0.13% C, 0.37% Si, 0.82% Mn, 0.004% S, 0.005% P, 10.6% Cr, 0.87% Ni, 0.77% Mo, 0.22% V, 0.16% Nb, 0.054% Al, 0.0075% B, 0.02% N, 0.01% Co, 0.015% Cu, 0.053% Zr
0.10-0.14% C, 0.40-0.60% Si, 0.15-0.45% Mn, 11.0-12.0% Cr, 0.10-0.40% Ni, 0.20-0.40% Mo, 0.20-0.30% V, 1.30-1.70% W, 0.03-0.08% Nb, 1.4-1.8% Co, 0.030-0.070% N, 0.0030-0.0060% B, max. 0.020% Al
0.10-0.15% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.020% S, 0.30-0.60% Cr, 0.50-0.70% Mo, msx. 0.30% Ni, 0.22-0.28% V, max. 0.30% Cu, max. 0.040% Al
0.10-0.17% C, <1.00% Si, <1.00% Mn, 15.50-17.50% Cr, Mo+S
0.10-0.17% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 0.65-0.85% Cr, 1.35-1.50% Ni
0.10-0.17% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 0.65-0.85% Cr, 1.35-1.50% Ni
0.10-0.18% C, 0.10-0.35% Si, 0.40-0.70% Si, max. 0.030% P, max. 0.035% S, 0.30-0.60% Cr, 0.50-0.70% Mo, 0.22-0.32% V
0.10-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.10-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.10-0.25% C, max. 1.00% Si, max. 1.00% Mn, max. 0.035% P, max. 0.035% S, 15.50-18.00% Cr, 1.00-2.50% Ni
0.10-1.15% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 1.20% Cr, 0.25% Mo, 0.25% Cu
0.1C, 0.1C-Mo, 0.1C-Cr, 0.1C-Mo-Cr. See the table 1.
0.10-0.15% C, 0.30-0.60% Mn, max. 0.04% P, max. 0.05% S
0.10% C, 0.34% Mn, 0.24% Mn, 0.014% P, 0.002% S, 8.35% Cr, 0.14% Ni, 0.907% Mo, 0.16% Cu, 0.012% Al, 0.215% V, 0.074% Nb, 0.004% Ti, 0.066% N, 0.024% Co, 0.002% W, 0.0002% B
0.10% C, 0.48% Mn, 0.21% Si, 0.016% P, 0.005% S, 8.96% Cr, 0.13% Ni, 0.36% Mo, 0.11% Cu, 0.018% Al, 0.18% V, 0.047% Nb, 0.003% Ti, 0.0435% N, 0.0437% Nb, 2.18% W, 0.0022% B
0.10% C, 0.58 Mn, 0.36% Si, 0.009% P, 0.002% S, 2.30% Cr, 0.18% Ni, 1.051% Mo, 0.19% Cu, 0.262% V, 0.0068% Nb, 0.081% Ti, 0.0082% N, 0.015% Co, 0.004% W, 0.004% B
0.1% C, 0.5% Si, 0.5% Mn, 2-2.5% Cr, 0.9-1.2% Mo
0.10-0.20% C, max. 1.00% Mn, 0.90-1.20% Si, 0.80-1.20% Cr, 2.30-2.70% Ni, 1.70-2.20% Mo, max. 0.50% V
0.10% C, 1.08% Si, 1.55% Mn, 0.020% P, 0.028% S, 0.20% Cu, 0.08% Cr, 0.07% Ni, 0.005% Al, 0.005% N
0.10% C, 0.41% Si, 1.32% Mn, 0.035% P, 0.028% S, 0.24% Cu, 0.16% Cr, 0.39% Ni, 0.14% Mo, 0.01% Ti, 0.017% Al, 0.07% V
0.10% C, 0.42% Si, 1.67% Mn, 0.026% P, 0.010% S, 0.05% Cu, 0.05% Cr, 0.03% Ni, 0.046% Nb, 0.028% Al, 0.01% V
0.10% C, 1.01% Si, 0.86% Mn, 0.018% P, 0.033% S, 0.77% Cr, 0.64% Ni, 0.50% Cu, 0.004% As
0.10% C, 0.36% Si, 0.33% Mn, 0.065% P, 0.033% S, 0.36% Cu, 0.52% Cr, 0.02% Ni, 0.016% Al, 0.01% N, 0.20% V
0.10% C, 0.42% Si, 0.84% Mn, 0.018% P, 0.023% S, 0.18% Cu, 0.05% Cr, 0.09% Ni, 0.23% Mo, 0.04% Ti, 0.01% V
0.10% C, 0.48% Si, 0.81% Mn, 0.019% P, 0.024% S, 0.16% Cu, 0.04% Cr, 0.09% Ni, 0.66% Mo, 0.04% Ti, 0.01% V
0.10% C, 0.65% Si, 1.17% Mn, 0.01% P, 0.02% S, 0.003% Al, 0.03% Cr, 0.04% Ni, 0.11% Cu, 0.01% Mo
0.10% C, 0.72% Si, 2.02% Mn, 0.02% P, 0.015% S, 0.018% Al, 0.04% Cr, 2.08% Ni, 0.020% Cu, 0.60% Mo
0.10% C, 0.54% Si, 1.42% Mn, 0.045% Cr, 1.20% Ni, 0.347% Mo
0.1030% C, 0.0178% Si, 0.4830% Mn, 0.0083% P, 0.0061% S, 0.0362% Cu, 0.0124% Mo, 0.0003% V, 0.0456% Ni, 0.0011% Nb, 0.0392% Al, 0.0009% Ti, 0.0079% W, 0.0066% Co, 0.0005% B
0.1030% C, 0.0178% Si, 0.4830% Mn, 0.083% P, 0.061% S, 0.0362% Cu, 0.0505% Cr, 0.0124% Mo, 0.0003% V, 0.0456% Ni, 0.0011% Nb, 0.0392% Al, 0.0009% Ti, 0.0079% W, 0.0066% Co, 0.0005% B
0.105% C, 0.0035% Si, 0.0015% P, 0.003% S, 0.0005% O
0.105% C, 1.53% Mn, 0.0035% Si, 0.0015% P, 0.003% S, 0.0005% O
0.105% C, 16.8% Cr, 6.36% Ni, 0.95% Si, 1.20% Mn, 0.3% Cu, 0.065% N
0.106% C, 0.45% Mn, 8.96% Cr, 0.47% Mo, 0.20% V, 0.069% Nb, 1.83% W
0.106% C, 8.96% Si, 0.47% Mo, 0.051% N, 0.069% Nb, 0.20% V, 1.83% W
0.11% C, 0.02% Si, 0.61% Mn, 0.02% Ni, 0.03% Cr, 0.005% Al
0.11% C, 0.02% Si, 0.61% Mn, 0.02% Ni, 0.03% Cr, 0.005% V
0.11% C, 0.13% Si, 0.38% Mn, 0.016% S, 0.023% P, 3.26% Ni, 0.87% Cr, 0.08% Mo
0.11% C, 0.13% Si, 0.38% Mn, 0.016% S, 0.023% P, 3.26% Ni, 0.87% Cr, 0.08% Mo
0.11% C, 0.17% Si, 1.24% Mn, 0.21% Ni, 0.18% Cr, 0.15% Mo, 0.029% Al
0.11% C, 0.17% Si, 1.24% Mn, 0.21% Ni, 0.18% Cr, 0.15% Mo, 0.029% Al
0.11% C, 0.20% Si, 0.46% Mn
0.11% C, 0.21% Mn
0.11% C, 0.21% Si, 0.36% Mn, 0.028% S, 0.010% P, 2.89% Ni, 0.28% Cr, 0.09% Mo
0.11% C, 0.21% Si, 0.47% Mn, 0.010% P, 0.010% S, 2.29% Cr, 1.02% Mo, 0.14% Ni, 0.010% V, 0.18% Cu
0.11% C, 0.21% Si, 0.47% Mn, 0.010% P, 0.010% S, 2.29% Cr, 1.02% Mo, 0.14% Ni, 0.010% V, 0.18% Cu
0.11% C, 0.21% Si, 1.06% Mn
0.11% C, 0.21% Si, 1.06% Mn
0.11% C, 0.21% Si
0.11% C, 0.22% Si, 0.35% Mn, 0.47% Cr
0.11% C, 0.22% Si, 0.35% Mn, 0.47% Cr
0.11% C, 0.22% Si, 0.37% Mn, 1.66% Mo
0.11% C, 0.22% Si, 0.46% Mn
0.11% C, 0.22% Si, 0.50% Mn, 0.002% P, 0.007% S, 0.56% Mo, 0.002% N, 0.003% Al
0.11% C, 0.23% Si, 0.35% Mn, 0.10% Ti
0.11% C, 0.23% Si, 0.35% Mn, 0.10% Ti
0.11% C, 0.23% Si, 0.37% Mn, 1.66% Mo
0.11% C, 0.23% Si, 0.40% Mn
0.11% C, 0.23% Si, 0.40% Mn
0.11% C, 0.23% Si, 0.41% Mn, 0.10% V
0.11% C, 0.23% Si, 0.41% Mn, 0.10% V
0.11% C, 0.23% Si, 0.42% Mn, 0.087% Al
0.11% C, 0.23% Si, 0.42% Mn, 0.087% Al
0.11% C, 0.23% Si, 0.42% Mn, 0.095% Nb
0.11% C, 0.23% Si, 0.42% Mn, 0.095% Nb
0.11% C, 0.23% Si, 0.43% Mn, 0.96% Mo
0.11% C, 0.23% Si, 0.43% Mn, 0.96% Mo
0.11% C, 0.25% Si, 0.59% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.74% Mo
0.11% C, 0.25% Si, 0.62% Mn, 3.40% Ni, 1.43% Cr, 0.42% Mo
0.11% C, 0.25% Si, 0.62% Mn, 3.40% Ni, 1.43% Cr, 0.42% Mo
0.11% C, 0.28% Si, 0.97% Mn, 3.47% Ni, 1.50% Cr, 0.38% Mo
0.11% C, 0.28% Si, 0.97% Mn, 3.47% Ni, 1.50% Cr, 0.38% Mo
0.11% C, 0.29% Si, 0.53% Mn, 0.01% P, 0.01% S, 1.09% Cr, 0.4% Mo
0.11% C, 0.29% Si, 0.53% Mn, 0.01% P, 0.01% S, 1.09% Cr, 0.44% Mo
0.11% C, 0.29% Si, 1.47% Mn, 0.035% Al, 0.027% Nb
0.11% C, 0.29% Si, 1.47% Mn, 0.035%% Al, 0.027% Nb
0.11% C, 0.31% Si, 0.40% Mn, 0.025% P, 2.25% Cr, 0.90% Mo
0.11% C, 0.31% Si, 0.49% Mn, 2.03% Ni, 1.25% Cr, 0.37% Mo, 0.035% Al
0.11% C, 0.31% Si, 0.49% Mn, 2.03% Ni, 1.25% Cr, 0.37% Mo, 0.035% Al
0.11% C, 0.31% Si, 0.53% Mn, 0.013% P, 0.013% S, 2.43% Cr, 1.00% Mo, 0.25% V, 0.010% B, 0.010% Al
0.11% C, 0.32% Si, 0.46% Mn, 3.38% Ni, 0.98% Cr, 0.29% Mo
0.11% C, 0.32% Si, 0.46% Mn, 3.38% Ni, 0.98% Cr, 0.29% Mo
0.11% C, 0.32% Si, 0.47% Mn, 0.014% P, 0.003% S, 8.50% Cr, 0.85% Mo, 0.13% Ni, 0.22% V, 0.076% Nb, 0.038% N, 0.018% Al
0.11% C, 0.32% Si, 0.47% Mn, 0.014% P, 0.0030% S, 0.038% N, 0.018% Al, 8.50% Cr, 0.13% Ni, 0.85% Mo, 0.22% V, 0.076% Nb
0.11% C, 0.34% Si, 1.21% Mn, 0.012% P, 0.015% S, 0.45% Ni, 0.20% Cr, 0.15% Mo, 0.19% Cu
0.11% C, 0.34% Si, 1.21% Mn, 0.45% Ni, 0.20% Cr, 0.15% Mo
0.11% C, 0.34% Si, 1.51% Mn, 0.003% S, 0.029% Nb
0.11% C, 0.34% So, 1.21% Mn, 0.45% Ni, 0.20% Cr, 0.15% Mo
0.11% C, 0.36% Mn, 0.21% Si, 2.89% Ni, 0.28% Cr 0.09% Mo
0.11% C, 0.36% Mn, 0.21% Si, 2.89% Ni, 0.28% Cr 0.09% Mo
0.11% C, 0.37% Si, 0.44% Mn, 0.16% Ni, 12.18% Cr
0.11% C, 0.37% Si, 0.44% Mn, 0.16% Ni, 12.20% Cr
0.11% C, 0.37% Si, 1.34% Mn, 0.47% Ni, 0.27% Cr, 0.10% V, 0.017% Al
0.11% C, 0.37% Si, 1.34% Mn, 0.47% Ni, 0.27% Cr, 0.10% V, 0.017% Al
0.11% C, 0.38% Mn, 0.09% Si, 4.15% Ni, 1.33% Cr 0.07% Mo
0.11% C, 0.38% Mn, 0.09% Si, 4.15% Ni, 1.33% Cr 0.07% Mo
0.11% C, 0.38% Mn, 0.13% Si, 3.26% Ni, 0.87% Cr 0.08% Mo
0.11% C, 0.38% Mn, 0.13% Si, 3.26% Ni, 0.87% Cr 0.08% Mo
0.11% C, 0.38% Mn, 0.33% Si, <0.005% P, <0.015% S, 7.25% Ni, 15.60% Cr, 0.005% N
0.11% C, 0.38% Mn, 0.44% Si, 5.46% Cr, 0.42% Mo
0.11% C, 0.38% Si, 0.99% Mn, 0.86% Ni, 0.54% Cr, 0.30% Mo
0.11% C, 0.38% Si, 0.99% Mn, 0.86% Ni, 0.54% Cr, 0.30% Mo
0.11% C, 0.38% Si, 1.06% Mn, 0.44% Cr, 0.48% Mo, 0.12% V
0.11% C, 0.38% Si, 1.06% Mn, 0.44% Cr, 0.48% Mo, 0.12% V
0.11% C, 0.40% Si, 1.60% Mn, 0.13% Ti, 0.08% Nb, 0.001% Al, 0.001% N
0.11% C, 0.41% Mn, 0.43% Si, 0.012% P, 0.012% S, 0.25% Ni, 2.10% Cr, 1.02% Mo
0.11% C, 0.41% Si, 0.38% Mn, 8.80% Cr, 0.17% Ni, 1.00% Mo, 0.25% V, 0.07% Nb
0.11% C, 0.42% Si, 1.12% Mn, 0.47% Ni, 0.27% Cr, 0.16% Mo, 0.13% V, 0.047% Al, 0.015% Ti
0.11% C, 0.42% Si, 1.12% Mn, 0.47% Ni, 0.27% Cr, 0.16% Mo, 0.13% V, 0.047% Al, 0.015% Ti
0.11% C, 0.44% Mn, 0.22% Si, 0.007% S, 0.010% P 3.47% Ni, 0.10% Cr, 0.04% Mo, 0.15% Cu, 0.007% Al
0.11% C, 0.44% Mn, 0.22% Si, 0.007% S, 0.010% P 3.47% Ni, 0.10% Cr, 0.04% Mo, 0.15% Cu, 0.007% Al
0.11% C, 0.44% Mn, 0.37% Si, 0.16% Ni, 12.18% Cr
0.11% C, 0.44% Si, 0.38% Mn, 5.46% Cr, 0.42% Mo
0.11% C, 0.45% Mn, 0.017% P, 0.009% S, 0.18% Si, 3.33% Ni, 1.52% Cr, 0.03% Mo
0.11% C, 0.45% Mn, 0.018% P, 0.005% Si, 0.022% Ni, 0.02% Cr, 0.038% Al
0.11% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.11% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.11% C, 0.45% Si, 0.49% Mn, 0.005% S, 0.012% P, 0.13% Ni, 12.00% Cr, 0.20% Mo
0.11% C, 0.46% Mn, 0.21% Si, 0.060% S, 0.020% P 2.18% Cr, 0.31% Mo, 0.485% Al
0.11% C, 0.46% Mn
0.11% C, 0.46% Mn
0.11% C, 0.47% Mn, 0.24% Si, 0.015% S, 0.016% P 0.23% Ni, 4.48% Cr, 0.52% Mo, 0.15% Cu
0.11% C, 0.47% Mn, 0.24% Si, 0.015% S, 0.016% P 0.23% Ni, 4.48% Cr, 0.52% Mo, 0.15% Cu
0.11% C, 0.48% Si, 1.20% Mn, 0.08% Ni, 0.05% Cr, 0.001% Al
0.11% C, 0.48% Si, 1.20% Mn, 0.08% Ni, 0.05% Cr, 0.001% Al
0.11% C, 0.49% Mn, 0.10% Si, 0.016% P, 0.013% S, 0.48% Ni, 12.80% Cr
0.11% C, 0.49% Mn, 0.45% Si, 0.050% S, 0.012% P 0.13% Ni, 12.00% Cr, 0.02% Mo, 0.07% Cu, 0.020% V, 0.06% W
0.11% C, 0.50% Mn, 0.22% Si, 0.002% P, 0.007% S 0.56% Mo, 0.003% Al, 0.002% N
0.11% C, 0.50% Mn, 0.30% Si, 0.005% S, 0.017% P 1.59% Ni, 0.64% Cr, <0.10% Mo, 0.31% Cu, <0.03% V
0.11% C, 0.50% Mn, 0.30% Si, 0.005% S, 0.017% P 1.59% Ni, 0.64% Cr, <0.10% Mo, 0.31% Cu, <0.03% V
0.11% C, 0.50% Mn, 10.22% Cr, 1.42% Mo, 0.55% Ni, 0.20% V, 0.50% Nb
0.11% C, 0.52% Mn, 0.26% Si, 0.012% S, 0.007% P, 0.56% Cr, 4.92% Ni, 0.53% Mo, 0.08% V, 0.10% Cu, 0.04% Al
0.11% C, 0.53% Mn, 0.35% Si, 0.010% S, 0.015% P, 2.28% Cr, 0.04% Ni, 1.00% Mo, 0.20% V, 0.03% Nb, 0.03% Cu, sol. 0.010% Al
0.11% C, 0.53% Si, 0.49% Mn, 0.017% S, 0.098% P, 0.20% Ni, 0.60% Cr, 0.27% Cu, 0.41% Mo
0.11% C, 0.53% Si, 0.49% Mn, 0.017% S, 0.098% P, 0.20% Ni, 0.60% Cr, 0.27% Cu, 0.41% Mo
0.11% C, 0.56% Mn, 0.28% Si, 0.005% S, 0.017% P, 1.08% Cr, 0.04% Ni, 0.31% Mo, 0.22% V, 0.03% Cu, sol. 0.01% Al
0.11% C, 0.56% Mn, 0.30% Si, 0.015% P, 0.015% S, 0.07% Ni, 0.84% Cr, 0.48% Mo, 0.01% V, 0.002% Al, 0.011% N
0.11% C, 0.56% Si, 0.47% Mn
0.11% C, 0.56% Si, 0.47% Mn
0.11% C, 0.70% Mn, 0.35% Si, 0.28% Cr, 0.0045% B, 0.25% Mo
0.11% C, 0.70% Mn, 0.35% Si, 0.28% Cr, 0.0057% B, 0.50% Mo
0.11% C, 0.70% Mn, 3.19% Ni, 1.26% Cr, 0.11% Mo
0.11% C, 0.72% Mn, 0.31% Si, 3.03% Ni, 0.0052% B
0.11% C, 0.72% Mn, 0.32% Si, 0.75% Cr, 0.0052% B, 0.22% Mo
0.11% C, 0.73% Mn, 0.31% Si, 0.35% Ni, 0.0053% N, 0.53% Mo
0.11% C, 0.73% Mn, 0.32% Si, 3.06% Ni, 0.24% Mo, 0.0050% B
0.11% C, 0.74% Mn, 0.34% Si, 3.03% Ni, 0.55% Mo, 0.0057% B
0.11% C, 0.75% Mn, 0.31% Si, 0.34% Ni, 0.0047% N, 0.24% Mo
0.11% C, 0.75% Mn, 0.32% Si, 1.44% Cr, 0.0066% B, 0.56% Mo
0.11% C, 0.75% Mn, 0.33% Si, 1.46% Cr, 0.0059% B, 0.25% Mo
0.11% C, 0.85% Mn, 0.31% Si, 0.009% S, 0.007% P, 0.51% Cr, 1.30% Ni, 0.48% Mo, 0.03% V, 0.002% B, 0.27% Cu, sol. 0.077% Al
0.11% C, 0.85% Mn, 0.38% Si, 1.42% Ni, 0.76% Cr, 0.005% B, 0.54% Mo
0.11% C, 0.86% Mn, 0.36% Si, 1.44% Ni, 0.76% Cr, 0.005% B, 0.21% Mo
0.11% C, 0.87% Mn, 0.37% Si, 1.45% Ni, 0.77% Cr, 0.005% B
0.11% C, 1.07% Mn
0.11% C, 1.07% Ni
0.11% C, 1.16% Mn, 0.29% Si, 0.013% P, 0.011% S, 0.08% Mo, 0.10% Cu, 0.043% Ti, 0.0034% B, 0.0057% N, 0.020% O
0.11% C, 1.19% Si, 1.67% Mn, 0.013% P, 0.038% Al, 0.44% CE
0.11% C, 1.23% Mn, 0.31% Si, 0.018% S, 0.031% P, 0.08% V, 0.005% N
0.11% C, 1.23% Mn, 0.31% Si, 0.018% S, 0.031% P, 0.08% V, 0.005% N
0.11% C, 1.40% Mn, 0.55% Si, 0.063% V
0.11% C, 1.43% Mn, 0.35% Si, 0.0062% B, 0.52% Mo
0.11% C, 1.51% Mn, 0.34% Si, 0.003% S, 0.029% Nb
0.11% C, 1.58% Mn, 0.28% Si, 0.013% P, 0.009% S
0.11% C, 1.60% Mn, 0.30% Si, 0.002% S, 0.017% P, 0.09% V, 0.005% Ti, 0.032% Nb, sol. 0.021% Al
0.11% C, 1.73% Mn, 0.29% Si, 0.009% P, 0.010% S
0.11% C, 1.76% Mn, 0.70% Si, 0.02% P, 0.011% S, 19.75% Ni, 24.66% Cr, 0.31% Mo, 0.051% Al, 0.12% Cu, 0.0015% B, 0.005% Pb, 0.004% Sn
0.11% C, 1.99% Mn, 0.29% Si, 0.012% P, 0.009% S
0.11% C, 3.00% Mn, 0.16% Si, 1.70% Ni, 0.25% Mo
0.11% C, 3.49% Ni
0.11% C, 3.49% Ni
0.11-0.12% C, 0.04-0.06% Si, 0.42% Mn, 8.87-8.82% Cr, 0.19-0.20% V, 1.09-1.10% W(Mo), 0.14% Ta(Nb)
0.11-0.17% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.10-0.25% Mo, 3.0-3.50% Ni
0.11-0.17% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.10-0.25% Mo, 3.0-3.50% Ni
0.11-0.17% C, max. 0.25% Si, 0.80-1.00% Mn, max. 0.020% P, max. 0.015% S, 1.25-1.50% Cr, 0.80-1.00% Mo, 0.20-0.300% V
0.11-0.17% C, max. 0.25% Si, 0.80-1.00% Mn, max. 0.020% P, max. 0.015% S, 1.25-1.50% Cr, 0.80-1.00% Mo, 0.20-0.300% V
0.11% C, 1.20% Mn, 0.039% Al, 0.0084% N, Ti/N=2.02
0.11% C, 5.00% Ni, 0.55% Cr, 0.47% Mo, 0.075% V
0.11% C, 0.45% Mn, 0.22% Si, 0.007% P, 0.003% S, 2.02% Cr, 0.09% Ni, 0.96% Mo, 0.10% Cu, 0.018% Al, 0.007% V, 0.0014% Nb, 0.003% Ti, 0.0094% N, 0.014% Co, 0.004% W, 0.0002% B
0.11% C, 0.32% Si, 0.47% Mn, 0.014% P, 0.003% S, 8.50% Cr, 0.85% Mo, 0.13% Ni, 0.22% V, 0.076% Nb, 0.038% N, 0.018% Al
0.11% C, 2.1% Mn, 0.15% Si, 0.02% Nb
0.11% C, 0.05% Si, 0.001% S, 0.009% P, 0.49% Mn, 10.79% Cr, 0.75% Ni, 1.09% Mo, 0.007% Cu, 0.001% Al, 0.002% Sn, 0.004% Al, 0.17% V, 1.02% W, 0.005% Ti, 0.03% Nb, 0.056% N
0.11% C, 0.37% Si, 1.26% Mn, 0.016% P, 0.016% S, 0.15% Cu, 0.07% Cr, 0.06% Mo, 0.04% Nb, 0.055% Al
0.11% C, 0.46% Si, 1.60% Mn, 0.015% P, 0.012% S, 0.048% Al, 1.45% Cr, 0.42% Mo, 0.067% Nb, 0.18% Cu, 0.23% Ni, 0.047% Ti, 0.007% B, 0.02% V
0.11% C, 0.46% Si, 1.44% Mn, 0.017% S, 0.017% P, 0.04% Al, 1.37% Cr, 0.17% Cu, 0.41% Mo, 0.03% Ni, 0.08% Nb, 0.01% Ti
0.11% C, 0.45% Si, 1.60% Mn, 0.025% S, 0.016% P, 0.017% Al, 1.29% Cr, 0.17% Cu, 0.32% Mo, 0.05% Ni, 0.07% Nb, 0.05% Ti, 0.02% V
0.11% C, 0.25% Si, 0.46% Mn, 0.018% P, 0.016% S, 1.02% Cr, 0.29% Mo, 0.19% V
0.11% C, 0.28% Si, 0.96% Mn, 0.038% P, 0.025% S, 1.82% Cr, 0.51% Ni, 0.43% Mo, 0.10% V, 0.01% Ti, 0.055% Al, 0.07% Cu
0.11% C, 0.34% Si, 1.65% Mn, 0.018% P, 0.008% S, 0.065% Al, 0.032% Ni, 0.039% Cr, 0.015% Cu, 0.063% Nb, 0.012% Ti, 0.068% V
0.11% C, 0.51% Si, 0.89% Mn, 0.020% P, 0.023% S, 0.07% Cr, 0.10% Ni, 0.02% Mo, 0.05% Ti, 0.009% Al, 0.01% V
0.11% C, 0.42% Si, 1.55% Mn, 0.020% P, 0.021% S, 0.19% Cu, 0.07% Cr, 0.12% Ni, 0.03% Mo, 0.004% Al, 0.01% V
0.11% C, 0.46% Si, 0.83% Mn, 0.020% P, 0.024% S, 0.27% Cr, 0.33% Ni, 0.02% Mo, 0.04% Ti, 0.007% Al, 0.02% V
0.11% C, 0.51% Si, 1.04% Mn, 0.020% P, 0.024% S, 0.44% Cr, 0.11% Ni, 0.03% Mo, 0.05% Ti, 0.016% Al, 0.02% V
0.11% C, 0.57% Si, 0.95% Mn, 0.019% P, 0.026% S, 0.86% Cr, 0.10% Ni, 0.02% Mo, 0.06% Ti, 0.018% Al, 0.02% V
0.11% C, 0.40% Si, 0.93% Mn, 0.021% P, 0.015% S, 1.02% Cr, 0.06% Ni, 0.37% Mo
0.11% C, 0.68% Si, 1.24% Mn, 0.01% P, 0.02% S, 0.003% Al, 0.04% Cr, 0.04% Ni, 0.13% Cu, 0.01% Mo
0.11% C, 0.70% Si, 1.27% Mn, 0.01% P, 0.01% S, 0.01% Al, 0.03% Cr, 0.05% Ni, 0.13% Cu, 0.01% Mo
0.11% C, 0.70% Si, 1.27% Mn, 0.01% P, 0.01% S, 0.01% Al, 0.03% Cr, 0.05% Ni, 0.13% Cu, 0.01% Mo
0.115% C, 0.20% Si, 0.51% Mn, 0.017% P, 0.002% S, 0.007% Al, 8.85% Cr, 0.24% Ni, 0.94% Mo, 0.22% V, 0.95% W, 0.084% N, 0.069% Nb
0.115% C, 0.20% Si, 0.51% Mn, 0.017% P, 0.002% S, 0.07% Al, 8.85% Cr, 0.24% Ni, 0.94% Mo, 0.22% V, 0.95% W, 0.084% N, 0.069% N
0.117% C, 0.223% Si, 0.954% Mn, 0.005% P, 0.15% S, 0.041% Cr, 0.583% Mo, 1.97% Ni, 0.048% Cu, 0.014% Al, 0.02% N
0.118% C, 0.226% Si, 1.476% Mn, 0.010% P, 0.002% S, 0.505% Cr, 0.930% Ni, 0.449% Mo, 0.005% V, 0.108% Cu, 0.001% Nb, 0.002% Ti, 0.023% Al, 0.006% N 0.12% C, 0.02% Mn, 0.02% Mo, 0.46% V, 0.002% N
0.12% C, 0.03% Si, 0.48% Mn, 8.96% Cr, 0.18% V, 0.06% Ni, 1.04% W, 0.15% Ta, 0.022% N
0.12% C, 0.08% Si, 0.50% Mn, 3.00% Cr, 1.00% Mo, 0.25% V, 0.020% Ti, 0.0020% B
0.12% C, 0.096% Si, 0.36% Mn, 0.0054% P, 0.0034% S, 2.40% Cr, 3.64% Ni, 0.60% Mo, 0.016% Al
0.12% C, 0.16% Si, 0.45% Mn, 0.48% Mo
0.12% C, 0.16% Si, 0.45% Mn, 0.48% Mo
0.12% C, 0.16% Si, 0.50% Mn, 0.010% S, 0.004% P, 0.0005% N
0.12% C, 0.16% Si, 0.70% Mn, 0.02% P, 0.01% S, 0.60% Cr, 0.65% Mo, 0.03% Al, below 0.010% Ti
0.12% C, 0.17% Si, 0.47% Mn, 0.016% P, 0.003% S, 8.62% Cr, 0.94% Mo, 0.93% W, 0.20% V, 0.0018% B, 0.067% N, 0.08% Nb, 0.007% Al
0.12% C, 0.20% Si, 0.77% Mn, 0.84% Ni, 0.71% Cr, 0.47% Mo, 0.09% V, 0.015% Al, 0.002% B
0.12% C, 0.20% Si, 0.77% Mn, 0.84% Ni, 0.71% Cr, 0.47% Mo, 0.090% V, 0.015% Al, 0.002% B
0.12% C, 0.21% Si, 2.05% Mn
0.12% C, 0.21% Si, 2.05% Mn
0.12% C, 0.22% Si, 0.60% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.49% Mo
0.12% C, 0.23% Si, 0.36% Mn, 1.94% Cr, 1.32% Mo
0.12% C, 0.23% Si, 0.36% Mn, 1.94% Cr, 1.32% Mo
0.12% C, 0.25% Si, 0.40% Mn, 0.00% Cr, 4.90% Ni
0.12% C, 0.25% Si, 0.45% Mn, 0.00% Cr, 3.50% Ni
0.12% C, 0.25% Si, 0.46% Mn, 0.04% Ni, 0.64% Cr, 0.51% Mo, 0.006% Al
0.12% C, 0.25% Si, 0.48% Mn, 0.04% Ni, 0.64% Cr, 0.51% Mo, 0.006% Al
0.12% C, 0.25% Si, 0.50% Mn, 2.15% Cr, 1.00% Mo
0.12% C, 0.25% Si, 0.50% Mn, 2.15% Cr, 1.00% Mo
0.12% C, 0.25% Si, 0.63% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.31% Mo
0.12% C, 0.26% Si, 0.46% Mn, 0.08% Ni, 2.00% Cr, 0.96% Mo, 0.08% V, 0.014% Al
0.12% C, 0.26% Si, 0.48% Mn, 0.08% Ni, 2.00% Cr, 0.96% Mo, 0.080% V, 0.014% Al
0.12% C, 0.26% Si, 0.65% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.008% Mo
0.12% C, 0.26% Si, 0.86% Mn, 0.85% Ni, 0.53% Cr, 0.54% Mo, 0.05% V, 0.050% Al, 0.0041% B.
0.12% C, 0.26% Si, 0.86% Mn, 0.85% Ni, 0.53% Cr, 0.54% Mo, 0.050% V, 0.018% Al, 0.0041% B
0.12% C, 0.26% Si, 1.49% Mn, 0.015% P, 0.099% S, 0.06% Cr, 0.009% Mo, 0.06% Ni, 0.16% Cu, 0.039% Nb, 0.006% Sn
0.12% C, 0.27% Si, 0.61% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.13% Mo
0.12% C, 0.27% Si, 0.86% Mn, 0.94% Ni, 0.41% Mo, 0.004% V, 0.012% B
0.12% C, 0.27% Si, 0.86% Mn, 0.94% Ni, 0.41% Mo, 0.004% V, 0.012% B
0.12% C, 0.28% Si, 0.37% Mn, 0.011% P, 0.010% S, 0.95% Cr, 4.55% Ni
0.12% C, 0.28% Si, 0.37% Mn, 0.011% P, 0.010% S, 0.95% Cr, 4.55% Ni
0.12% C, 0.28% Si, 0.59% Mn, 0.019% P, 0.012% S, 1.08% Cr, 0.31% Mo, 0.23% V
0.12% C, 0.28% Si, 0.59% Mn, 0.019% P, 0.012% S, 1.08% Cr, 0.31% Mo, 0.23% V
0.12% C, 0.29% Si, 0.57% Mn, 1.86% Ni, 0.47% Cr, 0.18% Mo, 0.07% V, 0.0014% B
0.12% C, 0.30% Si, 0.69% Mn, 0.82% Ni, 0.54% Cr, 0.47% Mo, 0.068% V, 0.004% Al
0.12% C, 0.30% Si, 0.69% Mn, 0.82% Ni, 0.54% Cr, 0.47% Mo, 0.068% V, 0.004% B
0.12% C, 0.31% Si, 0.38% Mn, 0.012% P, 0.029% S, 0.87% Cr, 3.37% Ni, 0.28% Cu, 0.38% Mo, 0.057% Co, 0.016% Sn
0.12% C, 0.31% Si, 0.38% Mn, 0.012% P, 0.029% S, 0.87% Cr, 3.37% Ni, 0.28% Cu, 0.38% Mo, 0.057% Co, 0.016% Sn
0.12% C, 0.31% Si, 0.53% Mn, 3.55% Ni, 0.52% Cr, 0.30% Mo
0.12% C, 0.31% Si, 0.53% Mn, 3.55% Ni, 0.52% Cr, 0.30% Mo
0.12% C, 0.31% Si, 1.53% Mn, 0.005% P, 0.005% S, 0.67% Ni, 0.056% Al, 0.0090% N
0.12% C, 0.33% Si, 0.77% Mn, 0.003% P, 0.003% S, 0.92% Ni, 0.25% Cu, 0.48% Cr, 0.49% Mo, 0.02% V
0.12% C, 0.33% Si, 0.77% Mn, 0.003% P, 0.003% S, 0.92% Ni, 0.48% Cr, 0.49% Mo, 0.020% V
0.12% C, 0.33% Si, 1.37% Mn, 0.19% Ni, 0.03% Cr, 0.01% Mo, 0.008% V, 0.042% Al
0.12% C, 0.33% Si, 1.37% Mn, 0.19% Ni, 0.03% Cr, 0.01% Mo, 0.080% V, 0.042% Al
0.12% C, 0.34% Si, 0.80% Mn, 0.014% P, 0.010% S, 1.20% Ni, 0.44% Cr, 0.32% Mo, 0.24% Cu
0.12% C, 0.34% Si, 0.80% Mn, 1.20% Ni, 0.44% Cr, 0.32% Mo
0.12% C, 0.34% Si, 0.80% Mn, 1.20% Ni, 0.44% Cr, 0.32% Mo
0.12% C, 0.35% Si, 1.38% Mn, 0.04% Ni, 0.18% Cr, 0.078% Al, 0.167% Nb
0.12% C, 0.36% Si, 0.45% Mn, 0.05% Ni, 4.61% Cr, 0.50% Mo, 0.007% Al
0.12% C, 0.36% Si, 0.45% Mn, 0.05% Ni, 4.61% Cr, 0.50% Mo, 0.007% Al
0.12% C, 0.36% Si, 0.52% Mn, 0.09% Ni, 0.97% Cr, 0.61% Mo, 0.003% Al
0.12% C, 0.36% Si, 0.52% Mn, 0.09% Ni, 0.97% Cr, 0.61% Mo, 0.003% Al
0.12% C, 0.37% Si, 0.97% Mn, 0.007% P, 0.013% S, 0.27% Cr, 0.33% Mo, 1.12% Ni, 0.53% Cu, 0.030% Nb
0.12% C, 0.37% Si, 0.97% Mn, 0.007% P, 0.013% S, 0.27% Cr, 0.33% Mo, 1.12% Ni, 0.53% Cu, 0.030% Nb
0.12% C, 0.39% Mn, 0.016% P, 0.030% S, 1.87% Ni, 1.05% Cu
0.12% C, 0.40% Mn, 0.26% Si, 0.017% P, 0.016% S, 0.34% Ni, 2.95% Cr, 0.94% Mo
0.12% C, 0.40% Si, 0.45% Mn, 0.12% P, 0.31% Ni, 0.62% Cr, 0.26% Cu
0.12% C, 0.40% Si, 1.28% Mn, 0.015% P, 0.016% S, 0.62% Ni, 0.18% Ti, 0.67% Cu, 0.021% Al
0.12% C, 0.40% Si, 1.28% Mn, 0.015% P, 0.016% S, 0.62% Ni, 0.67% Cu, 0.024% Al
0.12% C, 0.42% Si, 0.49% Mn, 0.41% Ni, 0.25% Cr, 0.41% Mo, 0.028% Al, 0.002% B
0.12% C, 0.42% Si, 0.49% Mn, 0.41% Ni, 0.25% Cr, 0.41% Mo, 0.028% Al, 0.002% B
0.12% C, 0.45% Mn, 0.30% Si, 0.015% P, 0.015% S, 0.85% Cr, 0.60% Mo
0.12% C, 0.45% Mn, 0.41% Si, 0.62% Cr, 0.31% Ni, 0.12% P, 0.26% P
0.12% C, 0.45% Si, 1.17% Mn, 0.32% Cr, 0.25% Mo, 0.14% V
0.12% C, 0.45% Si, 1.17% Mn, 0.32% Cr, 0.25% Mo, 0.14% V
0.12% C, 0.46% Mn, 0.35% Si, 0.012% P, 0.016% S, 0.20% Ni, 4.79% Cr, 0.54% Mo
0.12% C, 0.47% Mn, 0.31% Si, 0.010% S, 0.014% P, 2.16% Cr, 0.16% Ni, 0.88% Mo, 0.17% V, 0.05% Cu, sol. 0.010% Al
0.12% C, 0.48% Si, 1.32% Mn, 0.014% P, 0.003% S, 0.26% Cr, 0.065% V
0.12% C, 0.49% Mn, 0.09% Si, 0.024% P, 0.012% S, 0.46% Ni, 12.50% Cr, 0.45% Co
0.12% C, 0.50% Mn, 0.004% P, 0.010% S, 0.0005% S
0.12% C, 0.50% Mn, 0.16% Si, 0.004% P, 0.010% S 0.0005% N
0.12% C, 0.50% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.90% Cr, 3.25% Ni
0.12% C, 0.50% Mn, 0.40% Si, 0.020% P, 0.010% S, 12.50% Cr, 0.20% Ni
0.12% C, 0.50% Mn, 0.45% Si, 0.013% P, 0.017% S, 0.28% Ni, 8.40% Cr, 0.96% Mo
0.12% C, 0.50% V
0.12% C, 0.50% V
0.12% C, 0.51% Mn, 0.29% Si, 0.014% S, 0.013% P 2.69% Ni, 0.70% Cr, 0.06% Mo, 0.18% Cu
0.12% C, 0.51% Mn, 0.29% Si, 0.014% S, 0.013% P 2.69% Ni, 0.70% Cr, 0.06% Mo, 0.18% Cu
0.12% C, 0.52% Mn, 0.22% Si, 0.014% S, 0.015% P 4.15% Ni, 0.86% Cr
0.12% C, 0.53% Mn, 0.28% Si, 0.020% P, 0.010% S, 0.85% Cr, 3.20% Ni, 0.20% Mo
0.12% C, 0.53% Mn, 0.55% Si, 0.015% P, 0.036% S, 0.07% Ni, 7.50% Cr, 0.45% Mo
0.12% C, 0.55% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.40% Cr, 0.15% Ni, 0.60% Mo, 0.25% V
0.12% C, 0.55% Mn, 0.68% Si, 0.010% S, 0.012% P, 2.05% Cr, 0.55% Mo, 0.32% V, 0.08% Ti, 0.006% B, 0.32% W
0.12% C, 0.57% Mn, 0.29% Si, 1.86% Ni, 0.47% Cr, 0.18% Mo, 0.07% V, 0.0014% B
0.12% C, 0.57% Mn, 0.47% Cr, 1.86% Ni, 0.18% Mo, 0.07% V, 0.001% B
0.12% C, 0.65% Mn, 0.26% Si, 0.015% S, 0.007% P, 1.16% Cr, 0.01% Ni, 1.02% Mo, 0.26% V, 0.02% Cu, sol. 0.010% Al
0.12% C, 0.65% Si, 0.55% Mn, 0.06% Ni, 1.42% Cr, 0.54% Mo, 0.019% Al
0.12% C, 0.65% Si, 0.55% Mn, 0.06% Ni, 1.42% Cr, 0.54% Mo, 0.019% Al
0.12% C, 0.70% Mn, 0.30% Si, 0.025% P, 0.020% S, 9.00% Cr, 1.00% Mo
0.12% C, 0.73% Mn, 0.37% Si, 0.003% S, 0.008% P, 5.75% Cr, 0.55% Mo, 0.24% V, 0.16% Ti, 0.011B, 0.26% W
0.12% C, 0.74% Si, 0.79% Mn, 0.017% P, 0.19% S, 0.25% Ni, 12.82% Cr, 0.05% Mo, 0.08% Zr, 0.037% N
0.12% C, 0.74% Si, 0.79% Mn, 0.190% S, 0.017% P, 0.25% Ni, 12.82% Cr, 0.08% Zr, 0.037% N
0.12% C, 0.75% Mn, 0.06% Si, 0.008% S, 0.007% P, 0.57% Cr, 2.62% Ni, 0.48% Mo, 0.05% V, 0.002% B, 0.25% Cu, sol. 0.062% Al
0.12% C, 0.79% Mn, 0.74% Si, 0.017% P, 0.19% S, 0.25% Ni, 12.82% Cr, 0.05% Mo, 0.037% N, 0.08% Zr
0.12% C, 0.83% Mn, 0.30% Si, 0.004% P, 0.005% S, 0.30% Cu, 1.11% Ni, 0.53% Cr, 0.49% Mo, 0.03% V, 0.031% sol. Al
0.12% C, 0.83% Mn, 0.30% Si, 0.004% P, 0.005% S, 0.30% Cu, 1.11% Ni, 0.53% Cr, 0.49% Mo, 0.03% V, 0.031% sol. Al
0.12% C, 0.83% Mn, 0.30% Si, 0.005% S, 0.004% P, 0.53% Cr, 1.11% Ni, 0.49% Mo, 0.03% V, 0.30% Cu, sol. 0.031% Al
0.12% C, 0.85% Mn, 0.33% Si, 1.41% Ni, 0.76% Cr, 0.45% Mo
0.12% C, 0.87% Mn, 0.34% Si, 1.43% Ni, 0.77% Cr, 0.19% Mo
0.12% C, 0.87% Mn, 0.35% Si, 1.44% Ni, 0.76% Cr
0.12% C, 0.90-1.20% Si, 0.35-0.75% Mn, max. 0.035% P, max. 0.035% S, 1.60-2.00% Cr, 0.25-0.35% Mo, 0.25-0.35% V
0.12% C, 1.10% Si, 0.43% Mn
0.12% C, 1.10% Si, 0.43% Mn
0.12% C, 1.16% Si, 0.71% Mn, 0.018% P, 0.006% S, 6.65% Cr, 0.20% Ni, 0.090% Ti, 0.68% Al
0.12% C, 1.23% Mn, 0.23% Si, 0.03% Al, (with and without 0.036% Nb)
0.12% C, 1.28% Mn, 0.40% Si, 0.015% P, 0.016% S, 0.021% Al, 0.67% Cu, 0.62% Ni, 0.015% V, 0.18% Ti
0.12% C, 1.28% Mn, 0.40% Si, 0.015% P, 0.016% S, 0.024% Al, 0.67% Cu, 0.62% Ni, 0.015% V
0.12% C, 1.30% Mo
0.12% C, 1.33% Mn, 0.28% Si, 0.011% P, 0.009% S
0.12% C, 1.64% Si, 0.40% Mn
0.12% C, 1.64% Si, 0.40% Mn
0.12% C, 1.72% Mn, 0.28% Si, 0.005% S, 0.016% P, 0.20% Mo, 0.06% V, 0.038% Nb, 0.068% Al, 0.0001% N
0.12% C, 12.30% Cr
0.12% C, 2.03% Si, 2.96% Mn
0.12-0.16% C, 0.40% Si, 0.60-0.90% Mn, 0.045% P, 0.045% S
0.12-0.17% C, <1.00% Si, <1.00% Mn, 12.00-14.00% Cr
0.12-0.17% C, <1.00% Si, <1.00% Mn, 12.00-17.00% Cr, 1.00-1.30% Mo
0.12-0.17% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.15% Cr, 1.20-1.60% Ni
0.12-0.17% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.15% Cr, 1.20-1.60% Ni
0.12-0.18% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S
0.12-0.18% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 0.10% Mo, 2.50-3.00% Ni
0.12-0.18% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.70% Cr
0.12-0.18% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.70% Cr
0.12-0.18% C, 0.30-0.60% Mn, 0.15-0.40% Si, 0.60-0.90% Cr, 2.50-3.00% Ni
0.12-0.18% C, max. 0.20% Si, 0.80-1.10% Mn, max. 0.020% P, max. 0.015% S, 1.25-1.50% Cr, 0.80-1.00% Mo, 0.20-0.30% V
0.12-0.18% C, max. 0.40% Si, 0.30-0.60% Mn, max. 0.035% P, 0.020-0.040% S
0.12-0.20% C, max. 0.35% Si, 0.40-0.90% Mn, max. 0.025% P, max. 0.010% S, 0.25-0.35% Mo, max. 0.30% Ni, max. 0.30% Cu
0.12% C, 0.16% Si, 0.50% Mn, 0.004% P, 0.010% S, 0.0005% N
0.12% C, 0.28% Mn, 0.46% Si, 0.026% P, 0.004% S, 11.99% Cr, 0.25% Ni, 0.18% Mo, 0.08% Cu, 0.002% Al, 0.25% V, 0.038% Nb, 0.006% Ti, 0.0465% N, 1.54% Co, 1.69% W, 0.0044% B
0.12-0.21% C, 0.85% Mn, 0.28% Si, 0.48% Cr, 0.05% V, 0.003% B
0.12% C, 0.37% Si, 1.15% Mn, 0.019% P, 0.034% S, 0.008% Al, 0.005% N
0.12% C, 0.32% Si, 1.73% Mn, 0.027% P, 0.031% S, 0.008% Al, 0.005% N, 0.04% Cr, 0.08% Cu, 0.02% Ni
0.12% C, 0.39% Si, 1.77% Mn, 0.022% P, 0.040% S, 0.001% Al, 0.005% N, 0.05% Cr, 0.045% Cu, 0.05% Ni
0.12% C, 0.35% Si, 1.58% Mn, 0.022% P, 0.010% S, 0.17% Cu, 0.15% Cr, 0.62% Ni, 0.018% Al, 0.012% N, 0.13% V
0.12% C, 0.47% Si, 1.26% Mn, 0.016% P, 0.017% S, 0.040% Al, 1.19% Cr, 0.18% Cu, 0.38% Mo, 0.04% Ni, 0.08% Nb, 0.06% Ti, 0.02% V
0.12% C, 1.04% Si, 2.02% Mn, 0.007% P, 0.011% S
0.12% C, 0.46% Si, 1.10% Mn, 0.021% P, 0.024% S, 0.07% Cr, 0.10% Ni, 0.02% Mo, 0.04% Ti, 0.006% Al, 0.02% V
0.12% C, 0.38% Si, 1.15% Mn, 0.016% P, 0.020% S, 0.11% Cu, 0.08% Cr, 0.06% Ni, 0.25% Mo, 0.026% Al, 0.10% V
0.12% C, 0.24% Si, 0.48% Mn, 0.012% P, 0.008% S, 2.17% Cr, 0.11% Ni, 1.06% Mo, 0.01% V, 0.12% Cu, 0.03% W, 0.004% Al, 0.00046% B, 0.002% Ti, 0.005% Nb, 0.008% N, 0.02% Co, 0.008% As
0.12% C, 0.24% Si, 0.48% Mn, 0.012% P, 0.008% S, 2.17% Cr, 0.11% Ni, 1.06% Mo, 0.01% V, 0.12% Cu, 0.03% W, 0.004% Al, 0.00046% B, 0.002% Ti, 0.005% Nb, 0.008% N, 0.02% Co, 0.008% As
0.12% C, 0.26% Si, 0.83% Mn, 0.52% Cr, 1.49% Ni, 0.50% Mo, 0.011% Nb, 0.035% Al, 0.041% V, 0.001% Ti, 0.015% W, 0.023% Cu
0.124% C, 0.157% Si, 0.42% Mn, 0.012% P, 0.001% S, 0.004% Al, 0.10% Cu, 9.32% Cr, 0.24% Ni, 0.49% Mo, 0.20% V, 1.75% W, 0.0013% B, 0.055% Nb, 0.049% N
0.124% C, 0.465% Si, 1.42% Mn, 0.026% Cr, 0.017% Ni, 0.040% Al, 0.018% Cu, 0.003% V, 0.003% Ti, 0.020% Nb
0.124% C, 0.36% Si, 0.82% Mn, 0.52% Cr, 1.48% Ni, 0.49% Mo, 0.011% Nb, 0.037% Al, 0.041% V, 0.001% Ti, 0.017% W, 0.022% Cu
0.125% C, 0.232% Si, 0.508% Mn, 0.013% P, 0.004% S, 2.280% Cr, 0.038% Ni, 0.956% Mo, 0.031% Al, 0.027% Cu, 0.004% Nb, 0.001% Ti, 0.008% V
0.127% C, 0.213% Si, 0.951% Mn, 0.017% P, 0.005% S, 0.626% Cr, 0.483% Mo, 1.86% Ni, 0.029% Al, 0.044% Cu, 0.002% Ti, 0.067% V
0.128% C, 0.39% Si, 1.26% Mn, 0.022% P, 0.004% S, 0.035% Cr, 0.03% Ni, 0.001% Mo, 0.02% Cu, 0.049% Al, 0.07% V, 0.005% Nb, 0.011% N
0.13% C, 9.00% Cr, 1.95% W, 0.021% Ni, 0.20% Ti
0.13% C, 0.002% Mn, 0.001% Si, 0.001% P, 0.006% S, 2.99% Cr
0.13% C, 0.01% Si, 0.17% Mn, 0.005% S, 0.006% P, 0.70% Ni, 10.45% Cr, 1.18% Mo, 0.23% V, 0.75% W, 0.02% Nb, 0.004% B, 0.023% N, 0.005% Ni, 0.005% Sn, 0.002% Mo
0.13% C, 0.07% Si, 1.20% Mn, 0.015% P, 0.025% S
0.13% C, 0.16% Mn, 3.03% Ni, 1.76% Cr, 0.49% Mo
0.13% C, 0.16% Mn, 3.08% Ni, 1.76% Cr, 0.49% Mo
0.13% C, 0.23% Si, 1.16% Mn, 0.04% Ni, 0.04% Cr, 0.016% Al
0.13% C, 0.23% Si, 1.18% Mn, 0.04% Ni, 0.04% Cr, 0.018% Al
0.13% C, 0.24% Si, 0.40% Mn, 0.017% P, 0.020% S, 0.14% Cr, 0.04% Mo, 1.44% Ni, 0.19% Cu
0.13% C, 0.25% Si, 0.35% Mn, 2.50% Ni, 1.17% Cr, 0.27% Mo
0.13% C, 0.25% Si, 0.35% Mn, 2.50% Ni, 1.17% Cr, 0.27% Mo
0.13% C, 0.25% Si, 0.52% Mn, 0.009% Ni, 0.007% S, 0.21% Cr, 1.02% Mo
0.13% C, 0.25% Si, 0.52% Mn, 0.009% P, 0.007% S, 2.21% Cr, 1.02% Mo
0.13% C, 0.25% Si, 0.60% Mn, 1.00% Cr, 0.45% Mo
0.13% C, 0.26% Si, 0.56% Mn, 0.019% P, 0.027% S, 0.035% Al
0.13% C, 0.28% Si, 0.30% Mn, 0.030% P, 0.014% S, 13.79% Cr, 0.08% Mo, 0.40% Ni
0.13% C, 0.28% Si, 0.43% Mn, 0.005% P, 0.005% S, 0.02% Cr, 0.02% Mo, 4.85% Ni, 0.05% Cu
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 0.010% Al, 1.50% Cr, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.010% Al, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.010% Al, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.010% Al, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.010% Al, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.06% Mo, 1.55% Ni, 0.010% V, 0.010% Al
0.13% C, 0.31% Si, 0.51% Mn, 0.023% P, 0.009% S, 1.50% Cr, 0.06% Mo, 1.55% Ni, 0.010% V, 0.010% Al
0.13% C, 0.32% Si, 0.45% Mn, 2.51% Ni, 1.59% Cr, 0.44% Mo
0.13% C, 0.32% Si, 0.45% Mn, 2.51% Ni, 1.59% Cr, 0.44% Mo
0.13% C, 0.33% Si, 0.86% Mn, 0.006% P, 0.005% S, 0.05% Ni, 0.27% Cu, 0.74% Cr, 0.45% Mo, 0.049% V
0.13% C, 0.33% Si, 0.86% Mn, 0.006% P, 0.005% S, 0.05% Ni, 0.27% Cu, 0.74% Cr, 0.45% Mo, 0.049% V
0.13% C, 0.346% Si, 1.418% Mn, 0.007% S, 0.023% P, 0.012% Ni, 0.026% Cr, 0.015% Cu, 0.028% Al, 0.002% Sn, 0.020% Nb
0.13% C, 0.35% Mn, 0.33% Si, 0.015% S, 0.008% P 3.42% Ni, 0.86% Cr, 0.08% Mo, 0.16% Cu
0.13% C, 0.35% Si, 0.91% Mn, 0.81% Ni, 0.46% Cr, 0.33% Mo, 0.09% Al
0.13% C, 0.35% Si, 0.91% Mn, 0.81% Ni, 0.46% Cr, 0.33% Mo, 0.090% Al
0.13% C, 0.37% Si, 0.84% Mn, 0.025% P, 0.022% S, 12.40% Cr
0.13% C, 0.38% Si, 0.63% Mn, 0.016% P, 0.012% S, 0.95% Cr, 0.86% Mo, 0.07% Ni, 0.19% V
0.13% C, 0.38% Si, 0.89% Mn, 3.34% Ni, 0.58% Cr, 0.36% Mo, 0.09% V
0.13% C, 0.38% Si, 0.89% Mn, 3.34% Ni, 0.58% Cr, 0.36% Mo, 0.090% V
0.13% C, 0.38% Si, 1.16% Mn, 0.56% Ni, 0.27% Cr, 0.12% V
0.13% C, 0.38% Si, 1.16% Mn, 0.56% Ni, 0.27% Cr, 0.12% V
0.13% C, 0.38% Si, 1.16% Mn, 0.56% Ni, 0.27% Cr, 0.120% Al
0.13% C, 0.39% Si, 0.40% Mn, 4.55% Ni, 0.08% Cr
0.13% C, 0.39% Si, 0.42% Mn, 0.013% P, 0.008% S, 0.78% Cr, 3.53% Ni
0.13% C, 0.39% Si, 0.42% Mn, 0.013% P, 0.008% S, 0.78% Cr, 3.53% Ni
0.13% C, 0.40% Si, 0.83% Mn, 0.95% Ni, 0.48% Cr, 0.50% Mo
0.13% C, 0.40% Si, 0.83% Mn, 0.95% Ni, 0.48% Cr, 0.50% Mo
0.13% C, 0.40% Si, 0.97% Mn, 0.52% Ni, 0.55% Cr, 0.28% Mo, 0.05% V, 0.044% Al
0.13% C, 0.40% Si, 0.97% Mn, 0.52% Ni, 0.55% Cr, 0.28% Mo, 0.050% V, 0.044% Al
0.13% C, 0.40% Si, 1.43% Mn, 0.014% P, 0.006% S, 0.21% Cu, 0.01% Ni, 0.21% Cr
0.13% C, 0.41% Si, 0.95% Mn, 0.009% P, 0.003% S, 0.21% Mo
0.13% C, 0.41% Si, 0.95% Mn, 0.009% P, 0.003% S, 0.28% Cr, 0.21% Mo
0.13% C, 0.41% Si, 1.08% Mn, 0.02% Ni, 0.02% Cr, 0.052% Al
0.13% C, 0.41% Si, 1.08% Mn, 0.02% Ni, 0.02% Cr, 0.052% Al
0.13% C, 0.42% Mn, 0.33% Si, 0.025% P, 0.012% S, 0.49% Ni, 13.50% Cr, 11.90% Co
0.13% C, 0.44% Si, 1.44% Mn, 0.18% Ni, 0.028% Al, 0.026% Nb
0.13% C, 0.44% Si, 1.44% Mn, 0.18% Ni, 0.028% Al, 0.026% Nb
0.13% C, 0.45% Si, 1.08% Mn, 0.05% Ni, 0.32% Cr, 0.15% V, 0.019% Al
0.13% C, 0.45% Si, 1.08% Mn, 0.05% Ni, 0.32% Cr, 0.15% V, 0.019% Al
0.13% C, 0.46% Mn, 0.26% Si, 0.013% P, 0.012% S, 0.012% Al, 0.78% Cr, 0.16% Cu, 0.04% Mo, 8.69% Ni
0.13% C, 0.46% Mn, 1.22% Mn, 0.08% Ni, 0.010% V
0.13% C, 0.46% Si, 1.22% Mn, 0.08% Ni, 0.01% Al
0.13% C, 0.47% Si, 1.44% Mn, 0.10% Ni, 0.19% Cr, 0.15% Nb
0.13% C, 0.47% Si, 1.44% Mn, 0.10% Ni, 0.19% Cr, 0.15% Nb
0.13% C, 0.48% Si, 1.37% Mn, 0.22% Cr, 0.13% V, 0.022% Al
0.13% C, 0.48% Si, 1.37% Mn, 0.22% Cr, 0.13% V, 0.022% Al
0.13% C, 0.48% Si, 1.40% Mn, 0.03% Ni, 0.04% Cr, 0.023% Al
0.13% C, 0.48% Si, 1.40% Mn, 0.03% Ni, 0.04% Cr, 0.023% Mo
0.13% C, 0.49% Mn, 0.15% Si, 0.012% P, 0.010% S, 0.51% Ni, 12.40% Cr, 4.90% Co
0.13% C, 0.50% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.85% Cr, 3.40% Ni, 0.18% Mo
0.13% C, 0.50% Mn, 0.45% Si, 0.034% P, 0.010% S, 0.52% Ni, 13.20% Cr, 0.99% Co
0.13% C, 0.51% Mn, 0.31% Si, 0.023% P, 0.009% S, 0.010% Al, 1.50% Cr, 0.06% Mo, 1.55% Ni, <0.01% V
0.13% C, 0.51% Mn, 0.31% Si, 1.5% Cr, 1.55% Ni, 0.06% Mo, 0.01% V
0.13% C, 0.51% Mn, 0.31% Si, 1.5% Cr, 1.55% Ni, 0.06% Mo, 0.01% V
0.13% C, 0.52% Mn, 0.22% Si, 0.023% P, 0.008% S, 0.48% Ni, 12.80% Cr, 1.87% Co
0.13% C, 0.55% Si, 0.54% Mn, 2.54% Ni, 1.23% Cr, 0.50% Mo
0.13% C, 0.55% Si, 0.54% Mn, 2.54% Ni, 1.23% Cr, 0.50% Mo
0.13% C, 0.60% Mn, 0.29% Si, 0.016% S, 0.010% P, 0.98% Cr, 0.01% Ni, 0.31% Mo, 0.20% V, 0.02% Cu, sol. 0.010% Al
0.13% C, 0.63% Mn, 0.32% Si, 0.012% S, 0.016% P, 0.95% Cr, 0.07% Ni, 0.86% Mo, 0.19% V
0.13% C, 0.71% Mn, 0.56% Si, 5.43% Cr, 0.47% Mo, 0.20% V, 0.16% Ti, 0.010% B, 0.19% W
0.13% C, 1.08% Mn, 0.14% Si, 0.020% S, 0.027% P 1.13% Ni, 0.88% Cr, 0.040% Mo
0.13% C, 1.16% Mn, 0.31% Si, 0.017% S, 0.018% P, 0.23% Cr, 0.01% Ni, 0.27% Mo, 0.05% V, 0.01% Cu, sol. 0.010% Al
0.13% C, 1.54% Mn, 0.39% Si, 0.024% P, 0.015% S, 13.40% Ni, 23.21% Cr. Type-310: 0.05% C, 1.95% Mn, 0.37% Si, 0.023% P, 0.007% S, 21.09% Ni, 27.23% Cr
0.13-0.17% C, max. 0.30% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.13-0.18% C, <0.40% Si, 0.80-1.10% Mn, <0.025% P, <0.030% S, 1.20-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.18% C, <0.40% Si, 0.80-1.10% Mn, <0.025% P, <0.030% S, 1.20-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.18% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40-0.60% Cr, 0.15-0.25% Mo, 0.35-0.65% Ni
0.13-0.18% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.80-1.10% Ni
0.13-0.18% C, 0.15-0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.80-1.10% Ni
0.13-0.18% C, max. 0.20% Si, 0.80-1.10% Mn, max. 0.020% P, max. 0.015% S, 1.25-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.18% C, max. 0.40% Si, 0.80-1.10% Mn, max. 0.025% P, max. 0.035% S, 1.20-1.50% Cr, 0.80-1.10% Mo, 0.20-0.30% V
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.80-1.1% Cr, 0.30-0.40% Mo, 2.70-3.20% Ni
0.13-0.19% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.80-1.1% Cr, 0.30-0.40% Mo, 2.70-3.20% Ni
0.13-0.19% C, 0.40% Si, 0.70-1.00% Mn, 0.035% P, 0.020-0.040% S, 0.60-1.00% Cr, 0.80-1.10% Ni
0.13-0.20% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.20-0.30% Mo, max. 0.40% Ni
0.13-0.20% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.20-0.30% Mo, max. 0.40% Ni
0.13% C, 0.15-0.40% Si, max. 0.90% Mn, max. 0.015% P, max. 0.015% S, 8.50-9.50% Ni
0.13% C, 0.26% Si, 0.46% Mn, 0.78% Cr, 0.04% Mo, 3.59% Ni
0.13% C, 0.26% Si, 0.46% Mn, 0.78% Cr, 0.04% Mo, 3.59% Ni
0.13% C, 0.32% Si, 0.48% Mn, 0.010% P, 0.024% S, 0.006% Al, 0.0037% N
0.13% C, 0.37% Si, 1.84% Mn, 0.020% P, 0.023% S, 0.005% Al, 0.011% N, 0.04% Cr, 0.08% Cu, 0.03% Ni
0.13% C, 0.28% Si, 1.40% Mn, 0.028% P, 0.023% S, 0.13% Cu, 0.13% Cr, 0.57% Ni, 0.03% Mo, 0.02% Nb, 0.19% Al, 0.012% V
0.13% C, 0.46% Si, 1.39% Mn, 0.019% P, 0.006% S, 0.02% Nb, 0.02% Ti, 0.040% Al, 0.012% N, 0.12% V
0.13% C, 0.40% Si, 1.68% Mn, 0.020% P, 0.006% S, 0.58% Cu, 0.50% Ni, 0.18% V, 0.03% Nb, 0.052% Al, 0.007% N
0.13% C, 0.40% Si, 1.68% Mn, 0.020% P, 0.006% S, 0.58% Cu, 0.50% Ni, 0.18% V, 0.03% Nb, 0.052% Al, 0.007% N
0.13% C, 0.49% Si, 1.91% Mn, 0.016% P, 0.007% S, 0.56% Cu, 0.61% Ni, 0.16% V, 0.11% Nb, 0.052% Al, 0.012% N
0.13% C, 0.44% Si, 1.25% Mn, 0.124% P, 0.013% S, 0.36% Cu, 0.77% Cr, 0.02% Ni, 0.018% Al, 0.026% N, 0.06% V
0.13% C, 0.02% Si, 0.38% Mn, 0.013% P, 0.018% S
0.13% C, 0.40% Si, 1.52% Mn, 0.020% P, 0.022% S, 0.22% Cu, 0.03% Cr, 0.11% Ni, 0.04% Mo, 0.03% Ti, 0.01% V
0.13% C, 0.45% Si, 0.85% Mn, 0.021% P, 0.022% S, 0.08% Cr, 0.22% Ni, 0.03% Mo, 0.05% Ti, 0.008% Al, 0.02% V
0.13% C, 0.43% Si, 0.85% Mn, 0.021% P, 0.024% S, 0.08% Cr, 0.38% Ni, 0.02% Mo, 0.04% Ti, 0.006% Al, 0.02% V
0.13% C, 0.50% Si, 0.96% Mn, 0.021% P, 0.023% S, 0.08% Cr, 0.58% Ni, 0.02% Mo, 0.04% Ti, 0.008% Al, 0.02% V
0.135% C, 1.50% Mn, 0.50% Si, 0.015% Nb
0.137% C, 0.455% Si, 1.36% Mn, 0.009% P, 0.003% S, 0.066% Cr, 0.076% Ni, 0.010% Mo, 0.003% V, 0.002% Ti, 0.038% Al, 0.212% Cu
0.139% C, 0.34% Si, 1.30% Mn, 0.026% P, 0.0078% S, 0.039% Cu, 0.031% Al, 0.51% Cr, 0.26% Ni, 0.25% Mo, 0.018% Ti, 0.0016% B, 0.0053% N
0.14% C, <0.003% Mn, 0.0009% Si, 0.002% P, 0.002% S,   < 0.005% Ni, 0.004% Cr, 2.29% Mo, <0.002% Cu, <10 ppm N, 168 ppm O. D = 0.15% C, <0.002% Mn, 0.001% Si, 0.001% P, 0.006% S, 2.55% Mo. G = 0.17% C, <0.002% Mn, 0.003% Si, 0.002% P, 0.004% S, 0.030% Ni, 0.002% Cr, 2.94% Mo, 0.007% Co, 0.004% Cu, 0.002% Al, 0.003% V, 0.004% N. J = 0.15% C - 3.40% Mo. L = 0.15% C - 3.67% Mo. O = 0.14% C - 3.98% Mo. Compositions: B = 0.19% C - 2.30% Mo. E = 0.19% C - 2.56% Mo. H = 0.19% C - 2.98% Mo. M = 0.17% C - 3.76% Mo. P = 0.20% C - 4.00% Mo. R = 0.18% C - 4.25% Mo. Compositions: C = 0.24% C - 2.31% Mo. F = 0.24% C - 2.56% Mo. I = 0.26% C - 2.94% Mo. K = 0.25% C - 3.19% Mo. N = 0.24% C - 3.76% Mo. Q = 0.23% C - 4.00% Mo. S = 0.24% C - 2.28% Mo
0.14% C, 0.09% Si, 0.96% Mn, 0.06% Ni, 0.07% Cr, 0.054% Al
0.14% C, 0.09% Si, 0.96% Mn, 0.06% Ni, 0.07% Cr, 0.054% V
0.14% C, 0.15% Si, 0.36% Mn, 0.017% P, 0.011% S, 1.40% Cr, 0.96% Mo, 0.27% V
0.14% C, 0.15% Si, 0.40% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.14% C, 0.15% Si, 0.96% Mn, 0.017% P, 0.011% S, 1.40% Cr, 0.96% Mo, 0.27% V
0.14% C, 0.16% Si, 0.75% Mn, 1.90% Ni, 0.63% Cr, 0.47% Mo, 0.01% Al
0.14% C, 0.16% Si, 0.75% Mn, 1.91% Ni, 0.63% Cr, 0.47% Mo, 0.010% Al
0.14% C, 0.17% Si, 0.71% Mn, 0.99% Cr, 0.48% Mo, 0.03% B
0.14% C, 0.17% Si, 0.91% Mn, 0.99% Cr, 0.48% Mo, 0.003% B
0.14% C, 0.17% Si, 0.91% Mn, 0.99% Cr, 0.48% Mo, 0.003% B
0.14% C, 0.18% Si, 0.52% Mn, 0.012% P, 0.013% S, 0.93% Cr, 0.47% Mo, 0.13% Ni, 0.15% Cu
0.14% C, 0.19% Si, 2.21% Mn, 0.27% Cr, 0.063% P, 0.023% Nb
0.14% C, 0.20% Si, 0.40% Mn, 0.015% P, 0.009% S, 1.12% Cr, 4.43% Ni
0.14% C, 0.20% Si, 0.40% Mn, 0.015% P, 0.009% S, 1.12% Cr, 4.43% Ni
0.14% C, 0.21% Si, 0.34% Mn, 4.39% Ni, 1.29% Cr, 0.34% Mo
0.14% C, 0.21% Si, 0.41% Mn, 0.19% Ni, 5.12% Cr, 0.51% Mo
0.14% C, 0.22% Si, 0.45% Mn, 3.42% Ni, 0.21% Mo
0.14% C, 0.22% Si, 0.53% Mn, 0.012% P, 0.017% S, 1.53% Cr, 1.54% Ni, 0.20% Cu, 0.06% Mo, 0.0014% Sn
0.14% C, 0.22% Si, 1.40% Mn, 0.76% Ni, 0.55% Mo
0.14% C, 0.22% Si, 1.40% Mn, 0.76% Ni, 0.55% Mo
0.14% C, 0.23% Si, 0.48% Mn, 0.014% P, 0.032% S, 0.07% Cr, 0.07% Ni, 0.19% Cu, 0.014% Al
0.14% C, 0.23% Si, 0.65% Mn, 0.02% Ni, 0.02% Cr, 0.008% Al
0.14% C, 0.23% Si, 0.65% Mn, 0.02% Ni, 0.02% Cr, 0.008% Al
0.14% C, 0.23% Si, 1.02% Mn, 0.50% Ni, 0.55% Cr, 0.47% Mo, 0.06% V
0.14% C, 0.23% Si, 1.02% Mn, 0.50% Ni, 0.55% Cr, 0.47% Mo, 0.060% V
0.14% C, 0.24% Si, 1.40% Mn, 0.10% Cr, 0.52% Mo, 0.10% Ni, 0.068% V, 0.11% Cu
0.14% C, 0.25% S, 16.50% Cr, 0.40% Mo
0.14% C, 0.25% Si, 0.45% Mn, 0.45% Cr, 0.30% V, 0.60% Mo
0.14% C, 0.25% Si, 0.55% Mn, 0.50% Cr, 0.28% Ni, 0.60% Mo
0.14% C, 0.25% Si, 0.55% Mn, 0.50% Cr, 0.28% V, 0.60% Mo
0.14% C, 0.25% Si, 0.55% Mn, 0.75% Cr, 3.50% Ni
0.14% C, 0.25% Si, 0.55% Mn, 0.75% Cr, 3.50% Ni
0.14% C, 0.25% Si, 0.55% Mn, 1.10% Cr, 4.50% Ni
0.14% C, 0.25% Si, 0.55% Mn, 1.10% Cr, 4.50% Ni
0.14% C, 0.25% Si, 0.56% Mn, 0.019% P, 0.020% S, 1.59% Cr, 1.46% Ni
0.14% C, 0.25% Si, 0.56% Mn, 0.019% P, 0.020% S, 1.59% Cr, 1.46% Ni
0.14% C, 0.25% Si, 0.58% Mn, 0.015% P, 0.031% S
0.14% C, 0.25% Si, 0.58% Mn, 0.015% P, 0.031% S
0.14% C, 0.25% Si, 0.60% Mn, 0.80% Cr, 2.70% Ni
0.14% C, 0.25% Si, 0.60% Mn, 0.80% Cr, 2.70% Ni
0.14% C, 0.26% Mn, 2.21% Ni, 1.05% Cr, 0.26% Mo
0.14% C, 0.26% Mn, 2.21% Ni, 1.05% Cr, 0.26% Mo
0.14% C, 0.26% Si, 0.27% Mn, 0.038% P, 0.013% S, 12.98% Cr, 0.53% Ni
0.14% C, 0.26% Si, 0.49% Mn, 0.020% P, 0.004% S, 0.66% Cr, 3.31% Ni, 0.19% Cu, 0.08% Mo
0.14% C, 0.26% Si, 0.49% Mn, 0.020% P, 0.004% S, 0.66% Cr, 3.31% Ni, 0.19% Cu, 0.08% Mo
0.14% C, 0.26% Si, 0.82% Mn, 0.86% Ni, 0.51% Cr, 0.46% Mo, 0.03% V, 0.05% Al, 0.0024% B
0.14% C, 0.26% Si, 0.82% Mn, 0.86% Ni, 0.51% Cr, 0.46% Mo, 0.030% V, 0.005% Al, 0.0024% B
0.14% C, 0.26% Si, 0.83% Mn, 1.06% Ni, 0.61% Cr, 0.45% Mo, 0.05% V
0.14% C, 0.26% Si, 0.83% Mn, 1.06% Ni, 0.61% Cr, 0.45% Mo, 0.050% V, 0.020% B
0.14% C, 0.26% Si, 1.28% Mn, 0.86% Ni, 0.50% Cr, 0.46% Mo
0.14% C, 0.26% Si, 1.28% Mn, 0.86% Ni, 0.50% Cr, 0.46% Mo
0.14% C, 0.27% Mn, 0.01% Si, 0.005% S, 0.09% P 9.12% Ni, 4.07% Co
0.14% C, 0.27% Si, 0.77% Mn, 0.91% Ni, 0.49% Cr, 0.45% Mo, 0.08% V, 0.0028% B
0.14% C, 0.27% Si, 0.77% Mn, 0.91% Ni, 0.49% Cr, 0.45% Mo, 0.080% V, 0.0028% B
0.14% C, 0.29% Si, 0.33% Mn, 0.025% P, 0.187% S, 15.65% Cr, 0.21% Mo, 0.33% Ni, 0.07% Cu, 0.005% Al
0.14% C, 0.29% Si, 0.85% Mn, 0.86% Ni, 0.56% Cr, 0.46% Mo, 0.090% V, 0.020% Al
0.14% C, 0.29% Si, 0.87% Mn, 0.81% Ni, 0.56% Cr, 0.46% Mo, 0.09% V, 0.02% Al
0.14% C, 0.31% Si, 0.97% Mn, 0.017% P, 0.137% S, 12.65% Cr, 0.07% Mo, 0.24% Ni, 0.003% Al, 0.0350% N
0.14% C, 0.31% Si, 0.97% Mn, 0.017% P, 0.137% S, 12.65% Cr, 0.07% Mo, 0.24% Ni, 0.003% Al, 0.0350% N
0.14% C, 0.32% Si, 1.32% Mn, 0.003% V
0.14% C, 0.32% Si, 1.32% Mn, 0.003% V
0.14% C, 0.35% Si, 0.52% Mn, 3.06% Ni, 0.95% Cr, 0.31% Mo, 0.06% V
0.14% C, 0.35% Si, 0.52% Mn, 3.06% Ni, 0.95% Cr, 0.31% Mo, 0.060% V
0.14% C, 0.35% Si, 0.91% Mn, 1.36% Ni, 0.49% Cr, 0.47% Mo, 0.02% V
0.14% C, 0.35% Si, 0.91% Mn, 1.36% Ni, 0.49% Cr, 0.47% Mo, 0.020% V
0.14% C, 0.41% Mn, 0.21% Si, 0.19% Ni, 5.12% Cr, 0.51% Mo
0.14% C, 0.43% Si, 1.16% Mn, 0.026% P, 0.24% S, 16.30% Cr, 0.31% Ni, 0.14% Cu, 0.37% Mo
0.14% C, 0.43% Si, 1.16% Mn, 0.026% P, 0.24% S, 16.30% Cr, 0.31% Ni, 0.14% Cu, 0.37% Mo
0.14% C, 0.43% Si, 1.29% Mn, 0.33% Cr, 0.33% Mo, 0.87% Ni, 0.020% V, 0.14% Cu, 0.033% Al, 0.0150% Nb
0.14% C, 0.44% Si, 1.21% Cr, 0.015% P, 0.010% S, 0.02% Ni, 0.043% V
0.14% C, 0.45% Mn, 0.22% Si, 3.42% Ni, 0.21% Mo
0.14% C, 0.45% Mn, 0.26% Si, 0.016% P, 0.025% S, 4.66% Cr, 0.56% Mo, 0.13% Ni
0.14% C, 0.45% Si, 1.22% Mn, 0.48% Ni, 0.32% Cr, 0.12% V, 0.033% Al
0.14% C, 0.45% Si, 1.22% Mn, 0.48% Ni, 0.32% Cr, 0.12% V, 0.033% Al
0.14% C, 0.46% Mn, 0.19% Si, 3.55% Ni, 1.11% Cr 0.12% Mo
0.14% C, 0.46% Mn, 0.19% Si, 3.55% Ni, 1.11% Cr 0.12% Mo
0.14% C, 0.46% Mn, 0.23% Si, 0.010% P, 0.010% S, 2.28% Cr, 0.21% Ni, 1.05% Mo, 0.00% V
0.14% C, 0.47% Si, 1.50% Mn, 0.015% P, 0.003% S, 0.57% Ni, 0.05% V
0.14% C, 0.48% Si, 1.16% Mn, 0.41% Ni, 0.62% Cr, 0.42% Mo, 0.07% V, 0.062% Al
0.14% C, 0.48% Si, 1.16% Mn, 0.41% Ni, 0.62% Cr, 0.42% Mo, 0.070% V, 0.062% Al, 0.0021% B
0.14% C, 0.50% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.55% Cr, 1.55% Ni
0.14% C, 0.50% Mn, 0.30% Si, 0.005% S, 0.008% P, 0.38% Cr, 0.03% Ni, 0.55% Mo, 0.27% V, 0.01% Cu, sol. 0.010% Al
0.14% C, 0.53% Mn, 0.54% Si, 0.006% S, 0.022% P, 1.43% Cr, 0.54% Mo, 0.03% V, 0.006% Ti
0.14% C, 0.53% Si, 1.12% Mn, 0.06% Ni, 0.04% Cr, 0.040% Al
0.14% C, 0.53% Si, 1.12% Mn, 0.06% Ni, 0.04% Cr, 0.040% Al
0.14% C, 0.55% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.60% Cr, 0.55% Mo
0.14% C, 0.68% Mn, 0.67% Si, 0.012% S, 0.024% P 2.95% Ni, 17.98% Cr, 0.06% Mo, 0.04% Al, 0.10% Co, 0.10% Cu
0.14% C, 0.68% Mn, 0.67% Si, 0.024% P, 0.012% S, 17.98% Cr, 2.95% Ni, 0.06% Mo, 0.04% Al, 0.10% Co
0.14% C, 0.70% Mn, 0.64% Si, 0.021% P, 0.030% S, 25.51% Cr. Lab experimental heat: 0.04% C, 0.38% Mn, 0.54% Si, 0.024% P, 0.015% S, 0.08% Ni, 27.78% Cr
0.14% C, 0.74% Mn, 0.014% P, 0.005% Si, 0.024% Ni, 0.014% Cr, 0.032% Al
0.14% C, 0.81% Mn, 1.81% Ni, 0.49% Cr, 0.27% Mo, 0.0030% B
0.14% C, 0.96% Mn, 0.15% Si, 0.011% S, 0.017% P 1.14% Cr, 0.96% Mo, 0.27% Cu
0.14% C, 0.98% Mn, 0.35% Si, 0.009% P, 0.012% S, 1.21% Ni, 0.32% Cr, 0.40% Mo, 0.63% Cu, 0.032% Al, 0.014% N, 0.02% Cb(Nb)
0.14% C, 1.00% Mn, 0.018% P, 0.01% Si, 0.02% Ni, 0.015% Cr, 0.03% Al
0.14% C, 1.02% Mn, 0.23% Si, 0.017% S, 0.016% P 0.15% Ni, 0.10% Cr, 0.48% Mo, 0.15% Cu, 0.065% V
0.14% C, 1.02% Mn, 0.23% Si, 0.017% S, 0.016% P 0.15% Ni, 0.10% Cr, 0.48% Mo, 0.15% Cu, 0.065% V
0.14% C, 1.20% Mn, 0.23% Si, 0.017% S, 0.016% P 0.15% Ni, 0.10% Cr, 0.48% Mo, 0.15% Cu
0.14% C, 1.20% Mn, 0.23% Si, 0.017% S, 0.016% P 0.15% Ni, 0.10% Cr, 0.48% Mo, 0.15% Cu
0.14% C, 1.30% Mn. Extremely-low Carbon Bainitic Steel: 0.02% C, 1.60% Mn
0.14% C, 1.34% Mn, 0.015% Nb
0.14% C, 1.34% Mn, 0.015% Nb
0.14% C, 1.34% Mn, 0.015% Nb
0.14% C, 1.44% Mn, 0.23% Si, 0.007% S, 0.011% P, 0.065% Cr, 0.23% Ni, 0.035% Mo, 0.10% V, 0.03% Nb, 0.488% Cu, 0.028% Al, 0.013% N
0.14% C, 1.52% Mn, 0.48% Si, 0.004% S, 0.011% P, 0.071% V
0.14% C, 1.53% Mn, 0.36% Si, 0.008% S, 0.009% P, 0.06% Cr, 0.03% Ni, 0.01% Mo, 0.04% V, 0.02% Cu, 0.057% Al
0.14% C, 2.43% Ni
0.14% C, 2.43% Ni
0.14% C, 7.02% Ni
0.14% C, 7.02% Ni
0.14-0.17% C, 0.15% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Ni, 0.45-0.55% Mo, 0.15-0.25 V
0.14-0.17% C, 0.30% Si, 1.20-1.40% Mn, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Ni, 0.45-0.55% Mo
0.14-0.17% C, 1.20-1.40% Mn, 0.30% Si, 0.020% P, 0.002% S, 2.10-2.30% Cr, 0.45-0.55% Ni, 0.45-0.55% Mo
0.14-0.19% C, <0.40% Si, 1.10-1.30% Mn, <0.035% S, 0.80-1.10% Cr. 16MnCrS5: 0.14-0.19% C, <0.40% Si, 1.10-1.30% Mn, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.035% P, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.035% P, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.0008-0.0050% B
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr
0.14-0.19% C, 0.40% Si, 1.00-1.30% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 0.40-0.90% Mn, max. 0.035% P, max. 0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.19% C, max. 0.40% Si, 0.40-0.90% Mn, max. 0.035% P, max. 0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, 0.020-0.040% S, 0.80-1.10% Cr
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.80-1.10% Cr, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.015% S, 0.80-1.10% Cr, max. 0.30% Cu, max. 0.050% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr, 0.0008-0.0050% B
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr
0.14-0.20% C, <0.40% Si, 0.40-0.70% Mn, <0.050% P, <0.035% S, 0.60-0.90% Cr, 3.60-3.50% Ni
0.14-0.20% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.70-1.00% Cr
0.14-0.20% C, <0.40% Si, 0.60-0.90% Mn, <0.035% S, <0.035% P, 0.70-1.00% Cr, (Pb)
0.14-0.20% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr, 3.00-3.50% Ni
0.14-0.20% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.40-1.70% Cr, 1.40-1.70% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.70-1.00% Cr
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.80-1.10% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.14-0.20% C, 0.60-1.00% Mn, 0.17-0.37% Si, 0.070% S, 0.070% P, 0.25% Cr, 0.25% Ni, 0.05-0.09% V, 0.25% Cu
0.14-0.20% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 0.60-0.90% Cr, 3.00-3.50% Ni
0.14-0.20% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 0.60-0.90% Cr, 3.00-3.50% Ni
0.14-0.21% C, 0.10-0.40% Si, 0.50-0.80% Mn, 0.040% P, 0.040% S
0.14-0.19% C, 1.00-1.30% Mn, 0.80-1.10% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P. 20MnCrS5 steel: 0.17-0.22% C, 1.10-1.40% Mn, 1.00-1.30% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P
0.14-0.19% C, 1.00-1.30% Mn, 0.80-1.10% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P. 20MnCrS5 steel: 0.17-0.22% C, 1.10-1.40% Mn, 1.00-1.30% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P
0.14-0.19% C, 1.00-1.30% Mn, 0.80-1.10% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P
0.14-0.19% C, 1.00-1.30% Mn, 0.80-1.10% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P. 20MnCrS5 steel: 0.17-0.22% C, 1.10-1.40% Mn, 1.00-1.30% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P
0.14% C, 0.22% Si, 0.53% Mn, 0.004% P, 0.004% S, 2.43% Cr, 0.16% Ni, 1.07% Mo, 0.04% Cu, 0.014% Al
0.14-0.19% C, max. 0.40% Si, 1.00-1.30% Mn, max. 0.025% P, max. 0.035% S, 0.80-1.10% Cr
0.14% C, 1.7% Mn, 0.18% Si, 0.3% Cr, 0.15% Mo
0.140% C, 0.20% Si, 2.19% Mo, 0.0088% P, 0.0006% S, 0.058% Al, 0.28% Cr, 0.022% Nb, 0.0054% N
0.14% C, 0.18% Si, 0.58% Mn, 0.027% P, 0.029% S
0.14% C, 0.36% Si, 1.06% Mn, 0.023% P, 0.06% Cr, 0.05% Ni, 0.01% Mo, 0.03% Nb, 0.038% Al, 0.005% N, 0.01% V
0.14% C, 0.43% Si, 1.16% Mn, 0.018% P, 0.030% S, 0.18% Cu, 0.12% Cr, 0.07% Ni, 0.01% N, 0.012% Al, 0.037% V
0.14% C, 0.45% Si, 1.46% Mn, 0.022% P, 0.027% S, 0.10% Cr, 0.02% Ni, 0.01% Ti, 0.023% Al, 0.099% V
0.14% C, 0.44% Si, 1.65% Mn, 0.018% P, 0.009% S, 0.14% Cu, 0.13% Cr, 0.63% Ni, 0.041% Al, 0.013% N, 0.014% V
0.14% C, 0.51% Si, 1.58% Mn, 0.021% P, 0.004% S, 0.01% Nb, 0.01% Ti, 0.043% Al, 0.012% N, 0.13% V
0.14% C, 0.03% Si, 0.35% Mn, 0.007% P, 0.011% S
0.14% C, 0.03% Si, 0.35% Mn, 0.007% P, 0.011% S
0.14% C, 0.50% Si, 1.42% Mn, 0.022% P, 0.024% S, 0.08% Cr, 0.11% Ni, 0.03% Mo, 0.04% Ti, 0.007% Al, 0.02% V
0.14% C, 0.35% Si, 1.17% Mn, 0.65% Cr, 0.06% Ni, 0.10% Mo, 0.001% Nb, 0.064% Al, 0.0056% V, 0.004% Ti, 0.015% W, 0.014% Cu
0.142% C, 0.437% Si, 1.577% Mn, 0.003% S, 0.022% P, 0.024% Ni, 0.026% Cr, 0.016% Mo, 0.003% V, 0.002% Ti, 0.011% Nb, 0.017% Cu
0.142% C, 0.437% Si, 1.577% Mn, 0.003% S, 0.022% P, 0.024% Ni, 0.026% Cr, 0.016% Mo, 0.003% V, 0.002% Ti, 0.011% Nb, 0.017% Cu
0.142% C, 1.20% Mn, 0.56% Si, 19.08% P, 22.45% Cr
0.143% C, 0.171% Si, 0.44% Mn, 0.017% S, 0.015% P
0.143% C, 0.438% Si, 1.599% Mn, 0.003% S, 0.022% P, 0.025% Ni, 0.027% Cr, 0.017% Mo, 0.003% V, <0.001% Nb, 0.017% Cu, 0.002% Ti
0.143% C, 0.438% Si, 1.599% Mn, 0.003% S, 0.022% P, 0.025% Ni, 0.027% Cr, 0.017% Mo, 0.003% V, <0.001% Nb, 0.017% Cu, 0.002% Ti
0.144% C, 0.420% Si, 1.430% Mn, 0.017% P, 0.007% S, 0.024% Cr, 0.028% Ni, 0.015% Mo, 0.039% Al, 0.011% Cu, 0.021% Nb, 0.006% Ti, 0.004% V
0.145% C, 0.27% Mn, 0.02% Si, 0.005% S, 0.012% P 9.12% Ni
0.147% C, 0.311% Si, 1.45% Mn, 0.01% P, 0.007% S, 0.008% Cr, 0.004% Ni, 0.001% Mo, 0.028% V, 0.022% Nb, 0.025% Al
0.149% C, 0.445% Si, 1.607% Mn, 0.003% S, 0.024% P, 0.026% Ni, 0.027% Cr, 0.016% Mo, 0.003% V, 0.026% Nb, 0.018% Cu, 0.002% Ti
0.149% C, 0.445% Si, 1.607% Mn, 0.003% S, 0.024% P, 0.026% Ni, 0.027% Cr, 0.016% Mo, 0.003% V, 0.026% Nb, 0.018% Cu, 0.002% Ti
0.149% C, 0.207% Si, 1.910% Mn, 0.016% P, 0.006% S, 0.200% Cr, 0.003% Mo, 0.015% Ni, 0.028% Al, 0.013% Cu, 0.005% Nb, 0.024% Ti, 0.007% V
0.15% C, 0.12% Si, 0.24% Mn, 2.91% Cr
0.15% C, 0.12% Si, 0.61% Mn, 0.023% P, 0.027% S, 0.24% Cr, 0.11% Ni, 0.17% Cu, 0.31% Mo, 0.009% Al, 0.004% Sn
0.15% C, 0.12% Si, 1.22% Mn, 0.016% P, 0.012% S, 0.12% Cr, 0.03% Mo, 0.62% Ni
0.15% C, 0.15% Si, 0.34% Mn, 0.018% P, 0.005% S, 11.40% Cr, 1.65% Ni, 0.27% V, 1.91% W, 0.09% Cu, 0.42% Mo
0.15% C, 0.15% Si, 0.90% Mn, 1.35% Cr, 0.25% V, 0.90% Mo
0.15% C, 0.15% Si, 0.90% Mn, 1.35% Cr, 0.25% V, 0.90% Mo
0.15% C, 0.19% Si, 0.81% Mn, 0.55% Ni, 0.63% Cr, 0.11% Mo
0.15% C, 0.20% Si, 0.38% Mn, 0.018% S, 0.027% P, 4.33% Ni, 1.16% Cr, 0.17% Mo
0.15% C, 0.20% Si, 0.38% Mn, 0.018% S, 0.027% P, 4.33% Ni, 1.16% Cr, 0.17% Mo
0.15% C, 0.20% Si, 0.45% Mn, 0.013% P, 0.020% S, 4.03% Ni, 1.54% Cr, 0.03% Mo
0.15% C, 0.22% Si, 0.41% Mn, 0.021% P, 0.024% S, <0.005% Al, 0.06% Cr, 0.15% Cu, 0.005% N, 0.06% Ni
0.15% C, 0.22% Si, 0.41% Mn, 0.021% P, 0.024% S, 0.06% Cr, 0.15% Cu
0.15% C, 0.24% Si, 0.48% Mn, 0.012% P, 0.006% S, 0.10% Cr, 3.52% Ni
0.15% C, 0.24% Si, 0.67% Mn, 0.015% P, 0.033% S, 0.15% Cr, 0.25% Mo, 0.08% Ni, 0.10% Cu
0.15% C, 0.24% Si, 0.67% Mn, 0.015% P, 0.033% S, 0.15% Cr, 0.25% Mo, 0.08% Ni, 0.10% Cu
0.15% C, 0.25% Si, 0.40% Mn, 0.020-0.035% S, other: Pb
0.15% C, 0.25% Si, 0.40% Mn
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr, (Pb)
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr, (Pb)
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr
0.15% C, 0.25% Si, 0.50% Mn, 0.60% Cr
0.15% C, 0.25% Si, 0.50% Mn, 0.65% Cr
0.15% C, 0.25% Si, 0.50% Mn, 0.65% Cr
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Mo
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Mo
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni, (Pb)
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni, (Pb)
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni
0.15% C, 0.25% Si, 0.50% Mn, 1.55% Cr, 1.55% Ni
0.15% C, 0.25% Si, 0.60% Mn, 0.90% Cr, 0.50% Mo
0.15% C, 0.25% Si, 0.60% Mn, 0.90% Cr, 0.50% Mo
0.15% C, 0.25% Si, 0.65% Mn, 0.30% Mo
0.15% C, 0.25% Si, 0.65% Mn, 0.30% Mo
0.15% C, 0.25% Si, 0.85% Mn, 0.86% Ni, 0.52% Cr, 0.42% Mo, 0.055% V, 0.099% Al
0.15% C, 0.25% Si, 0.85% Mn, 0.86% Ni, 0.52% Cr, 0.42% Mo, 0.055% V, 0.099% Al
0.15% C, 0.25% Si, 1.10% Mn, 0.65% Ni, 0.11% Cr, 0.21% Mo
0.15% C, 0.25% Si, 1.10% Mn, 0.65% Ni, 0.11% Cr, 0.21% Mo
0.15% C, 0.25% Si, 1.10% Mn, 0.65% Ni, 0.11% Cr, 0.21% Mo
0.15% C, 0.25-1.00% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 8.00-11.00% Cr, 0.90-1.10% Mo
0.15% C, 0.26% Si, 0.79% Mn, 0.020% P, 0.240% S, 17.10% Cr, 0.34% Mo, 0.10% Ni
0.15% C, 0.26% Si, 1.02% Mn, 0.60% Ni, 0.10% Cr, 0.37% Mo, 0.08% V
0.15% C, 0.26% Si, 1.02% Mn, 0.60% Ni, 0.10% Cr, 0.37% Mo, 0.080% V
0.15% C, 0.27% Si, 0.40% Mn, 2.49% Ni, 1.19% Cr, 0.26% Mo
0.15% C, 0.27% Si, 0.40% Mn, 2.49% Ni, 1.19% Cr, 0.26% Mo
0.15% C, 0.27% Si, 0.47% Mn, 0.012% P, 0.007% S, 1.34% Cr, 0.18% Mo, 3.54% Ni, 0.15% Cu
0.15% C, 0.27% Si, 0.79% Mn, 0.84% Ni, 0.51% Cr, 0.50% Mo, 0.053% V, 0.006% B
0.15% C, 0.27% Si, 0.79% Mn, 0.84% Ni, 0.51% Cr, 0.50% Mo, 0.053% V, 0.006% B
0.15% C, 0.28% Si, 0.92% Mn, 0.08% Ni, 0.04% Cr, 0.46% Mo, 0.006% B
0.15% C, 0.28% Si, 0.92% Mn, 0.08% Ni, 0.04% Cr, 0.46% Mo, 0.040% V, 0.006% B
0.15% C, 0.28% Si, 0.97% Mn, 0.02% Ni, 0.01% Cr
0.15% C, 0.28% Si, 0.97% Mn, 0.02% Ni, 0.01% Cr
0.15% C, 0.28% Si, 1.34% Mn, 1.15% Ni, 0.02% Cr, 0.31% Mo
0.15% C, 0.28% Si, 1.34% Mn, 1.15% Ni, 0.02% Cr, 0.31% Mo
0.15% C, 0.29% Si, 1.20% Mn, 0.71% Ni, 0.36% Cr, 0.51% Mo, 0.01% V
0.15% C, 0.29% Si, 1.20% Mn, 0.71% Ni, 0.36% Cr, 0.51% Mo, 0.010% V
0.15% C, 0.30% Si, 0.55% Mn, 0.001% S, 0.013% P, 1.30% Ni, 0.82% Cr, 0.09% Mo
0.15% C, 0.30% Si, 1.47% Mn, 0.008% P, 0.001% S, 0.04% Cr, 0.02% Mo, 0.67% Ni, 0.03% Cu, 0.038% Al
0.15% C, 0.30% Si, 1.47% Mn, 0.008% P, 0.001% S, 0.04% Cr, 0.02% Mo, 0.67% Ni, 0.03% Cu, 0.038% Al
0.15% C, 0.31% Si, 1.52% Mn, 0.05% Al, + Nb and Mo
0.15% C, 0.31% Si, 1.52% Mn, 0.05% Al, + Nb and Mo
0.15% C, 0.31% Si, 1.52% Mn, 1.00% Al, + Nb and Mo
0.15% C, 0.31% Si, 1.52% Mn, 1.00% Al, + Nb and Mo
0.15% C, 0.32% Mn, 0.31% Si, 2.72% Ni, 1.52% Cr, 0.41% Mo
0.15% C, 0.32% Mn, 0.35% Si, 0.005% S, 0.016% P 3.09% Ni, 0.84% Cr, 0.14% Mo, 0.12% Cu
0.15% C, 0.32% Si, 1.41% Mn
0.15% C, 0.33% Si, 1.03% Mn, 0.36% Cr, 0.44% Mo
0.15% C, 0.33% Si, 1.03% Mn, 0.80% Ni, 0.38% Cr, 0.44% Mo
0.15% C, 0.34% Si, 0.26% Mn, 0.025% P, 0.003% S, 1.13% Cr, 0.32% Mo, 2.78% Ni, 0.01% W, 0.09% Co, 0.08% Cu, 0.031% Al
0.15% C, 0.34% Si, 0.38% Mn, 2.92% Ni, 0.74% Cr, 0.53% Mo
0.15% C, 0.34% Si, 0.38% Mn, 2.92% Ni, 0.74% Cr, 0.53% Mo
0.15% C, 0.34% Si, 0.49% Mn, 0.017% P, 0.033% S, 2.06% Cr, 1.91% Ni, 0.24% Cu, 0.05% Mo
0.15% C, 0.34% Si, 0.92% Mn, 0.29% Ni, 0.10% Cr, 0.51% Mo
0.15% C, 0.34% Si, 0.92% Mn, 0.29% Ni, 0.10% Cr, 0.51% Mo
0.15% C, 0.35% Si, 1.00% Mn, 0.35% Ni, 1.20% Mo, 0.65% Cu, 0.02% Nb
0.15% C, 0.35% Si, 1.00% Mn, 1.20% Ni, 0.35% Mo, 0.65% Cu, 0.02% Nb
0.15% C, 0.35% Si, 1.03% Mn, 0.80% Ni, 0.38% Cr, 0.44% Mo
0.15% C, 0.35% Si, 1.03% Mn, 0.80% Ni, 0.38% Cr, 0.44% Mo
0.15% C, 0.35% Si, 1.06% Mn, 0.81% Ni, 0.43% Cr, 0.40% Mo
0.15% C, 0.35% Si, 1.06% Mn, 0.81% Ni, 0.43% Cr, 0.40% Mo
0.15% C, 0.35% Si, 1.28% Mn, 0.47% Ni, 0.08% Cr, 0.21% Mo, 0.10% V
0.15% C, 0.35% Si, 1.28% Mn, 0.47% Ni, 0.08% Cr, 0.21% Mo, 0.10% V
0.15% C, 0.36% Mn, 0.44% Si, 0.020% S, 0.022% P 0.09% Ni, 2.24% Cr, 0.85% Mo, 0.23% Cu, 0.097% Al, 0.01% Ti
0.15% C, 0.36% Mn, 0.44% Si, 0.020% S, 0.022% P 0.09% Ni, 2.24% Cr, 0.85% Mo, 0.23% Cu, 0.097% Al, 0.01% Ti
0.15% C, 0.38% Mn, 0.20% Si, 4.33% Ni, 1.16% Cr 0.17% Mo
0.15% C, 0.38% Mn, 0.20% Si, 4.33% Ni, 1.16% Cr 0.17% Mo
0.15% C, 0.4% Mn, 3.0% Cr, 0.7% Mo, 0.28% V, 0.7% Ni
0.15% C, 0.40% Mn, 0.15% Si, 0.020% P, 0.020% S, 1.15% Cr, 4.10% Ni
0.15% C, 0.40% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.40% Cr
0.15% C, 0.40% Mn, 0.25% Si, 0.020% P, 0.018% S, 1.15% Cr, 4.10% Ni, 0.20% Mo
0.15% C, 0.40% Si, 1.19% Mn, 0.09% Ni
0.15% C, 0.40% Si, 1.19% Mn, 0.09% Ni
0.15% C, 0.42% Si, 0.40% Mn, 0.02% S, 1.31% Cr, 2.44% Ni, 0.22% V, 0.52% Cu, 0.0026% Al, 0.0091% N, 0% B. B5 steel: 0.09% C, 0.29% Si, 0.41% Mn, 0.02% S, 1.30% Cr, 2.42% Ni, 0.22% V, 0.50% Cu, 0.0031% Al, 0.0087% N, 0.0214% B.
0.15% C, 0.42% Si, 1.21% Mn, 0.06% Ni, 0.04% Cr, 0.051% Al
0.15% C, 0.42% Si, 1.21% Mn, 0.06% Ni, 0.04% Cr, 0.051% Al
0.15% C, 0.45% Mn, 0.013% P, 0.020% S, 0.20% Si, 4.03% Ni, 1.54% Cr, 0.03% Mo
0.15% C, 0.45% Mn, 0.20% Si, 0.013% P, 0.020% S 4.03% Ni, 1.54% Cr, 0.03% Mo
0.15% C, 0.45% Si, 1.27% Mn, 0.009% P, 0.011% S, 0.07% Ni, 0.05% Cr, 0.02% Mo, 0.21% Cu
0.15% C, 0.45% Si, 1.27% Mn, 0.009% P, 0.011% S, 0.07% Ni, 0.05% Cr, 0.21% Cu, 0.02% Mo
0.15% C, 0.45% Si, 1.27% Mn, 0.07% Ni, 0.05% Cr, 0.02% Mo
0.15% C, 0.45% Si, 1.27% Mn, 0.07% Ni, 0.05% Cr, 0.02% Mo
0.15% C, 0.45% Si, 1.33% Mn, 0.29% Cr, 0.14% V, 0.033% Al
0.15% C, 0.45% Si, 1.33% Mn, 0.29% Cr, 0.14% V, 0.033% Al
0.15% C, 0.47% Si, 1.54% Mn, 0.0145% P, 0.005% S, 0.82% Ni, 0.34% Cr, 0.355% Mo, 0.009% Nb
0.15% C, 0.47% Si, 1.54% Mn, 0.0145% P, 0.005% S, 0.82% Ni, 0.34% Cr, 0.355% Mo, 0.009% Nb
0.15% C, 0.48% Mn, 0.33% Si, 0.010% S, 0.012% P 4.21% Ni, 1.00% Cr, 0.20% Mo, 0.21% Cu
0.15% C, 0.48% Si, 0.67% Mn, 0.044% P, 0.024% S, 1.20% Cr, 0.18% Cu, 0.25% Ni, 0.31% V
0.15% C, 0.50% Mn, 0.18% Si, 0.018% P, 0.012% S, 0.165% Ni, 2.12% Cr, 0.94% Mo, 0.077% Cu 0.009% Sn
0.15% C, 0.50% Mn, 0.18% Si, 0.018% P, 0.012% S, 0.165% Ni, 2.12% Cr, 0.94% Mo, 0.077% Cu 0.009% Sn
0.15% C, 0.50% Mn, 0.18% Si, 0.018% P, 0.012% S, 0.165% Ni, 2.12% Cr, 0.94% Mo, 0.077% Cu 0.009% Sn
0.15% C, 0.50% Mn, 2.12% Cr, 0.90% Mo, 0.17% Ni
0.15% C, 0.50-1.00% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 6.00-8.00% Cr, 0.45-0.65% Mo
0.15% C, 0.53% Mn, 0.26% Si, 0.013% S, 0.020% P 0.11% Ni, 1.04% Cr, 1.05% Mo, 0.15% Cu, 0.25% V, 0.028% Al
0.15% C, 0.53% Si, 1.20% Mn, 0.09% Ni, 0.03% Cr, 0.08% Al
0.15% C, 0.53% Si, 1.20% Mn, 0.09% Ni, 0.03% Cr, 0.080% Al
0.15% C, 0.55% Mn, 0.30% Si, <0.010% S, 0.013% P 1.38% Ni, 0.82% Cr, 0.09% Mo, 0.11% Cu
0.15% C, 0.55% Mn, 0.30% Si, <0.010% S, 0.013% P 1.38% Ni, 0.82% Cr, 0.09% Mo, 0.11% Cu
0.15% C, 0.57% Mn, 0.28% Si, 0.019% S, 0.013% P, 0.63% Cr, 0.91% Ni, 0.61% Mo, 0.30% V, 0.032% Al
0.15% C, 0.60% Mn, 0.30% Si, 0.030% P, 0.030% S, 1.25% Cr, 0.50% Mo
0.15% C, 0.63% Mn, 0.019% P, 0.026% S, 0.28% Si, 1.90% Cr, 0.05% Cr, 0.24% Mo
0.15% C, 0.63% Mn, 1.90% Ni, 0.24% Mo /0.16% C, 0.60% Mn, 1.92% Ni, 0.27% Mo
0.15% C, 0.63% Mn, 1.90% Ni, 0.24% Mo
0.15% C, 0.63% Mn, 1.90% Ni, 0.24% Mo
0.15% C, 0.63% Si, 1.09% Mn, 14.53% Cr, 5.30% Ni, 2.32% Mo, 0.12% Al
0.15% C, 0.65% Mn, 0.58% Si, 0.009% P, 0.005% S, 1.40% Cr, 0.59% Mo, 0.027% sol Al
0.15% C, 0.67% Mn, 0.48% Si, 0.024% S, 0.044% P, 1.20% Cr, 0.25% Ni, 0.31% V, 0.18% Cu, 17.89% W
0.15% C, 0.71% Mn, 0.28% Si, 0.005% S, 0.007% P, 0.25% Cr, 1.05% Ni, 0.05% Mo, 0.08% V, 0.15% Cu
0.15% C, 0.75% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.95% Cr, 1.45% Ni
0.15% C, 0.77% Mn, 0.20% Si, 0.011% S, 0.010% P, 1.27% Cr, 4.25% Ni, 0.45% Mo, 0.10% V, 0.23% Nb
0.15% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.15% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.63% Cr, 0.85% Ni, 0.05% Mo
0.15% C, 0.86% Mn, 0.28% Si, 0.010% S, 0.014% P 0.14% Ni, 0.84% Cr, 0.20% Mo
0.15% C, 0.90% Mn, 0.40% Si, 0.05% V, 0.014% N
0.15% C, 0.92% Mn, 0.014% P, 0.020% S, 0.26% Si, 0.88% Ni, 0.50% Cr, 0.46% Mo, 0.32% Cu, 0.06% V, 0.003% B
0.15% C, 0.92% Mn, 0.26% Si, 0.014% P, 0.020% S 0.88% Ni, 0.50% Cr, 0.46% Mo, 0.32% Cu, 0.06% V, 0.003% B
0.15% C, 0.92% Mn, 0.50% Cr, 0.88% Ni, 0.46% Mo, 0.06% V, 0.003% B, 0.32% Cu
0.15% C, 0.92% Mn, 0.88% Ni, 0.50% Cr, 0.46% Mo, 0.06% V, 0.32% Cu, 0.0031% B
0.15% C, 0.92% Mn, 0.88% Ni, 0.50% Cr, 0.46% Mo, 0.06% V, 0.32% Cu, 0.0031% Cu
0.15% C, 1.00% Mn, 0.23% Si, 0.014% P, 0.023% S, 0.94% Ni, 0.53% Cr, 0.45% Mo, 0.34% Cu, 0.004% Ti, 0.0014% B, 0.05% V, 0.008% Sn
0.15% C, 1.01% Si, 1.55% Mn, 0.013% P, 0.003% N
0.15% C, 1.30% Mn, 0.27% Si, 0.009% S, 0.010% P, 0.15% Cr, 0.15% Ni, 0.04% Mo, 0.13% V, 0.19% Cu, 0.02% Al, 0.010% N
0.15% C, 1.39% Mn, 0.40% Si, 0.013% S, 0.016% P, 0.27% Mo, 0.05% V, sol. 0.018% Al, 0.004% N
0.15% C, 1.40% Mn, 0.25% Si, 0.020% P, 0.020% S
0.15% C, 1.49% Mn, 0.39% Si, 0.018% P, 0.015% S, 0.50% Mo, 0.16% V, 0.14% N
0.15% C, 3.06% Mn, 0.59% Si, 0.005% S, 0.020% P, 0.14% Cr, 0.04% Ni, 0.46% Mo, 0.09% V, 0.09% Cu, 0.70% W
0.15% C, max. 0.50% Si, max. 1.00% Mn, max. 0.04% P, max. 0.03% S, 11.50-13.00% Cr
0.15% C, max. 1.00% Si, max. 1.00% Mn, max. 0.04% P, max. 0.03% S, 11.50-13.50% Cr, max. 0.75% Ni
0.15% C, max. 1.00% Si, max. 1.50% Mn, 16.50% Cr, 0.40% Mo, 0.25% S
0.15% C, max.1.00% Mn, max.0.50% Si, max.0.04% P, max.0.03% S, 11.50-13.00% Cr
0.15% C
0.15% C
0.15-0.18% C, 0.15-0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.005% S, 1.30-1.60% Cr, 3.25-3.75% Ni, 0.15-0.25% Mo
0.15-0.19% C, 1.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.025% Cu
0.15-0.20% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% Si, 2.70-3.00% Cr, 0.20-0.30% Mo, 0.10-0.20% V
0.15-0.20% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% Si, 2.70-3.00% Cr, 0.20-0.30% Mo, 0.10-0.20% V
0.15-0.20% C, 0.15-0.40% Si, 0.40-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.10% Cr, 1.80-2.10% Ni
0.15-0.20% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.80-2.10% Cr, 1.80-2.10% Ni
0.15-0.20% C, 0.15-0.40% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.80-2.10% Cr, 1.80-2.10% Ni
0.15-0.21% C, <0.40% Si, 0.50-0.90% Mn, <0.035% P, <0.035% S, 1.50-1.80% Cr, 1.40-1.70% Ni, 0.25-0.35% Mo
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, 0.40% Si, 0.50-0.90% Mn, 0.035% P, 0.035% S, 1.50-1.80% Cr, 0.25-0.35% Mo, 1.40-1.70% Ni
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.0% Cr, 1.20-1.50% Ni
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.0% Cr, 1.20-1.50% Ni
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.25% Mo
0.15-0.21% C, 0.60-0.90% Mn, 0.15-0.40% Si, 0.70-1.00% Cr, 0.15-0.25% Mo, 1.20-1.50% Ni
0.15% C, 0.26% Si, 0.92% Mn, 0.88% Ni, 0.50% Cr, 0.46% Mo, 0.32% Cu, 0.06% V, +B
0.15% C, 1.39% Mn, 0.33% Si, 0.008% P, 0.012% S, 0.04% Cr, 0.09% Ni, 0.03% Mo, 0.15% Cu, 0.031% Al, 0.002% V, 0.001% Nb, 0.004% Ti, 0.01% N, 0.01% Co, 0.004% W, 0.0005% B
0.15% C, 0.50% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 2.00-2.50% Cr, 0.90-1.10% Mo
0.15% C, 0.50% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 4.00-6.00% Cr, 0.45-0.65% Mo
0.15% C, 0.45% Si, 1.27% Mn, 0.009% P, 0.011% S, 0.07% Ni, 0.05% Cr, 0.21% Cu, 0.02% Mo
0.15% C, 0.23% Si, 1.3% Mn, 0.09% Cr, 0.019% Ni, 0.01% V, 0.05% Nb, 0.025% Al, 0.007% N, 0.013% S, 0.017% P
0.15% C, 0.04% Si, 0.51% Mn, 0.033% P, 0.017% P, 11.8% Cr, 0.23% Ni
0.15% C, 0.30% Si, 1.57% Mn, 0.30% Mo, 3.00% Ni, 1.00% Cu, 1.00% Al, 0.0007% S, 0.021% P
0.15% C, 0.22% Si, 0.41% Mn, 0.021% P, 0.024% S, 0.005% Al, 0.06% Cr, 0.15% Cu, 0.005% N, 0.06% Ni
0.15% C, 0.27% Si, 0.40% Mn, 0.021% P, 0.013% S, 16.91% Cr, 0.13% Mo, 1.62% Ni, 0.07% W, 0.16% Cu, 0.074% Co
0.15% C, 0.22% Si, 0.41% Mn, 0.021% P, 0.024% S, 0.005% Al, 0.06% Cr, 0.15% Cu, 0.005% N, 0.06% Ni
0.15% C, 0.21% Si, 0.47% Mn, 0.005% P, 0.022% S, 0.044% Al, 1.49% Cr, 0.03% Co, 0.05% Cu, 0.03% Mo, 0.006% N, 1.44% Ni
0.15% C, 0.21% Si, 0.47% Mn, 0.005% P, 0.022% S, 0.044% Al, 1.49% Cr, 0.03% Co, 0.05% Cu, 0.03% Mo, 0.006% N, 1.44% Ni
0.15% C, 0.25% Si, 0.48% Mn, 0.022% P, 0.045% S, 0.14% Cu, 0.13% Cr, 0.09% Ni, 0.02% Mo, 0.01% Ti, 0.024% Al, 0.04% V
0.15% C, 0.16% Si, 0.48% Mn, 0.020% P, 0.035% S
0.15% C, 0.36% Si, 1.52% Mn, 0.012% P, 0.012% S, 0.20% Cu, 0.11% Cr, 0.53% Ni, 0.006% Ti, 0.022% Al
0.15% C, 0.92% Si, 0.78% Mn, 0.026% P, 0.03% S, 0.79% Cr, 0.63% Ni, 0.51% Cu, 0.034% Al, 0.07% Mo, 0.01% Ti, 0.07% V
0.15% C, 0.35% Si, 1.10% Mn, 0.024% P, 0.011% S, 0.18% Cu, 1.54% Cr, 0.17% Ni, 0.42% Mo, 0.002% B, 0.05% V
0.15% C, 0.44% Si, 1.48% Mn, 0.032% P, 0.018% S, 0.02% Cr, 0.01% Ni, 0.0008% Mo, 0.002% Nb, 0.003% Ti, 0.019% Al, 0.02% Cu
0.15% C, 0.344% Si, 1.23% Mn, 0.019% P, 0.001% S, 0.027% Cr, 0.013% Mo, 0.042% Ni, 0.046% Al, 0.041% Nb, 0.02% Ti, 0.007% V
0.15% C, 0.468% Si, 1.31% Mn, 0.014% P, 0.003% S, 0.545% Cr, 0.318% Mo, 0.787% Ni, 0.041% Al, 0.042% Cu, 0.025% Nb, 0.039% V
0.15% C, 0.59% Si, 0.79% Mn, 0.007% P, 0.011% S
0.15% C, 0.44% Si, 0.80% Mn, 0.020% P, 0.013% S, 0.07% Cu, 0.16% Cr, 0.09% Ni, 0.05% Mo, 0.01% Al, 0.05% V
0.15% C, 0.41% Si, 0.76% Mn, 0.024% P, 0.007% S, 0.09% Cu, 1.40% Cr, 0.47% Ni, 0.95% Mo, 0.025% Al, 0.32% V
0.152% C, 0.467% Si, 1.545% Mn, 0.004% S, 0.021% P, 0.025% Ni, 0.02% Cr, 0.152% C, 0.288% Si, 0.637% Mn, 0.016% P, 0.014% S, 0.918% Cr, 0.029% Ni, 0.473% Mo, 0.042% Al, 0.052% Cu, 0.002% Nb, 0.001% Ti
0.153% C, 0.29% Si, 0.998% Mn, 0.007% P, 0.004% S, 0.626% Cr, 0.492% Mo, 1.99% Ni, 0.004% Al, 0.016% Cu, 0.001% Nb, 0.078% V
0.155% C, 0.351% Si, 0.857% Mn, 0.009% P, 0.004% S, 0.512% Cr, 1.830% Ni, 0.439% Mo, 0.049% Al, 0.024% Cu, 0.016% Nb, 0.002% Ti, 0.042% V
0.156% C, 1.6% Mn, 0.38% Ni, 0.75% Cr, 0.007% Ti, 0.034% Al
0.158% C, 1.6% Mn, 0.39% Si, 0.83% Cr, 0.0013% Ti, 0.043% Al, 0.056% Nb
0.158% C, 0.365% Si, 0.84% Mn, 0.015% P, 0.003% S, 0.050% Cr, 1.48% Ni, 0.51% Mo, 0.036% Al, 0.042% V, 0.012% Nb, 0.011% N
0.159% C, 0.307% Si, 1.44% Mn, 0.01% P, 0.007% S, 0.008% Cr, 0.003% Ni, 0.028% V, 0.023% Nb, 0.025% Al, 0.001% Mo
0.159% C, 0.33% Si, 1.54% Mn, 0.008% P, 0.005% S, 0.031% Cr, 0.599% Ni, 0.013% Mo, 0.021% Cu, 0.022% Al, 0.002% Nb, 0.022% Ti, 0.163% V
0.16% C, <0.02% Ni, 2.40% Cr, <0.02% Mo, <0.001% B. Alloy C2: 0.17% C, <0.02% Ni, 3.16% Cr, <0.02% Mo, <0.001% B. Alloy C3: 0.14% C, <0.02% Ni, 3.83% Cr, <0.02% Mo, <0.001% B. Alloy C4: 0.15% C, <0.02% Ni, 4.15% Cr, <0.02% Mo, <0.001% B
0.16% C, 0.015% Si, 1.30% Mn, 0.007% S, 0.010% P, 0.74% Ni, 0.18% Cr, 0.48% Mo, 0.06% Cu, 0.01% Co
0.16% C, 0.21% Si, 0.27% Mn, 0.11% Cr
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.015% Al, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.01% V
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.015% Al, 0.99% Cr, 0.022% Mo, 0.12% Ni, 0.01% V
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.01% V
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.01% V
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.010% V, 0.015% Al
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.010% V, 0.015% Al
0.16% C, 0.23% Si, 0.82% Mn, 2.00% Ni, 0.76% Cr, 0.49% Mo, 0.07% V, 0.023% Al
0.16% C, 0.23% Si, 0.82% Mn, 2.00% Ni, 0.78% Cr, 0.49% Mo, 0.070% V, 0.023% Al
0.16% C, 0.23% Si, 1.16% Mn, 1.54% Ni, 0.50% Cr, 0.42% Mo, 0.026% V, 0.035% Al, 0.056% Nb
0.16% C, 0.23% Si, 1.16% Mn, 1.54% Ni, 0.50% Cr, 0.42% Mo, 0.026% V, 0.035% Al, 0.056% Nb
0.16% C, 0.24% Si, 0.43% Mn, 0.008% P, 0.005% S, 1.55% Cr, 1.44% Ni, 0.26% Mo, 0.01% V, 0.01% Ti, 0.033% Al, 0.9 ppm H2
0.16% C, 0.24% Si, 0.83% Mn, 0.03% Ni, 0.04% Cr, 0.04% Al
0.16% C, 0.24% Si, 0.83% Mn, 0.03% Ni, 0.04% Cr, 0.04% Al
0.16% C, 0.25% Si, 0.21% Mn, 1.59% Cr, 0.52% Mo, 3.02% Ni, 0.04% Cu
0.16% C, 0.25% Si, 0.50% Mn, 0.018% P, 0.018% S, 1.62% Cr, 0.27% Mo, 1.48% Ni
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni, (Pb). 16NiCrS4: 0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni, (Pb)
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni, (Pb). 16NiCrS4: 0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni, (Pb)
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.16% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr + B
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, <0.035% S, (Pb). 16MnCrS5: 0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, 0.020-0.035% S, (Pb)
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, <0.035% S, (Pb). 16MnCrS5: 0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, 0.020-0.035% S, (Pb)
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr, +B, (Pb)
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.25% Si, 1.15% Mn, 0.95% Cr
0.16% C, 0.26% Si, 0.75% Mn, 0.79% Ni, 0.51% Cr, 0.46% Mo, 0.005% B
0.16% C, 0.26% Si, 0.75% Mn, 0.79% Ni, 0.51% Cr, 0.46% Mo, 0.050% V, 0.005% B
0.16% C, 0.27% Si, 0.47% Mn, 0.012% P, 0.007% S, 1.34% Cr, 0.18% Mo, 3.54% Ni, 0.15% Cu
0.16% C, 0.27% Si, 1.47% Mn, 0.033% P, 0.009% S, 0.33% Mo, 0.55% Ni, 0.14% V, 0.005% Al, 0.021% N
0.16% C, 0.28% Si, 0.36% Mn, 2.25% Ni, 1.20% Cr, 0.42% Mo
0.16% C, 0.28% Si, 0.36% Mn, 2.25% Ni, 1.20% Cr, 0.42% Mo
0.16% C, 0.28% Si, 0.58% Mn, 0.008% P, 0.027% S, 0.47% Cr, 0.26% Mo, 1.83% Ni, 0.11% Cu
0.16% C, 0.30% Si, 0.21% Mn, 0.012% P, 0.017% S, 2.96% Cr, 0.21% Ni, 0.19% V, 0.79% Cu, 0.020% Al
0.16% C, 0.30% Si, 0.68% Mn, 0.012% P, 0.038% S, 0.29% Mo
0.16% C, 0.31% Si, 0.50% Mn, 0.013% P, 0.014% S, 1.95% Cr, 0.03% Al, 0.03% Mo, 2.02% Ni, 0.01% V
0.16% C, 0.31% Si, 0.50% Mn, 0.013% P, 0.014% S, 1.95% Cr, 0.03% Al, 0.03% Mo, 2.02% Ni, 0.01% V
0.16% C, 0.32% Si, 0.48% Mn, 0.015% P, 0.010% S, 1.65% Cr, 0.29% Mo, 1.50% Ni
0.16% C, 0.32% Si, 0.48% Mn, 0.015% P, 0.010% S, 1.65% Cr, 0.29% Mo, 1.50% Ni
0.16% C, 0.32% Si, 0.48% Mn, 0.015% P, 0.010% S, 1.65% Cr, 0.29% Mo, 1.50% Ni
0.16% C, 0.32% Si, 0.48% Mn, 1.65% Cr, 0.29% Mo, 1.50% Ni
0.16% C, 0.32% Si, 0.48% Mn, 1.65% Cr, 0.29% Mo, 1.50% Ni
0.16% C, 0.32% Si, 0.50% Mn, 0.016% P, 0.017% S, 1.57% Cr, 0.29% Mo, 1.47% Ni
0.16% C, 0.34% Si, 0.46% Mn, 0.029% P, 0.022% S, 0.69% Cr, 0.15% Mo, 3.50% Ni, 0.035% Al
0.16% C, 0.34% Si, 0.46% Mn, 0.029% P, 0.022% S, 0.69% Cr, 0.15% Mo, 3.50% Ni, 0.035% Al
0.16% C, 0.34% Si, 1.43% Mn, 0.47% Cr, 0.36% Mo, 0.11% Ni, 0.03% V, 0.010% Cu, 0.065% Al
0.16% C, 0.36% Si, 0.58% Mn, 0.016% P, 0.011% S, 1.05% Cr, 0.42% Mo
0.16% C, 0.36% Si, 0.58% Mn, 0.016% P, 0.011% S, 1.05% Cr, 0.42% Mo
0.16% C, 0.39% Si, 1.48% Mn, 0.021% P, 0.015% S
0.16% C, 0.39% Si, 1.48% Mn, 0.021% P, 0.015% S
0.16% C, 0.41% Si, 1.22% Mn, 0.02% Ni
0.16% C, 0.41% Si, 1.22% Mn, 0.02% Ni
0.16% C, 0.43% Si, 1.31% Mn, 0.04% Ni, 0.06% Cr, 0.02% Mo, 0.017% V, 0.05% Al
0.16% C, 0.43% Si, 1.31% Mn, 0.04% Ni, 0.06% Cr, 0.02% Mo, 0.017% V, 0.050% Al
0.16% C, 0.45% Si, 1.12% Mn, 0.04% Ni, 0.06% Cr, 0.02% Mo, 0.011% V, 0.017% Al
0.16% C, 0.45% Si, 1.12% Mn, 0.04% Ni, 0.06% Cr, 0.02% Mo, 0.011% V, 0.017% Al
0.16% C, 0.45% Si, 1.16% Mn, 0.02% Ni, 0.02% Cr, 0.049% Al
0.16% C, 0.45% Si, 1.18% Mn, 0.02% Ni, 0.02% Cr, 0.049% Al
0.16% C, 0.46% Mn, 0.20% Si, 0.013% S, 0.008% P 3.02% Ni, 1.02% Cr, 0.26% Mo, 0.12% Cu
0.16% C, 0.46% Mn, 0.20% Si, 0.013% S, 0.008% P 3.02% Ni, 1.02% Cr, 0.26% Mo, 0.12% Cu
0.16% C, 0.46% Si, 1.35% Mn, 0.020% Al
0.16% C, 0.46% Si, 1.35% Mn, 0.020% Al
0.16% C, 0.47% Si, 1.24% Mn, 0.029% P, 0.29% S, 0.024% Al, 0.0085% N, 0.10% Cr, 0.17% Cu, 0.06% Ni
0.16% C, 0.47% Si, 1.40% Mn, 0.04% Ni, 0.05% Cr, 0.061% Al
0.16% C, 0.48% Si, 1.42% Mn
0.16% C, 0.48% Si, 1.42% Mn
0.16% C, 0.49% Mn, 1.14% Si, 0.080% S, 0.010% P 0.25% Ni, 1.22% Cr, 1.05% Mo, 0.19% Cu, 0.46% V, 0.030% Ti
0.16% C, 0.49% Mn, 1.14% Si, 0.080% S, 0.010% P 0.25% Ni, 1.22% Cr, 1.05% Mo, 0.19% Cu, 0.46% V, 0.030% Ti
0.16% C, 0.50% Mn, 0.25% Si, 0.020% P, 0.025% S, 1.65% Cr, 1.55% Ni, 0.20% Mo
0.16% C, 0.50% Mn, 0.31% Si, 0.013% P, 0.014% S, 0.03% Al, 1.95% Cr, 0.03% Mo, 2.02% Ni, 0.01% V
0.16% C, 0.50% Mn, 0.31% Si, 0.013% P, 0.014% S, 1.95% Cr, 2.02% Ni, 0.03% Mo, 0.030% Al
0.16% C, 0.50% Mn, 0.31% Si, 0.014% S, 0.013% P, 1.95% Cr, 2.02% Ni, 0.03% Mo, 0.01% V, sol. 0.030% Al
0.16% C, 0.51% Mn, 0.27% Si, 0.019% S, 0.010% P 2.59% Ni, 0.67% Cr, 0.49% Mo, 0.20% Cu, 0.080% V
0.16% C, 0.51% Mn, 0.27% Si, 0.019% S, 0.010% P 2.59% Ni, 0.67% Cr, 0.49% Mo, 0.20% Cu, 0.080% V
0.16% C, 0.51% Si, 1.10% Mn, 0.04% Ni, 0.06% Cr, 0.01% Mo, 0.011% V, 0.047% Al
0.16% C, 0.51% Si, 1.10% Mn, 0.04% Ni, 0.06% Cr, 0.01% Mo, 0.047% Al
0.16% C, 0.52% Mn, 0.009% P, 0.010% S, 0.27% Si, 3.36% Ni, 0.09% Cr, 0.19% Mo, 0.04% Cu
0.16% C, 0.52% Mn, 3.36% Ni, 0.19% Mo
0.16% C, 0.52% Mn, 3.36% Ni, 0.19% Mo
0.16% C, 0.53% Mn, 0.18% Si, 1.56% Ni, 0.26% Cr 0.25% Mo
0.16% C, 0.53% Mn, 0.18% Si, 1.56% Ni, 0.26% Cr 0.25% Mo
0.16% C, 0.58% Mn, 0.53% Si, 0.009% P, 0.005% S, 1.41% Cr, 0.59% Mo, 0.062% sol Al, 0.0003% B
0.16% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.015% S, 0.20% Cr, 1.50% Ni, 0.05% Mo
0.16% C, 0.60% Mn, 0.26% Si, 0.015% P, 0.009% S, 0.31% Mo, 0.03% V, 0.004% Al, 0.009% N
0.16% C, 0.60% Mn, 1.92% Ni, 0.27% Mo, 0.0017% B
0.16% C, 0.70% Mn, 0.42% Si, 0.008% P, 0.029% S, 1.84% Ni, 0.78% Cr, 0.35% Mo, 0.00% Cu
0.16% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.85% Cr, 1.15% Ni, 0.05% Mo
0.16% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.05% Cr, 1.80% Ni, 0.15% Mo
0.16% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.025% S, 1.05% Cr, 1.40% Ni, 0.15% Mo
0.16% C, 0.81% Mn, 0.19% Si, 1.80% Ni, 0.48% Cr, 0.66% Mo
0.16% C, 0.85% Mn, 0.34% Si, 0.009% P, 0.019% S, 0.92% Cr, 0.15% V
0.16% C, 1.12% Mn, 0.22% Si, 0.008% S, 0.030% P, 0.99% Cr, 0.12% Ni, 0.02% Mo, 0.01% V, sol. 0.015% Al
0.16% C, 1.15% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.95% Cr
0.16% C, 1.30% Mn, 0.035% Si, 0.066% V, 0.013% Al
0.16% C, 1.30% Mn, 0.035% Si, 0.13% V, 0.013% Al
0.16% C, 1.40% Mn, 0.04% Si, 0.012% S, 0.004% P, 0.11% V, 0.04% Al, 0.018% N
0.16% C, 1.40% Mn, 0.25% Si, 0.020% P, 0.015% S, 0.20% Cr, 1.50% Ni, 0.05% Mo
0.16% C, 1.41% Mn, 0.36% Si, 0.018% P, 0.017% S, 0.031% Nb, 0.020% sol. Al, 0.0054% N
0.16% C, 1.42% Mn, 0.44% Si, 0.021% S, 0.032% P, 0.025% V, 0.003% Ti, 0.002% Nb, 0.042% Al
0.16% C, 5.06% Ni
0.16% C, 5.06% Ni
0.16-0.19% C, 0.20-0.40% Si, 0.75-1.00% Mn, 0.020-0.030% S, 1.75-2.00% Cr, 0.30% Ni, 0.50-0.60% Mo
0.16-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.50% Cr, 1.20-1.50% Ni
0.16-0.21% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.50% Cr, 1.20-1.50% Ni
0.16-0.22% C, 0.10-0.40% Si, 0.15-0.45% Mn, max. 0.030% P, max. 0.030% S, 1.10-1.40% Cr, 0.15-0.25% Mo, 3.80-4.30% Ni
0.16% C, 1.45% Mn, 1.48% Cr, 0.81% Ni, 0.41% Mo
0.16% C, 1.45% Mn, 1.48% Cr, 0.81% Ni, 0.41% Mo, 0.017% B
0.16% C, 0.22% Si, 1.12% Mn, 0.030% P, 0.008% S, 0.015% Al, 0.99% Cr, 0.02% Mo, 0.12% Ni, 0.01% V
0.16% C, 0.32% Si, 0.5% Mn, 0.016% P, 0.017% S, 1.57% Cr, 1.47% Ni, 0.29% Mo
0.16% C, 0.31% Si, 1.18% Mn, 0.017% P, 0.025% S, 0.96% Cr
0.16% C, 0.16% Si, 0.24% Mn, 9.51% Cr, 5.15% Mo, 0.50% V, 0.96% Co
0.16% C, 0.25% Si, 0.57% Mn, 0.016% P, 0.019% S, 0.003% Al, 1.56% Cr, 0.12% Cu, 0.004% N, 1.50% Ni
0.16% C, 0.25% Si, 0.57% Mn, 0.016% P, 0.019% S, 0.003% Al, 1.56% Cr, 0.12% Cu, 0.004% N, 1.50% Ni
0.16% C, 1.51% Cr, 4.30% Ni
0.16% C, 0.18% Si, 0.46% Mn, 0.020% P, 0.025% S, 0.09% Cr, 0.15% Cu, 0.06% Ni, 0.042% Al
0.16% C, 0.37% Si, 1.00% Mn, 0.027% P, 0.028% S, 0.08% Cu, 0.11% Cr, 0.04% Ni, 0.001% Ti, 0.018% Al
0.16% C, 0.41% Si, 1.35% Mn, 0.016% P, 0.017% S, 0.03% Nb, 0.009% Al, 0.036% Cr, 0.01% Ni, 0.02% Cu, 0.005% N
0.16% C, 0.50% Si, 1.55% Mn, 0.023% P, 0.031% S, 0.015% Al, 0015% N, 0.15% V, 0.14% Cr, 0.17% Cu, 0.02% Ni
0.16% C, 0.43% Si, 0.58% Mn, 0.020% P, 0.018% S, 2.38% Cr, 0.88% Mo, 0.10% V
0.16% C, 0.32% Si, 0.50% Mn, 0.010% P, 0.040% S, 0.84% Cr, 0.40% Mo
0.16% C, 0.20% Si, 0.49% Mn, 0.014% P, 0.024% S, 0.79% Cr, 0.41% Mo
0.16% C, 0.28% Si, 0.53% Mn, 0.014% P, 0.037% S, 0.75% Cr, 0.45% Mo, 0.017% V
0.16% C, 0.30% Si, 0.58% Mn, 0.012% P, 0.038% S, 0.29% Mo
0.16% C, 0.47% Si, 1.41% Mn, 0.008% P, 0.003% S, 0.037% Al, 0.063% Cr, 0.073% Ni, 0.20% Cu, 0.01% Mo, 0.02% Nb, 0.002% Ti
0.16% C, 0.392% Si, 0.812% Mn, 0.014% P, 0.001% S, 0.429% Cr, 0.500% Mo, 1.61% Ni, 0.048% Al, 0.03% Nb, 0.006% Ti, 0.043% V
0.16% C, 0.54% Si, 1.42% Mn, 0.013% P, 0.004% S, 0.60% Si, 0.39% Mo, 0.76% Ni, 0.017% Al, 0.06% Cu, 0.007% N, 0.05% V
0.16% C, 0.382% Si, 0.82% Mn, 0.014% P, 0.001% S, 0.431% Cr, 0.502% Mo, 1.62% Ni, 0.047% Al, 0.03% Nb, 0.006% Ti, 0.043% V
0.16% C, 0.29% Si, 0.99% Mn, 0.010% P, 0.002% S, 0.66% Cr, 0.52% Mo, 1.98% Ni, 0.030% Al, 0.05% Cu, 0.002% Ti, 0.075% V
0.16% C, 0.27% Si, 0.87% Mn, 0.012% P, 0.009% S, 0.47% Cr, 0.46% Mo, 1.95% Ni, 0.061% Al, 0.22% Cu, 0.02% V, 0.013% Nb, 0.003% Ti
0.16% C, 0.02% Si, 0.08% Mn, 0.004% P, 0.023% S
0.163% C, 0.288% Si, 1.24% Mn, 0.021% P, 0.003% S, 0.049% Cr, 0.013% Ni, 0.102% Mo, 0.070% Al, 0.004% V, 0.029% Nb, 0.006% N, 0.001% B
0.163% C, 0.360% Si, 1.420% Mn, 0.013% P, 0.007% S, 0.038% Cr, 0.003% Mo, 0.008% Ni, 0.035% Al, 0.009% V, 0.008% Nb, 0.005% Ti, 0.002% V, 0.040% W
0.164% C, 0.245% Si, 1.04% Mn, 0.011% P, 0.002% S, 0.542% Cr, 0.499% Mo, 1.95% Ni, 0.029% Al, 0.045% Cu, 0.003% Ti, 0.074% V
0.165% C, 0.361% Si, 1.60% Mn, 0.016% P, 0.005% S, 0.003% Nb, 0.017% Al, 0.045% Cr, 0.528% Ni, 0.025% Cu
0.17% C max., 0.55% Ni, 1.35% Cr, 0.20% Mo
0.17% C, 0.17% Si, 0.87% Mn, 0.021% P, 0.003% S, 1.39% Cr, 0.85% Mo, 0.38% Ni, 0.23% V, 0.058% Ti
0.17% C, 0.21% Si, 0.40% Mn, 0.026% P, 0.027% S, 11.61% Cr, 0.98% Mo
0.17% C, 0.21% Si, 0.41% Mn, 0.007% P, 0.006% S, 1.36% Cr, 3.32% Ni, 0.26% Cu, 0.05% Mo, 0.018% Sn
0.17% C, 0.21% Si, 1.35% Mn, 0.017% P, 0.005% S, 0.019% Nb, 0.50% Ni, 0.001% B, 0.004% N, 0.005% O
0.17% C, 0.22% Si, 0.40% Mn, 0.11% Nb
0.17% C, 0.22% Si, 0.40% Mn, 0.110% Nb
0.17% C, 0.22% Si, 0.57% Mn, 0.027% P, 0.025% S, 12.00% Cr, 0.51% Mo, 0.81% Ni, 0.25% V, 0.20% Nb
0.17% C, 0.22% Si, 0.79% Mn, 0.036% P, 0.041% S
0.17% C, 0.22% Si, 0.79% Mn, 0.036% P, 0.041% S
0.17% C, 0.22% Si, 1.35% Mn, 0.11% Cr, 0.12% Ni, 0.10% Cu, 0.024% Al
0.17% C, 0.24% Si, 1.34% Mn, 0.04% Ni, 0.02% Cr, 0.027% Al
0.17% C, 0.24% Si, 1.34% Mn, 0.04% Ni, 0.02% Cr, 0.027% Al
0.17% C, 0.24% Si, 1.46% Mn, 0.008% P, 0.005% S, 0.04% Cr, 0.76% Ni, 0.53% Mo, 0.11% Cu, 0.035% Al. Steel 2: 0.20% C, 0.21% Si, 1.46% Mn, 0.010% P, 0.007% S, 0.03% Cr, 0.78% Ni, 0.50% Mo, 0.10% Cu, 0.021% Al
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 0.30% Mo, 1.55% Ni, (Pb)
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 0.30% Mo, 1.55% Ni, (Pb)
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 1.55% Ni, 0.30% Mo
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 1.55% Ni, 0.30% Mo
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 1.55% Ni, 0.30% Mo
0.17% C, 0.25% Si, 0.50% Mn, 1.65% Cr, 1.55% Ni, 0.30% Mo
0.17% C, 0.25% Si, 0.60% Mn, 0.30% Cr, 0.35% V, 0.90% Mo
0.17% C, 0.25% Si, 0.60% Mn, 0.30% Cr, 0.35% V, 0.90% Mo
0.17% C, 0.25% Si, 0.60% Mn, 0.30% Mo
0.17% C, 0.25% Si, 0.60% Mn, 0.30% Mo
0.17% C, 0.25% Si, 0.60% Mn, 0.30% Mo
0.17% C, 0.25% Si, 0.60% Mn, 0.30% Mo
0.17% C, 0.26% Si, 0.77% Mn, 0.011% P, 0.032% S, 1.15% Cr, 0.08% Ni, 0.015% Cu, 0.23% Mo, 1.50 ppm H2, 0.026% Al
0.17% C, 0.26% Si, 0.77% Mn, 0.011% P, 0.032% S, 1.15% Cr, 0.08% Ni, 0.015% Cu, 0.23% Mo, 1.50 ppm H2, 0.026% Al
0.17% C, 0.27% Si, 0.43% Mn, 1.48% Cr, 0.25% Mo, 3.45% Ni, 0.13% Cu, 0.026% Al
0.17% C, 0.27% Si, 0.43% Mn, 1.48% Cr, 0.25% Mo, 3.45% Ni, 0.13% Cu, 0.026% Al
0.17% C, 0.27% Si, 0.46% Mn, 0.038% P, 0.018% S, 11.88% Cr, 1.16% Mo, 0.01% Ni
0.17% C, 0.27% Si, 0.79% Mn, 0.009% P, 0.020% S, 0.08% Cr, 0.16% Cu, 0.41% Mo, 0.45% Ni, 0.02% V
0.17% C, 0.27% Si, 0.79% Mn, 0.009% P, 0.020% S, 0.08% Cr, 0.41% Mo, 0.45% Ni, 0.020% V, 0.16% Cu
0.17% C, 0.27% Si, 1.31% Mn, 0.009% P, 0.10% S, 0.71% Ni, 0.10% Cr, 0.45% Mo, <0.01% V
0.17% C, 0.28% Si, 0.57% Mn, 0.014% P, 0.013% S, 1.70% Cr, 2.60% Ni, 0.46% Mo, 0.03% Ti
0.17% C, 0.30% Si, 1.06% Mn, 0.004% S, 0.018% P, 0.01% Cu, 0.09% Cr, 0.09% Mo, 0.04% V, 0.02% Ni, 0.001% Nb, 0.092% Al, 0.002% Ti, 0.007% N, 0.0079% Co, 0.0019% B
0.17% C, 0.30% Si, 1.10% Mn
0.17% C, 0.30% Si, 1.10% Mn
0.17% C, 0.30% Si, 1.10% Mn
0.17% C, 0.30% Si, 1.12% Mn, 0.020% P, 0.037% S, 0.00% Cr, 0.15% Ni, 0.22% Cu, 0.04% Mo, 0.026% Al, 0.015% Sn
0.17% C, 0.30% Si, 1.12% Mn, 0.020% P, 0.037% S, 0.00% Cr, 0.15% Ni, 0.22% Cu, 0.04% Mo, 0.026% Al, 0.015% Sn
0.17% C, 0.31% Si, 0.48% Mn, 0.017% P, 0.030% S, 1.85% Cr, 1.87% Ni
0.17% C, 0.31% Si, 0.82% Mn, 0.52% Ni, 0.50% Cr, 0.20% Mo
0.17% C, 0.33% Si, 1.37% Mn, 0.77% Ni, 0.66% Cr, 0.008% Mo, 0.002% V, 0.00% Mo
0.17% C, 0.33% Si, 1.37% Mn, 0.77% Ni, 0.66% Cr, 0.008% Mo, 0.002% V
0.17% C, 0.34% Si, 1.31% Mn
0.17% C, 0.34% Si, 1.31% Mn
0.17% C, 0.35% Si, 0.54% Mn, 0.015% P, 0.011% S, 1.58% Cr, 1.54% Ni
0.17% C, 0.37% Si, 1.51% Mn, 0.07% Cr, 0.03% Mo, 0.54% Ni, 1.50% V, 0.07% Cu, 0.022% Al, 0.0170 N
0.17% C, 0.38% Si, 1.31% Mn, 0.04% Ni, 0.01% Mo, 0.04% V
0.17% C, 0.38% Si, 1.31% Mn, 0.04% Ni, 0.01% Mo, 0.040% Al
0.17% C, 0.39% Mn, 0.43% Si, 0.016% S, 0.017% P 0.60% Ni, 11.30% Cr, 0.75% Mo, 0.37% V, 0.41% Nb, 0.070% N2
0.17% C, 0.40% Mn, 0.38% Si, 0.020% P, 0.020% S, 12.50% Cr, 0.20% Ni
0.17% C, 0.41% Si, 1.34% Mn, 0.028% P, 0.017% S, 0.48% Ni, 0.12% V, 0.054% Al
0.17% C, 0.43% Mn, 0.008% P, 0.003% S, 0.35% Si, 0.03% Cr, 0.03% Nb, 0.004% Al, 0.007% N, 0.04% Cu
0.17% C, 0.49% Mn, 0.010% P, 0.015% S, 0.29% Si, 5.07% Ni, 0.18% Cr, 0.24% Mo, 0.10% Cu
0.17% C, 0.49% Mn, 0.29% Si, 0.010% P, 0.015% S 5.07% Ni, 0.18% Cr, 0.24% Mo, 0.10% Cu
0.17% C, 0.51% Si, 1.37% Mn, 0.025% P, 0.024% S, 0.069% Al
0.17% C, 0.51% Si, 1.39% Mn, 0.025% OP, 0.024% S, 0.069% Al, 0.005% N
0.17% C, 0.51% Si, 1.39% Mn, 0.025% P, 0.024% S, 0.069% Al, 0.005% N
0.17% C, 0.54% Si, 0.84% Mn, 0.019% P, 0.011% S, 0.89% Cr, 0.40% Mo, 0.031% Al
0.17% C, 0.55% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.25% Mo, 1.80% Ni
0.17% C, 0.55% Si, 1.45% Mn, 0.016% P, 0.017% S, 0.74% Ni, 0.18% Ti, 0.055% Al
0.17% C, 0.56% Mn, 0.46% Si, 0.35% Ni, 20.96% Cr, 0.04% Mo, 0.013% Al, 0.12% N
0.17% C, 0.57% Mn, 0.016% P, 0.023% S, 0.27% Si, 1.87% Ni, 0.45% Cr, 0.24% Mo
0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo /0.14% C, 0.81% Mn, 1.81% Ni, 0.49% Cr, 0.27% Mo, 0.0030% B
0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo
0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo
0.17% C, 0.57% Mn, 1.87% Ni, 0.45% Cr, 0.24% Mo
0.17% C, 0.59% Mn, 0.30% Si, 3.18% Ni, 1.12% Cr 0.13% Mo
0.17% C, 0.59% Mn, 0.30% Si, 3.18% Ni, 1.12% Cr, 0.13% Mo
0.17% C, 0.60% Mn, 0.14% Si, 0.020% P, 0.020% S, 3.25% Cr, 0.55% Mo
0.17% C, 0.60% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.55% Cr, 2.00% Ni, 0.20% Mo
0.17% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.30% Mo
0.17% C, 0.63% Mn, 0.25% Si, 0.013% S, 0.013% P 2.02% Ni, 0.38% Cr, 0.13% Mo, 0.07% Cu
0.17% C, 0.63% Mn, 0.25% Si, 0.013% S, 0.013% P 2.02% Ni, 0.38% Cr, 0.13% Mo, 0.07% Cu
0.17% C, 0.63% Mn, 0.28% Si, 0.011% S, 0.022% P 1.13% Ni, 0.49% Cr, 0.13% Mo, 0.10% Cu
0.17% C, 0.79% Mn, 0.27% Si, 0.020% S, 0.009% P, 0.08% Cr, 0.45% Ni, 0.47% Mo, 0.02% V, 0.16% Cu
0.17% C, 0.80% Mn, 0.23% Si, 0.025% S, 0.020% P 0.21% Ni, 1.06% Cr, 0.24% Mo, 0.18% Cu, 0.006% V, 0.032% Ti
0.17% C, 0.82% Mn, 0.31% Si, 0.52% Ni, 0.50% Cr, 0.20% Mo
0.17% C, 0.84% Mn, 0.54% Si, 0.011% S, 0.019% P, 0.89% Cr, 0.05% Ni, 0.40% Mo, 0.01% V, 0.07% Cu, 0.031% Al, 0.008% N
0.17% C, 0.84% Mn, 0.54% Si, 0.019% P, 0.011% S, 0.031% Al, 0.89% Cr, 0.07% Cu, 0.40% Mo, 0.05% Ni, 0.01% V, 0.019% As, 0.008% Sn, 0.09% Zr, 0.008% N
0.17% C, 0.84% Mn, 0.54% Si, 0.019% P, 0.011% S, 0.89% Cr, 0.40% Mo, 0.031% Al, 0.09% Zr
0.17% C, 0.85% Mn, 1.85% Cr, 0.55% Mo
0.17% C, 0.88% Mn, 0.22% Si, 0.86% Ni, 0.59% Cr 0.05% Mo
0.17% C, 0.88% Mn, 0.22% Si, 0.86% Ni, 0.59% Cr 0.05% Mo
0.17% C, 0.92% Mn
0.17% C, 0.92% Mn
0.17% C, 0.92% Mn
0.17% C, 1.23% Mn, 0.25% Si, 0.013% S, 0.015% P 2.45% Ni, 0.94% Cr, 0.40% Mo, 0.012% N2, 0.042% Al
0.17% C, 1.23% Mn, 0.25% Si, 0.013% S, 0.015% P 2.45% Ni, 0.94% Cr, 0.40% Mo, 0.012% N2, 0.042% Al
0.17% C, 1.45% Mn, 0.55% Si, 0.016% P, 0.017% S, 0.055% Al, 0.74% Ni, 0.18% Ti
0.17% C, 1.48% Mn, 0.30% Si, 0.021% S, 0.034% P, 0.035% Cr, 0.075% Ni, 0.02% Mo, 0.15% V, 0.04% Cu, 0.028% Al, 0.018% N
0.17% C, 1.50% Mn, 0.34% Si, 0.018% S, 0.017% P 0.11% V, 0.025% N, 0.082% Al
0.17% C, 1.54% Mn, 0.44% Si, 0.006% S, 0.012% P, 0.01% Cr, 0.02% Ni, 0.47% Mo, 0.14% V, 0.002% Nb, 0.01% Cu, 0.010% Al, 0.006% N
0.17% C, 1.65% Mn, 1.07% Ni
0.17% C, 1.75% Mn, 0.20% Si, 0.10% V, 0.02% Al, 0.038% N
0.17% C, 16.00% Cr, 2.00% Ni
0.17-0.20% C, 0.30-0.45% Si, 1.45-1.60% Mn, 0.030% P, 0.020-0.035% S, 0.20-0.30% Cr, 0.30% Ni, 0.08-0.12% Mo
0.17-0.21% C, 0.20-0.30% Si, 0.30-0.50% Mn, 0.020% P, 0.015-0.030% S, 1.20-1.40% Cr, 2.50-2.90% Ni, 0.20-0.26% Mo
0.17-0.22% C, <0.40% Si, 1.10-1.40% Mn, <0.035% P, <0.035% S, 1.00-1.30% Cr. 20MnCrS5: 0.17-0.22% C, <0.40% Si, 1.10-1.40% Mn, <0.035% P, 0.020-0.040% S, 1.00-1.30% Cr
0.17-0.22% C, <1.00% Si, <1.00% Mn, 12.00-14.00% Cr, 1.00-1.30% Mo
0.17-0.22% C, <1.00% Si, <1.00% Mn, 12.00-14.00% Cr
0.17-0.22% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.30-0.50% Cr, 0.40-0.50% Mo
0.17-0.22% C, 0.15-0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr
0.17-0.22% C, 0.20-0.30% Si, 0.55-0.65% Mn, 0.015% P, 0.005% S, 0.50-0.60% Cr, 1.65-2.00% Ni, 0.23-0.28% Mo
0.17-0.22% C, 0.20-0.30% Si, 0.55-0.65% Mn, 0.015% P, 0.005% S, 0.50-0.80% Cr, 1.65-2.00% Ni, 0.23-0.28% Mo
0.17-0.22% C, 0.20-0.35% Si, 0.60-0.80% Mn, max. 0.040% P, max. 0.040% S, 1.10-1.40% Ni, 0.55-0.75% Cr
0.17-0.22% C, 0.30-0.50% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 12.50-13.50% Cr
0.17-0.22% C, 0.40% Si, 0.45-0.65% Mn, 0.035% P, 0.035% S, 0.40-0.70% Cr, 0.20-0.30% Mo, 1.60-2.00% Ni
0.17-0.22% C, 0.40% Si, 0.45-0.65% Mn, 0.035% P, 0.035% S, 0.40-0.70% Cr, 0.20-0.30% Mo, 1.60-2.00% Ni
0.17-0.22% C, 0.40% Si, 1.10-1.40% Mn, 0.035% P, 0.020-0.040% S, 1.00-1.30% Cr
0.17-0.22% C, 1.10-1.40% Mn, <0.40% Si, 1.00-1.30% Cr
0.17-0.22% C, 1.10-1.40% Mn, 0.15-0.40% Si, 1.00-1.30% Cr
0.17-0.23% C, <0.40% Si, 0.65-0.95% Mn, <0.035% P, <0.035% S, 0.35-0.70% Cr, 0.40-0.70% Ni. 20MnCrS4: 0.17-0.23% C, <0.40% Si, 0.65-0.95% Mn, <0.035% P, 0.020-0.040% S, 0.35-0.70% Cr, 0.40-0.70% Ni
0.17-0.23% C, <0.40% Si, 0.70-1.00% Mn, <0.035% P, <0.035% S, 0.30-0.60% Cr, 0.40-0.50% Mo. 20MnCrS4: 0.17-0.23% C, <0.40% Si, 0.70-1.00% Mn, <0.035% P, 0.020-0.040% S, 0.30-0.60% Cr, 0.40-0.50% Mo
0.17-0.23% C, 0.15-0.30% Si, 1.20-1.50% Mn, max. 0.012% P, max. 0.008% S, max. 0.20% Cr, 0.40-0.55% Mo, 0.50-0.80% Ni, max. 0.020% V, max. 0.03% Co, max. 0.12% Cu, 0.010-0.040% Al
0.17-0.23% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.025% P, max. 0.020% S, 3.00-3.30% Cr, 0.50-0.60% Mo, max. 0.30% Ni, 0.45-0.55% V, max. 0.30% Cu, max. 0.040% Al
0.17-0.23% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 3.00-3.30% Cr, 0.50-0.60% Mo, 0.45-0.55% V
0.17-0.23% C, 0.15-0.35% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 3.00-3.30% Cr, 0.50-0.60% Mo, 0.45-0.55% V
0.17-0.23% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, 0.020-0.035% S, 0.30-0.50% Cr, 0.40-0.50% Mo, 1.40-1.80% Ni
0.17-0.23% C, 0.40% Si, 0.65-0.95% Mn, 0.035% P, 0.035% S, 0.35-0.70% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, 0.40% Si, 0.65-0.95% Mn, 0.035% P, 0.035% S, 0.35-0.70% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, 0.60-0.90% Mn, 0.15-0.40% Si, 0.35-0.65% Cr, 0.15-0.25% Mo, <0.035% P, <0.035% P
0.17-0.23% C, 0.65-0.95% Mn, <0.40% Si, 0.35-0.70% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, max. 0.025% P, max. 0.035% S, 0.35-0.70% Cr, 0.15-0.25% Mo, 0.40-0.70% Ni
0.17-0.23% C, max. 0.40% Si, 0.65-0.95% Mn, max. 0.025% P, max. 0.035% S, 0.35-0.75% Cr, 0.15-0.25% Mo, 0.40-0.0% Ni
0.17-0.23% C, max. 0.40% Si, 1.00-1.50% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni, min. 0.020% Al
0.17-0.23% C, max. 0.50% Si, max. 1.00% Mn, max. 0.030% P, max. 0.030% S, 10.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.25-0.35% V
0.17-0.24% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%
0.17-0.25% C, <1.00% Si, <1.00% Mn, 16.00-19.00% Cr, 1.50-2.50% Ni
0.17-0.25% C, 0.10-0.50% Si, 0.30-0.80% Mn, max. 0.045% P, max. 0.030% S, 11.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.40-0.90% W, 0.25-0.35% V
0.17-0.25% C, 0.10-0.50% Si, 0.30-0.80% Mn, max. 0.045% P, max. 0.030% S, 11.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.40-0.90% W, 0.25-0.35% V
0.17-0.25% C, 0.30-0.60% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 1.00-1.20% Mo, max. 0.60% Ni, 0.25-0.35% V
0.17-0.25% C, max. 0.35% Si, 0.20-0.40% Mn, max. 0.020% P, max. 0.020% S, 1.50-2.00% Cr, 0.40-0.60% Mo, 3.00-3.80% Ni, max. 0.030% V, max. 0.050% Al
0.17-0.22% C, 1.10-1.40% Mn, 1.00-1.30% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P.
0.17-0.22% C, 1.10-1.40% Mn, 1.00-1.30% Cr, max. 0.40% Si, max. 0.035% S, max. 0.035% P
0.17% C, 0.26% Si, 0.37% Mn, 2.82% Cr, 0.38% Ni, 0.75% Mo, 0.26% V
0.17% C, 1.46% Mn, 0.15% Si
0.17-0.22% C, 0.15-0.40% Si, 0.30-0.60% Mn, 0.80-1.20% Cr, 0.30-0.50% Mo, 3.00-3.50% Ni
0.17% C, 16.00% Cr, 2.00% Ni
0.17% C, 0.70% Si, 1.50% Mn, 1.00% Cr, 0.70% Mo, 0.10% V, + B
0.17% C, 0.22% Si, 0.60% Mn, 0.017% S, 0.022% P
0.17% C, 0.31% Si, 1.54% Mn, 0.022% P, 0.025% S, 0.02% Cr, 0.06% Ni, 0.09% Cu, 0.072% Al, 0.042% Nb
0.17% C, 0.47% Si, 1.22% Mn, 0.023% P, 0.037% S, 0.01% Al, 0.0085% N, 0.10% Cr, 0.17% Cu, 0.06% Ni
0.17% C, 0.28% Si, 0.42% Mn, 0.014% P, 0.013% S, 2.60% Cr, 0.21% Mo, 0.16% V
0.173% C, 0.285% Si, 1.330% Mn, 0.015% P, 0.001% S, 0.052% Cr, 0.540% Ni, 0.460% Mo, 0.001% V, 0.001% Nb, 0.041% Al, 0.004% N
0.173% C, 0.285% Si, 1.33% Mn, 0.015% P, 0.001% S, 0.052% Cr, 0.54% Ni, 0.46% Mo, 0.001% V, 0.001% Nb, 0.041% Al, 0.004% N
0.173% C, 0.68% Si, 0.89% Mn, 0.009% P, 0.007% S, 0.68% Cr, 0.04% Ni, 0.324% Mo, 0.021% Cu, 0.049% Al
0.173% C, 0.285% Si, 1.330% Mn, 0.015% P, 0.001% S, 0.052% Cr, 0.540% Ni, 0.460% Mo, 0.001% V, 0.001% Nb, 0.041% Al, 0.004% N
0.174% C, 0.23% Si, 0.90% Mn, 0.003% S, 0.009% P, 0.52% Cr, 1.32% Ni, 0.402% Mo, 0.02% V, 0.012% Nb, 0.047% Al, 0.0041% N, 0.37% Cu, 0.0007% B
0.1740% C, 0.3040% Si, 1.0600% Mn, 0.0189% P, 0.0045% S, 0.0100% Cu, 0.0935% Cr, 0.0970% Mo, 0.0409% V, 0.0255% Ni, 0.0010% Nb, 0.0922% Al, 0.0027% Ti, 0.0079% W, 0.0065% Co, 0.0019% B
0.175% C, 0.159% Si, 1.133% Mn, 0.014% O, 0.022% S, 1.02% Cr, 0.017% Mo, 0.10% Ni, 0.02% Al
0.175% C, 0.38% Si, 1.07% Mn, 0.015% P, 0.005% S, 0.85% Cr, 0.10% Ni, 0.43% Mo, 0.065% Cu, 0.051% Al
0.175% C, 0.84% Si, 1.04% Mn, 0.013% P, 0.015% S, 0.84% Cr, 0.10% Ni, 0.419% Mo, 0.064% Cu, 0.046% Al
0.178% C, 0.256% Si, 0.870% Mn, 0.0009% P, 0.003% S, 0.510% Cr, 0.383% Mo, 0.980% Ni, 0.044% Al, 0.020% Cu, 0.019% Nb, 0.006% Ti, 0.022% V, 0.001% B
0.179% C, 0.04% Si, 0.79% Mn, 8.39% Cr, 0.24% V, 2.79% W, 0.0480% N, 0.09% Ta
0.18% C, 0.048% Si, 0.61% Mn, 0.023% P, 0.028% S, 0.025% Ni, 0.02% Cr
0.18% C, 0.16% Si, 1.00% Mn, 0.012% P, 0.004% S, 1.33% Cr, 0.15% Ni, 0.28% V, 0.24% Cu, 0.88% Mo, 0.021% Al
0.18% C, 0.16% Si, 1.00% Mn, 0.012% P, 0.004% S, 1.33% Cr, 0.15% Ni, 0.28% V, 0.24% Cu, 0.88% Mo, 0.021% Al
0.18% C, 0.18% Si, 1.15% Mn, 0.030% S, 0.015% P, <0.003% V, <0.005% Nb, 0.026% Al, 0.009 Cu, 0.0073% N
0.18% C, 0.20% Si, 0.81% Mn, 0.010% P, 0.010% S, 0.40% Cr, 0.48% Mo, 0.72% Ni, 0.09% Cu, 0.020% Al
0.18% C, 0.20% Si, 0.81% Mn, 0.010% P, 0.010% S, 0.40% Cr, 0.48% Mo, 0.72% Ni, 0.09% Cu, 0.020% Al
0.18% C, 0.22% Si, 0.43% Mn, 0.012% P, 0.028% S, 1.56% Cr, 1.48% Ni, 0.15% Cu, 0.28% Mo, 0.023% Al
0.18% C, 0.22% Si, 0.43% Mn, 0.012% P, 0.028% S, 1.56% Cr, 1.48% Ni, 0.15% Cu, 0.28% Mo, 0.023% Al
0.18% C, 0.23% Si, 0.87% Mn, 0.54% Cr, 0.48% Mo, 0.82% Ni, 0.03% V, 0.21% Cu, 0.010% Al
0.18% C, 0.25% Si, 0.50% Mn, 1.50% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni
0.18% C, 0.25% Si, 0.62% Mn, 0.011% P, 0.017% S, 0.80% Cr, 0.40% Mo, 0.14% Ni, <0.01% V
0.18% C, 0.25% Si, 0.62% Mn, 0.011% P, 0.017% S, 0.80% Cr, 0.40% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo, (Pb)
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo, (Pb)
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo, +Pb
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo, +Pb
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 0.75% Mn, 1.00% Cr, 0.25% Mo
0.18% C, 0.25% Si, 1.15% Mn, 1.05% Cr, 0.0030% B
0.18% C, 0.25% Si, 1.59% Mn, 0.32% Ni, 0.17% V, 0.012% Al, 0.0190% N
0.18% C, 0.26% Si, 1.44% Mn, 0.014% P, 0.018% S, 0.35% Cr, 1.11% Ni, 0.19% Cu, 0.42% Mo
0.18% C, 0.26% Si, 1.44% Mn, 0.014% P, 0.018% S, 0.35% Cr, 1.11% Ni, 0.19% Cu, 0.42% Mo
0.18% C, 0.28% Si, 0.54% Mn, 0.020% P, 0.005% S, 0.030% N, 0.001% Al, 0.05% Cu, 12.07% Cr, 0.63% Ni, 0.90% Mo, 0.32% V, 0.07% W
0.18% C, 0.28% Si, 0.54% Mn, 0.020% P, 0.005% S, 0.05% Cu, 0.030% N, 12.07% Cr, 0.63% Ni, 0.90% Mo, 0.32% V
0.18% C, 0.29% Si, 0.74% Mn, 0.015% P, 0.017% S, 0.50% Cr, 0.23% Mo, 0.52% Ni
0.18% C, 0.29% Si, 0.74% Mn, 0.015% P, 0.017% S, 0.50% Cr, 0.23% Mo, 0.52% Ni
0.18% C, 0.31% Si, 0.56% Mn, 0.22% Cr, 0.89% Mo, 0.03% Ni, 0.30% V, 0.16% Cu, 0.022% Al
0.18% C, 0.32% Si, 1.20% Mn, 0.65% Ni, 0.22% Cr, 0.13% Mo, 0.13% V, 0.040% Al, 0.015% Ti
0.18% C, 0.32% Si, 1.20% Mn, 0.65% Ni, 0.22% Cr, 0.13% Mo, 0.13% V, 0.040% Al, 0.015% Ti
0.18% C, 0.32% Si, 1.32% Mn, 0.33% Ni, 0.168% V, 0.020% Al
0.18% C, 0.34% Si, 0.87% Mn, 0.025% P, 0.011% S, 0.28% Cr, 0.38% Mo, 0.93% Cu
0.18% C, 0.35% Si, 0.83% Mn, 0.76% Ni, 0.63% Cr, 0.55% Mo, 0.06% V, 0.043% Al
0.18% C, 0.35% Si, 0.83% Mn, 0.76% Ni, 0.63% Cr, 0.55% Mo, 0.060% V, 0.043% Al, 0.003% B
0.18% C, 0.35% Si, 1.18% Mn, 0.028% P, 0.020% Al
0.18% C, 0.36% Si, 0.27% Mn, 0.022% P, 0.018% S, 13.61% Cr, 1.16% Mo, 0.11% Ni
0.18% C, 0.38% Si, 1.34% Mn, 0.014% P, 0.012% S
0.18% C, 0.38% Si, 1.34% Mn, 0.014% P, 0.012% S
0.18% C, 0.40% Si, 1.16% Mn, 0.08% Cr, 0.12% V
0.18% C, 0.40% Si, 1.16% Mn, 0.08% Cr, 0.12% V
0.18% C, 0.40% Si, 1.28% Mn, 0.004% P, 0.012% S, 0.09% V, 0.07% Al, 0.018% N
0.18% C, 0.47% Mn, 0.27% Si, 0.009% P, 0.010% S, 0.18% Cr, 3.33% Ni, 0.23% Mo
0.18% C, 0.47% Si, 1.24% Mn, 0.029% P, 0.029% S, 0.024% Al, 0.0085% N, 0.10% Cr, 0.17% Cu, 0.06% Ni
0.18% C, 0.47% Si, 1.40% Mn, 0.04% Ni, 0.05% Cr, 0.00% Mo, 0.061% Al
0.18% C, 0.47% Si, 1.40% Mn, 0.04% Ni, 0.05% Cr, 0.061% Al
0.18% C, 0.47% Si, 1.40% Mn, 0.04% Ni, 0.05% Cr, 0.061% V
0.18% C, 0.50% Si, 0.66% Mn, 0.012% P, 0.011% S, 0.12% Cr, 0.67% Mo, 0.13% Ni, 0.31% V
0.18% C, 0.53% Mn, 0.26% Si, 0.007% S, 0.012% P, 1.00% Cr, 0.96% Mo, 0.19% V
0.18% C, 0.54% Si, 1.27% Mn, 0.12% Ni, 0.14% Cr, 0.018% Al
0.18% C, 0.57% Mn, 0.31% Ni, 0.31% Cr, 0.15% Mo, 0.0009% B
0.18% C, 0.57% Mn, 0.31% Ni, 0.31% Cr, 0.15% Mo, 0.0009% B
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1N+0.75Si: 0.18% C, 0.75% Mn, 0.71% Si, 1.07% Ni
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+0.25Mo: 0.18% C, 0.65% Mn, 1.09% Ni, 0.26% Mo
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+0.5Cr: 0.21% C, 0.75% Mn, 1.08% Ni, 0.48% Cr
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+0.5Mo: 0.21% C, 0.70% Mn, 1.08% Ni, 0.49% Mo
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+1Cr: 0.21% C, 0.78% Mn, 1.09% Ni, 0.99% Cr
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+2Cr: 0.22% C, 0.77% Mn, 1.08% Ni, 1.91 Cr
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+2Si: 0.19% C, 0.75% Mn, 2.09% Si, 1.06% Ni
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+Mn: 0.17% C, 1.65% Mn, 1.07% Ni
0.18% C, 0.67% Mn, 1.07% Ni. 1021+1Ni+B: 0.19% C, 0.75% Mn, 1.04% Ni, 0.0021% B
0.18% C, 0.67% Mn, 1.07% Ni
0.18% C, 0.71% Si, 0.75% Mn, 1.07% Ni
0.18% C, 0.75% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.00% Cr, 0.20% Mo
0.18% C, 0.79% Mn, 0.021% P, 0.023% S, 0.21% Si, 0.52% Ni, 0.56% Cr, 0.19% Mo
0.18% C, 0.79% Mn, 0.52% Ni, 0.56% Cr, 0.19% Mo
0.18% C, 0.79% Mn, 0.52% Ni, 0.56% Cr, 0.19% Mo
0.18% C, 0.81% Mn, 0.26% Si, 0.40% Ni, 0.49% Cr, 0.17% Mo, 0.056% Al, 66 ppm N
0.18% C, 0.86% Mn, 0.27% Si, 0.009% S, 0.0010% P 1.53% Ni, 1.005% Cr, 0.16% Mo, 0.13% Cu
0.18% C, 0.86% Mn, 0.29% Si, 0.012% S, 0.018% P, 0.57% Cr, 0.87% Ni, 0.48% Mo, 0.05% V, 0.003% B, 0.29% Cu
0.18% C, 0.93% Mn, 0.26% Si, 1.34% Ni, 1.11% Cr 0.11% Mo
0.18% C, 0.93% Mn, 0.26% Si, 1.34% Ni, 1.11% Cr 0.11% Mo
0.18% C, 1.09% V
0.18% C, 1.10% Mn, 0.27% Si, 0.025% S, 0.023% P 0.28% Ni, 1.02% Cr, 0.04% Mo, 0.18% Cu
0.18% C, 1.10% Mn, 0.27% Si, 0.025% S, 0.023% P 0.28% Ni, 1.02% Cr, 0.04% Mo, 0.18% Cu
0.18% C, 1.28% Mn, 0.40% Si, 0.004% P, 0.012% S, 0.09% V, 0.07% Al, 0.018% N
0.18% C, 1.30% Mn, 0.27% Si
0.18% C, 1.36% Mn, 0.21% Si, 0.025% S, 0.014% P 0.91% Ni, 0.26% Cr, 0.37% Mo, 0.057% V, 0.048% Al
0.18% C, 1.60% Mn, 0.50% Si, 0.20% Cr, 0.30% Ni, 0.10% Mo, 0.10% V, 0.02% Nb, 0.30% Cu
0.18% C, max. 0.50% Si, 1.10-1.70% Mn, max. 0.020% P, max. 0.010% S, max. 0.30% Cr, max. 0.09% Mo, max. 0.50% Ni, max. 0.10% V, max. 0.030% Ti, max. 0.30% Cu, min. 0.020% Al, max. 0.05% Nb
0.18% Si, 0.58% Mn, 0.027% P, 0.029% S
0.18-0.22% C, max. 1.00% Si, max. 1.00% Mn, max. 0.045% P, max. 0.030% S, 12.00-14.00% Cr
0.18-0.23% C, 0.10% Si, 0.30-0.60% Mn, 0.040% P, 0.050% S, 0.0005-0.0030% B, 0.20% Cu, 0.10-0.35% Pb
0.18-0.23% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.035% P, 0.020-0.040% S, 0.50-0.70% Cr, 0.30-0.40% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.035% P, 0.020-0.040% S, 0.50-0.70% Cr, 0.30-0.40% Mo
0.18-0.23% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.20% Cr
0.18-0.23% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10% Mo, 0.90-1.20% Ni
0.18-0.23% C, 0.15-0.40% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10% Mo, 0.90-1.20% Ni
0.18-0.23% C, 0.80-1.10% Mn, 0.15-0.40% Si, 0.90-1.20% Cr, 0.90-1.2-% Ni
0.18-0.23% C, 0.80-1.10% Mn, 0.15-0.40% Si, 0.90-1.20% Cr, 0.90-1.2-% Ni
0.18-0.24% C, 0.15-0.35% Si, 1.10-1.40% Mn, max. 0.030% P, max. 0.030% S, 1.00-1.30% Cr
0.18-0.24% C, 0.15-0.35% Si, 1.10-1.40% Mn, max. 0.030% P, max. 0.030% S, 1.00-1.30% Cr
0.18-0.28% C, max. 0.40% Si, 0.50-0.70% Mn, <0.035% P, 0.20-0.040% S, 0.65-0.85% Cr, 1.50-1.90% Ni, 0.25-0.40% Mo
0.18C-0.65% Mn, 1.09% Ni, 0.26% Mo
0.18% C, 0.50% Si, 1.60% Mn, 0.017% P, 0.003% S, 1.45% Cr, 0.50% Mo, 2.39% Ni, 0.12% V
0.18% C, 1.80% Mn, 0.33% Si, 0.015% P, 0.002% S, 0.08% Cu, 0.05% Ni, 0.43% Cr, 0.03% Nb, 0.015% Mo, 0.026% Ti, 0.004% V, 0.0007% B
0.18% C, 0.35% Si, 1.6% Mn, 0.01% P, 0.008% S, 0.006% N
0.18% C, 0.35% Si, 1.15% Mn, 0.014% P, 0.024% P, 0.09% Cr, 0.08% Ni, 0.02% Al, 0.27% Cu
0.18% C, 0.37% Si, 1.32% Mn, 0.017% P, 0.028% S, 0.005% Al, 0.09% V, 0.01% N
0.18-0.23% C, 0.60-0.90% Mn, max. 0.040% P, max. 0.050% S
0.18% C, 1.68% Cr, 3.73% Ni
0.18% C, 0.21% Si, 0.49% Mn, 0.023% P, 0.027% S, 0.08% Cu, 0.02% Cr, 0.01% Ni, 0.038% Al, 0.006% N
0.18% C, 0.47% Si, 1.24% Mn, 0.029% P, 0.029% S, 0.024% Al, 0.0085% N, 0.10% Cr, 0.17% Cu, 0.06% Ni
0.18% C, 0.37% Si, 1.32% Mn, 0.017% P, 0.028% S, 0.005% Al, 0.09% V, 0.01% N
0.18% C, 0.24% Si, 0.43% Mn, 0.14% P, 0.008% S, 4.16% Cr, 0.59% Mo, 0.11% Ti, 0.032% Al, 0.54% V 0.18% C, 0.46% Si, 0.49% Mn, 0.020% P, 0.021% S, 0.14% Cu, 1.12% Cr, 0.15% Ni, 0.47% Mo, 0.073% Al, 0.014% V
0.183% C, 0.41% Si, 1.41% Mn, 0.010% P, 0.004% S, 0.020% Ni, 0.020% Cr, 0.001% Mo, 0.012% Cu, 0.030% Al
0.19% C, <0.002% Mn, 0.004% Si, 0.006% P, 0.002% S, 1.81% Mo
0.19% C, 0.04% Si, 1.00% Mn, 0.02% Ni, 0.62% Cr
0.19% C, 0.04% Si, 1.00% Mn, 0.02% Ni, 0.62% Cr
0.19% C, 0.14% Si, 1.37% Mn, 0.026% P, 0.012% S, 0.56% Ni, 0.20% Cr, 0.31% Mo
0.19% C, 0.20% Si, 1.35% Mn, 0.70% Ni, 0.55% Mo
0.19% C, 0.20% Si, 1.35% Mn, 0.70% Ni, 0.55% Mo
0.19% C, 0.20% Si, 1.35% Mn, 0.70% Ni, 0.55% Mo
0.19% C, 0.20% Si, 1.35% Mn, 0.70% Ni, 0.55% Mo
0.19% C, 0.21% Si, 0.41% Mn, 0.007% P, 0.006% S, 1.36% Cr, 4.06% Ni, 0.26% Cu, 0.21% Mo, 0.018% Sn
0.19% C, 0.21% Si, 0.48% Mn, 0.008% P, 0.028% S, 0.79% Cr, 0.18% Ni, 0.23% Cu, 0.05% Mo
0.19% C, 0.23% Si, 0.85% Mn, 0.021% P, 0.010% S, 0.12% Cr, 0.05% Ni, 0.03% Ti, 0.14% Cu, 0.015% Al
0.19% C, 0.23% Si, 1.25% Mn, 0.66% Ni, 0.07% Cr, 0.54% Mo
0.19% C, 0.23% Si, 1.25% Mn, 0.66% Ni, 0.07% Cr, 0.54% Mo
0.19% C, 0.28% Si, 1.39% Mn, 0.011% P, 0.008% S, 0.27% Cr, 1.01% Ni, 0.24% Cu, 0.42% Mo, 0.034% Al
0.19% C, 0.30% Mn, 0.04% Si, 0.007% P, 0.005% S, 3.30% Ni, 1.78% Cr, 0.50% Mo, 0.004% Al
0.19% C, 0.34% Si, 0.46% Mn, 0.019% P, 0.013% S, 7.87% Cr, 2.02% Mo
0.19% C, 0.35% Si, 0.55% Mn, 2.68% Ni, 1.21% Cr, 0.54% Mo, 0.017% Al
0.19% C, 0.35% Si, 0.55% Mn, 2.68% Ni, 1.21% Cr, 0.54% Mo, 0.017% Al
0.19% C, 0.35% Si, 0.70% Mn, 0.019% P, 0.024% S, 0.50% Cr, 0.36% Mo, 1.84% Ni, 0.20% V
0.19% C, 0.38% Si, 1.12% Mn, 0.037% P, 0.036% S, 0.28% Cr, 0.27% Mo, 0.79% Ni, 0.98% Cu
0.19% C, 0.38% Si, 1.12% Mn, 0.037% P, 0.036% S, 0.28% Cr, 0.98% Cu, 0.27% Mo, 0.79% Ni
0.19% C, 0.4% Si, 0.47% Mn
0.19% C, 0.41% Si, 1.17% Mn, 0.06% Cr
0.19% C, 0.41% Si, 1.17% Mn, 0.06% Cr
0.19% C, 0.42% Si, 0.34% Mn, 0.010% P, 0.002% S, 1.31% Cr, 0.48% Ni, 0.28% V, 0.13% Cu, 1.09% Mo
0.19% C, 0.42% Si, 1.20% Mn, 0.025% P, 0.025% S, 0.08% Cr, 0.01% Mo, 0.06% Ni, 0.01% V, 0.21% Cu
0.19% C, 0.42% Si, 1.20% Mn, 0.025% P, 0.025% S, 0.08% Cr, 0.01% Mo, 0.06% Ni, 0.01% V, 0.21% Cu
0.19% C, 0.42% Si, 1.20% Mn, 0.025% P, 0.025% S, 0.08% Cr, 0.21% Cu, <0.01% Mo, 0.06% Ni, <0.01% V
0.19% C, 0.46% Mn, 0.34% Si, 0.019% P, 0.013% S, 0.09% Ni, 7.83% Cr, 2.02% Mo, 0.01% V, 0.005% Al, 0.013% N
0.19% C, 0.47% Si, 0.62% Mn, 0.013% P, 0.012% S, 1.71% Cr, 2.75% Ni, 0.20% Cu, 0.43% Mo, 0.028% Al
0.19% C, 0.47% Si, 0.62% Mn, 0.013% P, 0.012% S, 1.71% Cr, 2.75% Ni, 0.20% Cu, 0.43% Mo, 0.028% Al
0.19% C, 0.55% Mn, 0.30% Si, 0.010% S, 0.018% P 1.52% Ni, 0.81% Cr, <0.10% Mo, 0.20% Cu, <0.030% V
0.19% C, 0.55% Mn, 0.30% Si, 0.010% S, 0.018% P 1.52% Ni, 0.81% Cr, <0.10% Mo, 0.20% Cu, <0.030% V
0.19% C, 0.57% Mn, 0.015% P, 0.023% S, 0.22% Si, 3.60% Ni, 0.09% Cr, 0.05% Mo
0.19% C, 0.57% Mn, 0.22% Si, 0.015% P, 0.023% S 3.60% Ni, 0.09% Cr, 0.05% Mo
0.19% C, 0.57% Mn, 0.35% Si, 0.018% P, 0.009% S, 2.72% Ni, 0.87% Cr, 0.257% Mo, 0.10% V, 0.0017% B
0.19% C, 0.60% Mn, 0.30% Si, 0.023% P, 0.021% S, 1.07% Cr, 0.48% Mo, 0.047% Al
0.19% C, 0.60% Si, 1.62% Mn, 0.10% Cr, 0.09% Ni, 0.11% Cu, 0.10% V, 0.032% Al, 0.012% Nb
0.19% C, 0.62% Mn, 0.36% Si, 0.022% P, 0.025% S, 1.03% Cr, 0.49% Mo, 0.041% Al, 0.006% B
0.19% C, 0.67% Mn, 0.20% Si, 0.020% S, 0.019% P 2.00% Ni, 0.39% Cr, 0.09% Mo, 0.05% Cu
0.19% C, 0.71% Mn, 0.015% P, 0.024% S, 1.80% Ni, 0.97% Cu
0.19% C, 0.77% Mn, 0.42% Ni, 0.40% Cr, 0.12% Mo, 0.0018% B
0.19% C, 0.77% Mn, 0.42% Ni, 0.40% Cr, 0.12% Mo, 0.0018% B
0.19% C, 0.81% Mn, 0.32% Si, 0.75% Cr, 0.17% Mo, 1.25% Ni
0.19% C, 0.90% Mn, 0.21% Si, 1.87% Ni, 1.08% Cr 0.18% Mo
0.19% C, 0.90% Mn, 0.21% Si, 1.87% Ni, 1.08% Cr 0.18% Mo
0.19% C, 0.90% Si, 0.74% Mn, 0.019% P, 0.017% S, 1.35% Cr, 2.38% Ni, 1.58% W, 0.19% Cu, 0.29% Mo
0.19% C, 0.92% V, b.) 0.21% C, 0.95% V, 0.97% Al, c.) 0.20% C, 1.46% Ni, 0.96% V
0.19% C, 1.20% Mn, 0.20% Si, 0.020% S, 0.020% P
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 1.30% Cr, 0.30% Mo, 1.10% Ni
0.19% C, 1.37% Mn, 0.14% Si, 0.56% Ni, 0.20% Cr 0.31% Mo
0.19% C, 1.39% Mn, 0.26% Si, 0.019% S, 0.029% P 0.029% Nb, 0.007% N, 0.046% Al
0.19% C, 1.44% Mn, 0.37% Si, 0.007% S, 0.011% P, 0.10% Cr, 0.08% Ni, 0.01% Mo, 0.17% V, 0.20% Cu, 0.03% Al, 0.010% N
0.19% C, 1.50% Mn, 0.20% Si, 0.020% S, 0.020% P
0.19% C, 1.50% Mn, 1.20% Cr, 2.50% Ni, 0.35% Mo, +Nb, others: V
0.19% C, 1.55% Mn, 0.32% Si, 0.005% S, 0.013% P, 0.57% Ni, 0.13% V, 0.01% Al, 0.017% N
0.19% C, 1.60% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.25% Mo, 0.55% Ni
0.19% C, 1.64% Mn
0.19% C, 2.09% Si, 0.75% Mn, 1.06% Ni
0.19% C, 4.50% Cr
0.19-0.25% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.19-0.25% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.19-0.25% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.19% C, 0.20% Si, 1.05% Mn, 0.028% P, 0.02% S, 0.08% Cr, 0.11% Ni, 0.006% Al
0.19-0.25% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.19% C, 1.05% Mn, 0.2% Si, 0.08% Cr, 0.11% Ni, 0.006% Al, 0.028% P, 0.02% S
0.19% C, 1.30% Cr, 0.20% Mo, 4.10% Ni
0.19% C, 3.73% Ni, 1.69% Cr, 0.50% Mo, 0.28% Mn, 0.15% Si, 0.003% S, 0.002% P, 0.002% Al, 0.004% Cu, 0.003% V, 0.004% Nb, 0.001% Ti
0.19-0.25% C, max. 0.40% Si, 1.10-1.40% Mn, max. 0.025% P, max. 0.015% S, 0.15-0.35% Cr, 0.020-0.050% Ti, 0.020-0.060% Al, 0.0008-0.0050% B
0.19% C, 0.32% Si, 1.15% Mn, 0.026% P, 0.020% S, 0.032% Al
0.19% C, 0.55% Si, 1.54% Mn, 0.028% P, 0.035% S, 0.24% Cr, 0.06% Ni, 0.02% Mo, 0.14% Cu, 0.044% Al
0.19% C, 0.29% Si, 0.67% Mn, 0.007% P, 0.011% S
0.19% C, 0.33% Si, 1.74% Mn, 0.007% P, 0.011% S
0.19% C, 0.94% Si, 0.65% Mn, 0.007% P, 0.011% S
0.19% C, 0.96% Si, 1.61% Mn, 0.007% P, 0.011% S
0.19% C, 0.42% Si, 0.72% Mn, 0.028% P, 0.013% S, 0.13% Cu, 0.17% Cr, 0.10% Ni, 0.05% Mo, 0.034% V
0.19% C, 0.51% Si, 0.58% Mn, 0.020% P, 0.016% S, 0.19% Cu, 1.36% Cr, 0.06% Ni, 0.86% Mo, 0.020% Al, 0.20% V
0.19% C, 0.51% Si, 0.65% Mn, 0.006% P, 0.005% S, 0.11% Cu, 2.16% Cr, 0.21% Ni, 0.98% Mo, 0.027% Al, 0.001% V
0.19% C, 0.50% Si, 1.43% Mn, 0.023% Cr, 0.03% Ni, 0.005% Mo, 0.001% Nb, 0.026% Al, 0.0054% V, 0.002% Ti, 0.014% W, 0.01% Cu
0.193% C, 0.656% Si, 0.965% Mn, 0.011% P, 0.006% S, 0.893% Cr, 0.042% Ni, 0.401% Mo, 0.005% V, 0.019% Cu, 0.045% Al, 0.026% Ti, 0.002% Nb, 0.007% N
0.197% C, 0.56% Si, 1.19% Mn, 0.007% P, 0.013% S, 0.18% Cu, 0.24% Cr, 0.27% Ni, 0.063% Mo, 0.002% Nb, 0.057% Al, 0.005% V
0.198% C, 0.372% Si, 0.700% Mn, 0.011% P, 0.006% S, 0.017% Cr, 0.047% Ni, 0.340% Mo, 0.066% Al, 0.032% Cu, 0.001% Nb, 0.001% Ti, 0.002% V
0.20% C, 0.023% Nb, 1.04% V, 15 ppm N, 13 ppm O. b.) 0.15% C, 0.020% Nb, 0.75% V, 40 ppm N, 41 ppm O
0.20% C, 0.03% Si, 1.30% Mn, 0.018% P, 0.022% S, 0.05% V
0.20% C, 0.08% Si, 1.19% Mn, 0.014% P, 0.00% S, 0.026% Cr, 1.27% Ni, 0.15% V, 0.21% Cu, 0.04% Mo
0.20% C, 0.08% Si, 1.19% Mn, 0.014% P, 0.00% S, 0.026% Cr, 1.27% Ni, 0.15% V, 0.21% Cu, 0.04% Mo
0.20% C, 0.15% Si, 0.61% Mn, 0.009% P, 0.014% S, 11.7% Cr, 0.84% Mo, 0.25% V, 0.011% Al, 0.65% Ni
0.20% C, 0.15% Si, 0.89% Mn, 0.024% S, 0.010% P, 0.07% Ni, 0.04% Cr, 0.014% Mo, 0.15% Cu, 0.004% Al, 0.012% Sn, 0.004% B
0.20% C, 0.17% Si, 0.25% Mn, 0.011% P, 0.012% S, 0.06% Ni, 3.02% Cr
0.20% C, 0.18% Si, 0.28% Mn, 0.09% Cr, 0.25% Mo, 3.40% Ni, 0.13% V, 0.14% Cu
0.20% C, 0.20% Si, 0.50% Mn, 9.50% Cr, 2.00% Mo, 5.50% W, 10.00% Co
0.20% C, 0.20% Si, 0.70% Mn, 0.60% Ni, 0.68% Cr, 0.12% Mo
0.20% C, 0.20% Si, 1.00% Mn, +B
0.20% C, 0.21% Si, 1.26% Mn, 0.80% Ni, 0.30% Cr, 0.55% Mo
0.20% C, 0.21% Si, 1.26% Mn, 0.80% Ni, 0.30% Cr, 0.55% Mo
0.20% C, 0.23% Si, 1.14% Mn, 0.009% S, 0.013% P, 0.030% Al, 0.0030% B, 0.0021% O, 0.0047% N
0.20% C, 0.25% Si, 0.40% Mn, 3.15% Cr, 0.50% V, 0.55% Mo
0.20% C, 0.25% Si, 0.40% Mn, 3.15% Cr, 0.55% Mo
0.20% C, 0.25% Si, 0.65% Mn, 0.40% Cr, 0.75% Ni, 0.65% Mo, <0.03% V
0.20% C, 0.25% Si, 0.65% Mn, 0.40% Cr, 0.75% Ni, 0.65% Mo, <0.03% V
0.20% C, 0.25% Si, 0.65% Mn, 0.40% Cr, 0.75% Ni, 0.65% Mo, <0.03% V
0.20% C, 0.25% Si, 0.65% Mn, 0.40% Cr, 0.75% Ni, 0.65% Mo, <0.03% V
0.20% C, 0.25% Si, 0.70% Mn, 0.60% Cr, 0.35% Mo
0.20% C, 0.25% Si, 0.70% Mn, 0.60% Cr, 0.35% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo, 0.020-0.035% S, (Pb)
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo, 0.020-0.035% S, (Pb)
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.75% Mn, 0.40% Cr, 0.45% Mo
0.20% C, 0.25% Si, 0.80% Mn, 0.50% Cr, 1.70% Ni, 0.45% Mo
0.20% C, 0.25% Si, 0.80% Mn, 0.50% Cr, 1.70% Ni, 0.45% Mo
0.20% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.20% C, 0.25% Si, 0.80% Mn, 1.05% Cr, 1.45% Ni
0.20% C, 0.25% Si, 1.00% Mn, +B
0.20% C, 0.25% Si, 1.15% Mn, 1.15% Cr + B
0.20% C, 0.25% Si, 1.15% Mn, 1.15% Cr, +B, (Pb)
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr, <0.035% S, (Pb). 20MnCrS5: 0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr, 0.020-0.035% S, (Pb)
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.25% Mn, 1.15% Cr
0.20% C, 0.25% Si, 1.38% Mn, 0.009% S, 0.017% P, 0.83% Ni, 0.15% Cr, 0.49% Mo, 0.14% Cu, 0.024% Al, 0.0017 As, <0.0006 Sn, 0.005% Ti, 0.006% Nb, 0.005% V
0.20% C, 0.25% Si, 1.45% Mn
0.20% C, 0.25% Si, 1.45% Mn
0.20% C, 0.27% Si, 0.49% Mn, 0.013% P, 0.005% S, 1.53% Cr, 4.12% Ni, 0.50% W, 0.13% Cu, 0.25% Mo, 0.128% Co, 0.011% Sn
0.20% C, 0.28% Si, 1.25% Mn, 0.015% P, 0.008% S, 0.15% Cr, 0.044% Al, 25 ppm B
0.20% C, 0.28% Si, 1.25% Mn, 0.015% P, 0.008% S, 0.15% Cr, 0.044% Al, 25 ppm B
0.20% C, 0.29% Si, 0.60% Mn, 0.009% P, 0.021% S, 0.52% Cr, 0.26% Mo, 1.67% Ni, 0.09% Cu
0.20% C, 0.30% Si, 0.40% Mn, 0.010% P, 0.005% S, 2.50% Cr, 0.40% Mo
0.20% C, 0.30% Si, 0.72% Mn, 0.010% P, 0.010% S, 0.79% Cr, 0.02% Mo, 0.27% Ni, 0.02% Cu
0.20% C, 0.30% Si, 0.72% Mn, 0.010% P, 0.010% S, 0.79% Cr, 0.02% Mo, 0.27% Ni, 0.02% Cu
0.20% C, 0.30% Si, 0.72% Mn, 0.010% S, 0.010% P, 0.27% Ni, 0.79% Cr, 0.02% Mo
0.20% C, 0.32% Si, 0.45% Mn, 0.015% P, 0.024% S, 11.96% Cr, 1.00% Mo, 0.68% Ni, 0.29% V
0.20% C, 0.33% Si, 0.52% Mn, 0.010% P, 0.013% S, 12.10% Cr, 1.07% Mo, 0.75% Ni, 0.36% V
0.20% C, 0.33% Si, 0.52% Mn, 0.010% P, 0.013% S, 12.10% Cr, 1.07% Mo, 0.75% Ni, 0.36% V
0.20% C, 0.34% Si, 0.45% Mn, 0.014% P, 0.008% S, 17.00% Cr, 0.04% Mo, 1.87% Ni
0.20% C, 0.38% Si, 1.20% Mn, 0.039% P, 0.08% S, 0.91% Cr, 0.55% Ni
0.20% C, 0.39% Si, 0.37% Mn, 0.023% P, 0.012% S, 12.85% Cr, 0.21% N
0.20% C, 0.40% Si, 1.12% Mn, 0.05% Ni, 0.09% Cr, 0.01% Mo, 0.009% V, 0.046% Al
0.20% C, 0.40% Si, 1.12% Mn, 0.05% Ni, 0.09% Cr, 0.01% Mo, 0.009% V, 0.048% Al
0.20% C, 0.45% Mn, 1.03% V, 0.02% N
0.20% C, 0.46% Si, 1.44% Mn, 0.015% P, 0.018% S, 0.10% Cr, 1.44% Ni, 0.02% V, 1.40% Cu, 0.01% Mo, 0.023% Al
0.20% C, 0.47% Mn, 0.24% Si, 0.026% P, 0.009% S, 0.39% Ni, 11.49% Cr, 0.98% Mo, 0.28% V, 0.002% Al, 0.0323% N
0.20% C, 0.47% Mn, 0.24% Si, 0.026% P, 0.009% S, 0.39% Ni, 11.59% Cr, 0.98% Mo, 0.002% Al, 0.28% V, 0.0323% N
0.20% C, 0.48% Mn, 0.36% Si, 0.012% S, 0.016% P, 12.80% Cr, 0.13% Ni, 0.03% Mo, 0.05% V, 0.01% Cu, sol. 0.036% Al
0.20% C, 0.48% Si, 0.33% Mn, 0.027% P, 0.009% S, 11.83% Cr, 1.02% Mo, 0.69% Ni, 0.31% V, 0.51% W
0.20% C, 0.50% Mn, 0.25% Si, 0.020% P, 0.020% S, 3.10% Cr, 0.52% Mo
0.20% C, 0.50% Si, 1.15% Mn
0.20% C, 0.51% Mn, 0.33% Si, 0.006% S, 0.022% P, 11.80% Cr, 0.49% Ni, 1.00% Mo, 0.31% V, 0.03% Cu, sol. 0.010% Al
0.20% C, 0.53% Si, 1.20% Mn, 0.032% P, 0.026% S, 0.10% Cr, 0.17% Cu
0.20% C, 0.58% Mn, 0.31% Si, 2.90% Ni, 0.25% Mo
0.20% C, 0.60% Mn, 1.00% Ni, 0.40% Mo
0.20% C, 0.61% Mn, 0.23% Si, 2.00% Ni, 1.65% Cr 0.19% Mo
0.20% C, 0.61% Mn, 0.23% Si, 2.00% Ni, 1.65% Cr 0.19% Mo
0.20% C, 0.62% Mn, 0.15% Si, 0.015% P, 0.020% S, 0.015% Al, 0.47% Cr, <0.0005% B, 0.48% Mo, 1.58% Ni
0.20% C, 0.63% Mn, 0.32% Si, 0.026% S, 0.017% P 3.85% Ni, 0.25% Cr, 0.94% Mo, 0.17% Cu
0.20% C, 0.63% Mn, 0.32% Si, 0.026% S, 0.017% P 3.85% Ni, 0.25% Cr, 0.94% Mo, 0.17% Cu
0.20% C, 0.70% Mn, 0.25% Si, 0.030% P, 0.030% S, 12.00% Cr, 0.65% Ni, 1.00% Mo, 0.30% V
0.20% C, 0.70% Mn, 0.29% Si, 0.10% Ni, 0.59% Cr, 0.09% Mo, 0.07% V, 0.021% Al, 0.34% Ti, 150 ppm N
0.20% C, 0.70% Mn, 0.57% Si, 0.009% S, 0.016% P 0.23% Ni, 1.18% Cr, 1.15% Mo, 0.27% V
0.20% C, 0.71% Mn, 0.15% Si, 1.13% Ni, 0.80% Cr 0.05% Mo
0.20% C, 0.71% Mn, 0.15% Si, 1.13% Ni, 0.80% Cr 0.05% Mo
0.20% C, 0.72% Mn, 0.30% Si, 0.010% S, 0.010% P 0.27% Ni, 0.79% Cr, 0.02% Mo, 0.02% Cu
0.20% C, 0.75% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.40% Cr, 0.45% Mo
0.20% C, 0.75% Mn, 0.30% Si, 0.020% P, 0.020% S, 0.95% Cr
0.20% C, 0.78% Mn, 0.60% Cr, 0.52% Ni, 0.16% Mo
0.20% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.80% Cr
0.20% C, 0.80% Mn, 0.27% Si, 0.017% S, 0.018% P 0.58% Ni, 0.49% Cr, 0.18% Mo
0.20% C, 0.81% Mn, 0.16% Si
0.20% C, 0.81% Mn/ - 0.18% C, 0.67% Mn, 1.07% Ni
0.20% C, 0.81% Mn
0.20% C, 0.81% Mn
0.20% C, 0.83% Mn. Steel 0.2C-2Mn: 0.20% C, 2.00% Mn
0.20% C, 0.87% Mn, 0.30% Si, 0.38% Mo, 0.003% B, 0.006% N, 0.052% Zr
0.20% C, 0.87% Mn, 0.30% Si, 0.38% Mo, 0.003% B, 0.006% N, 0.052% Zr
0.20% C, 0.89% Mn, 0.15% Si, 0.010% P, 0.024% S, 0.04% Cr, 0.07% Ni, 0.15% Cu, 0.004% Al, 0.014% Mo, 0.012% Sn, 0.004% B
0.20% C, 1.00% Mn, 0.08% S, 0.10% Mo
0.20% C, 1.25% Mn, 0.25% Si, 0.025% P, 0.015% S, 1.15% Cr, 0.02% Mo, 0.15% Ni
0.20% C, 1.30% Mn, 0.020% P, 0.020% S, 1.30% Cr, 0.40% Mo
0.20% C, 1.37% Mn, 0.35% Si, 0.0017% S, 0.022% P, 0.007% N, 0.054% Al
0.20% C, 1.44% Mn, 0.49% Ni, 0.16% V
0.20% C, 1.44% Mn, 0.49% Ni, 0.16% V
0.20% C, 1.45% Mn, 0.30% Si, 0.005% S, 0.012% P, 0.11% Cr, 0.10% Ni, 0.02% Mo, 0.08% V, 0.14% Cu, 0.01% Al, 0.010% N
0.20% C, 1.46% Mn, 0.34% Si, 0.008% S, 0.013% P, 0.12% Cr, 0.10% Ni, 0.02% Mo, 0.14% V, 0.19% Cu, 0.03% Al, 0.012% N
0.20% C, 1.80% Mn, 1.0% Si, 0.03% P, 0.10% V, 0.003% B,
0.20% C, 1.88% Mn
0.20% C, 1.88% Mn
0.20% C, 12.00% Cr, 1.00% Mo, 0.30% V
0.20% C, max. 1.0% Si, max. 1.50% Mn, 13.0% Cr
0.20% C, max. 1.00% Si, max. 1.00% Mn, 17.00% Cr, 1.70% Ni
0.20-0.25% C, 0.15-0.35% Si, 0.70-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.70-0.90% Cr, 0.30-0.40% Mo, 0.0008-0.0050% B
0.20-0.25% C, 0.30% Si, 0.90-1.20% Mn, 0.025% P, 0.025% S, 0.30% Cr, 0.0008-0.0050% B, 0.25% Cu
0.20-0.26% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.010% P, max. 0.007% S, 1.70-2.00% Cr, 0.60-0.80% Mo, 0.90-1.20% Ni
0.20-0.26% C, max. 0.50% Si, 0.30-0.80% Mn, max. 0.025% P, max. 0.020% S, 11.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.25-0.35% V
0.20-0.26% C, max. 0.50% Si, 0.30-0.80% Mn, max. 0.025% P, max. 0.020% S, 11.00-12.50% Cr, 0.80-1.20% Mo, 0.30-0.80% Ni, 0.25-0.35% V
0.20-0.28% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.50-0.60% Mo, max. 0.60% Ni, 0.15-0.25% V
0.20-0.28% C, 0.15-0.35% Si, 0.30-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.50-0.60% Mo, max. 0.60% Ni, 0.15-0.25% V
0.20-0.334% C, <0.40% Si, 0.30-0.60% Mn, <0.035% P, <0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.20-0.40% C, <0.40% Si, 0.80-1.40% Mn, <0.025% P, <0.002% S, 1.00-2.00% Cr, 0.20-0.50% Mo
0.20% C, 1.50% Si, 1.50% Mn, 0.015% P, 0.0008% S, 0.041% Al, 0.0005% N, 0.0008% O
0.20% C, 22% Cr, 5.3% Ni, 3% Mo, 0.16% N
0.2% C, 0.75-0.90% N, 16.5-17.5% Cr, 0.1% Ni, 3.0-3.5% Mo, 10.0-12.0% Mn, 1.0% Si, balance is Fe
0.20% C, 1.40% Si, 1.65% Mn, 0.014% P, 0.006% S, 1.05% Ni, 1.30% Cu, 1.07% Co, 1.50% Al
0.20-0.31% C, 0.56-0.94% Mn, max. 0.43% Si, max. 0.03% P, max. 0.04% S, 0.85-1.25% Cr, 0.12-0.33% Mo
0.20-0.31% C, 0.56-0.94% Mn, max. 0.43% Si, max. 0.03% P, max. 0.04% S, 0.85-1.25% Cr, 0.12-0.33% Mo
0.20-0.31% C, 0.56-0.94% Mn, max. 0.43% Si, max. 0.03% P, max. 0.04% S, 0.85-1.25% Cr, 0.12-0.33% Mo
0.20-0.31% C, 0.56-0.94% Mn, max. 0.43% Si, max. 0.03% P, max. 0.04% S, 0.85-1.25% Cr, 0.12-0.33% Mo
0.20-0.60% C, 1.25% Mn, 0.16% Si, 0.10% Ni, 1.35% Cr, 0.039% Mo, 0.22% Cu, 0.043% Al
0.20% C, 0.30% Cr, 0.50% Mo, with and without boron
0.20% C, 0.17% Si, 1.47% Mn, 0.13% Cr, 0.51% Mo, 0.89% Ni, 0.001% V, 0.039% Al, 0.014% N
0.20% C, 0.18% Si, 1.30% Mn, 0.017% P, 0.0033% S, 0.033% Al, 1.24% Cr, 0.21% Cu, 0.01% Mo, 0.011% N, 0.02% Ni
0.20% C, 0.19% Si, 1.19% Mn, 0.016% P, 0.0032% S, 0.004% Al, 1.22% Cr, 0.21% Cu, 0.01% Mo, 0.006% N, 0.03% Ni
0.20% C, 0.18% Si, 1.30% Mn, 0.017% P, 0.0033% S, 0.033% Al, 1.24% Cr, 0.21% Cu, 0.01% Mo, 0.011% N, 0.02% Ni
0.20% C, 0.28% Si, 0.48% Mn, 0.011% P, 0.016% S, 0.11% Cu, 0.95% Cr, 3.16% Ni, 0.54% Mo, 0.014% Al
0.20% C, 0.23% Si, 0.53% Mn, 0.016% P, 0.009% S, 1.28% Cr, 0.98% Mo, 0.29% V
0.20% C, 0.33% Si, 0.28% Mn, 0.023% P, 0.016% S, 13.40% Cr
0.20% C, 0.33% Si, 0.28% Mn, 0.023% P, 0.016% S, 13.40% Cr
0.20% C, 0.52% Si, 0.65% Mn, 0.010% P, 0.007% S, 0.17% Cu, 0.25% Cr, 0.20% Ni, 0.04% Mo, 0.036% V
0.201% C, 1.55% Mn, 0.26% Si, 0.019% S, 0.025% P 0.39% Cr, 0.005% Al, 0.11% Nb
0.203% C, 0.330% Si, 1.380% Mn, 0.007% P, 0.008% S, 0.600% Cr, 0.443% Mo, 0.042% Ni, 0.036% Al, 0.017% Cu, 0.005% Nb, 0.004% Ti, 0.052% V, 0.040% W, 0.001% B
0.21% C, 0.18% Si, 1.28% Mn, 0.014% P, 0.009% S, 0.55% Cr, 0.96% Ni, 0.22% Cu, 0.54% Mo, 0.028% Al
0.21% C, 0.18% Si, 1.28% Mn, 0.014% P, 0.009% S, 0.55% Cr, 0.96% Ni, 0.22% Cu, 0.54% Mo, 0.028% Al
0.21% C, 0.23% Si, 1.50% Mn, 0.004% P, 0.001% S, 0.92% Ni, 0.19% Cr, 0.50% Mo, <0.03% V. Steel SA508 grade 3 class 1: 0.17% C, 0.27% Si, 1.31% Mn, 0.009% P, 0.010% S, 0.71% Ni, 0.10% Cr, 0.45% Mo, <0.01% V 0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.20% Mo, 0.55% Ni, (Pb)
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.20% Mo, 0.55% Ni, (Pb)
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.25% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.21% C, 0.26% Si, 0.65% Mn, 0.010% P, 0.010% S, 0.34% Cr, 0.49% Mo, 0.11% Ni, 0.30% V
0.21% C, 0.26% Si, 0.65% Mn, 0.010% P, 0.010% S, 0.34% Cr, 0.49% Mo, 0.11% Ni, 0.30% V
0.21% C, 0.26% Si, 0.81% Mn, 0.026% P, 0.018% S, 0.59% Cr, 0.17% Mo, 0.53% Ni
0.21% C, 0.26% Si, 0.81% Mn, 0.026% P, 0.018% S, 0.59% Cr, 0.17% Mo, 0.53% Ni
0.21% C, 0.27% Si, 0.81% Mn, 0.012% P, 0.024% S, 0.50% Cr, 0.21% Mo, 0.50% Ni
0.21% C, 0.28% Si, 0.85% Mn, 0.015% P, 0.023% S, 0.48% Cr, 0.21% Mo, 0.55% Ni
0.21% C, 0.28% Si, 1.18% Mn, 0.015% P, 0.001% S, 0.18% Cr, 0.01% Ni, 0.030% Al, 0.0032% Nb, 0.0028% B, 0.0064% N
0.21% C, 0.29% Si, 0.55% Mn, 0.010% S, 0.008% P, 1.84% Ni, 0.07% Cr, 0.20% Mo
0.21% C, 0.30% Si, 1.11% Mn, 0.012% P, 0.017% S, 1.27% Cr, 0.18% Ni, 0.24% Cu, 0.22% Mo
0.21% C, 0.30% Si, 1.11% Mn, 0.012% P, 0.017% S, 1.27% Cr, 0.18% Ni, 0.24% Cu, 0.22% Mo
0.21% C, 0.31% Si, 1.64% Mn, 0.081% P, 1.37% Al, 0.073% V, 0.55% CE
0.21% C, 0.34% Si, 0.86% Mn, 11.28% Cr, 0.31% Ni, 0.50% Mo, 0.29% Mo
0.21% C, 0.35% Si, 0.35% Mn, 13.30% Cr
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 0.30% V, 1.10% Mo
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 1.10% Mo, 0.30% V
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 1.10% Mo, 0.30% V
0.21% C, 0.35% Si, 0.40% Mn, 1.35% Cr, 1.10% Mo, 0.30% V
0.21% C, 0.36% Si, 1.18% Mn, 0.016% P, 0.015% S, 0.22% Cr, 0.14% Ni, 0.21% Cu, 0.03% Mo
0.21% C, 0.37% Si, 0.25% Mn, 0.36% Ni, 13.20% Cr
0.21% C, 0.37% Si, 1.49% Mn, 0.23% Cr, 0.58% Mo, 0.21% Ni, 0.01% Co, 0.08% Cu, 0.019% Al
0.21% C, 0.38% Si, 0.52% Mn, 0.012% P, 0.020% S, 12.30% Cr, 1.22% Mo, 0.38% Ni
0.21% C, 0.40% Si, 1.52% Mn, 0.07% Ni, 0.13% V, 0.043% Al, 0.0190% N
0.21% C, 0.43% Si, 0.37% Mn, 0.024% P, 0.016% S, 1.28% Cr, 0.10% Ni, 0.30% V, 0.27% Cu, 1.06% Mo, 0.018% Sn
0.21% C, 0.43% Si, 0.37% Mn, 0.024% P, 0.016% S, 1.28% Cr, 0.10% Ni, 0.30% V, 0.27% Cu, 1.06% Mo, 0.018% Sn
0.21% C, 0.45% Si, 0.40% Mn, 1.40% Cr, 0.30% V, 1.10% Mo
0.21% C, 0.45% Si, 0.40% Mn, 1.40% Cr, 0.30% V, 1.10% Mo
0.21% C, 0.46% Si, 1.18% Mn, 0.10% Ni, 0.12% Cr, 0.02% Mo, 0.017% V, 0.014% Al
0.21% C, 0.46% Si, 1.18% Mn, 0.10% Ni, 0.12% Cr, 0.02% Mo, 0.017% V, 0.014% Al
0.21% C, 0.48% Mn, 0.97% Si, 2.92% Ni, 1.09% V, 0.01% Al
0.21% C, 0.48% Si, 1.19% Mn, 0.06% Ni, 0.05% Cr, 0.01% Mo, 0.009% V, 0.10% Al
0.21% C, 0.48% Si, 1.19% Mn, 0.06% Ni, 0.05% Cr, 0.01% Mo, 0.009% V, 0.100% Al
0.21% C, 0.55% Mn, 0.29% Si, 0.010% S, 0.008% P 1.84% Ni, 0.07% Cr, 0.20% Mo, 0.09% Cu
0.21% C, 0.56% Mn, 0.27% Si, 2.95% Ni, 0.51% Mo
0.21% C, 0.58% Mn, 0.28% Si, 2.95% Ni, 0.004% Mo
0.21% C, 0.61% Mn, 0.017% P, 0.016% S, 0.24% Si, 1.35% Ni, 0.67% Cr, 0.02% Mo, 0.04% Cu
0.21% C, 0.61% Mn, 0.24% Si, 0.017% P, 0.016% S 1.35% Ni, 0.67% Cr, 0.02% Mo, 0.04% Cu
0.21% C, 0.70% Mn, 1.08% Ni, 0.49% Mo
0.21% C, 0.71% Mn, 0.30% Si, 0.002% P, 0.006% S, 0.63% Ni, 0.49% Cr, 0.17% Mo, 0.014% Cu, 0.014% Al
0.21% C, 0.71% Mn, 0.30% Si, 0.002% P, 0.006% S, 0.63% Ni, 0.49% Cr, 0.17% Mo, 0.014% Cu, 0.014% Al
0.21% C, 0.75% Mn, 1.08% Ni, 0.48% Cr
0.21% C, 0.78% Mn, 1.09% Ni, 0.99% Cr
0.21% C, 0.88% Mn, 0.31% Si, 0.002% S, 0.017% P 0.65% Ni, 0.57% Cr, 0.26% Mo, 0.15% Cu
0.21% C, 0.88% Mn, 0.31% Si, 0.002% S, 0.017% P 0.65% Ni, 0.57% Cr, 0.26% Mo, 0.15% Cu
0.21% C, 1.18% Si, 1.52% Mn, 0.29% Mo, 0.57% Al, 0.03% Cu, 0.036% Nb, 0.027% P
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 1.30% Mn, 1.30% Si, 1.20% Cr
0.21% C, 1.46% Mn, 0.38% Si, 0.019% S, 0.016% P 0.45% Mo
0.21% C, 1.48% Si, 1.50% Mn, 0.20% Mo, 0.01% Al, 0.02% Cu, 0.036% Nb, 0.025% P
0.21% C, 1.52% Mn, 0.40% Si, 0.022% P, 0.023% S, 0.043% Al, 0.019% N, 0.07% Ni, 0.13% V
0.21% C, 1.52% Mn, 0.40% Si, 0.023% S, 0.022% P, 0.07% Ni, 0.13% V, 0.04% Al, 0.019% N
0.21% C, 1.55% Si, 1.55% Mn, 0.01% Al, 0.003% Cu, 0.005% Nb
0.21% C, 13.20% Cr, 0.024% N. F: 0.18% C, 0.58% Mn, 0.31% Si, 0.18% Ni, 11.70% Cr, 0.49% Mo, 0.01% Al, 0.38% V, 0.20% Nb, 0.033% N
0.21% C, 0.28% Si, 1.18% Mn, 0.015% P, 0.001% S, 0.030% Al, 0.0032% Nb, 0.18% Cr, 0.0028% B, 0.0064% N, 0.01% Ni, 0.02% Mo
0.21% C, 0.66% Mn, 0.19% Si, 0.022% P, 0.026% S, 0.05% Cr, 0.07% Ni, 0.17% Cu, 0.004% Al, 0.016% Mo, 0.01% Sn, 0.007% B
0.21% C, 0.18% Si, 1.45% Mn, 0.018% P, 0.008% S, 0.02% Al, 0.54% Cr, 0.62% Mo, 1.03% Ni
0.21% C, 1.30% Mn, 1.20% Cr
0.21% C, 0.34% Si, 0.41% Mn, 0.014% P, 0.009% S, 12.13% Cr, 0.05% Mo, 0.40% Ni
0.21% C, 0.95% Si, 0.05% Mn, 0.005% P, 0.024% S
0.218% C, 1.831% Si, 2.021% Mn, 0.227% Mo, 0.003% N, 0.006% P, 0.003% S. Cr-added steel: 0.221% C, 1.792% Si, 1.983% Mn, 1.002% Cr, 0.229% Mo, 0.003% N, 0.003% P, 0.003% S
0.218% C, 1.831% Si, 2.021% Mn, 0.227% Mo, 0.003% N, 0.006% P, 0.003% S. Cr-added steel: 0.221% C, 1.792% Si, 1.983% Mn, 1.002% Cr, 0.229% Mo, 0.003% N, 0.003% P, 0.003% S
0.22% C, 0.12% Si, 1.06% Mn, 0.01% Ti
0.22% C, 0.12% Si, 1.08% Mn, 0.01% Ti
0.22% C, 0.18% Si, 0.30% Mn, 8.60% Cr, 2.32% Mo, 0.10% Ni, 6.79% W, 0.07% Cu, 0.040% Nb
0.22% C, 0.18% Si, 0.45% Mn, 0.016% P, 0.008% S, 0.93% Cr, 3.90% Ni, 0.15% V, 0.24% Cu, 0.07% Mo, 0.019% Sn
0.22% C, 0.18% Si, 0.45% Mn, 0.016% P, 0.008% S, 0.93% Cr, 3.90% Ni, 0.15% V, 0.24% Cu, 0.07% Mo, 0.019% Sn
0.22% C, 0.20% Si, 0.70% Mn, 12.00% Cr, 0.70% Ni, 1.00% Mo, 0.30% V
0.22% C, 0.20% Si, 0.70% Mn, 12.00% Cr, 0.70% Ni, 1.00% Mo, 0.30% V
0.22% C, 0.21% Si, 0.74% Mn, 0.008% P, 0.007% S, 0.40% Cr, 0.75% Ni, 0.26% Cu, 0.19% Mo, 0.042% Al
0.22% C, 0.21% Si, 0.74% Mn, 0.008% P, 0.007% S, 0.40% Cr, 0.75% Ni, 0.26% Cu, 0.19% Mo, 0.042% Al
0.22% C, 0.24% Si, 0.40% Mn, 0.03% S, 0.02% P, 0.11% Ni, 0.73% Cr, 0.40% Mo, 0.13% Cu, 0.02% W, 0.02% Co, 0.01% Nb
0.22% C, 0.24% Si, 0.40% Mn, 0.03% S, 0.02% P, 0.11% Ni, 0.73% Cr, 0.40% Mo, 0.13% Cu, 0.02% W, 0.02% Co, 0.01% Nb
0.22% C, 0.24% Si, 0.40% Mn, 0.03% S, 0.02% P, 0.11% Ni, 0.73% Cr, 0.40% Mo, 0.13% Cu, 0.02% W, 0.02% Co, 0.01% Nb
0.22% C, 0.25% Si, 0.36% Mn, max. 0.012% P, 2.35% Cr, 0.34% Mo, 0.030% Al
0.22% C, 0.25% Si, 0.40% Mn, 1.45% Cr, 3.65% Ni, 0.40% Mo
0.22% C, 0.25% Si, 0.40% Mn, 1.45% Cr, 3.65% Ni, 0.40% Mo
0.22% C, 0.25% Si, 0.64% Mn, 0.010% P, 0.011% S, 0.97% Cr, 0.16% Cu, 0.23% Mo, 0.33% Ni, <0.01% V
0.22% C, 0.25% Si, 0.64% Mn, 0.010% P, 0.011% S, 0.97% Cr, 0.16% Cu, 0.23% Mo, 0.33% Ni, <0.01% V
0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.090% N
0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.090% N
0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.0980% N
0.22% C, 0.25% Si, 1.33% Mn, 0.18% Cr, 0.02% Mo, 0.12% Ni, 0.033% Ti, 0.11% Cu, 0.034% Al, 0.0980% N
0.22% C, 0.26% Si, 0.82% Mn, 0.022% S, 0.014% P, 1.14% Cr, 0.024% Al, 0.0012% N
0.22% C, 0.28% Si, 0.70% Mn, 0.07% Cr, 0.25% Mo, 1.97% Ni, 0.010% V, 0.11% Cu.
0.22% C, 0.30% Si, 0.66% Mn, 0.018% P, 0.011% S, 0.56% Cr, 0.18% Cu, 0.44% Mo, 0.15% Ni, 0.020% N, 0.049% Al, max. 0.0005% B
0.22% C, 0.32% Si, 1.28% Mn, 0.18% Cr, 0.48% Mo, 0.54% Ni, 0.01% Co, 0.08% Cu, 0.025% Al
0.22% C, 0.34% Si, 1.18% Mn, 0.016% P, 0.022% S, 0.18% Cr, 0.15% Ni, 0.16% Cu, 0.01% Mo
0.22% C, 0.34% Si, 1.18% Mn, 0.022% P, 0.018% S, 0.22% Cr, 0.15% Ni, 0.21% Cu, 0.01% Mo, 0.16% Cu
0.22% C, 0.35% Si, 0.52% Mn, 0.011% P, 0.014% S, 12.00% Cr, 1.35% Mo, 0.59% Ni, 0.31% V, 0.40% W
0.22% C, 0.50% Mn, 0.016% P, 0.026% S, 0.30% Si, 2.80% Ni, 2.95% Mo
0.22% C, 0.50% Mn, 0.30% Si, 0.016% P, 0.026% S 2.80% Ni, 2.95% Mo
0.22% C, 0.50% Mn, 0.30% Si, 0.016% P, 0.026% S, 2.80% Ni, 2.95% Mo
0.22% C, 0.50% Si, 0.98% Mn, 3.00% Ni, 0.51% Cr, 0.50% Mo, 0.01% V, 0.028% Al
0.22% C, 0.50% Si, 0.98% Mn, 3.00% Ni, 0.51% Cr, 0.50% Mo, 0.010% V, 0.028% Al
0.22% C, 0.52% Mn, 5.35% Cr, 0.27% Mo, 0.08% V, 0.00% Cr, 0.00% Ni, 0.00% Mo, 0.00% V
0.22% C, 0.54% Mn, 0.64% Ni, 12.46% Cr, 0.99% Mo, 0.29% V
0.22% C, 0.54% Mn, 0.64% Ni, 12.46% Cr, 0.99% Mo, 0.29% V
0.22% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.50% Mo
0.22% C, 0.60% Mn, 0.30% Si, 0.020% P, 0.020% S, 1.15% Cr, 0.13% Ni, 0.60% Mo, 0.22% V
0.22% C, 0.64% Mn, 0.25% Si, 0.97% Cr, 0.33% Ni, 0.23% Mo
0.22% C, 0.64% Mn, 0.25% Si, 0.97% Cr, 0.33% Ni, 0.23% Mo
0.22% C, 0.64% Mn, 0.25% Si, 0.97%Cr, 0.33% Ni, 0.23% Mo, 0.01% V, 0.16% Cu
0.22% C, 0.64% Mn, 0.25% Si, 0.97%Cr, 0.33% Ni, 0.23% Mo, 0.01% V, 0.16% Cu
0.22% C, 0.66% Mn, 0.30% Si, 0.018% P, 0.011% S, 0.049% Al, 0.56% Cr, 0.18% Cu, 0.44% Mo, 0.15% Ni, 0.0095% B, 0.020% N
0.22% C, 0.76% Mn, 0.32% Si, 0.023% S, 0.012% P 2.657% Ni, 1.276% Cr, 0.51% Mo, 0.203% V, 0.002% Al
0.22% C, 0.76% Mn, 0.57% Ni, 0.51% Cr, 0.20% Mo, 0.0025% B
0.22% C, 0.77% Mn, 1.08% Ni, 1.91% Cr
0.22% C, 0.79% Mn, 0.32% Si, 0.87% Ni, 0.52% Cr, 0.47% Mo
0.22% C, 0.79% Mn, 0.50% Mo
0.22% C, 0.79% Mn, 0.50% Mo
0.22% C, 0.79% Mn, 0.50% Mo
0.22% C, 0.79% Mn, 0.50% Mo
0.22% C, 0.83% Mn, 0.24% Si, 0.007% P, 0.011% S, 0.30% Cu, 1.06% Ni, 0.54% Cr, 0.51% Mo, 0.029% sol. Al
0.22% C, 0.83% Mn, 0.24% Si, 0.007% P, 0.011% S, 0.30% Cu, 1.06% Ni, 0.54% Cr, 0.51% Mo, 0.029% sol. Al
0.22% C, 0.85% Mn, 0.24% Si, 0.008% P, 0.012% S, 0.30% Cu, 1.05% Ni, 0.54% Cr, 0.51% Mo, 0.02% V, 0.024% sol. Al
0.22% C, 0.85% Mn, 0.24% Si, 0.008% P, 0.012% S, 0.30% Cu, 1.05% Ni, 0.54% Cr, 0.51% Mo, 0.02% V, 0.024% sol. Al
0.22% C, 0.86% Si, 1.80% Mn, 0.006% B, 0.07% Nb, 1.60% Cr, 0.14% V, 0.55% Cu, 0.07% Ti, 0.74% Mo, 2.10% Ni, 0.016% N, 0.025% P, 0.012% S
0.22% C, 1.10% Mn, 0.21% Si, 0.015% P, 0.020% S, 0.60% Cr, 0.18% Ni, 0.08% V, 0.30% Cu
0.22% C, 1.19% Si, 1.53% Mn, 0.004% Mo, 0.57% Al, 0.03% Cu, 0.037% Nb
0.22% C, 1.25% Mn, 0.25% Si, 0.04% S, 0.03% P 0.33% Cr
0.22% C, 1.30% Mn, 1.36% Si, 1.88% Ni, 0.22% Cr 0.38% Mo
0.22% C, 1.30% Mn, 1.36% Si, 1.88% Ni, 0.22% Cr, 0.38% Mo
0.22% C, 1.45% Mn, 0.30% Si, 0.006% S, 0.020% P, 0.98% Cr, 0.01% Ni, 0.45% Mo, 0.03% V, 0.01% Cu, sol. 0.044% Al
0.22% C, 1.54% Mn, 0.25% Si, 0.014% P, 0.036% S, 0.11% Mo, 0.11% V, 0.011% N
0.22% C, 10.60% Cr
0.22% C, 11.50% Cr, 0.60% Ni, 1.00% Mo, 0.30% V
0.22% C, 11.50% Cr, 0.60% Ni, 1.00% Mo, 0.30% V
0.22% C, 11.50% Cr, 0.60% Ni, 1.00% Mo, 0.30% V
0.22% C, 2.30% Mo
0.22-0.24% C, 0.60-1.10% Si, 0.80% Mn, max. 0.0010% P, max. 0.003% S, 1.00-1.20% Cr, 0.30% Mo, 0.10-0.11% V, max. 1.00% Ni
0.22-0.24% C, 0.60-1.10% Si, 0.80% Mn, max. 0.010% P, 0.003% S, 1.00-1.20% Cr, 0.30% Mo, 0.10-0.11% V, max. 1.00% Ni. TOOLOX 44: 0.32% C, 0.60-1.10% Si, 0.80% Mn, max. 0.010% P, 0.003% S, 1.35% Cr, 0.80% Mo, 0.14% V, max. 1.00% Ni
0.22-0.25% C, 0.20-0.35% Si, 0.65-0.75% Mn, 0.020% P, 0.015-0.025% S, 1.20-1.30% Cr, 3.60-3.90% Ni, 0.30-0.35% Mo
0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo. 25CrMoS4: 0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S,; 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.29% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.22-0.30% C, 0.30-0.50% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.60-0.90% Cr, 0.20-0.40% Mo, 0.15-0.20% V, 1.30-1.60% V
0.22-0.31% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.15% Cr, 1.20-1.60% Ni
0.22-0.31% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.15% Cr, 1.20-1.60% Ni
0.22% C, 1.26% Mn, 0.015% P, 0.008% S, 0.28% Si, 0.044% Al, 0.023% Ti, 0.16% Cr, 30 ppm B
0.22% C, 0.35% Si, 0.86% Mn, 0.015% P, 0.006% S, 0.04% Al, 0.008% N, 0.02% Nb, 0.072% Ti
0.22% C, 1.80% Si, 2.00% Mn, 1.00% Cr, 0.25% Mo, 0.50% Al
0.22% C, 1.80% Si, 2.00% Mn, 1.00% Cr, 0.25% Mo, 0.50% Al
0.22% C, 0.30% Si, 0.66% Mn, 0.018% P, 0.011% S, 0.049% Al, 0.0005% B, 0.56% Cr, 0.18% Cu, 0.44% Mo, 0.020% N, 0.15% Ni
0.22% C, 1.20% Mn, 1.50% Si, 0.03% Al, 0.23% Cr, 0.0027% B, 0.03% Ti
0.222% C, 0.28% Si, 1.17% Mn, 0.18% Cr, 0.014% Ni, 0.01% Cu, 0.028% Al, 0.005% N, 0.002% Nb, 0.005% V, 0.030% Ti, 0.0022% B, 0.001% S, 0.013% P
0.222% C, 0.28% Si, 1.17% Mn, 0.18% Cr, 0.014% Ni, 0.01% Cu, 0.028% Al, 0.005% N, 0.002% Nb, 0.005% V, 0.030% Ti, 0.0022% B, 0.001% S, 0.013% P
0.223% C, 1.32% Mn, 0.489% Si, 0.009% P, 0.004% S, 0.044% Ni, 0.784% Cr, 0.004% V, 0.035% Al, 0.02% Ti, 0.005% Nb, 0.0011% B, 0.015% Cu, 0.016% Co, 0.016% Mo, 0.016% As, 0.002% Pb
0.224% C, 0.498% Mn, 0.226% Si, 0.02% S, 0.022% P, 0.037% Ni, 0.33% Cr, 0.195% Mo, 0.054% Al
0.226% C, 0.471% Si, 1.430% Mn, 0.017% P, 0.008% S, 0.024% Cr, 0.031% Ni, 0.016% Mo, 0.045% Al, 0.033% Cu, 0.001% Nb, 0.001% Ti, 0.003% V
0.23% C, 0.67% Si, 0.90% Mn, 0.90% Cr, 0.23% Mo, 0.043% Al, 0.1% Zr, 0.013% P, 0.013% S
0.23% C, 0.09% Si, 0.51% Mn, 0.75% Cr, 0.0021% B, 0.03% Ti, 0.023% Al, 0.0071% N, 0.0023% O
0.23% C, 0.20% Si, 0.40% Mn, 1.78% Ni, 0.18% Cr, 0.27% Mo
0.23% C, 0.21% Si, 1.54% Mn, 0.012% P, 0.011% S, 0.23% Cr, 0.51% Mo, 1.07% Ni, 0.042% Al
0.23% C, 0.22% Mn, 0.22% Si, 0.004% S, 0.015% P, 1.70% Cr, 3.60% Ni, 0.53% Mo, 0.12% V
0.23% C, 0.23% Si, 0.42% Mn, 0.025% S, 0.023% P, 1.78% Ni, 0.23% C, 0.26% Mo
0.23% C, 0.24% Si, 0.68% Mn, 2.03% Cr, 0.83% Mo, 0.74% Ni, 0.68% W, 0.30% V
0.23% C, 0.25% Si, 0.80% Mn, 0.80% Cr, 0.35% Mo + B
0.23% C, 0.25% Si, 0.80% Mn, 0.80% Cr, 0.35% Mo + B
0.23% C, 0.25% Si, 1.38% Mn, 0.006% P, 0.013% S, 0.14% Cr, 0.51% Mo, 0.58% Ni, 0.12% Cu, 0.026% Al, 0.016% N
0.23% C, 0.29% Si, 1.25% Mn, 0.003% S, 0.013% P, 0.211% Cr, 30 ppm B
0.23% C, 0.30% Si, 0.65% Mn, 0.013% P, 0.030% S, 0.051% Al, 0.12% Cr, 0.08% Cu, 0.50% Mo, 0.05% Ni, 0.03% V
0.23% C, 0.30% Si, 0.65% Mn, 0.12% Cr, 0.50% Mo, 0.05% Ni, 0.030% V, 0.08% Cu, 0.051% Al
0.23% C, 0.30% Si, 0.84% Mn, 0.55% Ni, 0.66% Cr, 0.11% Mo
0.23% C, 0.30% Si, 1.51% Mn, 0.016% P, 0.014% S, 0.28% Cr, 0.27% Ni, 0.09% V, 0.25% Cu, 0.03% Mo, 0.030% Al, 0.021% Sn
0.23% C, 0.44% Si, 0.62% Mn, 0.014% P, 0.007% S, 13.50% Cr, 0.17% Mo, 0.70% N
0.23% C, 0.45% Si, 1.32% Mn, 0.029% P, 0.022% S, 0.05% Cr
0.23% C, 0.47% Si, 0.68% Mn, 0.026% P, 0.009% S, 0.96% Cr, 0.39% Mo
0.23% C, 0.52% Mn, 0.25% Si, 5.35% Ni, 0.20% Cr 0.27% Mo, 0.08% V
0.23% C, 0.52% Mn, 0.25% Si, 5.35% Ni, 0.20% Cr, 0.27% Mo, 0.08% V
0.23% C, 0.53% Mn, 0.30% Si, 0.018% P, 1.55% Cr, 0.30% Ni, 0.29% Mo, 0.21% V, 0.11% Cu
0.23% C, 0.56% Mn, 0.27% Si, 0.020% S, 0.021% P 2.06% Ni, 0.15% Cr, 0.01% Mo, 0.18% Cu
0.23% C, 0.65% Mn, 0.30% Si, 0.030% S, 0.013% P, 0.12% Cr, 0.05% Ni, 0.50% Mo, 0.03% V, 0.08% Cu, 0.051% Al
0.23% C, 0.72% Mn, 0.59% Ni, 0.52% Cr, 0.21% Mo /0.22% C, 0.76% Mn, 0.57% Ni, 0.51% Cr, 0.20% Mo, 0.0025% B
0.23% C, 0.82% Mn, 0.22% V, 1.22% Cr, 0.53% Mo
0.23% C, 0.82% Mn, 1.22% Cr, 0.53% Mo, 0.22% V
0.23% C, 0.85% V
0.23% C, 1.50% Si, 0.97% Mn, 1.86% Ni, 0.91% Cr, 0.39% Mo
0.23% C, 1.50% Si, 0.97% Mn, 1.86% Ni, 0.91% Cr, 0.39% Mo
0.23% C, 16.50% Cr, 1.80% Ni
0.23% C, 3.00% Cr, 11.10% Ni, 1.20% Mo, 13.40% Co
0.23% C, 3.10% Cr, 11.10% Ni, 1.20% Mo, 13.40% Co
0.23% C, 5.10% Cr
0.23-0.29% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.40-0.50% Mo
0.23-0.29% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.40-0.50% Mo
0.23-0.29% C, 0.15-0.40% Si, 1.40-1.70% Mn, max. 0.025% P, 0.005% S, 1.20-1.80% Cr, 0.30-0.70% Mo, 0.90-1.20% Ni
0.23% C, 0.01% Si, 0.25% Mn
0.23% C, 0.44% Mn, 0.10% Si, 0.034% P, 0.051% S
0.23% C, 0.02% Si, 0.38% Mn, 0.013% P, 0.020% S
0.233% C, 1.365% Si, 1.54% Mn, 0.004% S, 0.007% P, 0.080% Al
0.233% C, 1.365% Si, 1.540% Mn, 0.004% S, 0.007% P, 0.080% Al
0.24% C, cca. 0.60% Si, cca. 1.55% Mn, max. 0.035% P, max. 0.035% S, min. 0.025% Al, 0.12-0.20% Ti
0.24% C, 0.20% Si, 1.58% Mn, 0.014% S, 0.016% P, 0.20% Ni, 0.24% Cr, 0.022% Mo, 0.12% Cu, 0.040% As, 0.018% Co
0.24% C, 0.20% Si, 1.58% Mn, 0.014% S, 0.016% P, 0.20% Ni, 0.24% Cr, 0.022% Mo, 0.12% Cu, 0.040% As, 0.018% Co
0.24% C, 0.20% Si, 1.58% Mn, 0.016% P, 0.014% S, 0.24% Cr, 0.02% Mo, 0.20% Ni, 0.12% Cu
0.24% C, 0.20% Si, 1.58% Mn, 0.016% P, 0.014% S, 0.24% Cr, 0.02% Mo, 0.20% Ni, 0.12% Cu
0.24% C, 0.21% Si, 1.06% Mn, 0.014% P, 0.020% S, 0.79% Cr, 0.17% Cu, 0.02% Mo, 0.18% Ni, 0.10% V
0.24% C, 0.21% Si, 1.06% Mn, 0.014% P, 0.020% S, 0.79% Cr, 0.17% Cu, 0.02% Mo, 0.18% Ni, 0.10% V
0.24% C, 0.24% Si, 0.57% Mn, 0.012% P, 0.010% S, 1.10% Cr, 0.25% Mo
0.24% C, 0.24% Si, 0.57% Mn, 0.012% P, 0.010% S, 1.10% Cr, 0.25% Mo
0.24% C, 0.24% Si, 0.57% Mn, 0.012% P, 0.010% S, 1.10% Cr, 0.25% Mo
0.24% C, 0.24% Si, 0.57% Mn, 0.012% P, 0.010% S, 1.10% Cr, 0.25% Mo
0.24% C, 0.24% Si, 1.16% Mn, 0.020% P, 0.018% S, 0.52% Cr, 0.28% Mo, 0.47% Ni, 0.13% Cu, 0.025% Al
0.24% C, 0.24% Si, 1.33% Mn, 0.016% P, 0.006% S, 0.18% Cr, 0.025% Al, 0.004% B, 0.025% Ti
0.24% C, 0.25% Si, 0.45% Mn, 1.35% Cr, 0.20% V, 0.55% Mo
0.24% C, 0.25% Si, 0.45% Mn, 1.35% Cr, 0.20% V, 0.55% Mo
0.24% C, 0.25% Si, 0.45% Mn, 1.35% Cr, 0.55% Mo, 0.20% V
0.24% C, 0.25% Si, 0.45% Mn, 1.35% Cr, 0.55% Mo, 0.20% V
0.24% C, 0.25% Si, 0.45% Mn, 1.40% Cr, 0.20% V, 0.55% Mo
0.24% C, 0.25% Si, 0.60% Mn, 1.10% Cr, 0.25% Mo
0.24% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.24% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.24% C, 0.27% Mn, 0.37% Si, 0.021% P, 0.010% S, 13.30% Cr, 0.32% Ni, 0.06% Mo
0.24% C, 0.27% Mn, 0.37% Si, 0.32% Ni, 13.30% Cr 0.06% Mo
0.24% C, 0.27% Si, 1.51% Mn, 0.082% P, 1.12% Al, 0.54% CE
0.24% C, 0.28% Si, 0.43% Mn, 0.017% P, 0.009% S, 11.52% Cr, 0.93% Mo, 0.69% Ni, 0.30% V, 0.50% W
0.24% C, 0.29% Si, 0.39% Mn, 0.019% P, 0.015% S, 16.58% Cr, 0.20% Mo, 1.96% Ni
0.24% C, 0.33% Si, 0.52% Mn, 0.029% P, 0.006% S, 15.80% Cr, 0.38% Mo, 1.64% Ni, 0.12% Cu, 0.014% Al
0.24% C, 0.33% Si, 0.88% Mn, 0.23% Mo
0.24% C, 0.35% Mn, 0.13% Si, 0.008% S, 0.030% P, 1.75% Cr, 3.50% Ni, 0.49% Mo, 0.12% V
0.24% C, 0.35% Mn, 0.13% Si, 0.008% S, 0.030% P, 1.75% Cr, 3.50% Ni, 0.49% Mo, 0.12% V
0.24% C, 0.37% Si, 0.27% Mn, 13.30% Cr, 0.32% Ni, 0.06% Mo
0.24% C, 0.41% Si, 1.60% Mn, 0.016% P, 0.014% S, 0.22% Cr, 0.15% Ni, 0.20% Cu, 0.03% Mo
0.24% C, 0.45% Mn, 0.97% Si, 2.92% Ni, 1.09% V, 0.55% Al
0.24% C, 0.46% Mn, 0.42% Si, 0.26% Ni, 24.85% Cr, 0.02% Mo, 0.010% Al, 0.17% N
0.24% C, 0.47% Si, 0.94% Mn, 0.30% Ni, 0.34% Cr, 0.14% Mo
0.24% C, 0.50% Si, 1.53% Mn, 0.78% Cr, 0.08% Mo, 0.01% V, 0.025% Ti, 30 ppm B, 80 ppm N. 200 V steel: 0.24% C, 0.50% Si, 1.58% Mn, 0.79% Cr, 0.08% Mo, 0.21% V, 0.025% Ti, 30 ppm B, 80 ppm N.
0.24% C, 0.52% Mn, 0.27% Si, 0.012% S, 0.015% P 2.10% Ni, 0.05% Cr, 0.32% Mo, 0.10% Cu
0.24% C, 0.55% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.25% Mo, 1.80% Ni
0.24% C, 0.55% Si, 1.60% Mn, 0.035% P, 0.035% S.
0.24% C, 0.59% Mn, 0.011% P, 0.023% P, 0.22% Si, 0.99% Ni, 0.17% Mo
0.24% C, 0.63% Mn, 0.30% Si, 0.016% P, 0.027% S, 2.95% Mo
0.24% C, 0.69% Mn, 3.35% Ni, 0.09% V, 0.50% Mo
0.24% C, 0.69% Mn, 3.35% Ni, 0.50% Mo, 0.09% V
0.24% C, 0.74% Mn, 0.25% Si, 0.016% S, 0.012% P, 0.37% Cr, 0.67% Ni, 0.52% Mo, 0.03% V
0.24% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.24% C, 0.87% Mn, 0.40% Al, 0.010% P, 0.004% S, 0.034% Nb, 0.023% Ti
0.24% C, 0.88% Mn, 0.33% Si, 0.23% Mo
0.24% C, 0.90% Mn, 0.30% Si, 0.020% P, 0.020% S, 0.23% Mo
0.24% C, 0.94% Mn, 0.30% Ni, 0.47% Si, 0.34% Cr, 0.14% Mo
0.24% C, 1.06% Mn, 0.21% Si, 0.020% S, 0.014% P, 0.79% Cr, 0.18% Ni, 0.02% Mo, 0.10% V, 0.17% Cu
0.24% C, 1.06% Mn, 0.21% Si, 0.020% S, 0.014% P, 0.79% Cr, 0.18% Ni, 0.02% Mo, 0.10% V, 0.17% Cu
0.24% C, 1.06% Mn, 0.21% Si, 0.79% Cr, 0.18% Ni, 0.02% Mo, 0.1% V, 0.17% Cu
0.24% C, 1.06% Mn, 0.21% Si, 0.79% Cr, 0.18% Ni, 0.02% Mo, 0.1% V, 0.17% Cu
0.24% C, 1.49% Si, 0.97% Mn, 1.86% Ni, 0.99% Cr, 0.38% Mo, 0.08% Al
0.24% C, 1.49% Si, 0.97% Mn, 1.86% Ni, 0.99% Cr, 0.38% Mo, 0.080% Al
0.24% C, 1.58% Mn, 0.20% Si, 0.014% S, 0.016% P 0.20% Ni, 0.24% Cr, 0.02% Mo, 0.12% Cu, 0.018% Co
0.24% C, 1.58% Mn, 0.20% Si, 0.014% S, 0.016% P 0.20% Ni, 0.24% Cr, 0.02% Mo, 0.12% Cu, 0.018% Co
0.24% C, 1.59% Mn, 0.23% Si, 0.024% P, 0.019% S
0.24% C, 1.67% Mn, 0.39% Si, 0.14% Ni, 0.17% Cr, 0.22% Mo, 0.11% V
0.24% C, 1.67% Mn, 0.39% Si, 0.14% Ni, 0.17% Cr, 0.22% Mo, 0.11% V
0.24% C, 1.67% Mn, 0.39% Si, 0.14% Ni, 1.17% Cr, 0.22% Mo, 0.11% V
0.24% C, 1.72% Mn, 2.13% Si, 0.008% P, 0.010% S, 22.80% Ni, 25.70% Cr, 0.016% N
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, <0.040% S, <0.035% P, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24-0.30% C, 0.40% Si, 1.10-1.40% Mn, 0.025% P, 0.035% S, 0.30-0.60% Cr, 0.0008-0.0050% B
0.24% C, 1.49% Mn, 0.80% Cr, 0.07% Mo, 0.17% V, 0.080% S
0.24% C, 0.48% Si, 0.67% Mn, 0.009% P, 0.009% S, 0.17% Cu, 0.19% Cr, 0.12% Ni, 0.39% Mo, 0.054% Al, 0.001% V
0.25% C, 0.03% Si, 1.10% Mn, 0.011% P, 0.019% S
0.25% C, 0.15% Si, 0.52% Mn, 0.010% P, 0.024% S, 3.33% Ni, 1.14% Cr, 0.65% Mo, 0.16% V
0.25% C, 0.24% Si, 0.57% Mn, 0.029% S, 0.028% P, 1.78% Ni, 0.26% C, 0.21% Mo
0.25% C, 0.24% Si, 0.65% Mn, 2.36% Cr, 0.22% Mo, 0.19% Ni, 0.11% Cu, 0.012% Al
0.25% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.00% Cr, 1.45% Ni
0.25% C, 0.25% Si, 0.70% Mn, 1.00% Cr, 1.45% Ni
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo, (Pb)
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo, (Pb)
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.25% Mo
0.25% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.45% Mo
0.25% C, 0.25% Si, 0.75% Mn, 0.50% Cr, 0.45% Mo
0.25% C, 0.29% Si, 0.55% Mn, 0.012% P, 0.022% S, 0.53% Cr, 0.27% Mo, 1.89% Ni, 0.11% Cu
0.25% C, 0.35% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.25% C, 0.35% Si, 0.75% Mn, 1.05% Cr, 0.23% Mo
0.25% C, 0.37% Si, 0.65% Mn, 6.60% Ni, 0.40% Mo, 0.21% Cr, 0.011% V, 0.006% S, 0.013% P, 0.03% Cu, 0.009% Co, 0.005% W, 380 ppm O, 80 ppm Ti, 1 ppm B, 10 ppm Nb
0.25% C, 0.37% Si, 0.65% Mn, 6.60% Ni, 0.40% Mo, 0.21% Cr, 0.011% V, 0.006% S, 0.013% P, 0.03% Cu, 0.009% Co, 0.005% W, 380 ppm O, 80 ppm Ti, 1 ppm B, 10 ppm Nb
0.25% C, 0.40% Mn, <0.10% Si, 3.50% Ni, 1.50% Cr, 0.50% Mo, 0.10% V
0.25% C, 0.499% Mn, 0.235% Si, 0.023% S, 0.007% P, 3.65% Ni, 1.65% Cr, 0.395% Mo, 0.008% N2, 0.013% Al
0.25% C, 0.50% Si, 1.40% Mn, 0.80% Cr, 0.02% Ti, 2.00% Ni, 0.70% Mo, 0.04% Nb, 0.08% V, 0.10% Cu 0.25% C, 0.52% Mn, 0.15% Si, 3.33% Ni, 1.14% Cr 0.65% Mo, 0.16% V
0.25% C, 0.68% Mn, 0.21% Si, 0.090% S, 0.018% P 0.19% Ni, 1.10% Cr, 0.22% Mo, 0.16% Cu
0.25% C, 0.68% Mn, 0.21% Si, 0.090% S, 0.018% P 0.19% Ni, 1.10% Cr, 0.22% Mo, 0.16% Cu
0.25% C, 0.70% Mn, 0.20% Si, 0.015% Nb, 0.01% N. Steel 2: 0.25% C, 0.70% Mn, 0.20% Si, 0.03% Nb, 0.01% N. Steel 3: 0.20% C, 1.30% Mn, 0.20% Si, 0.02% Ti, 0.01% N
0.25% C, 0.88% Mn, 0.59% Ni, 0.73% Cr, 0.88% Mo, 0.23% V
0.25% C, 0.88% Mn, 0.59% Ni, 0.73% Cr, 0.88% Mo, 0.23% V
0.25% C, 1.30% Cr, 1.30% Mn, 0.02% P, 0.02% S, 0.050% Mo, +B
0.25% C, 1.30% Mn, 0.20% Si, 0.02% P, 0.06% S, 1.30% Cr, 0.40% Mo, +B
0.25% C, 1.30% Mn, 1.30% Cr, 0.40% Mo, <0.020% P, <O.020% S
0.25% C, 1.45% Si, 1.36% Mn, 1.74% Ni, 0.10% Cr, 0.40% Mo
0.25% C, 1.45% Si, 1.36% Mn, 1.74% Ni, 0.10% Cr, 0.40% Mo
0.25% C, 1.50% Si, 1.30% Mn, 1.80% Ni, 0.40% Mo
0.25% C, 1.76% Si, 1.32% Mn, 1.86% Ni, 0.10% Cr, 0.36% Mo, 0.024% Al
0.25% C, 1.76% Si, 1.32% Mn, 1.86% Ni, 0.10% Cr, 0.36% Mo, 0.024% Al
0.25-0.30% C, 0.50-0.80% Si, 1.30-1.60% Mn, max. 0.035% P, 0.030-0.050% S, 0.08-0.13% V
0.25-0.30% C, max. 0.15% Si, 0.30-0.80% Mn, max. 0.010% P, max. 0.007% S, 1.00-1.30% Cr, 0.75-1.00% Mo, 0.50-0.75% Ni, 0.25-0.35% V, 0.010% Al
0.25-0.30% C, max. 0.30% Si, 0.35-0.80% Mn, max. 0.015% P, max. 0.018% S, 1.10-1.40% Cr, 0.80-1.00% Mo, 0.50-0.75% Ni, 0.25-0.35% V
0.25-0.32% C, <0.40% Si, 1.30-1.60% Mn, <0.035% S, <0.035% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mn+Ni=<0.63
0.25-0.32% C, 0.40% Si, 1.30-1.65% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%
0.25-0.32% C, 0.40% Si, 1.30-1.65% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.25-0.32% C, 0.40% Si, 1.30-1.65% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.25-0.32% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, 0.15-0.25% S, 12.00-13.50% Cr, 0.60% Mo
0.25-0.35% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 2.20-2.50% Cr, 4.00-4.50% W, 0.50-0.70% V
0.25-0.35% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 2.20-2.50% Cr, 4.00-4.50% W, 0.50-0.70% V
0.25-0.35% C, 0.80-1.10% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 3.50-4.00% W, 0.15-0.20% V
0.25-0.35% C, 0.80-1.10% Si, 0.30-0.50% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 3.50-4.00% W, 0.15-0.20% V
0.25-0.35% C, max. 1.00% Si, max. 1.00% Mn, max. 0.030% P, max. 0.025% S, 14.00-16.00% Cr, 0.85-1.10% Mo, max. 0.50% Ni
0.25-0.35% C, max. 1.00% Si, max. 1.00% Mn, max. 0.030% P, max. 0.025% S, 14.00-16.00% Cr, 0.85-1.10% Mo, max. 0.50% Ni
0.25% C, 0.20% Si, 1.20% Mn, 0.04% Ni, 0.02% P, 0.003% S, 0.07% Cu
0.25% C, 1.80% Ni, 1.50% Si, 0.40% Mo
0.25% C, 1.20% Mn, 0.04% Ni, 0.07% Cu, 0.02% P, 0.003% S, 0.20% Si
0.25% C, 1.2% Mn, 0.72% Ni, 0.49% Mo, 0.05% Cr
0.25% C, max. 0.40% Si, max. 1.40% Mn, max. 0.025% P, max. 0.010% S, max. 0.015% Al, max. 0.05% Ti, max. 0.50% Cr+Mo, max. 0.005% B
0.25-0.31% C, 0.60-0.90% Mn, max. 0.040% P, max. 0.050% S
0.25% C, 1.50% Si, 2.82% Mn, 0.023% Al, 0.002% S, 0.015% Cr, 0.003% V, 0.002% Mo, 0.0008% Ti, 0.004% Nb, 0.0003% B
0.25% C, 0.43% Si, 0.64% Mn, 0.018% P, 0.025% S, 0.16% Cu, 0.80% Cr, 0.40% Ni, 0.29% Mo, 0.04% Ti, 0.043% Al, 0.03% V
0.25% C, 0.27% Si, 0.60% Mn, 0.002% P, 0.022% S, 0.17% Cu, 0.93% Cr, 0.33% Ni, 0.26% Mo, 0.025% Al, 0.01% V
0.256% C, 1.20% Si, 1.48% Mn, 0.017% P, 0.008% S, 1.51% Ni, 0.053% Nb
0.256% C, 1.20% Si, 1.48% Mn, 0.017% P, 0.008% S, 1.51% Ni, 0.053% Nb
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 1.05% Ni, 0.50% Mo, 0.10% V
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 1.05% Ni, 0.60% Mo, 0.12% V
0.26% C, 0.16% Si, 0.39% Mn, 0.014% P, 0.032% S, 1.36% Cr, 0.10% Ni, 0.15% V, 0.15% Cu, 0.53% Mo
0.26% C, 0.21% Si, 0.55% Mn, 0.010% P, 0.022% S, 0.25% Ni, 3.34% Cr, 0.54% Mo
0.26% C, 0.21% Si, 0.55% Mn, 0.022% S, 0.010% P, 0.25% Ni, 3.34% Cr, 0.54% Mo
0.26% C, 0.23% Si, 0.31% Mn, 0.014% P, 0.028% S, 3.11% Cr
0.26% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.26% C, 0.26% Si, 0.60% Mn, 0.008% P, 0.012% S, 1.28% Cr, 2.78% Ni, 1.58% W, 0.02% V, 0.09% Cu, 0.17% Mo, 0.004% Sn
0.26% C, 0.26% Si, 0.60% Mn, 0.008% P, 0.012% S, 1.28% Cr, 2.78% Ni, 1.58% W, 0.02% V, 0.09% Cu, 0.17% Mo, 0.004% Sn
0.26% C, 0.39% Si, 1.64% Mn, 0.049% P, 1.35% Al, 0.099% Ti, 0.053% V, 0.61% CE
0.26% C, 0.41% Mn, 0.22% Si, <0.002% P, 0.024% S, 2.91% Ni, 1.98% Cr, 0.69% Mo, <0.015% Al
0.26% C, 0.42% Si, 1.51% Mn, 0.021% P, 0.028% S, 0.45% Cr, 0.50% Mo
0.26% C, 0.55% Mn, 0.21% Si, 0.25% Ni, 3.34% Cr 0.54% Mo
0.26% C, 0.57% Mn, 2.20% Ni, 0.09% V, 0.48% Mo
0.26% C, 0.57% Mn, 2.20% Ni, 0.48% Mo, 0.09% V
0.26% C, 0.58% Mn, 0.49% Si, 0.010% S, 0.014% P 0.18% Ni, 1.65% Cr, 0.84% Mo, 0.07% Cu, 0.38% V
0.26% C, 0.58% Mn, 0.49% Si, 0.010% S, 0.014% P 0.18% Ni, 1.65% Cr, 0.84% Mo, 0.07% Cu, 0.38% V
0.26% C, 0.60% Mn, 0.14% Si, 0.020% P, 0.020% S, 3.25% Cr, 0.55% Mo
0.26% C, 0.60% Mn, 0.39% Si, 0.008% P, 0.007% S, 1.77% Ni, 0.70% Cr, 0.32% Mo, 0.00% Cu
0.26% C, 0.66% Mn, 0.07% Si, 0.026% P, 0.020% S, 3.53% Ni, 0.84% Cr
0.26% C, 0.70% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.05% Cr, 0.22% Mo
0.26% C, 0.72% Mn, 0.29% Si, <0.002% P, 0.025% S, 0.11% Ni, 1.01% Cr, 1.04% Mo, 0.23% V, <0.015% Al
0.26% C, 0.72% Si, 0.62% Mn, 0.028% P, 0.007% S, 0.32% Ni, 5.17% Cr, 0.46% Mo
0.26% C, 0.73% Mn, 0.243% Si, 0.016% S, 0.018% P 0.175% Ni, 1.065% Cr, 0.255% Mo
0.26% C, 0.75% Mn, 0.26% Si, 0.014% S, 0.010% P, 0.45% Cr, 0.81% Ni, 0.61% Mo, 0.05% V
0.26% C, 0.76% Mn, 0.32% Si, 0.012% S, 0.014% P, 1.08% Cr, 0.72% Ni, 1.25% Mo, 0.31% V
0.26% C, 0.87% Mn, 0.26 Mo
0.26% C, 0.87% Mn, 0.26% Mo
0.26% C, 1.48% Mn, 0.28% Si, 0.015% S, 0.015% P 0.08% Ni, 0.02% Cr, 0.01% Mo, 0.14% Cu
0.26% C, 1.63% Mn, 0.28% Si, 0.021% P, 0.034% S
0.26% C, 1.67% Mn, 0.30% Si, 0.015% S, 0.023% P, 0.05% Cr, 0.03% Ni, 0.11% Mo, 0.06% V, 0.01% Cu, sol. 0.013% Al
0.26% C, 1.67% Mn, 0.32% Si, 0.021% P, 0.032% S, 0.0034% B
0.26-0.33% C, 0.15-0.80% Si, 1.20-1.60% Mn, max. 0.025% P, 0.020-0.060% S, max. 0.30% Cr, max. 0.08% Mo, 0.08-0.20% V, 0.01-0.02% N
0.26-0.34% C, <0.40% Si, 0.40-0.70% Mn, <0.035% P, <0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, <0.60% Ni
0.26-0.34% C, 0.15-0.40% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 1.80-2.30% Cr, 0.30-0.65% Mo, 1.80-2.30% Ni
0.26-0.34% C, 0.15-0.40% Si, 0.30-0.60% Mn, max. 0.025% P, max. 0.025% S, 1.80-2.30% Cr, 0.30-0.65% Mo, 1.80-2.30% Ni
0.26-0.34% C, 0.40% Si, 0.30-0.60% Mn, 0.035% P, 0.035% S, 1.30-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, max. 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, max. 0.60% Ni, 0.10-0.20% V
0.26-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.80-2.20% Cr, 0.30-0.50% Mo, 1.80-2.20% Ni
0.26-0.34% C, max. 0.40% Si, max. 0.035% P, max. 0.030% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.26% C, 0.10% Si, 1.45% Mn, 0.015% P, 0.002% S, 1.25% Cr, 1.05% Ni, 0.50% Mo, 0.12% V
0.26% C, 0.65% Mn, 1.00% Si, 1.00% Ni, 2.70% Cr, 0.42% Mo, 1.00% W
0.26% C, 1.00% Mn, 0.35% Si, 0.60% Ni, 1.45% Cr, 0.55% Mo, + others
0.26% C, 1.00% Mn, 0.35% Si, 0.60% Ni, 1.45% Cr, 0.55% Mo, + others
0.26% C, 0.27% Si, 0.59% Mn, 0.018% P, 0.010% S, 1.13% Cr, 0.18% Mo
0.26% C, 0.36% Si, 0.97% Mn, 0.010% P, 0.024% S, 0.19% Cu, 0.13% Cr, 0.06% Ni, 0.04% Mo, 0.01% Al, 0.01% V
0.27-0.34% C, 98.67-99.13% Fe, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.27% C, 0.10% Si, 0.76% Mn, 0.013% P, 0.008% S, 0.23% Cr, 0.05% Mo, 0.18% Ni, 0.16% Cu, 0.040% Al
0.27% C, 0.13% Si, 0.60% Mn, 0.022% S, 0.030% P, 0.19% Ni, 0.74% Cr, 0.55% Mo
0.27% C, 0.26% Si, 0.53% Mn, 0.023% P, 0.011% S, 3.38% Ni, 0.71% Cr, 0.18% Mo
0.27% C, 0.30% Si, 1.07% Mn, 0.21% Cr, 0.02% Ti, 0.0032% B
0.27% C, 0.35% Si, 0.26% Mn, 13.51% Cr, 0.11% N
0.27% C, 0.35% Si, 0.26% Mn, 13.51% Cr, 0.11% N
0.27% C, 0.37% Si, 0.94% Mn, 0.011% P, 0.007% S, 1.85% Cr, 1.21% Ni, 0.01% V, 0.20% Cu, 0.32% Mo, 0.05% Al
0.27% C, 0.42% Si, 0.36% Mn, 0.82% Cr, 0.56% Mo, 2.36% Ni, 0.05% Co, 0.11% Cu, 0.013% Al
0.27% C, 0.43% Mn, 0.26% Si, 0.018% S, 0.08% P 0.10% Ni, 2.45% Cr, 0.13% Mo, 0.36% Cu, 8.70% W
0.27% C, 0.57% Si, 1.49% Mn, 0.013% P, 0.039% S, 0.18% Cr, 0.12% Ni, 0.09% V, 0.16% Cu, 0.03% Mo
0.27% C, 0.57% Si, 1.49% Mn, 0.013% P, 0.039% S, 0.18% Cr, 0.12% Ni, 0.09% V, 0.16% Cu, 0.03% Mo
0.27% C, 0.60% Mn, 0.13% Si, 0.030% P, 0.022% S, 0.74% Cr, 0.55% Mo, 0.19% Ni
0.27% C, 0.60% Mn, 0.13% Si, 0.19% Ni, 0.74% Cr 0.55% Mo
0.27% C, 0.66% Si, 1.43% Mn, 0.014% P, 0.036% S, 0.10% Cr, 0.00% Ni, 0.024% Al
0.27% C, 0.66% Si, 1.43% Mn, 0.014% P, 0.036% S, 0.10% Cr, 0.00% Ni, 0.024% Al
0.27% C, 0.67% Mn, 0.20% Si, 0.017% P, 0.022% S, 0.034% Al, 0.50% Cr, 0.002% B, 0.45% Mo, 0.11% Ni, 0.005% N
0.27% C, 0.77% Mn, 1.39% Si, 1.64% Cr, 0.20% Ni, 0.56% Mo, 0.07% V
0.27% C, 0.84% Mn, 0.60% Ni, 0.73% Cr, 0.90% Mo, 0.11% V
0.27% C, 0.84% Mn, 0.60% Ni, 0.73% Cr, 0.90% Mo, 0.11% V
0.27% C, 1.12% Mn
0.27% C, 1.12% Mn
0.27% C, 1.17% Mn, 0.31% Si, 0.48% Cr, 0.0013% B
0.27% C, 1.17% Mn, 0.31% Si, 0.48% Cr, 0.0013% B
0.27% C, 1.17% Mn, 0.31% Si, 0.48% Cr, 0.0013% B
0.27% C, 1.17% Mn, 0.31% Si, 0.48% Cr, 0.0013% B
0.27% C, 1.35% Mn, 0.24% Si, 0.025% P, 0.025% S, 0.45% Cr, 0.75% Ni, 0.20% Mo
0.27% C, 1.36% Mn, 0.50% Si, 0.006% S, 0.016% P, 0.58% Cr, 0.68% Ni, 0.34% Mo, 0.08% V
0.27% C, 1.55% Mn, 0.20% Si, 0.025% P, 0.025% S, 0.28% Mo
0.27% C, 2.11% Si, 1.60% Mn, 0.013% P, 0.013% S, 0.49% Cr, 0.003% Mo, 0.233% Al, 0.002% B, 0.001% Ti, 0.011% N
0.27% Cu, 0.30% Si, 0.65% Mn, 14.50% Cr, 0.85% Ni, 1.00% Mo + others
0.27-0.30% C, max. 0.40% Si, 1.15-1.45% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.27-0.32% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 2.20-2.50% Cr, 8.00-9.00% W, 0.20-0.30% V, 1.80-2.30% Co
0.27-0.32% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 2.20-2.50% Cr, 8.00-9.00% W, 0.20-0.30% V, 1.80-2.30% Co
0.27-0.34% C, <0.40% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, 0.10-0.40% Si, 0.35-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.80% Cr, 2.50-3.00% Ni
0.27-0.34% C, 0.10-0.40% Si, 0.35-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.80% Cr, 2.50-3.00% Ni
0.27-0.34% C, 0.15-0.25% Si, 0.35-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.15% Cr, 0.15-0.25% Mo
0.27-0.34% C, 0.15-0.25% Si, 0.35-0.60% Mn, 0.035% P, 0.035% S, 0.80-1.15% Cr, 0.15-0.25% Mo
0.27-0.34% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.30-2.70% Cr, 0.15-0.25% Mo, 0.10-0.20% V
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.27-0.34% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max.0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.27-0.34% C, 98.67-99.13% Fe, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S. AISI 1090 steel: 0.85-0.98% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S.
0.27% C, 0.24% Si, 1.15% Mn, 1.07% Cr, 0.10% Ti
0.27% C, 0.02% Si, 0.37% Mn, 0.011% P, 0.019% S
0.28% C, 0.11% Si, 0.36% Mn, 0.008% P, 0.004^ S, 2.57% Cr, 0.03% Mo, 0.04% Ni, 8.88% W, 0.35% V
0.28% C, 0.15% Si, 0.40% Mn, 0.80% Cr, 0.15% Mo, 0.15% Cu. Actual composition: 0.29% C, 0.24% Si, 0.55% Mn, 1.02% Cr, 0.15% Mo, 0.15% Cu/
0.28% C, 0.16% Si, 0.39% Mn, 0.020% P, 0.006% S, 2.35% Cr, 0.06% Mo, 0.06% Ni, 0.53% V, 3.18% W
0.28% C, 0.16% Si, 0.39% Mn, 0.020% P, 0.006% S, 2.35% Cr, 0.06% Mo, 0.06% Ni, 0.53% V, 3.18% W
0.28% C, 0.19% Si, 0.65% Mn, 0.016% P, 0.023% S, 0.16% Ni, 0.68% Cr, 0.22% Mo
0.28% C, 0.21% Si, 1.05% Mn, 0.017% P, 0.036% S, 0.18% Cr, 0.11% Ni, 0.24% Cu, 0.04% Mo, 0.040% Ti, 0.004% B
0.28% C, 0.24% Mn, 0.29% Si, 0.005% S, 0.024% P 0.18% Ni, 2.68% Cr, 2.84% Mo, 0.50% V
0.28% C, 0.24% Si, 0.79% Mn, 0.020% S, 0.020% P, 0.33% Ni, 1.65% Cr, 0.35% Mo, 0.14% Cu, 0.02% Al
0.28% C, 0.25% Si, 0.46% Mn, 0.011% P, 0.003% S, 0.76% Cr, 2.71% Ni, 0.06% W, 0.23% Cu, 0.04% Mo, 0.078% Co
0.28% C, 0.25% Si, 0.46% Mn, 0.011% P, 0.003% S, 0.76% Cr, 2.71% Ni, 0.06% W, 0.23% Cu, 0.04% Mo, 0.078% Co
0.28% C, 0.25% Si, 0.62% Mn, 3.78% Ni, 0.15% Cr
0.28% C, 0.28% Si, 0.49% Mn, 0.011% P, 0.030% S, 2.30% Cr, 0.16% Ni, 0.13% V, 0.28% Cu, 0.19% Mo
0.28% C, 0.28% Si, 0.49% Mn, 0.011% P, 0.030% S, 2.30% Cr, 0.16% Ni, 0.13% V, 0.28% Cu, 0.19% Mo
0.28% C, 0.28% Si, 0.49% Mn, 0.011% P, 0.030% S, 2.30% Cr, 0.16% Ni, 0.13% V, 0.28% Cu, 0.19% Mo
0.28% C, 0.28% Si, 0.68% Mn, 0.026% S, 0.019% P, 0.17% Ni, 3.32% Cr, 0.55% Mo
0.28% C, 0.30% Si, 0.70% Mn, 2.80% Cr, 0.60% Mo, 1.00% Ni, 0.40% V
0.28% C, 0.30% Si, 0.95% Mn, 0.030% P, 0.003% S, 14.20% Cr, 0.50% Ni, 1.10% Mo
0.28% C, 0.36% Mn, 0.11% Si, 0.004% S, 0.008% P, 2.57% Cr, 0.04% Ni, 0.03% Mo, 0.35% V, 8.88% W
0.28% C, 0.39% Mn, 0.16% Si, 0.006% S, 0.020% P, 2.35% Cr, 0.06% Ni, 0.06% Mo, 0.53% V, 4.10% W
0.28% C, 0.41% Si, 0.49% Mn, 0.011% P, 0.03% S, 0.04% Ni, 1.00% Cr, 0.41% Mo, 0.05% Cu
0.28% C, 0.41% Si, 0.69% Mn, 0.043% P, 0.028% S, 3.30% Ni, 0.12% Cr, 0.03% Mo
0.28% C, 0.41% Si, 0.69% Mn, 0.043% P, 0.028% S, 3.30% Ni, 0.12% Cr, 0.03% Mo
0.28% C, 0.47% Si, 0.70% Mn, 5.25% Cr, 0.62% Mo, 0.05% Al
0.28% C, 0.49% Mn, 0.32% Si, 0.050% S, 0.012% P 0.13% Ni, 1.65% Cr, 0.22% Mo, 1.05% Al
0.28% C, 0.50% Mn, 0.25% Si, 0.016% P, 0.025% S, 5.00% Cr, 0.55% Mo
0.28% C, 0.50% Mn, 0.25% Si, 0.020% P, 0.020% S, 3.10% Cr, 0.52% Mo
0.28% C, 0.54% Mn, 0.96% Si, 0.003% S, 0.025% P 0.54% Ni, 2.80% Cr, 0.13% Mo, 0.24% V, 8.77% W, 2.05% Co
0.28% C, 0.58% Si, 1.45% Mn, 0.015% P, 0.027% S, 0.15% Cr, 0.19% Ni, 0.09% V, 0.21% Cu, 0.07% Mo
0.28% C, 0.59% Mn, 1.25% Si, 0.048% S, 0.055% P <0.05% Ni, 0.92% Cr, 0.22% Mo, 0.03% Cu
0.28% C, 0.62% Si, 1.48% Mn, 0.010% P, 0.036% S, 0.20% Cr, 0.03% Ni, 0.09% V, 0.04% Cu, 0.071% Mo, 0.03% Ti, 0.005% Sn
0.28% C, 0.69% Mn, 0.043% P, 0.028% S, 0.41% Si, 3.30% Ni, 0.12% Cr, 0.03% Mo
0.28% C, 0.70% Mn, 0.29% Si, 0.014% S, 0.011% P 0.43% Ni, 0.70% Cr, 0.20% Mo, 0.20% Cu
0.28% C, 0.70% Mn, 0.29% Si, 0.014% S, 0.011% P 0.43% Ni, 0.70% Cr, 0.20% Mo, 0.20% Cu
0.28% C, 0.77% Si, 0.36% Mn, 0.008% P, 0.004% S, 2.57% Cr, 0.03% Mo, 0.04% Ni, 0.35% V, 8.88% W
0.28% C, 0.77% Si, 0.36% Mn, 0.008% P, 0.004% S, 2.57% Cr, 0.03% Mo, 0.04% Ni, 0.35% V, 8.88% W
0.28% C, 0.92% Mn, 1.049% Si, 0.018% S, 0.001% P 0.12% Ni, 0.99% Cr, 0.10% Cu
0.28% C, 1.00% Mn, 4.20% Cr, 0.34% V, 1.10% Mo, 0.067% Al, 0.0161% N, 0.031% P, 0.011% S
0.28% C, 1.20% Mn, 0.20% Si, 0.020% P, 0.020% S
0.28% C, 1.41% Mn, 0.29% Si, 0.008% P, 0.004% S, 0.26% Cr, 0.11% Ni, 0.22% Mo, 0.20% Cu, 0.027% Nb, 0.028% Ti, 0.019% V, 0.003% B and 0.025% Al
0.28% C, 1.41% Mn, 0.29% Si, 0.008% P, 0.004% S, 0.26% Cr, 0.11% Ni, 0.22% Mo, 0.20% Cu, 0.027% Nb, 0.028% Ti, 0.019% V, 0.003% B and 0.025% Al
0.28% C, 1.50% Mn, 0.20% Si, 0.020% P, 0.020% S
0.28% C, 3.25% Cr, 0.25% V, 9.00% W
0.28% C, 3.25% Cr, 0.25% V, 9.00% W
0.28-0.33% C, 0.70-0.90% Mn, max. 0.035% P, max. 0.04% S, 0.15-0.30% Si, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.28-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.020% S, 0.60-0.90% Cr, 0.40-0.60% Mo, 2.70-3.20% Ni
0.28-0.34% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.020% S, 0.60-0.90% Cr, 0.40-0.60% Mo, 2.70-3.20% Ni
0.28-0.34% C, max. 0.15% Si, 0.30-0.80% Mn, max. 0.010% P, max. 0.007% S, 1.10-1.40% Cr, 1.00-1.20% Mo, 0.50-0.75% Ni, 0.25-0.35% V, max. 0.010% Al
0.28-0.34% C, max. 0.30% Si, 0.30-0.80% Mn, max. 0.015% P, max. 0.018% S, 1.10-1.40% Cr, 1.00-1.20% Mo, 0.50-0.75% Ni, 0.25-0.35% V
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, max. 0.030% P, max. 0.020% S, 2.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.10-0.40% Si, 0.15-0.45% Mn, max. 0.030% P, max. 0.020% S, 2.70-3.20% Cr, 2.50-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.15-0.40% Si, 0.75-1.00% Mn, <0.025% P, <0.002% S, 0.90-1.20% Cr, 0.45-0.65% Mo, >0.004% V
0.28-0.35% C, 0.15-0.40% Si, 0.95-1.30% Mn, <0.030% P, 0.010-0.040% S, 0.60-0.90% Cr, 0.15-0.25% Mo, >0.02% V
0.28-0.35% C, 0.15-0.45% Mn, 0.10-0.40% Si, 2.70-3.20% Cr, 2.60-3.00% Mo, 0.40-0.70% V
0.28-0.35% C, 0.25-0.40% Si, 0.40-0.60% Mn, max. 0.030% P, max. 0.030% S, 0.40-0.70% Cr, 0.07-0.12% V
0.28-0.35% C, 0.25-0.40% Si, 0.40-0.60% Mn, max. 0.030% P, max. 0.030% S, 0.40-0.70% Cr, 0.070-0.12% V
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo, 0.60% Ni
0.28-0.35% C, 0.40% Si, 0.40-0.70% Mn, 0.035% P, 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo, 0.60% Ni
0.28-0.35% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.80-3.40% Cr, 0.30-0.50% Mo
0.28-0.35% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 2.80-3.40% Cr, 0.30-0.50% Mo
0.28-0.35% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.035% P, max. 0.035% S, 2.80-3.30% Cr, 0.30-0.50% Mo, max. 0.60% Ni
0.28-0.36% C, max. 0.50% Si, 1.40-1.80% Mn, max. 0.025% P, max. 0.040% S, 0.80-1.20% Cr, 0.25-0.40% Mo
0.28% C, 0.30% Si, 0.95% Mn, 0.030% P, 0.003% S, 14.20% Cr, ~0.50% Ni, 1.10% Mo
0.28-0.33% C, 0.70-0.90% Mn, max. 0.035% P, max. 0.04% S, 0.15-0.30% Si, 0.40-0.60% Cr, 0.40-0.70% Ni, 0.15-0.25% Mo
0.28-0.33% C, 0.40-0.60% Mn, 0.15-0.30% Si, max. 0.035% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.28% C, 0.36% Si, 0.44% Mn, 0.016% P, 0.008% S, 1.96% Cr, 0.11% Ni, 0.27% Mo, 0.01% V
0.28% C, 0.03% Si, 0.73% Mn, 0.007% P, 0.011% S
0.28% C, 0.03% Si, 2.11% Mn, 0.007% P, 0.011% S
0.28% C, 0.47% Si, 0.67% Mn, 0.017% P, 0.028% S, 0.17% Cu, 0.22% Cr, 0.06% Ni, 0.05% Mo, 0.07% Al, 0.01% V
0.285% C, 0.62% Mn, 0.30% Si, 2.55% Ni, 0.71% Cr
0.29% C, 0.056% Si, 0.21% Mn, 0.026% P, 0.017% S, 3.25% Ni, 1.45% Cr
0.29% C, 0.15% Mn, 0.13% Si, 0.010% P, 0.011% S 7.61% Ni
0.29% C, 0.20% Si, 0.70% Mn, 1.30% Cr, 0.70% Ni, 0.95% Mo, 0.30% V
0.29% C, 0.20% Si, 0.70% Mn, 1.30% Cr, 0.70% Ni, 0.95% Mo, 0.30% V
0.29% C, 0.21% Mn, 0.026% P, 0.017% S, 0.06% Si, 3.25% Ni, 1.45% Cr
0.29% C, 0.21% Mn, 0.06% Si, 0.026% P, 0.017% S 3.25% Ni, 1.45% Cr
0.29% C, 0.24% Si, 1.64% Mn, 0.02% Ni, 0.05% Cr, 0.45% Mo
0.29% C, 0.26% Si, 1.67% Mn, 0.030% S, 0.033% P, 0.21% Ni, 0.12% Cr, 0.04% Mo
0.29% C, 0.26% Si, 1.67% Mn, 0.033% P, 0.030% S, 0.21% Ni, 0.12% Cr, 0.04% Mo, 0.11% Cu
0.29% C, 0.29% Si, 0.47% Mn, 0.010% P, 0.028% S, 0.57% Cr, 0.28% Mo, 1.79% Ni, 0.11% Cu
0.29% C, 0.32% Si, 0.63% Mn, 0.013% P, 0.011% S, 0.84% Cr, 1.65% Ni, 0.03% V, 0.23% Cu, 0.31% Mo
0.29% C, 0.32% Si, 0.63% Mn, 0.013% P, 0.011% S, 0.84% Cr, 1.65% Ni, 0.03% V, 0.23% Cu, 0.31% Mo
0.29% C, 0.34% Si, 0.50% Mn, 0.008% P, 0.036% S, 0.03% Ni, 2.40% Cr, 0.34% Mo, 0.05% Cu
0.29% C, 0.35% Si, 1.49% Mn, 0.013% P, 0.012% S, 0.64% Cr, 0.43% Ni, 0.18% Cu, 0.47% Mo
0.29% C, 0.35% Si, 1.49% Mn, 0.013% P, 0.012% S, 0.64% Cr, 0.43% Ni, 0.18% Cu, 0.47% Mo
0.29% C, 0.36% Si, 0.70% Mn, 0.014% P, 0.015% S, 0.99% Cr, 0.19% Ni, 0.22% Cu, 0.21% Mo, 0.010% Sn, 0.057% Al
0.29% C, 0.40% Mn, 0.85% Si, 0.050% S, 0.023% P 0.18% Ni, 12.32% Cr, <0.10% Mo, 0.12% Cu, <0.05% V
0.29% C, 0.40% Si, 0.49% Mn, 0.011% P, 0.03% S, 0.04% Ni, 1.49% Cr, 0.41% Mo, 0.05% Cu
0.29% C, 0.40% Si, 1.53% Mn, 0.019% P, 0.010% S, 0.03% Cr
0.29% C, 0.52% Mn, 0.32% Si, 1.34% Ni, 0.77% Cr 0.25% Mo, 0.19% V
0.29% C, 0.77% Mn, 0.034% P, 0.031% S, 0.23% Si, 2.72% Ni, 0.04% Cr, 0.05% Mo, 0.29% C, 0.77% Mn, 0.23% Si, 0.034% P, 0.031% S 2.72% Ni, 0.04% Cr, 0.05% Mo
0.29% C, 0.78% Mn, 0.24% Si, 0.009% S, 0.011% P 1.62% Ni, 1.49% Cr, 0.44% Mo, 0.16% Cu, 0.010% Ti
0.29% C, 0.78% Mn, 0.24% Si, 0.009% S, 0.011% P 1.62% Ni, 1.49% Cr, 0.44% Mo, 0.16% Cu, 0.010% Ti
0.29% C, 0.85% Si, 0.40% Mn, 0.005% S, 0.023% P, 0.18% Ni, 12.30% Cr
0.29% C, 1.03% Si, 0.70% Mn, 0.012% P, 0.010% S, 3.09% Cr, 1.05% Ni, 0.10% V, 1.07% W, 0.14% Cu, 0.43% Mo
0.29% C, 1.11% Si, 1.70% Mn, 0.017% P, 0.014% S, 0.10% Ni, 0.01% Cr, 0.13% Mo
0.29% C, 1.28% Mn, 0.34% Si, 0.028% S, 0.017% P, 0.13% Cr, 0.08% Ni, 0.01% Mo, 0.09% V, 0.019% Ti, 0.134% Cu, 0.015% Sn, 0.036% Al, 106 ppm N2, 45 ppm O2, 10 ppm N free
0.29% C, 1.33% Mn, 1.30% Si, 0.016% S, 0.008% P 0.12% Ni, 0.10% Cu
0.29% C, 1.34% Mn, 0.41% Si, 0.026% S, 0.021% P, 0.09% Cr, 0.10% Ni, 0.02% Mo, 0.10% V, 0.003% Ti, 0.244% Cu, 0.020% Sn, 0.029% Al, 167 ppm N2, 30 ppm 02, 18 ppm N free
0.29% C, 1.67% Mn, 0.26% Si, 0.21% Ni, 0.12% Cr 0.04% Mo
0.29-0.36% C, max. 0.30% Si, 0.70-1.20% Mn, 1.10-1.60% Cr, 0.50-1.00% Ni, 0.90-1.40% Mo, 0.20-0.40% V, 0.10-0.30% Al
0.3% C, 1.43% Si, 1.40% Mn, 26.6% Cr, 30.8% Ni, 0.05% Cu, 0.17% Co, 0.03% Al, 0.68% Nb, 0.05% Ti, 0.049% V, 0.005% Pb, 0.25% W, 38/2% Fe
0.30-0.40% C, <0.40% Si, 1.40-1.60% Mn, <0.020% P, <0.002% S, 1.00-1.40% Cr, 0.30-0.60% Mo, 0.30-0.60% Ni, <0.30% V
0.30% C, 0.20% Si, 0.70% Mn, 1.30% Cr, 0.70% Ni, 1.05% Mo, 0.30% V
0.30% C, 0.20% Si, 0.70% Mn, 1.30% Cr, 0.70% Ni, 1.05% Mo, 0.30% V
0.30% C, 0.22% Si, 0.54% Mn, 0.030% S, 0.010% P, 1.84% Ni, 1.89% Cr, 0.00% Mo, 0.31% Cu
0.30% C, 0.22% Si, 0.64% Mn, 0.011% P, 0.012% S, 1.01% Cr, 0.19% Cu, 0.24% Mo, 0.11% Ni, <0.00% V
0.30% C, 0.22% Si, 0.64% Mn, 0.011% P, 0.012% S, 1.01% Cr, 0.19% Cu, 0.24% Mo, 0.11% Ni, <0.00% V
0.30% C, 0.22% Si, 0.69% Mn, 0.029% P, 0.051% S, 2.83% Ni, 0.85% Cr, 0.30% Mo, 0.12% Cu, 0.005% Al, 0.005% N, 0.0004% B, less than 0.01% V
0.30% C, 0.24% Si, 0.46% Mn, 0.030% P, 0.025% S, 1.44% Cr, 0.20% Cu, 0.37% Mo, 2.06% Ni, <0.01% V
0.30% C, 0.24% Si, 0.46% Mn, 0.030% P, 0.025% S, 1.44% Cr, 0.20% Cu, 0.37% Mo, 2.06% Ni, <0.01% V
0.30% C, 0.24% Si, 0.78% Mn, 0.025% S, 0.015% P, 1.00% Ni, 1.45% Cr, 0.40% Mo, 0.07% Cu, 0.04% Al
0.30% C, 0.25% Si, 0.20% Mn, 0.003% P, 0.002% S, 1.50% Cr, 3.00% Ni, 0.80% Mo, 0.30% V
0.30% C, 0.25% Si, 0.45% Mn, 2.00% Cr, 1.00% Ni, 0.40% Mo
0.30% C, 0.25% Si, 0.45% Mn, 2.00% Cr, 1.00% Ni, 0.40% Mo
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.50% Mn, 1.95% Cr, 1.95% Ni, 0.45% Mo
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.15% V, 0.20% Mo
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.15% V, 0.20% Mo
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.15% V, 0.20% Mo
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.20% Mo, 0.15% V
0.30% C, 0.25% Si, 0.55% Mn, 2.50% Cr, 0.20% Mo, 0.15% V
0.30% C, 0.25% Si, 0.60% Mn, 0.010% P, 0.005% S, 1.10% Cr, 0.25% Mo
0.30% C, 0.25% Si, 0.65% Mn, <0.03% S
0.30% C, 0.25% Si, 0.65% Mn, <0.03% S
0.30% C, 0.25% Si, 0.90% Mn, 0.012% P, 0.005% S, 0.90% Cr, 1.80% Ni, 0.43% Mo, 0.08% V, max. 20 ppm O2
0.30% C, 0.25% Si, 1.35% Mn
0.30% C, 0.25% Si, 1.35% Mn
0.30% C, 0.25% Si, 1.35% Mn
0.30% C, 0.25% Si, 1.35% Mn
0.30% C, 0.25% Si, 1.40% Mn
0.30% C, 0.26% Si, 0.44% Mn, 3.41% Ni, 1.00% Cr, 0.30% Mo, 0.0012% B
0.30% C, 0.26% Si, 0.44% Mn, 3.41% Ni, 1.00% Cr, 0.30% Mo, 0.0012% B
0.30% C, 0.26% Si, 1.26% Mn, 0.020% P, 0.004% S, 0.036% Al, 0.20% Cr, 0.0038% B
0.30% C, 0.27% Mn, 0.019% P, 0.019% S, 3.50% Ni, 1.25% Cr
0.30% C, 0.27% Si, 0.93% Mn, 0.017% P, 0.010% S, 1.09% Cr, 1.04% Mo, 0.54% Ni, 0.36% V
0.30% C, 0.29% Si, 0.54% Mn, 0.015% P, 0.008% S, 0.80% Cr, 3.47% Ni
0.30% C, 0.29% Si, 1.24% Mn, 0.012% P, 0.010% S, 0.41% Cr, 0.07% Mo, 0.21% Ni, 0.0030% B
0.30% C, 0.30% Mn, 3.64% Ni, 1.63% Cr, 0.49% Mo, 0.08% V
0.30% C, 0.30% Mn, 3.64% Ni, 1.63% Cr, 0.49% Mo, 0.08% V
0.30% C, 0.30% Mn, 3.64% Ni, 1.63% Cr, 0.49% Mo
0.30% C, 0.30% Mn, 3.64% Ni, 1.63% Cr, 0.49% Mo
0.30% C, 0.30% Si, 0.30% Mn, 0.025% P, 0.003% S, 3.00% Cr, 2.80% Mo, 0.60% V
0.30% C, 0.30% Si, 0.30% Mn, 2.35% Cr, 0.60% V, 4.50% W
0.30% C, 0.30% Si, 0.30% Mn, 2.50% Cr, 2.60% Mo, 1.59% Ni, 0.18% V, 0.025% P, 0.020% S, 0.005% Al, 0.20% Cu
0.30% C, 0.30% Si, 0.30% Mn, 2.50% Cr, 2.60% Mo, 1.59% Ni, 0.18% V, 0.025% P, 0.020% S, 0.005% Al, 0.20% Cu
0.30% C, 0.30% Si, 0.30% Mn, 2.70% Cr, 0.35% V, 9.00% W
0.30% C, 0.30% Si, 0.30% Mn, 2.70% Cr, 0.35% W, 9.00% W
0.30% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 2.80% Mo, 0.60% V.
0.30% C, 0.30% Si, 0.40% Mn, 0.016% S, 0.015% P, 3.20% Ni, 0.86% Cr, 0.40% Mo
0.30% C, 0.30% Si, 0.40% Mn, 0.016% S, 0.015% P, 3.20% Ni, 0.86% Cr, 0.40% Mo
0.30% C, 0.30% Si, 0.50% Mn, 2.0% Cr, 0.40% Mo, 2.0% Ni
0.30% C, 0.30% Si, 0.50% Mn, 2.0% Cr, 0.40% Mo, 2.0% Ni
0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.20% Mo, 0.55% Ni. 0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.30% C, 0.30% Si, 0.80% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.30% C, 0.30% Si, 1.20% Mn, 2.30% Cr, 0.80% Mo, 0.80% V, 4.00% Ni
0.30% C, 0.35% Si, 0.79% Mn, 0.024% P, 0.025% S, 0.53% Cr, 0.21% Mo, 0.48% Ni, 0.10% Cu
0.30% C, 0.36% Si, 0.60% Mn, 0.008% P, 0.027% S, 0.03% Ni, 2.04% Cr, 0.33% Mo, 0.04% Cu
0.30% C, 0.38% Si, 0.51% Mn, 0.011% P, 0.032% S, 0.07% Cr, 3.03% Ni, <0.01% V
0.30% C, 0.40% Mn, 0.30% Si, 0.016% S, 0.015% P 3.20% Ni, 0.86% Cr, 0.40% Mo, 0.17% Cu
0.30% C, 0.40% Mn, 0.30% Si, 0.016% S, 0.015% P 3.20% Ni, 0.86% Cr, 0.40% Mo, 0.17% Cu
0.30% C, 0.40% Mn, 0.30% Si, 2.20% Ni, 0.86% Cr 0.40% Mo
0.30% C, 0.40% Si, 0.38% Mn, 0.025% P, 0.009% S, 12.96% Cr, 0.20% Ni, 0.17% Cu, 0.09% Mo, 0.025% Al, 0.012% Sn
0.30% C, 0.41% Mn, 0.28% Si, <0.002% P, 0.014% S, 3.64% Ni, <0.05% Cr, 0.47% Mo, 0.058% Al
0.30% C, 0.41% Si, 0.49% Mn, 0.011% P, 0.03% S, 0.04% Ni, 0.51% Cr, 0.41% Mo, 0.05% Cu
0.30% C, 0.45% Si, 0.40% Mn, 0.018% P, 0.013% S, 13.53% Cr, 0.03% Mo, 0.11% Ni, 0.040% V
0.30% C, 0.45% Si, 0.80% Mn, 0.043% P, 0.033% S, 0.92% Cr
0.30% C, 0.46% Mn, 0.241% Si, 2.06% Ni, 1.44% Cr, 0.37% Mo, 0.03% P, 0.20% Cu, 0.025%S, 0.01% V
0.30% C, 0.46% Si, 0.75% Mn, 0.026% P, 0.040% S
0.30% C, 0.46% Si, 0.75% Mn, 0.026% P, 0.040% S
0.30% C, 0.46% Si, 0.75% Mn, 0.040% S, 0.026% P
0.30% C, 0.47% Si, 0.78% Mn, 0.041% P, 0.031% S, 3.65% Ni
0.30% C, 0.48% Mn, 0.25% Si, 0.020% P, 0.020% S, 2.00% Cr, 2.00% Ni, 0.40% Mo
0.30% C, 0.48% Mn, 2.20% Si, 0.012% S, <0.005% P 0.12% Ni, 10.50% Cr, 1.00% Mo, 0.07% Cu, 0.012% V
0.30% C, 0.49% Si, 1.63% Mn, 0.44% Cr, 0.33% Mo
0.30% C, 0.50% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.25% Cr, 4.10% Ni
0.30% C, 0.50% Mn, 0.25% Si, 0.016% S, 0.012% P 0.09% Ni, 1.28% Cr, 0.09% Cu, 0.05% V
0.30% C, 0.50% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.00% Cr, 0.20% Mo
0.30% C, 0.50% Si, 0.75% Mn, 0.80% Cr, 0.25% Mo
0.30% C, 0.50% Si, 1.00% Mn, 16.00% Cr, 0.10% S
0.30% C, 0.51% Mn, 0.32% Si, 0.011% P, 0.007% S, 0.07% Cr, 3.03% Ni, 0.032% Al, <0.01% Ti
0.30% C, 0.51% Si, 15.55% Cr, 0.98% Mo, 0.14% Ni, 0.42% N
0.30% C, 0.51% Si, 15.55% Cr, 0.98% Mo, 0.14% Ni, 0.42% N
0.30% C, 0.51% Si, 15.55% Cr, 0.98% Mo, 0.14% Ni, 0.42% N
0.30% C, 0.51% Si, 15.55% Cr, 0.98% Mo, 0.14% Ni, 0.42% N
0.30% C, 0.52% Mn, 0.18% Si, <0.002% P, 0.021% S, 2.64% Ni, <0.05% Cr, 0.37% Mo, <0.015% Al
0.30% C, 0.55% Mn, 0.018% P, 0.022% S, 3.34% Ni
0.30% C, 0.56% Mn, 0.27% Si, 0.014% S, 0.012% P 1.75% Ni, 1.85% Cr, 0.49% Mo
0.30% C, 0.60% Mn, 0.25% Si, 0.010% P, 0.015% S, 2.50% Cr, 0.30% Ni, 0.20% Mo, 0.18% V
0.30% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.25% Cr, 4.10% Ni, 0.30% Mo
0.30% C, 0.63% Mn, 0.29% Si, 0.016% S, 0.010% P 0.17% Ni, 2.99% Cr, 0.43% Mo, 0.13% Cu
0.30% C, 0.63% Mn, 0.29% Si, 0.016% S, 0.010% P 0.17% Ni, 2.99% Cr, 0.43% Mo, 0.13% Cu
0.30% C, 0.64% Mn, 1.0% Cr and 0.24% Mo
0.30% C, 0.64% Mn, 1.0% Cr, 0.24% Mo
0.30% C, 0.64% Mn, 1.00% Cr, and 0.24% Mo
0.30% C, 0.69% Mn, 0.38% Si, 1.79% Ni, 0.78% Cr, 0.24% Mo
0.30% C, 0.69% Mn, 0.40% Si, 0.20% Ni, 0.99% Cr, 0.43% Mo
0.30% C, 0.69% Mn, 1.40% Si, 0.78% Cr, 1.71% Ni, 0.31% Mo, 0.04% V
0.30% C, 0.70% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.05% Cr
0.30% C, 0.75% Mn, 0.50% Si, 0.80% Cr, 0.25% Mo
0.30% C, 0.80% Mn, 0.010% P, 0.015% S, 0.29% Si, 0.54% Ni, 0.55% Cr, 0.21% Mo
0.30% C, 0.80% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.30% C, 0.80% Mn, 0.54% Ni, 0.55% Cr, 0.21% Mo
0.30% C, 0.80% Mn, 0.54% Ni, 0.55% Cr, 0.21% Mo
0.30% C, 1.15% Mn, <1.00% Ni, 2.00% Cr, 0.65% Mo, +B
0.30% C, 1.40% Mn, 1.43% Si, 30.80% Ni, 26.60% Cr, 0.05% Cu, 0.27% Co, 0.003% Al, 0.68% Nb, 0.054% Ti, 0.049% V, 0.005% Pb, 0.25% W, 38.20% Fe.
0.30% C, 1.5% Si, 2.00% Mn, 1.30% Cr, 0.25% Mo, 0.1% V. Steel Ni1: 0.30% C, 1.5% Si, 3.5% Ni, 1.44% Cr, 0.1% V. Steel Ni2: 0.30% C, 1.5% Si, 3.5% Ni, 1.44% Cr, 0.25% Mo
0.30% C, 1.51% Si, 0.75% Mn, 1.84% Ni, 0.84% Cr, 0.45% Mo, 0.010% Al
0.30% C, 1.51% Si, 0.75% Mn, 1.84% Ni, 0.84% Cr, 0.45% Mo, 0.010% Al
0.30% C, 1.54% Mn, 0.97% Ni, 2.05% Cr, 0.43% Mo
0.30% C, 1.55% Mn, 0.20% Si, 0.025% P, 0.025% S, 0.28% Mo
0.30% C, 1.80% Mn, 0.15% Si, 0.020% P, 0.020% S
0.30% C, 1.91% Mn, 0.34% Si, 0.009% S, 0.016% P, 0.67% Mo, 0.07% V
0.30% C, 2.02% Mn, 1.11% Ni, 0.66% Cr, 0.55% Mo
0.30% C, 2.60% Cr, 8.50% W, 0.40% V
0.30% C, 2.70% Cr, 0.40% V, 8.50% W
0.30% C, 2.70% Cr, 0.40% V, 8.50% W
0.30% C, 3.00% Cr, 9.00% W, 0.30% V
0.30% C
0.30% C
0.30-0.35% C, max. 0.35% Si, max. 0.60% Mn, max. 0.025% P, max. 0.010% S, 2.80-3.20% Cr, 0.80-1.20% Mo, 0.25-0.35% V
0.30-0.37% C, <0.40% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S, 0.80-1.20% Al, 1.00-1.30% Cr, 0.15-0.25% Mo
0.30-0.37% C, <0.40% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S, 0.80-1.20% Al, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% V
0.30-0.37% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo. 25CrMoS4: 0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr. 34CrS: 0.30-0.37% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, 0.15-0.40% Si, 0.60-0.90% Mn, max. 0.10% P, 0.070-0.110% S, 1.00-1.30% Cr, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% Ni, 0.80-1.20% Al
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.60-0.90% Cr
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 0.15-0.25% Cr, 0.80-1.20% Al
0.30-0.37% C, max. 0.40% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.035% S, 1.50-1.80% Cr, 0.15-0.25% Mo, 0.85-1.15% V, 0.80-1.20% Al
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.80-1.10% Cr, 1.20-1.60% Ni
0.30-0.37% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, 0.80-1.10% Cr, 1.20-1.60% Ni
0.30-0.38% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, 0.50-0.80% Mn, <0.40% Si, 1.30-1.70% Cr, 1.30-1.70% Ni, 0.15-0.30% Mo
0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.38% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 1.30-1.70% Cr, 0.15-0.30% Mo, 1.30-1.70% Ni
0.30-0.40% C, <0.40% Si, 1.40-1.60% Mn, <0.020% P, <0.002% S, 1.00-1.40% Cr, 0.30-0.60% Mo, 0.30-0.60% Ni, <0.030% V
0.30-0.40% C, 0.80-1.10% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.80-2.10% W, 0.15-0.20% V
0.30% C, 0.30% Mn, 3.64% Ni, l.63% Cr, 0.49% Mo
0.30% C, 0.95% Cr, 0.20% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30-0.35% C, max. 0.20% Si, max. 0.25% Mn, max. 0.001% S, max. 0.005% P, max. 0.30% Ni, 2.80-3.20% Cr, 0.70-1.20% Mo, 0.15-0.35% V
0.30% C, 0.30% Si, 1.20% Mn, 2.30% Cr, 0.80% Mo, 0.80% V, 4.00% Ni
0.30-0.37% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.30% C, 0.24% Si, 0.46% Mn, 0.030% P, 0.025% S, 1.44% Cr, 0.20% Cu, 0.37% Mo, 2.06% Ni, 0.01% V
0.30% C, 0.35% Si, 0.60% Mn, 0.008% P, 0.023% S, 2.08% Cr, 1.21% Ni, 0.67% Mo, 0.30% V
0.302% C, 0.47% Si, 0.77% Mn, 0.012% P, 0.031% S, 1.01% Cr
0.303% C, 0.48% Si, 0.80% Mn, 0.013% P, 0.032% S, 3.49% Ni
0.31% C, 0.02% Si, 0.58% Mn, 0.010% P, 0.003% S, 0.72% Cr, 0.48% Mo, 2.82% Ni, 0.19% Cu, 0.014% Al
0.31% C, 0.15% Si, 0.73% Mn, 0.016% S, 0.008% P, 2.50% Ni, 1.59% Cr, 0.35% Mo, 0.03% Cu, 0.03% Al
0.31% C, 0.17% Si, 0.78% Mn, 0.020% S, 0.020% P, 4.10% Ni, 1.45% Cr, 0.35% Mo, 0.13% Cu, 0.03% Al
0.31% C, 0.20% Si, 0.44% Mn, 0.036% P, 0.033% S, 3.40% Ni, 1.26% Cr, 0.47% Mo
0.31% C, 0.20% Si, 0.62% Mn, 0.018% P, 0.012% S, 2.63% Ni, 0.64% Cr, 0.58% Mo
0.31% C, 0.25% Si, 0.48% Mn, 0.008% P, 0.003% S, 0.82% Cr, 2.64% Ni, 0.21% Cu, 0.06% Mo, 0.078% Co
0.31% C, 0.25% Si, 0.48% Mn, 0.008% P, 0.003% S, 0.82% Cr, 2.64% Ni, 0.21% Cu, 0.06% Mo, 0.078% Co
0.31% C, 0.25% Si, 0.60% Mn, 2.55% Cr, 0.15% V, 0.20% Mo
0.31% C, 0.25% Si, 0.60% Mn, 2.55% Cr, 0.15% V, 0.20% Mo
0.31% C, 0.26% Si, 0.40% Mn, 0.025% P, 0.028% S, 1.95% Cr, 0.39% Mo, 1.90% Ni, 0.15% Cu
0.31% C, 0.26% Si, 0.46% Mn, 0.26% Ni, 2.08% Cr, 0.48% Mo
0.31% C, 0.27% Si, 0.64% Mn, 0.020% P, 0.022% S, 0.79% Cr, 2.89% Ni
0.31% C, 0.28% Si, 0.26% Mn, 0.011% P, 0.010% S, 2.83% Cr, 0.13% Ni, 0.40% V, 8.60% W, 0.22% Cu, 0.16% Mo
0.31% C, 0.28% Si, 0.50% Mn, 0.005% S, 0.010% P, 3.33% Ni, 1.20% Cr, 0.50% Mo
0.31% C, 0.28% Si, 0.66% Mn, 0.014% P, 0.016% S, 1.67% Ni, 0.72% Cr, 0.34% Mo
0.31% C, 0.30% Si, 0.62% Mn, 0.016% P, 0.009% S, 2.65% Cr, 0.19% Ni, 0.18% V, 0.25% Cu, 0.29% Mo, 0.023% Al
0.31% C, 0.30% Si, 0.62% Mn, 0.016% P, 0.009% S, 2.65% Cr, 0.19% Ni, 0.18% V, 0.25% Cu, 0.29% Mo, 0.023% Al
0.31% C, 0.32% Mn, 0.41% Si, 0.014% S, 0.013% P 0.31% Ni, 2.36% Cr, 0.22% Mo, 0.32% V, 8.59% W, 0.16% Cu, 0.013% Al
0.31% C, 0.32% Si, 0.58% Mn, 1.07% Cr, 0.21% Mo, 0.15% Ni, 0.025% V, 0.028% Nb
0.31% C, 0.47% Mn, 0.34% Si, 0.021% P, 0.019% S, 0.26% Ni, 0.92% Cr, 0.17% Mo
0.31% C, 0.50% Mn, 0.28% Si, 0.005% S, 0.010% P 3.33% Ni, 1.20% Cr, 0.50% Mo, 0.15% Cu, <0.03% V, 0.08% W
0.31% C, 0.55% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.05% Cr, 3.00% Ni, 0.28% Mo
0.31% C, 0.55% Mn, 0.30% Si, 0.020% P, 0.020% S, 1.60% Cr, 0.20% Mo, 1.10% Al
0.31% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.65% Cr, 2.55% Ni, 0.55% Mo
0.31% C, 0.62% Mn, 0.20% Si, 2.63% Ni, 0.64% Cr 0.58% Mo
0.31% C, 0.65% Mn, 0.30% Si, 0.030% S, 0.013% P, 0.12% Cr, 0.05% Ni, 0.50% Mo, 0.03% V, 0.08% Cu, 0.051% Al
0.31% C, 0.67% Mn, 0.30% Si, 0.010% S, 0.010% P 0.94% Ni, 3.00% Cr, 0.51% Mo, 0.19% Cu
0.31% C, 0.67% Mn, 0.30% Si, 0.010% S, 0.010% P 0.94% Ni, 3.00% Cr, 0.51% Mo, 0.19% Cu
0.31% C, 0.69% Mn, 0.38% Si, 0.20% Ni, 0.79% Cr, 0.57% Mo
0.31% C, 0.94% Mn, 0.26% Si, 0.009% P, 0.023% S, 0.59% Ni, 0.53% Cr, 0.21% Mo
0.31% C, 2.02% Mn, 1.11% Ni, 0.66% Cr, 0.55% Mo
0.31% C, 2.20% Mn, 1.80% Ni, 0.66% Cr, 0.55% Mo
0.31-0.38% C, 0.30-0.60% Mn, 0.15-0.40% Si, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.70-4.20% Ni
0.31% C, 1.22% Mn, 0.10% Ni, 0.25% Si, 0.03% Mo, 0.004% V, 0.01% S
0.31% C, 2.50% Cr, 0.20% Mo, 0.15% V
0.31% C, 2.50% Cr, 0.20% Mo, 0.15% V
0.31% C, 0.36% Si, 1.79% Mn, 0.036% P, 0.035% S, 0.13% Cu, 0.36% Cr, 0.08% Ni, 0.01% Mo, 0.027% Al
0.315% C, 0.14% Mn, 0.01% Si, 0.006% S, 0.01% P 9.12% Ni
0.32% C, 0.13% Mn, 0.15% Si, 0.090% P, 0.005% S, 9.05% Ni, 4.07% Co
0.32% C, 0.19% Si, 0.51% Mn, 0.009% S, 0.013% P, 3.02% Ni, 1.37% Cr, 0.48% Mo, 0.18% V
0.32% C, 0.19% Si, 0.51% Mn, 0.009% S, 0.013% P, 3.02% Ni, 1.37% Cr, 0.48% Mo, 0.18% V
0.32% C, 0.19% Si, 0.51% Mn, 0.013% P, 0.009% S, 3.02% Ni, 1.37% Cr, 0.48% Mo, 0.18% V
0.32% C, 0.20% Si, 0.30% Mn, 5.20% Cr, 1.20% Mo, 0.50% V, 3.80% W
0.32% C, 0.22% Si, 0.57% Mn, 0.016% P, 0.016% S, 3.38% Ni, 0.65% Cr, 0.26% Mo
0.32% C, 0.24% Si, 0.70% Mn, 0.016% P, 0.013% S, 0.91% Cr, 1.38% Ni
0.32% C, 0.25% Si, 0.40% Mn, 3.10% Cr, 0.30% V, 1.00% Mo
0.32% C, 0.25% Si, 0.50% Mn, 0.80% Cr, 2.80% Ni
0.32% C, 0.25% Si, 0.50% Mn, 0.80% Cr, 2.80% Ni
0.32% C, 0.25% Si, 0.55% Mn, 3.00% Cr, 0.40% Mo
0.32% C, 0.25% Si, 0.55% Mn, 3.00% Cr, 0.40% Mo
0.32% C, 0.25% Si, 0.55% Mn, 3.05% Cr, 0.40% Mo
0.32% C, 0.27% Si, 0.56% Mn, 0.012% S, 0.018% P, 2.37% Ni, 0.74% Cr, 0.51% Mo
0.32% C, 0.27% Si, 0.56% Mn, 0.012% S, 0.018% P, 2.37% Ni, 0.74% Cr, 0.51% Mo
0.32% C, 0.27% Si, 0.56% Mn, 0.018% P, 0.012% S, 2.37% Ni, 0.74% Cr, 0.51% Mo
0.32% C, 0.27% Si, 0.56% Mn, 0.021% S, 0.018% P, 2.37% Ni, 0.74% Cr, 0.51% Mo
0.32% C, 0.27% Si, 0.56% Mn, 0.021% S, 0.018% P, 2.37% Ni, 0.74% Cr, 0.51% Mo
0.32% C, 0.28% Si, 0.61% Mn, 0.013% S, 0.018% P, 3.22% Ni, 0.63% Cr, 0.22% Mo
0.32% C, 0.28% Si, 0.61% Mn, 0.018% P, 0.013% S, 3.22% Ni, 0.63% Cr, 0.22% Mo, 0.025% V, 0.16% W, 0.12% Cu
0.32% C, 0.29% Si, 0.47% Mn, 0.022% P, 0.020% S, 4.13% Ni, 1.21% Cr, 0.30% Mo, 0.15% Cu, 0.013% V, 0.11% W
0.32% C, 0.30% Mn, 0.20% Si, 0.008% S, 0.017% P 2.95% Ni, 0.69% Cr, <0.10% Mo, 0.31% Cu, <0.030% V
0.32% C, 0.30% Mn, 0.20% Si, 0.008% S, 0.017% P 2.95% Ni, 0.69% Cr, <0.10% Mo, 0.31% Cu, <0.030% V
0.32% C, 0.30% Mn, 0.20% Si, 0.017% P, 0.008% S, 2.95% Ni, 0.69% Cr, 0.10% Mo, 0.31% Cu, 0.056% As
0.32% C, 0.30% Mn, 0.25% Si, 3.00% S, 2.80% Mo 0.50% V
0.32% C, 0.30% Mn, 0.25% Si, 3.00% S, 2.80% Mo 0.50% V
0.32% C, 0.30% Mn, 0.30% Si, 0.020% P, 0.010% S, 13.00% Cr, 0.20% Ni, 0.06% Mo
0.32% C, 0.30% Si, 0.76% Mn, 0.010% S, 0.021% P, 0.26% Ni, 1.08% Cr
0.32% C, 0.30% Si, 0.76% Mn, 0.010% S, 0.021% P, 0.26% Ni, 1.08% Cr
0.32% C, 0.34% Si, 0.37% Mn, 0.016% P, 0.013% S, 2.90% Cr, 2.85% Mo, 0.51% V
0.32% C, 0.34% Si, 0.37% Mn, 0.016% P, 0.013% S, 2.90% Cr, 2.85% Mo, 0.51% V
0.32% C, 0.35% Mn, 0.27% Si, 0.022% S, 0.018% P 2.10% Ni, 2.30% Cr, 0.64% Mo, 0.19% Cu
0.32% C, 0.35% Mn, 0.95% Si, 4.86% Cr, 1.45% Mo, 1.29% W
0.32% C, 0.36% Si, 0.54% Mn, 0.034% P, 0.021% S, 0.07% Ni, 0.75% Cr, 0.27% Mo
0.32% C, 0.36% Si, 0.54% Mn, 0.034% P, 0.021% S, 0.07% Ni, 0.75% Cr, 0.27% Mo
0.32% C, 0.40% Mn, 0.21% Si, 0.016% S, 0.007% P 0.11% Ni, 1.30% Cr, 0.10% Mo, 0.13% Cu
0.32% C, 0.40% Mn, 0.40% Si, 1.43% S, 3.30% Ni, 0.33% Mo, 0.19% V
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.50% V
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V, 3.00% W
0.32% C, 0.40% Si, 0.40% Mn, 3.00% Cr, 2.80% Mo, 0.60% V
0.32% C, 0.47% Mn, 0.29% Si, 4.13% Ni, 1.21% Cr 0.30% Mo
0.32% C, 0.51% Mn, 0.013% P, 0.009% S, 0.19% Si, 3.02% Ni, 1.37% Cr, 0.48% Mo, 0.18% V
0.32% C, 0.51% Mn, 0.19% Si, 0.013% P, 0.009% S 3.02% Ni, 1.37% Cr, 0.48% Mo, 0.18% V
0.32% C, 0.51% Mn, 1.37% Cr, 3.02% Ni, 0.48% Mo, 0.18% V
0.32% C, 0.55% Mn, 0.25% Si, 0.020% P, 0.020% S, 3.05% Cr, 0.40% Mo, 0.30% Ni
0.32% C, 0.55% Mn, 0.27% Si, 1.80% Cr, 1.90% Ni 0.58% Mo
0.32% C, 0.57% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.15% Cr, 3.00% Ni
0.32% C, 0.58% Mn, 0.30% Si, 0.032% P, 0.020% S, 2.35% Ni, 0.75% Cr, 0.52% Mo, 0.11% V
0.32% C, 0.60% Si, 1.49% Mn, 0.19% Cr, 0.04% Mo, 0.11% Ni, 0.080% V, 0.22% Cu, 0.026% Al, 0.0160% N
0.32% C, 0.60-1.00% Si, 0.80% Mn, max. 0.0010% P, max. 0.003% S, 1.35% Cr, 0.80% Mo, 0.14% V, max. 1.00% Ni
0.32% C, 0.61% Mn, 0.28% Si, 0.018% P, 0.013% S, 3.22% Ni, 0.63% Cr, 0.22% Mo
0.32% C, 0.61% Mn, 0.28% Si, 3.22% Ni, 0.63% Cr 0.22% Mo
0.32% C, 0.64% Mn, less then 0.10% Ni, 1.14% Cu
0.32% C, 0.71% Si, 0.38% Mn, 0.015% P, 0.001% S, 14.66% Cr, 0.97% Mo, 0.40% N
0.32% C, 0.72% Mn, 0.012% P, 0.021% S, 0.19% Si, 1.70% Ni, 0.82% Cr, 0.31% Mo, 0.12% Cu, 0.17% V
0.32% C, 0.72% Mn, 0.19% Si, 0.012% P, 0.021% S 1.70% Ni, 0.82% Cr, 0.31% Mo, 0.12% Cu, 0.17% V
0.32% C, 0.72% Mn, 0.82% Cr, 1.70% Ni, 0.31% Mo, 0.17% V
0.32% C, 0.74% Mn, 0.015% P, 0.014% S, 0.31% Si, 1.70% Ni, 0.12% Cu, 0.23% Mo
0.32% C, 0.74% Mn, 0.25% Si, 0.037% P, 0.036% S, 0.34% Ni, 1.04% Cr, 1.20% Mo, 0.24% V
0.32% C, 0.74% Mn, 0.31% Si, 0.015% P, 0.014% S 1.70% Ni, 0.12% Cr, 0.23% Mo
0.32% C, 0.76% Mn, 0.014% P, 0.018% S 0.70% Ni, 1.06% Cr, 1.01% Mo
0.32% C, 0.76% Mn, 0.014% P, 0.018% S, 0.70% Ni, 1.06% Cr, 1.01% Mo
0.32% C, 0.76% Mn, 0.30% Si, 0.010% S, 0.021% P 0.26% Ni, 1.08% Cr, 0.02% Mo, 0.17% Cu
0.32% C, 0.76% Mn, 0.30% Si, 0.010% S, 0.021% P 0.26% Ni, 1.08% Cr, 0.02% Mo, 0.17% Cu
0.32% C, 0.80% Mn, 0.30% Si, 0.025% P, 0.020% S, 0.26% Mo
0.32% C, 0.86% Mn, 1.44% Si, 0.51% Ni, 1.01% Cr, 0.49% Mo, 0.071% V
0.32% C, 0.86% Mn, 1.54% Si, 0.014% S, 0.024% P, 1.01% Cr, 0.51% Ni, 0.49% Mo, 0.07% V, 0.037% Al, 0.022% N
0.32% C, 0.95% Si, 0.35% Mn, 4.86% Cr, 1.45% Mo, 1.29% W
0.32% C, 1.39% Mn, 0.33% Si, 0.021% S, 0.015% P, 0.13% Cr, 0.14% Ni, 0.03% Mo, 0.129% V, 0.039% Ti, 0.129% Cu, 0.017% Sn, 0.049% Al, 148 ppm N2, 57 ppm O2, 14 ppm N free
0.32% C, 1.50% Mn, 0.18% Si, 0.020% P, 0.020% S, 0.27% Mo
0.32% C, 3.0% Cr, 2.8% Mo, 0.5% V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50 V
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V, 3.00% Co
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.32-0.38% C, 0.15-0.30% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 1.20-1.50% Cr, 0.20-0.40% Mo, 3.80-4.30% Ni
0.32-0.39% C, <0.40% Si, 0.30-0.60% Mn, <0.030% P, <0.025% S, 1.60-2.00% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, <0.40% Si, 0.50-0.80% Mn, <0.045% S, <0.045% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mo+Ni<=063
0.32-0.39% C, <0.40% Si, 0.50-0.80% Mn, <0.045% S, <0.045% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mo+Ni<=063
0.32-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.32-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.020-0.035% S, 0.25% Cu
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.020-0.035% S, 0.25% Cu
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.025% Cu
0.32-0.39% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.025% Cu
0.32-0.39% C, 0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.025% S, 1.60-2.50% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, 0.40% Si, 0.30-0.60% Mn, 0.030% P, 0.025% S, 1.60-2.50% Cr, 0.25-0.45% Mo, 3.60-4.10% Ni
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.32-0.39% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.32-0.39% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.39% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.32-0.40% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, 0.50-0.80% Mn, <0.40% Si, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.15-0.30% Ni
0.32-0.40% C, 0.90-1.20% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 5.00-5.60% Cr, 1.30-1.60% Mo, 1.20-1.40% W, 0.15-0.40% V
0.32-0.40% C, 0.90-1.20% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 5.00-5.60% Cr, 1.30-1.60% Mo, 1.20-1.40% W, 0.15-0.40% V
0.32-0.40% C, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.90-1.20% Ni
0.32-0.40% C, max. 0.40% Si, 1.20-1.50% Mn, max. 0.035% P, max. 0.035% S
0.32-0.42% C, 0.80-0.12% Si, <0.50% Mn, 0.00% Ni, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
0.32-0.42% C, 0.80-1.20% Si, 0.50% Mn, 4.50-5.50% Cr, 1.00-1.50% Mo, 0.80-1.20% V
0.32% C, 2.05% Cr, 2.02% Mo, 1.54% Ni, 0.32% Si, 0.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32-0.45% C, 0.80-1.20% Si, 4.75-5.50% Cr, 1.10-1.75% Mo, 0.80-1.20% V
0.32% C, 0.25% Si, 0.30% Mn, 2.95% Cr, 2.80% Mo, 0.55% V
0.32% C, 0.23% Si, 0.64% Mn, 0.015% P, 0.019% S, 3.23% Cr, 0.36% Mo, 0.02% Ni
0.32% C, 3.00% Cr, 2.80% Mo, 0.50% V
0.325% C, 0.13% Mn, 0.15% Si, 0.005% S, 0.09% P 9.05% Ni, 4.07% Co
0.325% C, 0.54% Mn, 0.22% Si, 1.103% Cr, 0.63% Mo, 0.17% V
0.33% C, 0.06% Si, 0.23% Mn, 0.013% P, 0.021% S, 3.78% Ni, 1.79% Cr
0.33% C, 0.17% Si, 0.51% Mn, 0.009% S, 0.013% P, 4.16% Ni, 1.44% Cr, 0.31% Mo
0.33% C, 0.17% Si, 0.51% Mn, 0.009% S, 0.013% P, 4.16% Ni, 1.44% Cr, 0.031% Mo
0.33% C, 0.18% Si, 1.48% Mn, 0.028% P, 0.028% S, 0.26% Ni, 0.16% Cr, 0.27% Mo, 0.14% Cu
0.33% C, 0.20% Si, 0.30% Mn, 13.70% Cr
0.33% C, 0.20% Si, 0.30% Mn, 13.70% Cr
0.33% C, 0.20% Si, 0.47% Mn, 0.009% P, 0.008% S, 1.60% Cr, 0.93% Ni, 0.23% Cu, 0.17% Mo, 1.01% Al
0.33% C, 0.20% Si, 0.47% Mn, 0.009% P, 0.008% S, 1.60% Cr, 0.93% Ni, 0.23% Cu, 0.17% Mo, 1.01% Al
0.33% C, 0.20% Si, 0.47% Mn, 0.009% P, 0.008% S, 1.60% Cr, 0.93% Ni, 0.23% Cu, 0.17% Mo, 1.01% Al
0.33% C, 0.21% Si, 0.62% Mn, 0.022% P, 0.025% S, 0.89% Ni, 0.10% Cr, 0.05% Mo
0.33% C, 0.22% Si, 0.57% Mn, 0.010% P, 0.004% S, 1.47% Cr, 2.85% Ni, 0.21% Cu, 0.37% Mo
0.33% C, 0.23% Mn, 0.06% Si, 0.013% P, 0.021% S, 3.78% Ni, 1.79% Cr
0.33% C, 0.23% Mn, 0.06% Si, 0.013% P, 0.021% S, 3.78% Ni, 1.79% Cr
0.33% C, 0.23% Mn, 0.06% Si, 0.013% P, 0.021% S, 3.78% Ni, 1.79% Cr
0.33% C, 0.23% Si, 0.57% Mn, 0.005% P, 0.007% S, 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.23% Si, 0.57% Mn, 0.007% S, 0.005% P, 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.23% Si, 0.57% Mn, 0.007% S, 0.005% P, 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.23% Si, 0.57% Mn, 0.007% S, 0.005% P, 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.23% Si, 0.74% Mn, 0.031% P, 0.027% S, 3.47% Ni, 0.07% Cr
0.33% C, 0.23% Si, 1.54% Mn, 0.021% P, 0.024% S, 0.18% Ni, 0.15% Cr, 0.05% Mo
0.33% C, 0.24% Si, 0.47% Mn, 0.008% P, 0.007% S, 1.09% Cr, 3.10% Ni, 0.25% Cu, 0.33% Mo, 0.018% Sn, 0.009% Al
0.33% C, 0.24% Si, 0.47% Mn, 0.008% P, 0.007% S, 1.09% Cr, 3.10% Ni, 0.25% Cu, 0.33% Mo, 0.018% Sn, 0.009% Al
0.33% C, 0.24% Si, 0.49% Mn, 0.015% P, 0.002% S, 2.99% Cr, 0.12% Ni, 0.29% V, 0.22% Cu, 0.92% Mo
0.33% C, 0.24% Si, 0.49% Mn, 0.015% P, 0.002% S, 2.99% Cr, 0.12% Ni, 0.29% V, 0.22% Cu, 0.92% Mo
0.33% C, 0.27% Si, 0.60% Mn, 0.014% P, 0.025% S, 1.06% Cr, 1.00% Ni, 0.01% V, 0.20% Cu, 0.24% Mo, 0.021% Sn
0.33% C, 0.27% Si, 0.60% Mn, 0.014% P, 0.025% S, 1.06% Cr, 1.00% Ni, 0.01% V, 0.20% Cu, 0.24% Mo, 0.021% Sn
0.33% C, 0.32% Si, 0.51% Mn, 0.016% S, 0.008% P, 3.38% Ni, 0.83% Cr, 0.03% Mo
0.33% C, 0.34% Si, 0.92% Mn, 0.011% P, max. 0.02% S, 5.43% Cr, 2.36% Mo, 0.53% V, 0.06% Cu
0.33% C, 0.38% Mn, 0.30% Si, 1.06% Cr, 1.01% W
0.33% C, 0.39% Mn, 0.16% Si, 0.005% S, 0.004% P, 1.09% Cr, 3.60% Ni, 0.72% Mo, 0.12% V, 0.002% Ti, 0.013% Nb, 0.09% Cu, 0.009% Al
0.33% C, 0.41% Mn, 1.96% Mn, 0.82% Mo
0.33% C, 0.41% Mn, 1.96% Mo
0.33% C, 0.41% Si, 0.69% Mn, 0.043% P, 0.028% S, 1.41% Ni, 0.72% Cr, 0.28% Mo
0.33% C, 0.41% Si, 0.69% Mn, 0.043% P, 0.028% S, 1.41% Ni, 0.72% Cr, 0.28% Mo
0.33% C, 0.45% Mn, 1.97% Cr
0.33% C, 0.45% Mn, 1.97% Cr
0.33% C, 0.51% Mn, 0.013% P, 0.009% S, 0.17% Si, 4.16% Cr, 1.44% Cr, 0.31% Mo
0.33% C, 0.51% Mn, 0.17% Si, 0.013% P, 0.009% S 4.16% Ni, 1.44% Cr, 0.31% Mo
0.33% C, 0.51% Mn, 0.32% Si, 0.016% S, 0.008% P 3.38% Ni, 0.83% Cr, 0.03% Mo, 0.13% Cu
0.33% C, 0.51% Mn, 0.82% Ni, 2.32% Cr, 0.36% Mo
0.33% C, 0.52% Mn, 0.11% Si, <0.002% P, 0.014% S, 2.02% Ni, 1.34% Cr, 0.47% Mo, 0.09% V, 0.040% Al
0.33% C, 0.53% Mn, 0.00% Ni, 0.90% Cr, 0.18% Mo
0.33% C, 0.53% Mn, 0.00% Ni, 0.90% Cr, 0.18% Mo
0.33% C, 0.53% Mn, 0.90% Cr, 0.18% Mo
0.33% C, 0.53% Mn, 0.90% Cr, 0.18% Mo
0.33% C, 0.57% Mn, 0.005% P, 0.007% S, 0.23% Si, 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.57% Mn, 0.23% Si, 0.005% P, 0.007% S 3.26% Ni, 0.85% Cr, 0.09% Mo
0.33% C, 0.62% Mn, 0.21% Si, 0.89% Ni, 0.10% Cr 0.05% Mo
0.33% C, 0.65% Mn, 0.30% Si, 0.020% P, 0.020% S, 1.15% Cr, 0.20% Mo, 1.00% Al
0.33% C, 0.69% Mn, 0.043% P, 0.028% S, 0.41% Si, 1.41% Ni, 0.72% Cr, 0.28% Mo
0.33% C, 0.69% Mn, 0.41% Si, 0.043% P, 0.026% S 1.41% Ni, 0.72% Cr, 0.28% Mo
0.33% C, 0.72% Mn, 0.24% Si, 0.010% S, 0.010% P 1.22% Ni, 0.54% Cr, 0.17% Mo, 0.22% Cu
0.33% C, 0.72% Mn, 0.24% Si, 0.010% S, 0.010% P 1.22% Ni, 0.54% Cr, 0.17% Mo, 0.22% Cu
0.33% C, 0.74% Mn, 0.23% Si, 0.031% P, 0.027% S, 0.07% Cr, 3.47% Ni, 0.11% Mo
0.33% C, 0.74% Mn, 0.23% Si, 0.031% P, 0.027% S, 0.07% Cr, 3.47% Ni, 0.11% Mo
0.33% C, 0.74% Mn, 0.23% Si, 3.47% Ni, 0.07% Cr 0.11% Mo
0.33% C, 0.84% Mn, 0.26% V, 1.05% Cr, 1.07% Mo
0.33% C, 0.84% Mn, 1.05% Cr, 1.07% Mo, 0.26% V
0.33% C, 0.86% Mn, 1.62% Si, 0.014% S, 0.024% P, 0.81% Cr, 1.80% Ni, 0.40% Mo, 0.07% V, 0.040% Al, 0.020% N
0.33% C, 0.86% Mn, 1.62% Si, 1.80% Ni, 0.81% Cr, 0.40% Mo, 0.067% V
0.33% C, 0.89% Mn, 0.24% Si, 0.009% S, 0.008% P, 1.13% Cr, 0.15% Ni, 1.19% Mo, 0.22% V
0.33% C, 1.12% Mn, 0.30% Si, 0.027% S, 0.018% P 0.24% Ni, 0.11% Cr, 0.04% Mo, 0.19% Cu, 0.010% Al
0.33% C, 1.12% Mn, 0.30% Si, 0.027% S, 0.018% P 0.24% Ni, 0.11% Cr, 0.04% Mo, 0.19% Cu, 0.010% Al
0.33% C, 1.35% Mn, 0.24% Si, 0.025% P, 0.025% S, 0.45% Cr, 0.75% Ni, 0.20% Mo
0.33% C, 1.48% Mn, 0.18% Si, 0.028% P, 0.028% S, 0.26% Ni, 0.16% Cr, 0.27% Mo
0.33% C, 1.48% Mn, 0.18% Si, 0.26% Ni, 0.16% Cr 0.27% Mo
0.33% C, 1.49% Mn, 2.07% Ni, 0.67% Cr, 0.50% Mo
0.33% C, 1.54% Mn, 0.23% Si, 0.18% Ni, 0.15% Cr 0.05% Mo
0.33% C, 16.00% Cr, 0.050% S, 0.50% Ni
0.33% C, 2.16% Mn, 0.32% Si, 2.02% Ni, 0.64% Mo, 0.14% V
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.33-0.39% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.33-0.39% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.15% Cr, 0.050% Mo, 0.25% Ni, 0.20% Cu, Cr+Mo+Ni=0.35
0.33-0.39% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.15% Cr, 0.050% Mo, 0.25% Ni, 0.20% Cu, Cr+Mo+Ni=0.35
0.33-0.40% C, 0.15-0.35% Si, 0.80-1.10% Mn, 0.035% P, 0.035% S, 1.00-1.30% Cr
0.33-0.41% C, 0.80-1.20% Si, 0.25-0.50% Mn, <0.025% P, <0.005% S, 4.80-5.50% Cr, 1.10-1.50% Mo, 0.30-0.50% V
0.33-0.43% C, <1.00% Si, <1.00% Mn, 15.50-17.50% Cr, 1.00-1.30% Mo
0.33-0.45% C, max. 1.0% Si, max. 1.50% Mn, max. 0.030% P, max. 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, max. 1.0% Ni
0.33-0.45% C, max. 1.00% Si, max. 1.50% Mn, max. 0.030% P, max. 0.030% S, 15.50-17.50% Cr, 0.80-1.30% Mo, max. 1.00% Ni
0.33-0.45% C, max. 1.00% Si, max. 1.50% Mn, max. 0.040% P, max. 0.015% S, 15.50-17.50% Cr, 0.80-1.30% Mo, max. 1.00% Ni
0.33% C, 0.93% Mn, 0.30% Si, 0.007% P, 0.001% S, 0.84% Ni, 0.99% Cr, 0.40% Mo, 0.005% V, 0.14% Cu, 0.026% Al, 0.003% Ti, 0.0010% Ca, 0.013% % Co, 1 ppm H2
0.33% C, 0.85% Mn, 0.35% Si, 0.55% Ni, 1.85% Cr, 0.50% Mo
0.33% C, 16.00% Cr, 0.05% S, 0.50% Ni
0.33% C, 0.36% Si, 0.66% Mn, 0.030% P, 0.015% S, 0.007% Al, 0.98% Cr, 0.22% Cu, 0.02% Mo, 0.0075% N, 0.01% Ni, 0.01% V
0.33% C, 0.21% Si, 0.75% Mn, 0.010% P, 0.011% S, 0.99% Al, 0.01% Co, 1.17% Cr, 0.03% Cu, 0.19% Mo, 0.0055% N, 0.08% Ni
0.33% C, 0.21% Si, 0.75% Mn, 0.010% P, 0.011% S, 0.99% Al, 0.01% Co, 1.17% Cr, 0.03% Cu, 0.19% Mo, 0.0055% N, 0.08% Ni
0.33% C, 0.29% Si, 0.50% Mn, 0.031% P, 0.025% S, 0.11% Cu, 1.03% Cr, 0.13% Ni, 0.23% Mo, 0.046% Al, 0.015% V
0.34% C, 0.18% Si, 1.53% Mn, 0.028% P, 0.026% S, 0.08% Cr, 0.02% Mo, 0.17% Ti
0.34% C, 0.20% Si, 0.23% Mn, 0.013% P, 0.003% S, 5.06% Cr, 0.10% Ni, 0.42% V, 0.03% W, 0.06% Cu, 1.24% Mo, 0.020% Al
0.34% C, 0.20% Si, 1.06% Mn, 0.037% P, 0.040% S, 0.75% Ni, 0.23% Cr, 0.02% Mo
0.34% C, 0.20% Si, 1.06% Mn, 0.04% S, 0.037% P, 0.75% Ni, 0.08% Cr, 0.02% Mo
0.34% C, 0.20% Si, 1.06% Mn, 0.04% S, 0.037% P, 0.75% Ni, 0.08% Cr, 0.02% Mo
0.34% C, 0.20% Si, 1.06% Mn, 0.04% S, 0.037% P, 0.75% Ni, 0.08% Cr, 0.02% Mo
0.34% C, 0.22% Si, 1.25% Mn, 0.11% Cr, 0.03% Ti, 0.0025% B
0.34% C, 0.23% Si, 0.55% Mn, 0.011% P, 0.022% S, 1.39% Cr, 4.59% Ni
0.34% C, 0.25% Si, 0.44% Mn, 0.014% P, 0.010% S, 1.21% Cr, 2.98% Ni, 0.10% Cu, 0.33% Mo, 0.021% Al
0.34% C, 0.25% Si, 0.50% Mn, 1.050% Cr, 0.25% Mo, 1.55% Ni, (Pb)
0.34% C, 0.25% Si, 0.50% Mn, 1.050% Cr, 0.25% Mo, 1.55% Ni, (Pb)
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.50% Mn, 1.50% Cr, 1.55% Ni, 0.25% Mo
0.34% C, 0.25% Si, 0.50% Mn, 1.70% Cr, 0.20% Mo, 1.00% Ni, 1.00% Al
0.34% C, 0.25% Si, 0.50% Mn, 1.70% Cr, 1.00% Ni, 0.20% Mo, 0.90% Al
0.34% C, 0.25% Si, 0.50% Mn, 1.70% Cr, 1.00% Ni, 0.20% Mo, 0.90% Al
0.34% C, 0.25% Si, 0.55% Mn, 1.55% Cr, 1.55% Ni, 0.20% Mo
0.34% C, 0.25% Si, 0.55% Mn, 1.55% Cr, 1.55% Ni, 0.20% Mo
0.34% C, 0.25% Si, 0.55% Mn, 1.65% Cr, 1.00% Al, 1.00% Ni, 0.20% Mo
0.34% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, <0.035% S, (Pb). 34CrMoS4: 0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, 0.020-0.035% S, (Pb)
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, <0.035% S, (Pb). 34CrMoS4: 0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, 0.020-0.035% S, (Pb)
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, <0.035% S
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo, <0.035% S
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.25% Mo
0.34% C, 0.25% Si, 0.75% Mn, 1.05% Cr
0.34% C, 0.25% Si, 0.75% Mn, 1.05% Cr
0.34% C, 0.25% Si, 0.75% Mn, 1.50% Cr, 1.00% Al
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, <0.035% S, (Pb). 34CrS4: 0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, 0.020-0.035% S, (Pb)
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, <0.035% S, (Pb). 34CrS4: 0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, 0.020-0.035% S, (Pb)
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, <0.035% S
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr, <0.035% S
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr
0.34% C, 0.25% Si, 0.85% Mn, 1.05% Cr
0.34% C, 0.26% Mn, 0.13% Si, 0.007% S, 0.010% P, 0.61% Cr, 5.10% Ni, 0.53% Mo, 0.09% V
0.34% C, 0.26% Si, 0.31% Mn, 2.97% Cr, 3.12% Mo, 0.66% V, 2.05% Co
0.34% C, 0.26% Si, 0.52% Mn, 0.011% P, 0.026% S, 3.12% Cr, 0.32% Ni, 0.23% V, 0.19% Cu, 0.98% Mo
0.34% C, 0.26% Si, 0.52% Mn, 0.011% P, 0.026% S, 3.12% Cr, 0.32% Ni, 0.23% V, 0.19% Cu, 0.98% Mo
0.34% C, 0.28% Si, 0.43% Mn, 0.011% P, 0.008% S, 0.75% Cr, 3.53% Ni
0.34% C, 0.29% Si, 0.59% Mn, 0.012% P, 0.007% S, 1.54% Cr, 0.24% Mo, 1.52% Ni
0.34% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.34% C, 0.30% Si, 0.95% Mn, 0.025% P, 0.10% S, 15.00% Cr
0.34% C, 0.30% Si, 0.95% Mn, 0.025% P, 0.10% S, 15.00% Cr
0.34% C, 0.35% Mn, 0.26% Si, 0.006% S, 0.008% P 3.55% Ni, 1.54% Cr, 0.31% Mo, 0.008% N2
0.34% C, 0.35% Si, 0.65% Mn, 1.15% Cr, 1.00% Al, 0.20% Mo
0.34% C, 0.39% Si, 0.64% Mn, 0.007% P, 0.005% S, 0.95% Cr, 0.14% Ni, 0.18% Cu, 0.21% Mo, 0.013% Sn
0.34% C, 0.39% Si, 0.64% Mn, 0.007% P, 0.005% S, 0.95% Cr, 0.14% Ni, 0.18% Cu, 0.21% Mo, 0.013% Sn
0.34% C, 0.46% Si, 1.75% Mn, 0.055% P, 1.32% Al, 0.12% Ti, 0.033% V, 0.71% CE
0.34% C, 0.49% Mn, 0.30% Si, 4.30% Ni, 1.86% Cr
0.34% C, 0.50% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.80% Cr, 4.00% Ni, 0.35% Mo
0.34% C, 0.52% Mn, 0.37% Si, 2.65% Ni, 1.80% Cr 0.53% Mo, 0.15% V, 0.20% Cu
0.34% C, 0.62% Mn, 0.27% Si, 0.010% S, 0.006% P, 1.22% Cr, 2.80% Ni, 0.50% Mo, 0.09% V
0.34% C, 0.65% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.05% Cr, 0.25% Mo
0.34% C, 0.71% Mn, 0.039% P, 0.028% S, 0.22% Si, 2.52% Ni, 0.14% Cr, 0.42% Mo, 0.02% V
0.34% C, 0.71% Mn, 0.22% Si, 0.039% P, 0.028% S 2.52% Ni, 0.14% Cr, 0.42% Mo, 0.02% V
0.34% C, 0.71% Mn, 2.52% Ni, 0.42% Mo, 0.02% V
0.34% C, 0.80% Mn, 0.38% Si, 0.34% Cr, 0.78% Mo
0.34% C, 0.95% Mn, 0.40% Si, 0.020% P, 0.005-0.020% S, 1.90% Cr, 0.40% Mo, +Ni
0.34% C, 0.98% Mn, 0.015% P, 0.005% S, 1.37% Si, 1.82% Ni, 0.95% Cr, 0.42% Mo, 0.14% V
0.34% C, 0.98% Mn, 1.37% Si, 0.95% Cr, 1.82% Ni, 0.42% Mo, 0.14% V
0.34% C, 0.98% Mn, 1.37% Si, 0.015% P, 0.005% S 1.82% Ni, 0.95% Cr, 0.42% Mo, 0.14% V
0.34% C, 1.31% Mn, 0.24% Si, 0.10% V, 0.018% Al
0.34% C, 1.55% Mn, 0.18% Si, 0.028% S, 0.026% P 0.17% Ni, 0.08% Cr, 0.02% Mo
0.34-0.41% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr. 37CrS4: 0.34-0.41% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.34-0.41% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr. 37CrS4: 0.34-0.41% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.34-0.41% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.34-0.41% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.34-0.41% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.34-0.41% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.035% S, 0.90-1.20% Cr
0.34% C, 0.30% Si, 0.95% Mn, 0.025% P, 0.10% S, 15.00% Cr
0.34% C, 0.02% Si, 0.38% Mn, 0.012% P, 0.019% S
0.34% C, 1.07% Cr, 0.17% Mo
0.34% C, 1.50% Cr, 0.25% Mo, 1.50% Ni
0.34% C, 1.50% Cr, 0.25% Mo, 1.50% Ni
0.34% C, 1.70% Cr, 0.20% Mo, 1.00% Ni, 1.00% Al
0.34% C, 1.70% Cr, 0.20% Mo, 1.00% Ni, 1.00% Al
0.34% C, 0.29% Si, 0.59% Mn, 0.012% P, 0.007% S, 1.54% Cr, 1.52% Ni, 0.24% Mo
0.34% C, 0.80% Mn, 1.70% Cr, 0.50% Ni, 0.40% Mo
0.34% C, 0.34% Si, 0.65% Mn, 0.017% P, 0.016% S, 0.008% Al, 1.07% Cr, 0.18% Cu, 0.17% Mo, 0.0072% N, 0.18% Ni, 0.01% V
0.34% C, 0.34% Si, 0.65% Mn, 0.017% P, 0.016% S, 0.008% Al, 1.07% Cr, 0.18% Cu, 0.17% Mo, 0.0072% N, 0.18% Ni, 0.01% V
0.34% C, 0.35% Si, 0.64% Mn, 0.023% P, 0.028% S, 0.24% Cu, 1.17% Cr, 0.15% Ni, 0.25% Mo, 0.003% Al
0.34% C, 0.02% Si, 0.38% Mn, 0.012% P, 0.019% S
0.345% C, 0.42% Mn, 0.43% Si, 0.015% S, 0.015% P 3.43% Ni, 1.36% Cr, 0.23% Mo, 0.041% Al, 0.19% Cu
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, < 0.030% P, 0.050-1.100% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35% C, 0.30% Mn, 1.00% Si, 5.00% Cr, 1.50% Mo, 1.25% W
0.35% C, 0.13% Si, 0.65% Mn, 0.032% S, 0.035% P, 1.27% Ni, 0.55% Cr, Nil Mo
0.35% C, 0.13% Si, 0.65% Mn, 0.032% S, 0.035% P, 1.27% Ni, 0.55% Cr, Nil Mo
0.35% C, 0.13% Si, 0.65% Mn, 0.032% S, 0.035% P, 1.27% Ni, 0.55% Cr
0.35% C, 0.13% Si, 0.85% Mn, 0.035% P, 0.032% S, 1.27% Ni, 0.55% Cr
0.35% C, 0.14% Si, 0.44% Mn, 0.008% S, 0.016% P, 4.23% Ni, 1.43% Cr, 0.13% Mo
0.35% C, 0.14% Si, 0.44% Mn, 0.008% S, 0.016% P, 4.23% Ni, 1.43% Cr, 0.13% Mo
0.35% C, 0.14% Si, 0.44% Mn, 0.016% P, 0.008% S, 4.23% Ni, 1.43% Cr, 0.13% Mo
0.35% C, 0.20% Si, 0.30% Mn, 5.20% Cr, 1.40% Mo, 0.55% V
0.35% C, 0.20% Si, 0.50% Mn, 2.30% Cr, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.20% Si, 0.70% Mn, <0.025% S, <0.025% P, <0.25% Cu
0.35% C, 0.20% Si, 0.70% Mn, <0.025% S, <0.025% P, <0.25% Cu
0.35% C, 0.23% Si, 0.65% Mn, 0.026% P, 0.013% S, 1.11% Cr, 0.18% Cu, 0.05% Mo, 0.28% Ni, <0.01% V
0.35% C, 0.23% Si, 0.65% Mn, 0.026% P, 0.013% S, 1.11% Cr, 0.18% Cu, 0.05% Mo, 0.28% Ni, <0.01% V
0.35% C, 0.23% Si, 0.65% Mn, 0.23% Ni, 1.11% Cr, 0.05% Mo, 0.18% Cu
0.35% C, 0.23% Si, 0.65% Mn, 0.23% Ni, 1.11% Cr, 0.05% Mo, 0.18% Cu
0.35% C, 0.23% Si, 0.65% Mn, 0.23% Ni, 1.11% Cr, 0.05% Mo, 0.18% Cu
0.35% C, 0.23% Si, 0.65% Mn, 0.23% Ni, 1.11% Cr, 0.05% Mo, 0.18% Cu
0.35% C, 0.23% Si, 0.65% Mn, 0.23% Ni, 1.11% Cr, 0.05% Mo, 0.18% Cu
0.35% C, 0.23% Si, 0.65% Mn, 0.23% Ni, 1.11% Cr, 0.05% Mo, 0.18% Cu
0.35% C, 0.23% Si, 0.65% Mn, 1.11% Cr, 0.05% Mo, 0.23% Ni, 0.11% Cu
0.35% C, 0.23% Si, 0.65% Mn, 1.11% Cr, 0.18% Cu, 0.23% Ni, 0.05% Mo
0.35% C, 0.23% Si, 0.65% Mn, 1.11% Cr, 0.18% Cu, 0.23% Ni, 0.05% Mo
0.35% C, 0.24% Si, 1.19% Mn, 0.024% P, 0.018% S, 0.20% Cr, 0.02% Mo, 0.026% Al, 0.005% V, 0.003% Nb, 0.054% Ti, 0.0027% B
0.35% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 3.55% Ni, 0.25% Mo
0.35% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 3.55% Ni, 0.25% Mo
0.35% C, 0.25% Si, 0.43% Mn, 2.52% Ni, 1.55% Cr, 0.53% Mo
0.35% C, 0.25% Si, 0.50% Mn, 0.025% P, 0.010% S, 1.35% Cr, 4.00% Ni, 0.30% Mo
0.35% C, 0.25% Si, 0.50% Mn, 1.35% Cr, 4.10% Ni, 0.30% Mo
0.35% C, 0.25% Si, 0.65% Mn, <0.03% S
0.35% C, 0.25% Si, 0.65% Mn, <0.03% S
0.35% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, (Pb)
0.35% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, (Pb)
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.25% Si, 0.65% Mn
0.35% C, 0.26% Si, 0.50% Mn, 0.010% P, 0.020% S, 0.49% Cr, 1.54% Ni
0.35% C, 0.30% Mn, 0.20% Si, <0.012% P, <0.003% S, 5.20% Cr, 1.40% Mo, 0.55% V, + Nb
0.35% C, 0.30% Si, 0.30% Mn, <0.003% S, 5.00% Cr, 1.35% Mo, 0.45% V
0.35% C, 0.30% Si, 0.40% Mn, <0.010% P, <0.003% S, 5.00% Cr, 1.35% Mo, 0.50% V
0.35% C, 0.30% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 3.50% Ni
0.35% C, 0.30% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 3.50% Ni
0.35% C, 0.30% Si, 0.75% Mn, 1.05% Cr, 1.45% Ni
0.35% C, 0.30% Si, 0.75% Mn, 1.05% Cr, 1.45% Ni
0.35% C, 0.30% Si, max. 0.003% C, 0.30% Mn, 5.0% Cr, 1.35% Mo, 0.45% V
0.35% C, 0.31% Si, 0.69% Mn, 0.011% P, 0.018% S, 0.31% Ni, 0.12% Cr, 0.04% Mo, 0.14% Cu
0.35% C, 0.34% Si, 0.38% Mn, 0.012% P, 0.010% S, 16.70% Cr, 1.15% Mo, 0.76% Ni
0.35% C, 0.35% Si, 0.69% Mn, 0.015% P, 0.009% S, 0.84% Cr, 1.41% Ni
0.35% C, 0.37% Mn, 0.009% P, 0.012% S, 0.21% Si, 0.06% Ni, 0.05% Cr, 0.70% Cu
0.35% C, 0.37% Mn/ 0.37% C, 0.37% Mn, 0.57% Cr/ 0.42% C, 0.68% Mn, 0.93% Cr/ 0.32% C, 0.45% Mn, 1.97% Cr Beginning of transformation at left, ending at right
0.35% C, 0.37% Mn/ 0.42% C, 0.20% Mn, 0.21% Mo/ 0.40% C, 0.43% Mn, 0.52% Mo/ 0.36% C, 0.17% Mn, 0.82% Mo/ 0.33% C, 0.14% Mn, 1.96% Mo Beginning of transformation at left, ending at right
0.35% C, 0.37% Mn
0.35% C, 0.37% Mn
0.35% C, 0.37% Mn
0.35% C, 0.40% Si, 1.00% Al, 1.70% Cr, 0.20% Mo, 1.00% Ni
0.35% C, 0.43% Si, 1.78% Mn, 0.024% P, 0.029% S, 0.22% Cr, 0.13% Ni, 0.22% Cu, 0.04% Mo
0.35% C, 0.43% Si, 1.78% Mn, 0.024% P, 0.029% S, 0.22% Cr, 0.13% Ni, 0.22% Cu, 0.04% Mo
0.35% C, 0.44% Mn, 0.016% P, 0.008% S, 0.14% Si, 4.23% Ni, 1.43% Cr, 0.13% Mo
0.35% C, 0.44% Mn, 0.14% Si, 0.016% P, 0.008% S 4.23% Ni, 1.43% Cr, 0.13% Mo
0.35% C, 0.55% Mn, 0.25% Si, 1.55% Ni, 1.55% Cr, 0.20% Mo, 0.025% P, 0.015% S
0.35% C, 0.55% Mn, 0.27% Si, 0.031% P, 0.022% S, 1.23% Cr, 0.51% Mo, 0.14% Ni
0.35% C, 0.65% Mn, 0.13% Si, 0.035% P, 0.032% S, 1.27% Ni, 0.55% Cr
0.35% C, 0.69% Mn, 0.24% Si, 3.25% Ni, 1.32% Cr, 0.48% Mo
0.35% C, 0.69% Mn, 0.31% Si, 0.018% S, 0.011% P 0.31% Ni, 0.12% Cr, 0.04% Mo, 0.14% Cu
0.35% C, 0.75% Mn, 0.23% Si, 0.020% P, 0.020% S, 0.65% Cr, 1.30% Ni
0.35% C, 0.80% Mn, 0.25% Mo
0.35% C, 0.80% Mn, 0.25% Mo
0.35% C, 0.80% Mn, 0.36% Si, 2.58% Ni, 0.78% Mo
0.35% C, 0.80% Mn, 0.38% Si, 0.35% Cr, 0.51% Mo
0.35% C, 0.80% Si, 5.00% Cr, 1.00% Mo, 0.85% V
0.35% C, 0.82% Mn, 0.36% Si, 1.51% Cr, 0.84% Mo
0.35% C, 0.83% Mn, 0.39% Si, 0.35% Cr, 0.24% Mo
0.35% C, 0.85% Mn, 0.027% P, 0.006% S, 0.005% Si, 0.032% Al, 0.07% Nb, 0.0006% Ti
0.35% C, 0.86% Mn, 1.55% Si, 0.014% S, 0.023% P, 1.21% Cr, 0.21% Ni, 0.58% Mo, 0.06% V, 0.037% Al, 0.021% N
0.35% C, 0.86% Mn, 1.55% Si, 0.014% S, 0.024% P, 1.50% Cr, 0.23% Ni, 0.58% Mo, 0.07% V, 0.039% Al, 0.022% N
0.35% C, 0.86% Mn, 1.55% Si, 0.21% Ni, 1.21% Cr, 0.58% Mo, 0.037% V
0.35% C, 0.86% Mn, 1.58% Si, 0.23% Ni, 1.50% Cr, 0.58% Mo, 0.071% V
0.35% C, 0.90% Si, 0.35% Mn, 0.012% P, 0.006% S, 1.16% Cr, 1.95% W, 0.19% V
0.35% C, 1.0% Si, 5.00% Cr, 1.30% Mo, 0.40% V
0.35% C, 1.00% Si, 0.50% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.50% Mo, 0.30% V, 1.30% W
0.35% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.35% C, 1.40% Mn, 0.76% Si, 0.06% Ni, 0.07% Cr, 0.19% Mo, 0.14% V
0.35% C, 1.40% Mn, 0.76% Si, 0.06% Ni, 0.07% Cr, 0.19% Mo, 0.16% V
0.35% C, 1.40% Mn, 0.76% Si, 0.06% Ni, 0.07% Cr, 0.19% Mo, 0.16% V
0.35% C, 1.51% Mn, 0.28% Si, 0.007% S, 0.015% P, 1.29% Mo, 0.21% V, 0.10% Cu
0.35% C, 1.55% Mn, 0.20% Si, 0.025% P, 0.025% S, 0.28% Mo
0.35% C, 1.62% Mn, 0.47% Si, 0.008% S, 0.001% P, 0.10% Cr, 0.10% Ni, 0.01% Mo, 0.11% V, 0.14% Cu, 0.02% Al
0.35% C, 1.70% Cr, 3.80% Ni, 0.30% Mo
0.35% C, 1.85% Mn
0.35% C, 1.85% Mn
0.35% C, 3.00% Cr, 1.00% Mo, 0.25% V
0.35% C, 3.00% Cr, 2.70% Mo, 0.50% V
0.35% C, 5.00% Cr, 1.30% Mo, 0.40% V
0.35-0.37% C, 0.15-0.19% Si, 0.50-0.53% Mn, 0.006-0.008% S, 0.001-0.003% P, 0.06-0.07% Ni, 4.98-5.11% Cr, 2.33-2.40% Mo, 0.01% W, 0.02% Co, 0.54-0.55% V, 0.01-0.02% Ti, 0.001% Nb, 0.04-0.06% Cu, 0.008-0.017% Al, 0.007% N, 3-5 ppm O
0.35-0.37% C, 0.15-0.19% Si, 0.50-0.53% Mn, 0.006-0.008% S, 0.001-0.003% P, 0.06-0.07% Ni, 4.98-5.11% Cr, 2.33-2.40% Mo, 0.01% W, 0.02% Co, 0.54-0.55% V, 0.01-0.02% Ti, 0.001% Nb, 0.04-0.06% Cu, 0.008-0.017% Al, 0.007% N, 3-5 ppm O
0.35-0.40% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.15% Cr
0.35-0.40% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.85-1.15% Cr
0.35-0.40% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.30% Mo, 0.25% Cu
0.35-0.40% C, 0.30% Si, 1.15-1.45% Mn, 0.025% P, 0.025% S, 0.30% Cr, 0.0008-0.0050% B, 0.25% Cu
0.35-0.40% C, 0.30-0.50% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.020% S, 4.80-5.20% Cr, 2.70-3.20% Mo, 0.40-0.60% V
0.35-0.40% C, 1.30-1.60% Mn, 0.20-0.40% Si, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.42% C, 0.25-0.50% Mn, 0.80-1.20% Si, 0.02% S, 0.03% P, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.25-0.50% Mn, 0.80-1.20% Si, 0.02% S, 0.03% P, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, max. 0.025% P, 0.005% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 0.80-1.20% Si, 0.25-0.50% Mn, max. 0.030% P, max. 0.020% S, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.85-1.15% V
0.35-0.42% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S
0.35-0.42% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.35-0.42% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.35-0.43% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.43% C, 0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-1.00% Cr, 0.15-0.25% Mo, 0.70-1.00% Ni
0.35-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo. 25CrMoS4: 0.22-0.29% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.35-0.45% C, 0.10-0.40% Si, 0.20-0.55% Mn, max. 0.030% P, max. 0.025% S, 1.40-1.70% Cr, 0.35-0.60% Mo, 4.30-4.90% Ni
0.35-0.45% C, 0.10-0.40% Si, 0.20-0.55% Mn, max. 0.030% P, max. 0.025% S, 1.40-1.70% Cr, 0.35-0.60% Mo, 4.30-4.90% Ni
0.35-0.45% C, 0.15-0.35% Si, 1.25-1.75% Mn, 0.040% P, 0.050% S, 0.0005-0.0030% B
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, <0.025% P, <0.005% S, 1.80-2.10% Cr, 0.15-0.25% Mo, 1.00-1.20% V
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, <0.025% P, <0.002% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.20-0.40% Si, 1.30-1.60% Mn, <0.025% P, <0.005% S, 1.80-2.10% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.14-1.60% Mn, <0.030% P, 0.050-1.10% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.45% C, 0.30-0.50% Si, 1.40-1.60% Mn, <0.030% P, 0.05-0.10% S, 1.80-2.00% Cr, 0.15-0.25% Mo
0.35-0.46% C, 0.12-0.42% Si, 0.66-1.04% Mn, 0.040% P, 0.040% S, 0.35-0.65% Cr, 0.12-0.33% Mo, 0.37-0.73% Ni, 0.015-0.035% Al
0.35% C, 1.80% Ni, 0.80% Cr, 0.35% Mo, 0.20% V
0.35% C, 0.89% Mn, 0.41% Si, 0.50% Ni, 1.86% Cr, 0.53% Mo, 0.16% Cu
0.35% C, 0.89% Mn, 0.41% Si, 0.50% Ni, 1.86% Cr, 0.53% Mo, 0.16% Cu
0.35% C, 1.4% Mn, 0.76% Si, 0.06% Ni, 0.16% V
0.35% C, 1.0% Si, 5.00% Cr, 1.30% Mo, 0.40% V
0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.35% C, 0.35% Si, 0.46% Mn, 0.019% P, 0.015% S, 3.05% Cr, 0.88% Mo, 0.05% Ni, 0.20% V, 0.05% Cu
0.35% C, 0.31% Si, 0.53% Mn, 0.02% P, 0.012% S, 0.92% Al, 1.69% Cr, 0.24% Mo, 0.97% Ni
0.35-0.42% C, 0.80-1.20% Si, 0.20-0.50% Mn, max. 0.025% P, max. 0.025% S, 4.75-5.50% Cr, 0.80-1.20% V, 1.20-1.50% Mo
0.35-0.42% C, 0.80-1.20% Si, 0.20-0.50% Mn, max. 0.025% P, max. 0.025% S, 4.75-5.50% Cr, 0.80-1.20% V, 1.20-1.50% Mo
0.35% C, 0.80% Si, 5.00% Cr, 1.00% Mo, 0.85% V
0.35% C, 0.40% Si, 1.00% Al, 1.70% Cr, 0.20% Mo, 1.00% Ni
0.35% C, 0.30% Si, 0.30% Mn, 5.00% Cr, 1.35% Mo, 0.45% V
0.35% C, 0.30% Si, 0.30% Mn, 5.00% Cr, 1.75% Mo, 0.80% V, + Others
0.35% C, 0.25% Si, 0.50% Mn, 1.35% Cr, 4.10% Ni, 0.30% Mo
0.35% C, 0.51% Si, 0.63% Mn, 0.012% P, 0.009% S, 0.15% Cu, 0.22% Cr, 0.18% Ni, 0.058% Mo, 0.001% Nb, 0.052% Al, 0.003% V
0.355% C, 0.26% Si, 1.53% Mn, 0.007% P, 0.001% S, 1.98% Cr, 1.15% Ni, 0.21% Mo
0.36% C, 0.17% Mn, 0.82% Mo
0.36% C, 0.17% Mn, 0.82% Mo
0.36% C, 0.21% Si, 0.31% Mn, 0.016% P, 0.011% S, 2.90% Cr, 2.78% Mo, 0.22% Ni, 0.47% V, 0.16% W, 2.72% Co
0.36% C, 0.21% Si, 0.31% Mn, 0.016% P, 0.011% S, 2.90% Cr, 2.78% Mo, 0.22% Ni, 0.47% V, 0.16% W, 2.72% Co
0.36% C, 0.22% Si, 0.52% Mn, 0.005% S, 0.007% P, 1.52% Ni, 1.17% Cr, 0.27% Mo
0.36% C, 0.22% Si, 0.52% Mn, 0.005% S, 0.007% P, 1.52% Ni, 1.17% Cr, 0.27% Mo
0.36% C, 0.22% Si, 0.52% Mn, 0.005% S, 0.007% P, 1.52% Ni, 1.17% Cr, 0.27% Mo
0.36% C, 0.22% Si, 0.52% Mn, 0.005% S, 0.007% P, 1.52% Ni, 1.17% Cr, 0.27% Mo
0.36% C, 0.22% Si, 0.58% Mn, 0.020% S, 0.015% P, 0.25% Ni, 0.08% Cr, <0.01% Mo, 0.50% Cu
0.36% C, 0.24% Si, 0.49% Mn, 0.030% P, 0.023% S, 1.48% Cr, 1.52% Ni, 0.01% V, 0.22% Cu, 0.17% Mo
0.36% C, 0.24% Si, 0.49% Mn, 0.030% P, 0.023% S, 1.48% Cr, 1.52% Ni, 0.01% V, 0.22% Cu, 0.17% Mo
0.36% C, 0.25% Mn, 0.20% Si, 5.00% Cr, 1.30% Mo, 0.45% V
0.36% C, 0.25% Si, 0.35% Mn, 5.00% Cr, 1.50% Ni, 1.75% Mo, 0.65% V
0.36% C, 0.25% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.25% Si, 0.40% Mn, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.25% Si, 0.49% Mn, 0.021% P, 0.020% S, 1.54% Cr, 0.16% Cu, 0.03% Mo, 0.21% Ni, <0.01% V
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.20% Mo, 1.05% Ni, (Pb)
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.20% Mo, 1.05% Ni, (Pb)
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 1.05% Ni, 0.20% Mo
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 1.05% Ni, 0.20% Mo
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 1.05% Ni, 0.20% Mo
0.36% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 1.05% Ni, 0.20% Mo
0.36% C, 0.25% Si, 1.35% Mn, (Pb)
0.36% C, 0.25% Si, 1.45% Mn
0.36% C, 0.27% Si, 0.66% Mn, 0.016% S, 0.020% P, 0.20% Ni, 0.21% Cr, 0.02% Mo, 0.22% Cu, 0.06% Al, 0.06% As
0.36% C, 0.27% Si, 0.66% Mn, 0.016% S, 0.020% P, 0.20% Ni, 0.21% Cr, 0.02% Mo, 0.22% Cu, 0.06% Al, 0.06% As
0.36% C, 0.27% Si, 0.66% Mn, 0.020% P, 0.016% S, 0.21% Cr, 0.02% Ni, 0.02% Mo, 0.22% Cu, 0.060% Al
0.36% C, 0.29% Si, 0.31% Mn, 0.010% P, 0.005% S, 1.24% Cr, 3.21% Ni, 0.14% V, 0.21% Cu, 0.39% Mo
0.36% C, 0.29% Si, 0.31% Mn, 0.010% P, 0.005% S, 1.24% Cr, 3.21% Ni, 0.14% V, 0.21% Cu, 0.39% Mo
0.36% C, 0.29% Si, 0.69% Mn, 0.011% P, 0.014% S, 1.09% Cr, 0.12% Cu, 0.07% Mo, 0.08% Ni, 0.01% V
0.36% C, 0.29% Si, 0.72% Mn, 0.015% P, 0.016% S, 1.07% Cr, 0.20% Ni, 0.12% W, 0.26% Cu, 0.17% Mo, 0.022% Sn
0.36% C, 0.29% Si, 0.72% Mn, 0.015% P, 0.016% S, 1.07% Cr, 0.20% Ni, 0.12% W, 0.26% Cu, 0.17% Mo, 0.022% Sn
0.36% C, 0.3% Si, 5.0% Cr, 1.3% Mo, 0.5% V
0.36% C, 0.30% Si, 0.40% Mn, <0.012% P, <0.003% S, 5.20% Cr, 1.90% Mo, 0.55% V
0.36% C, 0.33% Si, 0.59% Mn, 0.011% P, 0.03% S, 0.55% Cr, 0.15% Ni, 0.18% Cu, 0.03% Mo
0.36% C, 0.33% Si, 0.59% Mn, 0.011% P, 0.03% S, 0.55% Cr, 0.15% Ni, 0.18% Cu, 0.03% Mo
0.36% C, 0.33% Si, 0.59% Mn, 0.011% P, 0.03% S, 0.55% Cr, 0.15% Ni, 0.18% Cu, 0.03% Mo
0.36% C, 0.35% Si, 0.75% Mn, 0.018% P, 0.018% S, 1.07% Cr, 0.21% Mo, 1.09% Ni
0.36% C, 0.37% Si, 0.48% Mn, 3.08% Cr, 0.88% Mo, 0.04% Ni, 0.19% V, 0.04% Cu, 0.106% Al
0.36% C, 0.39% Mn, 0.30% Si, 0.005% S, 0.010% P 3.70% Ni, 1.65% Cr, 0.23% Mo, 0.12% Cu
0.36% C, 0.39% Mn, 0.30% Si, 0.005% S, 0.010% P 3.70% Ni, 1.65% Cr, 0.23% Mo, 0.12% Cu
0.36% C, 0.40% Si, 0.45% Mn, 0.020% P, 0.003% S, 5.00% Cr, 3.00% Mo, 0.65% V
0.36% C, 0.42% Si, 0.25% Mn, 0.025% P, 0.001% S, 12.88% Cr, 0.15% Mo, 0.40% Ni, 0.12% Cu
0.36% C, 0.49% Si, 0.43% Mn, 0.24% Ni, 13.50% Cr
0.36% C, 0.50% Mn, 0.31% Si, 0.014% S, 0.02% P 4.04% Ni, 1.99% Cr, 0.54% Mo, 0.28% Cu
0.36% C, 0.50% Mn, 0.32% Si, 0.0077% Mo
0.36% C, 0.50% Mn, 0.32% Si, 0.19% Mo
0.36% C, 0.53% Mn, 0.32% Si, 0.010% S, 0.013% P 3.74% Ni, 1.86% Cr, 0.05% Mo, 0.13% Cu, 0.002% Ti
0.36% C, 0.60% Mn, 0.26% Si, 0.032% S, 0.012% P
0.36% C, 0.60% Mn, 1.00% Si, 0.30% V, 5.00% Cr, 1.80% Mo
0.36% C, 0.63% Mn, 0.018% P, 0.021% S, 0.19% Si, 1.84% Ni, 0.06% Cr, 0.23% Mo
0.36% C, 0.63% Mn, 1.84% Ni, 0.23% Mo
0.36% C, 0.63% Mn, 1.84% Ni, 0.23% Mo
0.36% C, 0.63% Mn, 1.84% Ni, 0.23% Mo
0.36% C, 0.65% Mn, 0.25% Si, 0.020% P, 0.025% S, 1.05% Cr, 1.05% Ni, 0.22% Mo
0.36% C, 0.66% Mn, 0.27% Si, 0.016% S, 0.020% P 0.02% Ni, 0.21% Cr, 0.02% Mo, 0.22% Cu
0.36% C, 0.66% Mn, 0.27% Si, 0.016% S, 0.020% P 0.20% Ni, 0.21% Cr, 0.02% Mo, 0.20% Cu, 0.060% Al
0.36% C, 0.69% Mn, 0.29% Si, 0.014% S, 0.011% P, 1.09% Cr, 0.08% Ni, 0.07% Mo, 0.01% V, 0.12% Cu
0.36% C, 0.70% Mn, 0.25% Si, 0.020% P, 0.025% S, 1.50% Cr, 1.50% Ni, 0.25% Mo
0.36% C, 0.72% Mn, 0.28% Si, 0.018% S, 0.077% P 0.006% Ni, 0.97% Cr, 0.23% Mo, 0.10% Cu
0.36% C, 0.75% Mn, 0.29% Si, 0.72% Ni, 0.82% Mo
0.36% C, 0.77% Mn, 0.28% Si, 0.010% S, 0.019% P 0.16% Ni, 0.96% Cr, 0.28% Mo
0.36% C, 0.78% Mn, 0.31% Si, 0.73% Ni, 0.49% Mo
0.36% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.85% Ni
0.36% C, 0.80% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.00% Cr, 0.20% Mo
0.36% C, 0.80% Mn, 0.30% Si, 0.75% Ni, 0.02% Mo
0.36% C, 0.82% Mn, 0.35% Si, 1.41% Ni, 0.74% Mo
0.36% C, 0.82% Mn, 0.37% Si, 1.54% Cr, 0.01% Mo
0.36% C, 0.83% Mn, 0.36% Si, 2.60% Ni, 0.49% Mo
0.36% C, 0.83% Mn, 0.38% Si, 0.34% Cr, 0.01% Mo
0.36% C, 0.84% Mn, 0.38% Si, 2.60% Ni, 0.24% Mo
0.36% C, 0.85% Mn, 0.37% Si, 1.52% Cr, 0.50% Mo
0.36% C, 0.86% Mn, 0.37% Si, 2.62% Ni, 0.02% Mo
0.36% C, 0.86% Mn, 0.38% Si, 1.54% Cr, 0.26% Mo
0.36% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.30% V, 1.40% W
0.36% C, 1.20% Mn, 0.20% Si, 0.020% P, 0.020% S
0.36% C, 1.25% Si, 0.90% Mn, 0.010% P, 0.016% S, 1.21% Cr, 0.16% Ni, 0.15% Cu, 0.03% Mo, 0.009% Sn, 0.017% Al
0.36% C, 1.25% Si, 0.90% Mn, 0.010% P, 0.016% S, 1.21% Cr, 0.16% Ni, 0.15% Cu, 0.03% Mo, 0.009% Sn, 0.017% Al
0.36% C, 1.45% Mn, 0.25% Si
0.36% C, 1.45% Ni, 1.10% Cr, 0.27% Mo
0.36% C, 1.46% Mn, 0.42% Si, 0.75% Cr, 0.78% Mo
0.36% C, 1.47% Mn, 0.41% Si, 0.76% Cr, 0.50% Mo
0.36% C, 1.50% Mn, 0.20% Si, 0.020% P, 0.020% S
0.36% C, 1.59% Mn, 0.26% Si, 0.03% S, 0.02% P
0.36% C, 16.0% Cr, 1.2% Mo
0.36% C, 16.00% Cr, 1.20% Mn
0.36% C, 16.00% Cr, 1.20% Mo
0.36% C, 16.00% Cr, 1.20% Mo
0.36-0.42% C, 0.30-0.50% Mn, 0.90-1.20% Si, 4.80-5.50% Cr, 1.10-1.40% Mo, 0.25-0.50% V
0.36-0.42% C, 0.40% Si, 1.15-1.45% Mn, 0.025% P, 0.035% S, 0.0008-0.0050% B
0.36-0.42% C, 0.80-1.20% Si, 0.30-0.50% Mn, <0.015% P, <0.002% S, 4.80-5.20% Cr, 1.10-1.40% Mo, 0.30-0.50% V
0.36-0.42% C, max. 0.40% Si, 1.15-1.45% Mn, max. 0.025% P, max. 0.035% S, 0.0008-0.0050% B
0.36-0.42% C, max. 1.0% Si, nax. 1.0% Mn, max. 0.025% P, max. 0.005% S, 12.50-14.50% Cr
0.36-0.42% C, max. 1.00% Si, max. 1.00% Mn, max. 0.030% P, max. 0.030% S, max. 12.50-14.50% Cr
0.36% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 1.00% Ni, 0.20% Mo
0.36% C, 1.44% Mn, 0.63% Si, 0.17% Cr, 0.13% Ni, 0.02% Mo, 0.09% V, 0.020% Al, 0.022% Ti, 96 ppm N
0.36% C, 1.44% Mn, 0.63% Si, 0.17% Cr, 0.13% Ni, 0.02% Mo, 0.09% V, 0.020% Al, 0.022% Ti, 96 ppm N
0.36% C, 0.99% Mn, 0.2% Cr, 0.04% Mo, 0.29% V, 0.036% S
0.36% C, 0.27% Si, 0.62% Mn, 0.016% P, 0.023% S, 0.98% Cr, 0.21% Mo
0.36% C, 0.90% Mn, 1.90% Cr, 0.50% Ni, 0.50% Mo, + others
0.36% C, 0.30% Si, 1.30% Mn, 1.80% Cr, 1.00% Ni, 0.30% Mo
0.36% C, 16.00% Cr, 1.20% Mo
0.36% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.30% V, 1.40% W
0.36% C, 1.20% Si, 1.21% Mn, 0.017% P, 0.007% S, 0.034% Al, 0.24% Cr, 0.14% Cu, 0.03% Mo, 0.0125% N, 0.19% Ni, 0.03% V
0.36% C, 0.29% Si, 0.69% Mn, 0.011% P, 0.014% S, 0.011% Al, 1.09% Cr, 0.12% Cu, 0.07% Mo, 0.0145% N, 0.08% Ni, 0.01% V
0.36% C, 0.41% Si, 0.53% Mn, 0.023% P, 0.017% S, 0.12% Cu, 0.95% Cr, 2.27% Ni, 0.16% Mo, 0.045% Al
0.37-0.43% C, Cr 0.7-0.9% Cr, 0.7% Mn, 0.23% Si, 0.2-0.3% Mo, 1.83% Ni, max. 0.035% P, max. 0.04% S
0.37-0.43% C, Cr 0.7-0.9% Cr, 0.7% Mn, 0.23% Si, 0.2-0.3% Mo, 1.83% Ni, max. 0.035% P, max. 0.04% S
0.37% C, 0.16% Si, 0.60% Mn, 0.027% P, 0.020% S, 0.005% Al, 0.05% Ni
0.37% C, 0.16% Si, 0.86% Mn, 0.008% P, 0.20% S, 1.74% Cr, 0.21% Ni, 0.21% Cu, 0.21% Mo, 1.12% Al
0.37% C, 0.16% Si, 0.86% Mn, 0.008% P, 0.20% S, 1.74% Cr, 0.21% Ni, 0.21% Cu, 0.21% Mo, 1.12% Al
0.37% C, 0.20% Si, 0.18% Mn, <0.003% P, 0.002% S, 4.83% Cr, 1.23% Mo, 0.06% Ni, 0.44% V, <0.05% W, 0.0038% N, 0.011% Al
0.37% C, 0.20% Si, 0.18% Mn, <0.003% P, 0.002% S, 4.83% Cr, 1.23% Mo, 0.06% Ni, 0.44% V, <0.05% W, 0.0038% N, 0.011% Al
0.37% C, 0.20% Si, 0.74% Mn, 0.011% P, 0.028% S, 0.93% Cr, 2.90% Ni, 0.21% Cu, 0.27% Mo, 0.015% Sn
0.37% C, 0.20% Si, 0.74% Mn, 0.011% P, 0.028% S, 0.93% Cr, 2.90% Ni, 0.21% Cu, 0.27% Mo, 0.015% Sn
0.37% C, 0.22% Si, 0.20% Mn, 4.80% Cr, 2.80% Mo, 0.62% V
0.37% C, 0.24% Si, 0.28% Mn, 0.009% P, 0.009% S, 0.99% Cr, 3.20% Ni, 0.14% V, 0.22% Cu, 0.59% Mo
0.37% C, 0.24% Si, 0.28% Mn, 0.009% P, 0.009% S, 0.99% Cr, 3.20% Ni, 0.14% V, 0.22% Cu, 0.59% Mo
0.37% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S. 37CrS4: 0.37% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.020-0.035% S
0.37% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S. 37CrS4: 0.37% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.020-0.035% S
0.37% C, 0.25% Si, 0.75% Mn, 1.05% Cr
0.37% C, 0.25% Si, 0.75% Mn, 1.05% Cr
0.37% C, 0.25% Si, 0.87% Mn, 0.56% Ni, 0.44% Cr, 0.18% Mo
0.37% C, 0.25% Si, 1.45% Mn
0.37% C, 0.26% Si, 0.19% Mn, 0.006% P, 0.001% S, 1.69% Cr, 0.44% Mo, 3.34% Ni, 0.11% V, 0.012% Al
0.37% C, 0.28% Si, 0.37% Mn, 0.010% S, 0.009% P, 3.79% Ni, 1.49% Cr, 0.38% Mo
0.37% C, 0.34% Mn, 0.94% Si, 0.015% S, 0.02% P 4.80% Cr, 1.19% V
0.37% C, 0.34% Mn, 0.95% Si, 0.008% S, 0.018% P 0.17% Ni, 4.70% Cr, 1.40% Mo, 0.11% Cu, 0.50% V, 1.80% W
0.37% C, 0.34% Mn, 0.95% Si, 0.008% S, 0.018% P 0.17% Ni, 4.70% Cr, 1.40% Mo, 0.11% Cu, 0.50% V, 1.80% W
0.37% C, 0.40% Si, max. 0.003% S, 5.00% Cr, 3.00% Mo, 0.60% V
0.37% C, 0.47% Si, 0.37% Mn, 0.0021% P, 0.003% S, 4.88% Cr, 0.28% Ni, 0.50% V, 0.18% Cu, 2.78% Mo
0.37% C, 0.47% Si, 0.37% Mn, 0.0021% P, 0.003% S, 4.88% Cr, 0.28% Ni, 0.50% V, 0.18% Cu, 2.78% Mo
0.37% C, 0.49% Mn, 0.32% Si, 0.0033% Mo
0.37% C, 0.51% Mn, 1.00% Si, 5.10% Cr, 1.26% Mo, 0.97% V
0.37% C, 0.56% Si, 1.45% Mn, 0.043% S, 0.010% P, 0.04% Cr, 0.025% Mo, 0.11% V, 0.14% Cu, 0.024% Al, 0.015% Ti, 0.0162% N
0.37% C, 0.58% Mn, 0.41% Si, 0.007% S, 0.021% P 0.53% Ni, 16.20% Cr, 1.10% Mo
0.37% C, 0.59% Mn, 0.26% Si, 0.025% S, 0.017% P 2.54% Ni, 0.94% Cr, 0.12% Mo, 0.20% Cu
0.37% C, 0.59% Si, 1.38% Mn, 0.22% Cr, 0.01% Mo, 0.09% V, 0.027% Ti, 0.20% Cu, 0.027% Al
0.37% C, 0.62% Mn, 0.29% Si, 0.032% P, 0.026% S, 1.19% Cr, 0.13% Ni, 0.59% Mo, 0.22% V
0.37% C, 0.68% Mn, 3.41% Ni
0.37% C, 0.68% Mn, 3.41% Ni
0.37% C, 0.69% Mn, 0.33% Si, 0.019% S, 0.017% P 0.06% Ni, 0.04% Cr, 0.05% Mo, 0.013% N2
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.77% Mn, 0.98% Cr, 0.21% Mo
0.37% C, 0.79% Mn, 0.30% Si, 0.010% S, 0.019% P <0.17% Ni, 1.00% Cr, 0.18% Mo, 0.10% Cu
0.37% C, 0.79% Mn, 0.31% Si, 0.74% Ni, 0.24% Mo
0.37% C, 0.80% Mn, 1.47% Si, 0.79% Mo
0.37% C, 0.82% Mn, 0.38% Si, 0.73% Cr, 0.76% Mo
0.37% C, 0.83% Mn, 0.35% Si, 0.006% S, 0.017% P, 0.87% Cr, 1.70% Ni, 1.18% Mo, 0.18% V
0.37% C, 0.84% Mn, 0.36% Si, 1.40% Ni, 0.47% Mo
0.37% C, 0.84% Mn, 0.37% Si, 0.74% Cr, 0.50% Mo
0.37% C, 0.85% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.15% Cr, 0.20% Mo
0.37% C, 0.85% Mn, 0.36% Si, 1.44% Ni, 0.02% Mo
0.37% C, 0.85% Mn, 0.37% Si, 0.74% Cr, 0.02% Mo
0.37% C, 0.85% Mn, 0.37% Si, 1.44% Ni, 0.24% Mo
0.37% C, 0.85% Mn, 0.39% Si, 0.73% Cr, 0.26% Mo
0.37% C, 0.87% Mn, 0.25% Si, 0.56% Ni, 1.44% Cr, 0.18% Mo
0.37% C, 0.89% Mn, 0.28% Si, 1.24% Ni, 0.63% Cr 0.05% Mo
0.37% C, 0.95% Si, 0.34% Mn, 0.018% P, 0.008% S, 4.70% Cr, 0.17% Ni, 1.40% Mo, 0.11% Cu, 0.50% V, 1.80% W
0.37% C, 1.00% Si, 0.40% Mn, 0.001% S, 5.30% Cr, 1.35% Mo, 0.38% V
0.37% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.20% Mo, 0.40% V
0.37% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.25% Si, 1.25% Mn, (Pb)
0.37% C, 1.25% Si, 1.25% Mn, (Pb)
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.25% Si, 1.25% Mn
0.37% C, 1.30% Si, 1.30% Mn
0.37% C, 1.30% Si, 1.30% Mn
0.37% C, 1.35% Mn, 0.24% Si, 0.025% P, 0.025% S, 0.45% Cr, 0.75% Ni, 0.20% Mo
0.37% C, 1.45% Mn, 0.25% Si
0.37% C, 1.49% Mn, 0.41% Si, 0.77% Cr, 0.25% Mo
0.37% C, 1.50% Mn, 0.18% Si, 0.020% P, 0.020% S, 0.27% Mo
0.37% C, 1.93% Mn, 0.35% Si, 1.60% Cr, 0.43% Mo, 0.12% V
0.37% C, 3.70% Ni, 1.80% Cr, 0.30% Mo
0.37% C, 5.00% Cr, 3.00% Mo, 0.60% V
0.37% C, 5.00% Cr, 3.00% Mo, 0.60% V
0.37-0.40% C, max. 0.40% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.0008-0.0050% B
0.37-0.42% C, 0.90-1.20% Si, 0.30-0.50% Mn, max. 0.030% P, 0.080-0.120% S, 5.00-5.50% Cr, 1.20-1.15% Mo, 0.90-1.10% V
0.37-0.43% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.60-0.90% Cr, 0.15-0.30% Mo, 0.70-1.10% Ni
0.37-0.43% C, 0.30-0.50% Mn, 0.90-1.20% Si, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.90-1.10% V
0.37-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, 0.60-0.90% Cr, 0.20-0.30% Mo, 1.60-1.90% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.15-0.30% Mo, 0.40-0.70% Ni
0.37-0.44% C, 0.15-0.40% Si, 0.50-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, 0.15-0.30% Mo, 0.40-0.70% Ni
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.37-0.44% C, max. 0.40% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.0008-0.0050% B
0.37% C, 1% Cr and 0.46% C, 1% Cr
0.37% C, 0.68% Si, 0.88% Mn, 1.89% Cr, 0.42% Mo, 0.002% S, 0.009% P
0.37-0.43% C, Cr 0.7-0.9% Cr, 0.7% Mn, 0.23% Si, 0.2-0.3% Mo, 1.83% Ni, max. 0.035% P, max. 0.04% S
0.37% C, 0.25% Si, 0.25% Mn, 5.00% Cr, 2.48% Mo, 0.51% V, 0.010% P, 0.001% S, 0.006% Al
0.37-0.43% C, 0.30-0.50% Mn, 0.90-1.20% Si, 4.80-5.50% Cr, 1.20-1.50% Mo, 0.90-1.10% V
0.37-0.45% C, max. 0.60% Si, max. 0.60% Mn, 15.00-16.50% Cr, 1.50-1.90% Mo, 0.20-0.40% V, 0.16-0.25% N, max. 0.30% Ni
0.37-0.45% C, max. 0.60% Si, max. 0.60% Mn, 15.00-16.50% Cr, 1.50-1.90% Mo, 0.20-0.40% V, 0.16-0.25% N, max. 0.30% Ni

0.37% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.40% V
0.37% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.40% V
0.37% C, 0.30% Si, 0.40% Mn, 5.00% Cr, 3.00% Mo, 0.60% V
0.37% C, 0.30% Si, 0.64% Mn, 0.010% P, 0.011% S, 0.003% Al, 1.06% Cr, 0.03% Cu, 0.21% Mo, 0.0045% N, 0.03% Ni
0.375% C, 0.248% Si, 1.290% Mn, 0.054% P, 0.019% S, 0.570% Cr, 0.043% Mo, 0.110% Ni, 0.009% Co, 0.238% Cu, 0.005% Nb, 0.012% V, 0.041% Ti, 0.002% Al, 0.004% B
0.38-0.43% C, 0.8% Cr, 0.8% Mn, max. 0.035% P, max. 0.04% S, 0.23% Si
0.38% C, 0.05% Si, 1.46% Mn, 0.007% P, 0.003% S, 1.89% Cr, 0.17% Mo, 0.76% Ni, 0.006% Al
0.38% C, 0.15% Si, 0.56% Mn, 0.005% S, 0.011% P, 2.42% Ni, 0.74% Cr, 0.46% Mo
0.38% C, 0.15% Si, 0.56% Mn, 0.005% S, 0.011% P, 2.42% Ni, 0.74% Cr, 0.46% Mo
0.38% C, 0.15% Si, 0.56% Mn, 0.005% S, 0.011% P, 2.42% Ni, 0.74% Cr, 0.46% Mo
0.38% C, 0.15% Si, 0.56% Mn, 0.011% P, 0.005% S, 2.42% Ni, 0.74% Cr, 0.46% Mo
0.38% C, 0.18% Si, 0.20% Mn, 2.98% Cr
0.38% C, 0.18% Si, 0.87% Mn, 0.021% P, 0.008% S, 1.54% Cr, 0.63% Mo, 0.01% Ni, 0.27% V
0.38% C, 0.20% Si, 0.69% Mn, 0.010% S, 0.017% P, 1.58% Ni, 0.95% Cr, 0.26% Mo
0.38% C, 0.20% Si, 0.69% Mn, 0.017% P, 0.010% S, 1.58% Ni, 0.95% Cr, 0.26% Mo
0.38% C, 0.23% Si, 0.64% Mn, 0.019% P, 0.013% S, 0.99% Cr, 0.17% Cu, 0.16% Mo, 0.08% Ni, <0.01% V
0.38% C, 0.23% Si, 0.64% Mn, 0.019% P, 0.013% S, 0.99% Cr, 0.17% Cu, 0.16% Mo, 0.08% Ni, <0.01% V
0.38% C, 0.23% Si, 1.52% Mn, 0.013% P, 0.023% S, 1.87% Cr, 0.21% Mo, 1.02% Ni, 0.01% V, 0.01% W, 0.015% Cu, 0.008% Al
0.38% C, 0.24% Si, 0.70% Mn, 0.016% P, 0.013% S, 0.91% Cr, 1.38% Ni
0.38% C, 0.25% Si, 0.65% Mn, 0.50% Cr
0.38% C, 0.25% Si, 0.65% Mn, 0.80% Cr, 1.80% Ni, 0.35% Mo, 0.10% V
0.38% C, 0.25% Si, 0.65% Mn, 0.80% Cr, 1.80% Ni, 0.35% Mo, 0.10% V
0.38% C, 0.25% Si, 0.70% Mn, 0.015% P, 0.030% S, 0.063% Al, 0.003% N
0.38% C, 0.25% Si, 1.49% Mn, 0.036% P, 0.028% S, 0.41% Mo
0.38% C, 0.26% Si, 0.74% Mn, 0.010% S, 0.023% P, 0.26% Ni, 0.90% Cr
0.38% C, 0.26% Si, 0.74% Mn, 0.010% S, 0.023% P, 0.26% Ni, 0.90% Cr
0.38% C, 0.26% Si, 0.74% Mn, 0.023% P, 0.010% S, 0.26% Ni, 0.90% Cr, 0.04% Mo, 0.17% Cu
0.38% C, 0.26% Si, 0.74% Mn, 0.023% P, 0.010% S, 0.90% Cr, 0.26% Ni, 0.04% Mo, 0.17% Cu
0.38% C, 0.26% Si, 0.74% Mn, 0.03% P, 0.020-0.010% S, 0.90% Cr, 0.04% Mo, 0.26% Ni, 0.17% Cu
0.38% C, 0.26% Si, 1.51% Mn, 0.40% Ni, 0.99% Cr
0.38% C, 0.27% Si, 0.68% Mn, 0.021% P, 0.028% S, 3.01% Ni, 0.08% Mo, 0.025% Al
0.38% C, 0.30% Si, 0.75% Mn, 2.60% Cr, 2.25% Mo, 0.90% V
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 1.00% Ni, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.07% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.10% Ni
0.38% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.10% Ni
0.38% C, 0.33% Si, 0.29% Mn, 0.007% P, 0.001% S, 1.02% Cr, 3.12% Ni, 0.15% V, 0.22% Cu, 0.50% Mo
0.38% C, 0.33% Si, 0.29% Mn, 0.007% P, 0.001% S, 1.02% Cr, 3.12% Ni, 0.15% V, 0.22% Cu, 0.50% Mo
0.38% C, 0.37% Mn, 0.57% Cr
0.38% C, 0.37% Si, 0.52% Mn, 0.018% P, 0.022% S, 3.23% Cr, 0.44% Mo, 0.08% Ni, 0.58% V, 4.15% W
0.38% C, 0.40% Mn, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 0.40% Mn, 1.00% Si, 5.30% S, 1.30% Mo 0.40% V
0.38% C, 0.40% Mn, 1.00% Si, 5.30% S, 1.30% Mo 0.40% V
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.60% V
0.38% C, 0.40% Si, 0.40% Mn, 5.00% Cr, 2.80% Mo, 0.60% V
0.38% C, 0.40% Si, 0.50% Mn, 5.00% Cr, 3.00% Mo, 0.60% W
0.38% C, 0.40% Si, 0.50% Mn, 5.00% Cr, 3.00% Mo, 0.60% W
0.38% C, 0.40% Si, 1.43% Mn, 0.012% P, 0.017% S, 1.82^ Cr, 0.17% Mo, 0.16% Ni, 0.11%Cu
0.38% C, 0.40% V, 1.00% Si, 5.30% Cr, 1.30% Mo
0.38% C, 0.41% Mn, 0.21% Si, 0.010% S, 0.013% P 0.03% Ni, 1.29% Cr, <0.10% Mo, 0.05% Cu, 0.12% V
0.38% C, 0.41% Mn, 0.21% Si, 0.010% S, 0.013% P 0.03% Ni, 1.29% Cr, <0.10% Mo, 0.05% Cu, 0.12% V
0.38% C, 0.44% Mn, 0.22% Si, 0.003% S, 0.018% P 3.40% Ni, 1.50% Cr, 0.15% Mo, 0.13% Cu, 0.015% V
0.38% C, 0.44% Mn, 0.22% Si, 0.003% S, 0.018% P 3.40% Ni, 1.50% Cr, 0.15% Mo, 0.13% Cu, 0.015% V
0.38% C, 0.45% Mn, 0.40% Si, 5.00% S, 3.00% Mo 0.60% V
0.38% C, 0.45% Mn, 0.40% Si, 5.00% S, 3.00% Mo 0.60% V
0.38% C, 0.46% Mn, 0.26% Si, 0.008% S, 0.019% P, 2.94% Cr, 0.45% Ni, 0.45% Mo, 0.12% V, 0.05% Cu, sol. 0.010% Al
0.38% C, 0.52% Mn, 0.37% Si, 0.022% S, 0.018% P 0.08% Ni, 3.23% Cr, 0.44% Mo, 0.58% V, 4.15% W
0.38% C, 0.56% Mn, 0.15% Si, 0.011% P, 0.005% S, 2.42% Ni, 0.74% Cr, 0.46% Mo
0.38% C, 0.62% Si, 1.44% Mn, 0.041% S, 0.010% P, 0.07% Cr, 0.16% Mo, 0.10% V, 0.07% Cu, 0.026% Al, 0.016% Ti, 0.0122% N
0.38% C, 0.64% Mn, 0.23% Si, 0.99% Cr, 0.08% Ni, 0.16% Mo, 0.01% V, 0.17% Cu
0.38% C, 0.68% Mn, 0.29% Si, 3.48% Ni, 0.48% Mo
0.38% C, 0.68% Si, 1.50% Mn, 0.06% S, 0.022% P, 0.18% Cr, 0.11% V, 0.006% N
0.38% C, 0.69% Mn, 0.20% Si, 1.58% Ni, 0.95% Cr 0.26% Mo
0.38% C, 0.70% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.50% Cr
0.38% C, 0.70% Mn, 0.25% Si, 0.030% S, 0.015% P 0.063% Al, 0.003% N
0.38% C, 0.70% Mn, 0.25% Si, 0.030% S, 0.015% P 0.063% Al, 0.003% N
0.38% C, 0.70% Si, 1.08% Mn, 0.34% Ni, 0.40% Cr, 0.11% Mo, 0.030% Zr
0.38% C, 0.72% Mn, 0.019% P, 0.033% S, 0.21% Si, 1.32% Ni, 0.49% Cr, 0.02% Cu
0.38% C, 0.72% Mn, 0.49% No, 1.32% Ni
0.38% C, 0.72% Mn, 1.32% Ni, 0.49% Cr
0.38% C, 0.72% Mn, 1.32% Ni, 0.49% Cr
0.38% C, 0.72% Mn, 1.32% Ni, 0.49% Cr
0.38% C, 0.74% Mn, 0.26% Si, 0.010% S, 0.023% P 0.26% Ni, 0.90% Cr, 0.04% Mo, 0.17% Cu
0.38% C, 0.74% Mn, 0.26% Si, 0.010% S, 0.023% P 0.26% Ni, 0.90% Cr, 0.04% Mo, 0.17% Cu
0.38% C, 0.78% Mn, 0.29% Si, 0.030% S, 0.005% P, 0.99% Cr, 0.14% Ni, 0.08% Mo, 0.06% V, 0.021% Ti, 0.20% Cu, 0.022% Al
0.38% C, 0.80% Mn, 0.30% Si, 0.025% P, 0.021% S, 0.53% Mo
0.38% C, 0.80% Mn, 1.47% Si, 0.52% Mo
0.38% C, 0.80% Si, 1.48% Mn, 0.18% Cr, 0.04% Mo, 0.10% Ni, 0.01% W, 0.15% Cu, 0.006% Al, 0.0160% N
0.38% C, 0.82% Mn, 0.32% Si, 0.26% Mo
0.38% C, 0.82% Mn, 0.34% Si, 1.46% Ni, 0.75% Cr, 0.78% Mo
0.38% C, 0.82% Mn, 1.48% Si, 0.72% Cr, 0.77% Mo
0.38% C, 0.84% Mn, 0.34% Si, 1.46% Ni, 0.73% Cr, 0.48% Mo
0.38% C, 0.85% Mn, 0.33% Si, 1.46% Ni, 0.74% Cr, 0.01% Mo
0.38% C, 0.85% Mn, 0.35% Si, 1.45% Ni, 0.73% Cr, 0.24% Mo
0.38% C, 0.85% Si, 0.38% Mn, 0.014% P, 0.025% S, 5.16% Cr, 0.19% Ni, 0.40% V, 0.20% Cu, 1.33% Mo
0.38% C, 0.87% Mn, 0.18% Si, 0.008% S, 0.027% P, 1.54% Cr, 0.01% Ni, 0.63% Mo, 0.27% V
0.38% C, 0.9% Si, 0.5% Mn, 13.6% Cr, 0.3% V
0.38% C, 0.9% Si, 0.5% Mn, 13.6% Cr, 0.3% V
0.38% C, 0.99% Cr, 0.16% Mo
0.38% C, 1.0% Si, 0.4% Mn, 5.0% Cr, 1.3% Mo, 0.4% V
0.38% C, 1.0% Si, 5.10% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.0% Si, 5.10% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 0.35% Mn, 5.00% Cr, 1.30% Mo, 0.40% V, patent pending
0.38% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.00% Si, 5.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.05% Si, 1.14% Mn, 0.035% P, 0.019% S, 0.23% Cr, 0.02% V
0.38% C, 1.05% Si, 1.14% Mn, 0.035% P, 0.019% S, 0.23% Cr, 0.02% V
0.38% C, 1.08% Mn, 0.70% Si, 0.34% Ni, 0.40% Cr, 0.11% Mo
0.38% C, 1.14% Mn, 1.05% Si, 0.019% S, 0.035% P, 0.23% Cr, 0.02% V
0.38% C, 1.14% Mn, 1.05% Si, 0.019% S, 0.035% P, 0.23% Cr, 0.02% V
0.38% C, 1.14% Mn, 1.05% Si, 0.019% S, 0.041% P, 0.23% Cr, 0.02% V
0.38% C, 1.37% Si, 0.79% Mn, 0.011% P, 0.022% S, 0.15% Cr, 0.10% Cu, 0.16% Ni, 0.01% V
0.38% C, 1.37% Si, 0.79% Mn, 0.011% P, 0.022% S, 0.15% Cr, 0.10% Cu, 0.16% Ni, 0.01% V
0.38% C, 1.40% Mn, 0.25% Si, 0.030% P, 0.030% S, 0.50% Cr, 0.75% Ni, 0.20% Mo
0.38% C, 1.45% Mn, 0.35% Si, 0.76% Mo
0.38% C, 1.49% Mn, 0.25% Si, 0.036% P, 0.028% S, 0.24% Ni, 0.10% Cr, 0.41% Mo
0.38% C, 1.49% Mn, 0.25% Si, 0.24% Ni, 0.14% Cr 0.41% Mo
0.38% C, 1.50% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.45% Mo
0.38% C, 1.50% Mn, 0.40% Si, 0.77% Cr, 0.02% Mo
0.38% C, 1.63% Mn, 0.30% Si, 0.016% S, 0.018% P, 0.02% Cr, 0.01% Ni, 0.12% Mo, 0.07% V, 0.01% Cu, sol. 0.021% Al
0.38% C, 1.80% Mn, 0.25% Si, 0.025% P, 0.020% S
0.38% C, 16.00% Cr, 1.20% Mo, <1.00% Ni
0.38% C, 16.50% Cr, 1.20% Mo
0.38% C
0.38% C
0.38% C, 0.64% Mn, 0.23% Si, 0.99% Cr, 0.08% Ni, Mo (see the diagram)
0.38-0.42% C, 1.65-1.80% Si, 1.40-1.55% Mn, 0.020% P, 0.002% S, 1.50-1.60% Cr, 0.30% Ni, 0.43-0.47% Mo, 9 ppm O, 30 ppm Ti
0.38-0.43% C, 0.14-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.43% C, 0.14-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.43% C, 0.14-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.43% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.025% P, 0.020% S, 0.70-0.90% Cr, 0.20-0.30% Mo, 1.65-2.00% Ni
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.44% C, 0.30% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.70-0.90% Cr, 0.15-0.30% Mo, 1.65-2.00% Ni, 0.25% Cu
0.38-0.45% C, <0.40% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S, 0.80-1.20% Al, 1.50-1.80% Cr, 0.20-0.35% Mo
0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr. 37CrS4: 0.38-0.45% C, <0.40% Si, 0.60-0.90% Mn, <0.035% P, 0.020-0.040% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, 0.40% Si, 0.40-0.70% Mn, 0.025% P, 0.035% S, 1.50-1.80% Cr, 0.20-0.35% Mo, 0.80-1.20% Al
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.020-0.040% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38-0.45% C, 0.60-0.90% Mn, <0.40% Si, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.60-0.90% Mn, 0.15-0.40% Si, 0.90-1.20% Cr, 0.15-0.25% Mo
0.38-0.45% C, max. 0.40% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.380.43% C, 0.200.35% Si, 0.700.90% Mn, max. 0.040% P, max. 0.040% S, 0.550.75% Cr, 1.101.40% Ni
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.003% S, 2.00% Cr, 0.20% Mo
0.38% C, 0.30% Si, 1.50% Mn, 0.020% P, 0.070% S, 2.00% Cr, 0.20% Mo
0.38% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.30% Mo, 0.40% V
0.38% C, 0.23% Si, 0.64% Mn, 0.019% P, 0.013% S, 0.99% Cr, 0.08% Ni, 0.16% Mo, 0.17% Cu, 0.01% V
0.38% C, 1.56% Mn, 1.10% Cr, 0.98% Ni, 0.09% Si, 0.001% P
0.38% C, 1.44% Mn, 0.62% Si, 0.07% Cr, 0.04% Ni, 0.16% Mo, 0.10% V, 0.026% Al, 0.016% Ti, 122 ppm N
0.38% C, 1.44% Mn, 0.62% Si, 0.07% Cr, 0.04% Ni, 0.16% Mo, 0.10% V, 0.026% Al, 0.016% Ti, 122 ppm N
0.38-0.46% C, 0.15-0.35% Si, 0.75-1.70% Mn, =0.020% P, =0.005% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.46% C, 0.15-0.35% Si, 0.75-1.70% Mn, =0.020% P, =0.005% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.43% C, 0.14-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38% C, 0.73% Si, 0.63% Mn, 0.019% P, 0.013% S, 0.99% Cr, 0.17% Cu, 0.16% Mo, 0.08% Ni, 0.01% V
0.38-0.45% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr
0.38% C, 0.85% Si, 0.38% Mn, 0.014% P, 0.025% S, 5.16% Cr, 0.19% Ni, 0.40% V, 0.20% Cu, 1.33% Mo
0.38-0.43% C, 0.14-0.35% Si, 0.75-1.00% Mn, max. 0.040% P, max. 0.040% S, 0.80-1.10% Cr, 0.15-0.25% Mo
0.38% C, 0.20% Si, 0.55% Mn, 5.00% Cr, 1.75% Mo, 0.55% V, +N.
0.38-0.45% C, max. 0.40% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.38-0.45% C, 0.17-0.37% Si, 0.5-0.8% Mn, 0.9-1.2% Cr, 0.15-0.25% Mo, max. 0.035% S, max. 0.035% P
0.38% C, 0.20% Si, 0.70% Mn, 0.020% P, 0.020% S
0.38% C, 0.23% Si, 0.64% Mn, 0.019% P, 0.013% S, 0.99% Cr, 0.17% Cu, 0.16% Mo, 0.08% Ni, 0.01% V
0.38% C, 1.00% Si, 0.40% Mn, 5.00% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.05% Si, 0.40% Mn, 5.20% Cr, 1.25% Mo, 0.40% V
0.38% C, 5.00% Cr, 3.00% Mo, 0.50% V
0.38% C, 0.40% Si, 0.80% Mn, 1.70% Cr, 0.40% Mo
0.38% C, 0.40% Si, 0.80% Mn, 1.70% Cr, 0.40% Mo
0.38% C, 1.00% Si, 6.30% Cr, 1.30% Mo, 0.40% V
0.38% C, 1.05% Si, 1.14% Mn, 0.041% P, 0.019% S, 0.23% Cr, 0.02% V
0.38% C, 1.05% Si, 1.14% Mn, 0.041% P, 0.019% S, 0.23% Cr, 0.02% V
0.39% C, 0.004% Si, 0.004% Mn, 0.0001% S, 0.001% P, 0.028% Al, 0.0007% N, 0.006% O, 0.007% N
0.39% C, 0.20% Si, 0.86% Mn, 1.12% Ni, 0.13% Cr, 0.05% Mo
0.39% C, 0.21% Si, 1.56% Mn, 0.010% P, 0.024% S
0.39% C, 0.23% Si, 0.62% Mn, 0.021% P, 0.018% S, 1.44% Ni, 1.11% Cr, 0.18% Mo
0.39% C, 0.23% Si, 0.72% Mn, 0.010% P, 0.018% S
0.39% C, 0.26% Si, 0.67% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.49% Mo
0.39% C, 0.27% Si, 0.24% Mn, 0.009% P, 0.001% S, 0.96% Cr, 3.23% Ni, 0.13% V, 0.20% Cu, 0.58% Mo
0.39% C, 0.27% Si, 0.24% Mn, 0.009% P, 0.001% S, 0.96% Cr, 3.23% Ni, 0.13% V, 0.20% Cu, 0.58% Mo
0.39% C, 0.27% Si, 1.58% Mn, 0.05% Ni, 0.16% Cr, 0.44% Mo
0.39% C, 0.28% Mn, 0.20% Si, 8.04% Ni, 3.90% Co, 1.00% Mo
0.39% C, 0.28% Si, 0.27% Mn, 0.007% P, 0.001% S, 0.96% Cr, 3.17% Ni, 0.15% V, 0.22% Cu, 0.59% Mo
0.39% C, 0.28% Si, 0.27% Mn, 0.007% P, 0.001% S, 0.96% Cr, 3.17% Ni, 0.15% V, 0.22% Cu, 0.59% Mo
0.39% C, 0.28% Si, 0.88% Mn, 0.013% P, 0.009% S, 0.86% Cr, 0.23% Ni, 0.162% Mo, 0.19% Cu
0.39% C, 0.29% Mn, 0.22% Si, 7.78% Ni, 3.87% Co, 0.44% Mo
0.39% C, 0.30% Mn, 0.20% Si, 8.00% Ni, 3.89% Co
0.39% C, 0.30% Si, 0.24% Mn, 0.009% P, 0.003% S, 0.97% Cr, 3.03% Ni, 0.15% V, 0.21% Cu, 0.60% Mo
0.39% C, 0.32% Mn, 0.18% Si, 0.48% Mo, 3.72% Co
0.39% C, 0.34% Si, 0.27% Mn, 5.00% Cr, 3.11% Mo, 0.64% V, 0.24% W
0.39% C, 0.37% Si, 0.35% Mn, 0.025% P, 0.023% S, 16.54% Cr, 1.15% Mo, 0.54% Ni
0.39% C, 0.40% Si, 0.43% Mn, 0.010% P, 0.002% S, 1.50% Cr, 0.21% Ni, 0.25% Cu, 0.18% Mo, 0.97% Al
0.39% C, 0.40% Si, 1.46% Mn, 0.012% P, 0.062% S, 1.89% Cr, 0.10% Ni, 0.15% Cu, 0.18% Mo
0.39% C, 0.40% Si, 1.46% Mn, 0.012% P, 0.062% S, 1.89% Cr, 0.10% Ni, 0.15% Cu, 0.18% Mo
0.39% C, 0.45% Mn, 0.58% Si, 0.003% S, 0.018% P, 1.45% Cr, 0.13% Ni, 0.47% Mo, 0.70% V, 0.55% W
0.39% C, 0.48% Mn, 0.94% Si, 0.005% S, 0.013% P, 5.53% Cr, 0.04% Ni, 0.87% Mo, 0.48% V, 0.20% Cu
0.39% C, 0.48% Si, 0.58% Mn, 0.028% P, 0.009% S, 15.63% Cr, 0.93% Mo, 0.72% Ni, 0.05% W, 0.17% Cu, 0.031% Al
0.39% C, 0.48% Si, 0.89% Mn, 0.68% Ni, 0.95% Cr, 0.50% Mo, 0.03% V, 0.002% B
0.39% C, 0.55% Mn, 0.30% Si, 0.020% P, 0.020% S, 1.60% Cr, 0.20% Mo, 1.10% Al
0.39% C, 0.56% Mn, 3.53% Ni, 0.74% Mo
0.39% C, 0.56% Mn, 3.53% Ni, 0.74% Mo
0.39% C, 0.58% Si, 0.45% Mn, 0.018% P, 0.003% S, 1.45% Cr, 0.47% Mo, 0.13% Ni, 0.70% V, 0.55% W
0.39% C, 0.58% Si, 0.45% Mn, 0.018% P, 0.003% S, 1.45% Cr, 0.47% Mo, 0.13% Ni, 0.70% V, 0.55% W
0.39% C, 0.60% Mn, 0.15% Si, 0.020% P, 0.020% S, 3.25% Cr, 0.20% Ni, 0.95% Mo, 0.20% V
0.39% C, 0.62% Mn, 0.23% Si, 1.44% Ni, 1.11% Cr 0.18% Mo
0.39% C, 0.62% Si, 1.30% Mn, 0.016% P, 0.013% S, 0.11% V, 0.025% Al
0.39% C, 0.69% Mn, 0.29% Si, 3.56% Ni, 0.24% Mo
0.39% C, 0.70% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.05% Cr
0.39% C, 0.71% Mn, 0.39% Si, 3.53% Ni, 0.02% Mo
0.39% C, 0.72% Mn, 0.23% Si, 0.010% P, 0.018% S
0.39% C, 0.72% Mn, 0.23% Si, 0.018% S, 0.010% P
0.39% C, 0.73% Mn, 0.35% Si, 2.51% Ni, 0.75% Cr, 0.49% Mo
0.39% C, 0.75% Mn, 0.26% Si, 0.033% S, 0.008% P, 0.94% Cr, 0.19% Ni, 0.03% Mo, 0.003% V, 0.007% Ti, 0.21% Cu, 0.01% N
0.39% C, 0.76% Mn, 0.28% Si, 0.033% S, 0.007% P, 0.99% Cr, 0.14% Ni, 0.03% Mo, 0.12% V, 0.047% Ti, 0.21% Cu, 0.01% Al
0.39% C, 0.77% Mn, 0.39% Si, 0.032% S, 0.006% P, 0.96% Cr, 0.14% Ni, 0.08% Mo, 0.05% V, 0.21% Cu, 0.01% N
0.39% C, 0.80% Mn, 1.48% Si, 0.26% Mo
0.39% C, 0.82% Mn, 0.26% Si, 1.00% Cr, 0.21% Mo
0.39% C, 0.84% Mn, 1.49% Si, 0.74% Cr, 0.73% Mo
0.39% C, 0.86% Mn, 0.72% Cr, and 0.97% Ni
0.39% C, 0.89% Mn, 0.68% Ni, 0.95% Cr, 0.50% Mo, 0.48% Si, 0.03% V, 0.002% B
0.39% C, 0.94% Si, 0.48% Mn, 0.013% P, 0.005% S, 5.53% Cr, 0.20% Cu, 0.87% Mo, 0.04% Ni, 0.48% V
0.39% C, 0.94% Si, 0.48% Mn, 0.013% P, 0.005% S, 5.53% Cr, 0.20% Cu, 0.87% Mo, 0.04% Ni, 0.48% V
0.39% C, 0.94% Si, 0.48% Mn, 0.013% P, 0.005% S, 5.53% Cr, 0.87% Mo, 0.04% Ni, 0.48% V, 0.20% Cu
0.39% C, 0.97% Si, 0.43% Mn, 0.015% P, 0.006% S, 5.01% Cr, 1.14% Mo, 0.21% Ni, 0.35% V
0.39% C, 0.97% Si, 0.43% Mn, 0.015% P, 0.006% S, 5.01% Cr, 1.14% Mo, 0.21% Ni, 0.35% V
0.39% C, 1.00% Si, 0.38% Mn, 5.15% Cr, 1.00% V, 1.35% Mo
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V. DIEVAR: 0.35% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.60% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.40% Mn, 5.30% Cr, 1.30% Mo, 0.90% V
0.39% C, 1.00% Si, 0.48% Mn, 0.03% P, 0.01% S, 5.15% Cr, 1.40% Mo, 0.88% V
0.39% C, 1.10% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.95% V, <0.003% S
0.39% C, 1.10% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.95% V, <0.003% S
0.39% C, 1.39% Mn, 1.48% Si, 0.73% Cr, 0.77% Mo
0.39% C, 1.41% Mn, 1.49% Si, 0.74% Cr, 0.51% Mo
0.39% C, 1.45% Mn, 0.37% Si, 0.49% Mo
0.39% C, 1.46% Mn, 0.36% Si, 0.03% Mo
0.39% C, 1.56% Mn, 0.21% Si, 0.010% P, 0.024% S
0.39% C, 1.56% Mn, 0.21% Si, 0.024% S, 0.010% P
0.39% C, 1.67% Mn, less then 0.10% Ni
0.39% C, 17.00% Cr, 1.00% Mo, <1.00% V
0.39% C, 1.58% Mn, 1.02% Cr, 0.28% Mo, 0.09% Si, 0.001% Al, 0.01% P
0.39% C, 1.56% Mn, 0.21% Si, 0.24% S, 0.010% P
0.39% C, 16.50% Cr, 1.10% Mo
0.39% C, 0.25% Si, 0.90% Mn, 1.00% Cr, 0.20% Mo
0.39% C, 0.47% Si, 0.46% Mn, 0.027% P, 0.025% S, 16.40% Cr, 1.16% Mo, 0.41% Ni, 0.06% W
0.39% C, 0.31% Si, 0.87% Mn, 0.024% P, 0.025% S, 0.037% Al, 0.46% Cr, 0.01% Mo, 0.0112% N, 0.01% Ni, 0.01% V
0.39% C, 0.26% Si, 1.67% Mn, 0.025% P, 0.022% S, 0.14% Cu, 0.25% Cr, 0.09% Ni, 0.04% Mo, 0.01% Ti, 0.003% Al, 0.09% V
0.4% C, 0.3% Si, max. 1.50% Mn, max. 0.005% S, 0.012% P, 1.90% Cr, 0.20% Mo, 1.0% Ni.
0.4% C, 0.3% Si, max. 1.50% Mn, max. 0.005% S, 0.012% P, 1.90% Cr, 0.20% Mo.
0.4% C, 0.3% Si, max. 1.50% Mn, max. 0.005% S, 0.012% P, 1.90% Cr, 0.20% Mo.
0.4% C, 0.60% Mn, 3.51% Ni, 0.21% Mo
0.4% C, 1.0% Si, 5.3% Cr, 1.4% Mo, 1.0% V
0.4% C, 1.0% Si, max. 0.003% S, 5.3% Cr, 1.4% Mo, 1.0% V
0.4% C, 1.5% Mn, <0.005% S, 1.9% Cr, 0.2% Mo, 1.0% Ni, + Ca
0.4% C, 1.5% Mn, 1.9% Cr, 0.2% Mo
0.4% C, 1.88% Mn
0.40% C, 0.20% Si, 0.35% Mn, 0.010% P, 0.015% S, 1.27% Cr, 0.18% Cu, 0.24% Mo, 4.03% Ni, 0.04% V
0.40% C, 0.20% Si, 0.35% Mn, 0.010% P, 0.015% S, 1.27% Cr, 0.18% Cu, 0.24% Mo, 4.03% Ni, 0.04% V
0.40% C, 0.20% Si, 0.56% Mn, 0.011% P, 0.029% S, 1.57% Cr, 0.23% Ni, 0.25% Cu, 0.20% Mo, 0.96% Al
0.40% C, 0.20% Si, 0.56% Mn, 0.011% P, 0.029% S, 1.57% Cr, 0.23% Ni, 0.25% Cu, 0.20% Mo, 0.96% Al
0.40% C, 0.21% Si, 1.34% Mn, 0.028% P, 0.027% S, 1.03% Ni, 0.53% Cr, 0.22% Mo, 0.08% Cu
0.40% C, 0.24% Mo
0.40% C, 0.24% Si, 0.58% Mn, 0.010% P, 0.030% S, 1.07% Cr, 0.15% Ni, 0.01% V, 0.18% Cu, 0.23% Mo
0.40% C, 0.24% Si, 1.38% Mn, 0.031% S, 0.033% P, 0.74% Ni, 0.53% Cr, 0.16% Mo
0.40% C, 0.24% Si, 1.38% Mn, 0.031% S, 0.033% P, 0.74% Ni, 0.53% Cr, 0.16% Mo
0.40% C, 0.24% Si, 1.38% Mn, 0.031% S, 0.033% P, 0.74% Ni, 0.53% Cr, 0.16% Mo, 0.00% Cu
0.40% C, 0.24% Si, 1.38% Mn, 0.031% S, 0.033% P, 0.74% Ni, 0.53% Cr, 0.16% Mo
0.40% C, 0.24% Si, 1.38% Mn, 0.033% P, 0.031% S, 0.74% Ni, 0.53% Cr, 0.16% Mo
0.40% C, 0.25% Si, 0.25% Mn, 0.011% P, 0.009% S, 1.58% Cr, 4.35% Ni
0.40% C, 0.25% Si, 0.40% Mn, 1.55% Cr, 4.55% Ni, 0.50% Mo
0.40% C, 0.25% Si, 0.40% Mn, 1.55% Cr, 4.55% Ni, 0.50% Mo
0.40% C, 0.25% Si, 0.40% Mn, 1.65% Cr, 4.35% Ni
0.40% C, 0.25% Si, 0.40% Mn, 1.65% Cr, 4.35% Ni
0.40% C, 0.26% Si, 0.34% Mn, 0.032% P, 0.010% Si, 2.85% Cr, 0.12% Ni, 0.16% Mo, 0.14% Cu, 0.26% V, 3.39% W
0.40% C, 0.26% Si, 0.62% Mn, 0.005% S, 0.007% P, 3.45% Ni, 0.28% Cr, 0.10% Mo
0.40% C, 0.26% Si, 0.62% Mn, 0.005% S, 0.007% P, 3.45% Ni, 0.28% Cr, 0.10% Mo
0.40% C, 0.26% Si, 0.62% Mn, 0.005% S, 0.007% P, 3.45% Ni, 0.28% Cr, 0.10% Mo
0.40% C, 0.26% Si, 0.62% Mn, 0.005% S, 0.007% P, 3.45% Ni, 0.28% Cr, 0.10% Mo
0.40% C, 0.26% Si, 0.71% Mn, 0.019% P, 0.028% S, 3.00% Ni, 0.32% Mo, 0.025% Al
0.40% C, 0.28% Si, 0.68% Mn, 0.011% P, 0.005% S, 0.76% Cr, 1.76% Ni, 0.01% V
0.40% C, 0.29% Si, 0.62% Mn, 0.009% S, 0.012% P, 0.21% Ni, 3.49% Cr, 0.97% Mo, 0.26% V
0.40% C, 0.30% Mn, 0.90% Si, 4.80% S, 1.20% Mo 0.90% V
0.40% C, 0.30% Mn, 0.90% Si, 4.80% S, 1.20% Mo 0.90% V
0.40% C, 0.30% Si, 0.29% Mn, 0.027% P, 0.016% S, 15.39% Cr, 0.34% Ni, 0.08% V, 0.17% Cu, 1.12% Mo, 0.03% Co, 0.015% Al
0.40% C, 0.30% Si, 0.29% Mn, 0.027% P, 0.016% S, 15.39% Cr, 0.34% Ni, 0.08% V, 0.17% Cu, 1.12% Mo, 0.03% Co, 0.015% Al
0.40% C, 0.30% Si, 0.29% Mn, 0.027% P, 0.016% S, 15.39% Cr, 0.34% Ni, 0.08% V, 0.17% Cu, 1.12% Mo, 0.03% Co, 0.015% Al
0.40% C, 0.30% Si, 0.40% Mn, 4.50% Co, 4.5% Cr, 0.50% Mo, 2.10% V, 4.50% W
0.40% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 0.50% Mo, 2.10% V, 4.50% W, 4.50% Co
0.40% C, 0.30% Si, 0.61% Mn, 0.005% P, 0.007% S, 0.78% Cr, 0.35% Mo, 1.81% Ni, 0.090% V
0.40% C, 0.30% Si, 0.61% Mn, 0.005% P, 0.007% S, 0.78% Cr, 0.35% Mo, 1.81% Ni, 0.090% V
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.30% Si, 0.90% Mn, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, max. 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.30% Si, 1.50% Mn, max. 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
0.40% C, 0.32% Si, 0.69% Mn, 0.018% P, 0.028% S, 2.99% Ni, 0.18% Mo, 0.025% Al
0.40% C, 0.33% Mn, 0.16% Si, 0.95% Mo, 3.90% Co
0.40% C, 0.34% Mn, 0.17% Si, 0.01% Mo, 3.76% Co
0.40% C, 0.34% Mn, 0.26% Si, 0.010% S, 0.032% P 0.12% Ni, 2.85% Cr, 0.16% Mo, 0.14% Cu, 0.26% V, 3.39% W
0.40% C, 0.35% Mn, 0.20% Si, 0.015% S, 0.010% P, 1.27% Cr, 4.03% Ni, 0.24% Mo, 0.04% V, 0.16% Cu
0.40% C, 0.35% Mn, 0.90% Si, 5.00% Cr, 1.35% Mo, 0.45% V
0.40% C, 0.35% Mn, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V, Cr/C=13.3, Mo/C=3.5, V/C=2.5
0.40% C, 0.35% Si, 1.00% Mn
0.40% C, 0.35% Si, 1.00% Mn
0.40% C, 0.35% Si, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.05% S
0.40% C, 0.40% Mn, 1.00% Si, 5.25% Cr, 1.35% Mo, 1.00% V
0.40% C, 0.40% Si, 1.45% Mn, 2.00% Cr, 0.20% Mo
0.40% C, 0.42% Mn, 0.59% Mo
0.40% C, 0.42% Mo, 0.53% Mo
0.40% C, 0.45% Mn, 0.017% P, 0.009% S, 0.18% Si, 3.33% Ni, 1.52% Cr, 0.03% Mo
0.40% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.40% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.40% C, 0.48% Mn, 0.15% Si, 0.016% P, 0.040% S, 0.15% Cr, 0.25% Mo, 1.75% Ni
0.40% C, 0.48% Mn, 1.01% Si, 0.01% S, 0.014% P 0.36% Ni, 5.13% Cr, 1.72% Mo, 0.50% V, 0.25% W, 0.13% Cu, 0.015% Al, 0.11% Co
0.40% C, 0.52% Mn, 5.00% Ni
0.40% C, 0.52% Mn, 5.00% Ni
0.40% C, 0.53% Si, 0.56% Mn, 0.001% S, 0.012% P, 0.21% Ni, 1.65% Cr, 0.23% Mo, 1.10% Al
0.40% C, 0.53% Si, 0.56% Mn, 0.001% S, 0.012% P, 0.21% Ni, 1.65% Cr, 0.23% Mo, 1.10% Al
0.40% C, 0.53% Si, 0.56% Mn, 0.012% P, 0.001% S, 1.65% Cr, 0.23% Mo, 0.21% Ni, 0.15% Cu, 1.10% Al
0.40% C, 0.56% Mn, 0.53% Si, 0.001% S, 0.012% P 0.21% Ni, 1.65% Cr, 0.23% Mo, 0.15% Cu, 1.10% Al
0.40% C, 0.56% Mn, 0.53% Si, 0.001% S, 0.012% P 0.21% Ni, 1.65% Cr, 0.23% Mo, 0.15% Cu, 1.10% Al
0.40% C, 0.57% Mn, 3.49% Ni, 0.01% Mo
0.40% C, 0.57% Mn, 3.49% Ni, 0.01% Mo
0.40% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.65% Cr, 2.55% Ni, 0.55% Mo
0.40% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.20% Cr, 1.50% Ni, 0.30% Mo
0.40% C, 0.60% Mn, 0.25% Si, 0.020% P, 0.025% S, 1.20% Cr, 1.50% Ni, 0.15% Mo
0.40% C, 0.60% Mn, 1.00% Si, 0.003% S, 0.010% P, 5.00% Cr, 1.30% Mo, 0.40% V
0.40% C, 0.60% Mn, 1.00% Si, 0.003% S, 0.010% P, 5.00% Cr, 1.30% Mo, 0.40% V
0.40% C, 0.65% Mn, 0.25% Si, 0.020% P, 0.025% S, 0.75% Cr, 0.85% Ni, 0.25% Mo
0.40% C, 0.70% Mn, 0.31% Si, 0.010% P, 0.026% S, 0.16% Ni, 1.11% Cr, 0.16% Mo, 0.15% Cu
0.40% C, 0.72% Mn, 0.40% Si, 0.78% Ni, 0.75% Cr, 0.50% Mo
0.40% C, 0.73% Mn, 0.38% Si, 2.58% Ni, 0.75% Cr, 0.24% Mo
0.40% C, 0.73% Mn, 0.40% Si, 0.78% Ni, 0.75% Cr, 0.27% Mo
0.40% C, 0.73% Mn, 0.41% Si, 4.53% Ni, 0.75% Cr, 0.50% Mo
0.40% C, 0.74% Mn, 0.31% Si, 3.56% Ni, 0.77% Cr, 0.50% Mo
0.40% C, 0.74% Mn, 0.36% Si, 4.40% Ni, 0.47% Mo
0.40% C, 0.74% Mn, 0.38% Si, 2.57% Ni, 0.75% Cr, 0.03% Mo
0.40% C, 0.74% Mn, 0.40% Si, 0.78% Ni, 0.75% Cr, 0.03% Mo
0.40% C, 0.75% Mn, 0.23% Si, 0.020% P, 0.020% S, 0.65% Cr, 1.30% Ni
0.40% C, 0.75% Mn, 0.27% Si, 0.034% S, 0.007% P, 0.96% Cr, 0.13% Ni, 0.07% Mo, 0.06% V, 0.035% Ti, 0.20% Cu, 0.01% Al
0.40% C, 0.75% Mn, 0.35% Si, 4.43% Ni, 0.25% Mo
0.40% C, 0.78% Mn, 0.22% V, 1.25% Cr, 0.53% Mo
0.40% C, 0.78% Mn, 1.25% Cr, 0.53% Mo, 0.22% V
0.40% C, 0.80% Mn, 0.30% Si, 0.025% P, 0.020% S, 0.26% Mo
0.40% C, 0.80% Mn, 0.33% Si, 0.019% S, 0.018% P 0.58% Ni, 0.56% Cr, 0.28% Mo, 0.10% Cu
0.40% C, 0.80% Mn, 0.33% Si, 0.019% S, 0.018% P 0.58% Ni, 0.56% Cr, 0.28% Mo, 0.10% Cu
0.40% C, 0.80% Mn, 0.33% Si, 0.79% Mo
0.40% C, 0.80% Mn, 0.35% Si, 0.035% P, 0.007% S, 16.00% Cr, 1.03% Mo
0.40% C, 0.80% Si, 0.35% Mn, 0.010% P, 0.015% S, 1.27% Cr, 0.16% Cu, 0.24% Mo, 4.03% Ni, 0.04% V
0.40% C, 0.80% Si, 0.35% Mn, 0.010% P, 0.015% S, 1.27% Cr, 0.16% Cu, 0.24% Mo, 4.03% Ni, 0.04% V
0.40% C, 0.81% Mn, 1.48% Si, 0.02% Mo
0.40% C, 0.82% Mn, 0.35% Si, 0.53% Mo
0.40% C, 0.83% Mn, 0.33% Si, 0.007% S, 0.011% P, 1.00% Cr, 1.75% Ni, 0.46% Mo, 0.12% V, 0.07% Cu, sol. 0.010% Al
0.40% C, 0.83% Mn, 0.34% Si, 0.01% Mo
0.40% C, 0.84% Mn, 1.50% Si, 0.74% Cr, 0.02% Mo
0.40% C, 0.84% Mn, 1.50% Si, 0.74% Cr, 0.26% Mo
0.40% C, 0.85% Mn, 0.20% Si, 0.020% P, 0.020% S, 1.05% Cr, 0.30% Mo
0.40% C, 0.85% Mn, 1.75% Si, 0.030% P, 0.030% S
0.40% C, 0.87% Mn, 0.36% Si, 0.34% Cr, 0.25% Mo
0.40% C, 0.88% Si, 0.36% Mn, 0.12% Ni, 4.75% Cr, 1.24% Mo, 0.56% V
0.40% C, 0.88% Si, 0.36% Mn, 0.12% Ni, 4.75% Cr, 1.24% Mo, 0.560% V
0.40% C, 0.89% Mn, 0.021% P, 0.011% S, 0.31% Si, 3.34% Ni, 0.11% Cr
0.40% C, 0.89% Mn, 0.31% Si, 0.021% P, 0.011% S 2.34% Ni, 0.11% Cr
0.40% C, 0.90% Mn, 0.35% Si, 0.030% P, 0.005% S, 16.00% Cr, 1.00% Mo
0.40% C, 1.00% Mn, 0.05% P, 0.08% S, 0.10% Mo
0.40% C, 1.00% Mn, 1.40% Si, 0.40% Mo, 0.80% Cr
0.40% C, 1.00% Mn, 1.40% Si, 0.40% Mo, 0.80% Cr
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 0.40% Mn, 5.20% Cr, 1.30% Mo, 1.00% V
0.40% C, 1.00% Si, 5.00% Cr, 1.30% Mo, 1.20% V
0.40% C, 1.00% Si, 5.00% Cr, 1.30% Mo, 1.20% V
0.40% C, 1.00% Si, 5.25% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 0.10% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.00% Si, max. 0.020% P, max. 0.030$ S, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.05% Si, 5.00% Cr, 1.35% Mo, 0.35% V
0.40% C, 1.05% Si, 5.00% Cr, 1.35% Mo, 0.35% V
0.40% C, 1.05% Si, 5.00% Cr, 1.35% Mo, 1.10% V
0.40% C, 1.05% Si, 5.00% Cr, 1.35% Mo, 1.10% V
0.40% C, 1.05% Si, 5.00% Cr, 1.35% Mo, 1.10% V
0.40% C, 1.15% Si, 5.25% Cr, 4.25% W
0.40% C, 1.15% Si, 5.25% Cr, 4.25% W
0.40% C, 1.30% Mn, 1.85% Cr, 0.22% Mo. Steel 2: 0.35-0.40% C, 1.40-1.60% Mn, 1.80-2.00% Cr, 0.15-0.20% Mo, 30 ppm B
0.40% C, 1.32% Mn, 0.33% Si, 0.004% Mo, 0.004% B
0.40% C, 1.33% Mn, 0.35% Si, 0.08% Mo, 0.003% B
0.40% C, 1.33% Mn, 0.36% Si, 0.18% Mo, 0.003% B
0.40% C, 1.34% Mn, 0.21% Si, 1.03% Ni, 0.53% Cr 0.22% Mo
0.40% C, 1.37% Mn, 1.38% Si, 1.31% Ni, 0.75% Cr, 0.73% Mo
0.40% C, 1.38% Mn, 1.50% Si, 0.80% Mo
0.40% C, 1.39% Mn, 1.37% Si, 1.34% Ni, 0.76% Cr, 0.52% Mo
0.40% C, 1.40% Mn, 1.51% Si, 0.53% Mo
0.40% C, 1.43% Mn, 1.51% Si, 0.76% Cr, 0.26% Mo
0.40% C, 1.47% Mn, 0.37% Si, 0.26% Mo
0.40% C, 1.50% Mn, 0.05% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.07% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.30% Si, 0.012% P, 0.005% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.30% Si, 0.012% P, 0.005% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.30% Si, 0.012% P, 0.005% S, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 0.30% Si, 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 0.30% Si, 0.012% P, 0.060% S, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.17% Mo, 0.08% V, max. 0.00% V
0.40% C, 1.50% Mn, 1.90% Cr, 0.17% Mo, 0.08% V, max. 0.00% V
0.40% C, 1.50% Mn, 1.90% Cr, 0.17% Mo, 0.08% V
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.005% S
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.05% S
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.05% S
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.05% S
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.50% Mn, 2.00% Cr, 0.25% Mo, 1.00% Ni
0.40% C, 1.50% Si, 0.70% Mn, 1.10% Cr, 0.80% Mo, 0.10% V
0.40% C, 1.76% Mn, 0.41% Si, 0.016% P, 0.008% S, 9.82% Ni, 20.95% Cr
0.40% C, 1.76% Mn, 0.41% Si, 0.016% P, 0.008% S, 9.82% Ni, 20.95% Cr
0.40% C, 1.76% Mn, 0.41% Si, 0.016% P, 0.008% S, 9.82% Ni, 20.95% Cr
0.40% C, 1.76% Mn, 0.41% Si, 0.016% P, 0.008% S, 9.82% Ni, 20.95% Cr
0.40% C, 1.88% Mn
0.40% C, 13.00% Cr
0.40% C, 13.00% Cr
0.40% C, 14.00% Cr
0.40% C, 14.00% Cr
0.40% C, 14.50% Cr, 0.30% Mo
0.40% C, 2.50% Si, 0.00% Mn, 10.00% Cr, 1.00% Mo
0.40% C, 3.00% Cr, 1.00% Mo, 0.20% V
0.40% C, 5.00% Cr, 1.30% Mo, 0.40% V
0.40% C, 5.00% Cr, 3.00% Mo, 0.50% V
0.40% C, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, max. 1.00% Si, max. 1.00% Mn, 16.00% Cr, 1.20% Mo, max. 1.00% Ni
0.40-0.46% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S
0.40-0.46% C, 0.15-0.40% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S
0.40-0.46% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu, max. 0.050% Al
0.40-0.46% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu, max. 0.050% Al
0.40-0.50% C, 0.10-0.40% Si, 0.20-0.50% Mn, <0.030% P, <0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.10-0.40% Si, 0.20-0.50% Mn, max. 0.030% P, max. 0.030% S, 1.20-1.50% Cr, 0.15-0.35% Mo, 3.80-4.30% Ni
0.40-0.50% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 1.30-1.60% Cr, 0.25-0.35% V, 0.65-0.85% Mo
0.40-0.50% C, 0.15-0.45% Mn, 0.10-0.40% Si, 1.20-1.50% Cr, 0.15-0.35% Mo, 0.00% Al, 3.80-4.30% Ni
0.40-0.50% C, 0.30-0.50% Si, 0.30-0.50% Mn, max. 0.025% P, max. 0.025% S, 4.00-5.00% Cr, 0.40-0.60% Mo, 4.00-5.00% W, 1.80-2.10% V, 4.00-5.00% Co
0.40-0.50% C, 0.80-1.10% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.80-2.10% W, 0.15-0.20% V
0.40-0.50% C, 0.80-1.10% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.80-2.10% W, 0.15-0.20% V
0.40% C, 1.05% Si, 0.40% Mn, 0.025% P, 0.003% S, 5.20% Cr, 1.40% Mo, 1.00% V
0.40% C, 1.80% Ni, 0.80% Cr, 0.25% Mo
0.40% C, 5.00% Cr, 1.30% Mo, 0.50% V
0.4% C, 0.3% Si, 0.2% Mo, 1.0% Ni, 1.9% Cr, max. 0.012% P, max. 0.005% S
0.4% C, 0.3% Si, 0.2% Mo, 1.0% Ni, 1.9% Cr, max. 0.012% P, max. 0.005% S
0.40% C, 0.20% Si, 0.50% Mn, 12.00% Cr, 2.30% Mo, 0.50% V, +N
0.40% C, 13.50% Cr
0.40% C, 13.00% Cr
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo
0.40% C, 1.50% Mn, 1.90% Cr, 0.20% Mo, 0.05% S
0.40% C, 1.50% Mn, 1.90% Cr, 1.00% Ni, 0.20% Mo
0.40% C, 1.00% Si, 5.30% Cr, 1.40% Mo, 1.00% V
0.40% C, 0.24% Si, 0.73% Mn, 0.025% P, 1.05% Cr, 0.16% Ni, 0.16% Cu
0.40-0.46% C, 1.45-1.80% Si, 0.65-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.70-0.95% Cr, 1.65-2.00% Ni, 0.30-0.45% Mo, max. 0.050% V
0.40-0.46% C, 1.45-1.80% Si, 0.65-0.90% Mn, max. 0.035% P, max. 0.040% S, 0.70-0.95% Cr, 1.65-2.00% Ni, 0.30-0.45% Mo, max. 0.050% V
0.40% C, 1.06% Si, 0.38% Mn, 0.011% P, 0.005% S, 5.12% Cr, 0.20% Cu, 1.39% Mo, 0.04% Ni, 0.52% V
0.40% C, 1.06% Si, 0.38% Mn, 0.011% P, 0.005% S, 5.12% Cr, 0.20% Cu, 1.39% Mo, 0.04% Ni, 0.52% V
0.40% C, 0.72% Si, 0.27% Mn, 1.20% Cr, 1.85% W, 0.17% Ni
0.40% C, 0.60% Si, 0.05% Mn, 0.005% P, 0.024% S
0.40% C, 0.41% Si, 0.73% Mn, 0.023% P, 0.007% S, 0.26% Cu, 0.15% Cr, 0.10% Ni, 0.05% Mo, 0.034% V
0.403% C, 0.64% Mn, 0.26% Si, 0.06% Cr, 0.02% Ni, 0.002% Ti, 0.0002% B
0.403% C, 0.64% Mn, 0.26% Si, 0.06% Cr, 0.02% Ni, 0.002% Ti, 0.0002% B
0.41% C, 0.09% Si, 0.48% Mn, 0.016% P, 0.043% S, 1.75% Ni, 0.17% Cr, 0.22% Mo
0.41% C, 0.13% Si, 0.48% Mn, 0.043% S, 0.016% P, 1.75% Ni, 0.17% Cr, 0.22% Mo
0.41% C, 0.13% Si, 0.48% Mn, 0.043% S, 0.016% P, 1.75% Ni, 0.17% Cr, 0.22% Mo
0.41% C, 0.13% Si, 0.48% Mn, 0.043% S, 0.016% P, 1.75% Ni, 0.17% Cr, 0.22% Mo
0.41% C, 0.21% Si, 0.28% Mn, 0.009% P, 0.002% S, 0.91% Cr, 3.19% Ni, 0.14% V, 0.21% Cu, 0.58% Mo
0.41% C, 0.23% Si, 0.67% Mn, 0.015% P, 0.016% S, 0.20% Ni, 1.01% Cr, 0.23% Mo
0.41% C, 0.23% Si, 0.67% Mn, 0.016% S, 0.015% P, 0.20% Ni, 1.01% Cr, 0.23% Mo
0.41% C, 0.23% Si, 0.69% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.29% Mo
0.41% C, 0.25% Si, 0.65% Mn, 1.05% Cr
0.41% C, 0.25% Si, 0.65% Mn, 1.05% Cr
0.41% C, 0.25% Si, 0.71% Mn, 0.031% P, 0.024% S, 1.06% Cr, 0.17% Cu, 0.02% Mo, 0.22% Ni, <0.01% V
0.41% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.41% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.41% C, 0.25% Si, 0.82% Mn, 0.015% P, 0.22% S, 1.64% Cr, 0.15% Ni, 0.24% Cu, 0.28% Mo, 1.26% Al
0.41% C, 0.25% Si, 0.82% Mn, 0.015% P, 0.22% S, 1.64% Cr, 0.15% Ni, 0.24% Cu, 0.28% Mo, 1.26% Al
0.41% C, 0.26% Si, 0.86% Mn, 0.71% Cr, 1.28% Ni
0.41% C, 0.26% Si, 0.86% Mn, 1.28% Ni, 0.71% Cr
0.41% C, 0.27% Si, 0.48% Mn, 1.68% Ni, 1.05% Cr
0.41% C, 0.28% Si, 0.58% Mn, 0.036% S, 0.028% P, 0.15% Ni, 0.39% Cr, 0.74% Mo
0.41% C, 0.28% Si, 0.70% Mn, 0.019% P, 0.030% S, 3.02% Ni, 0.020% Al
0.41% C, 0.28% Si, 0.87% Mn, 1.83% Ni, 0.72% Cr, 0.20% Mo
0.41% C, 0.30% Mn, 0.36% Si, 0.006% S, 0.017% P 4.80% Ni, 0.54% Cr, 1.13% Mo, 0.52% V
0.41% C, 0.33% Si, 1.40% Mn, 0.027% P, 0.067% S, 1.87% Cr, 0.13% Ni, 0.17% Cu, 0.18% Mo, 0.014% Sn
0.41% C, 0.33% Si, 1.40% Mn, 0.027% P, 0.067% S, 1.87% Cr, 0.13% Ni, 0.17% Cu, 0.18% Mo, 0.014% Sn
0.41% C, 0.33% Si, 1.40% Mn, 0.027% P, 0.067% S, 1.87% Cr, 0.13% Ni, 0.17% Cu, 0.18% Mo, 0.014% Sn
0.41% C, 0.336% Si, 0.701% Mn, 0.011% P, 0.025% S, 0.998% Cr, 0.380% Cu, 0.171% Mo, 0.191% Ni, 0.029% Al, 0.019% Nb
0.41% C, 0.35% Mn, 1.00% Si, 5.35% Cr, 1.40% Mo, 0.90% V
0.41% C, 0.36% Si, 0.25% Mn, 0.006% P, 0.003% S, 0.98% Cr, 3.16% Ni, 0.14% V, 0.24% Cu, 0.59% Mo, 0.026% Al
0.41% C, 0.36% Si, 0.25% Mn, 0.006% P, 0.003% S, 0.98% Cr, 3.16% Ni, 0.14% V, 0.24% Cu, 0.59% Mo, 0.026% Al
0.41% C, 0.45% Mn, 0.66% Si, 0.001% S, 0.011% P 4.90% Ni, 1.07% Cr, 1.07% Mo, 0.09% Cu, 0.35% V
0.41% C, 0.45% Mn, 0.66% Si, 0.001% S, 0.011% P 4.90% Ni, 1.07% Cr, 1.07% Mo, 0.09% Cu, 0.35% V
0.41% C, 0.48% Mn, 0.13% Si, 0.016% P, 0.043% S, 1.75% Ni, 0.17% Cr, 0.22% Mo
0.41% C, 0.55% Mn, 0.24% Si, 0.007% S, 0.014% P 0.93% Ni, 0.80% Cr, 0.06% Mo, 0.10% Cu, 0.010% V
0.41% C, 0.55% Mn, 0.24% Si, 0.007% S, 0.014% P 0.93% Ni, 0.80% Cr, 0.06% Mo, 0.10% Cu, 0.010% V
0.41% C, 0.57% Mn, 1.57% Cr, 0.36% Mo, 1.26% Al
0.41% C, 0.57% Mn, 1.57% Cr, 0.36% Mo, 1.26% Al
0.41% C, 0.58% Mn, 0.28% Si, 0.15% Ni, 1.39% Cr 0.74% Mo
0.41% C, 0.60% Mn, 3.51% Ni, 0.21% Mo
0.41% C, 0.60% Mn, 3.51% Ni, 0.21% Mo
0.41% C, 0.66% Mn, 0.25% Si, 0.008% P, 0.024% S, 0.31% Ni, 1.03% Cr, 0.17% Mo, 0.28% Cu
0.41% C, 0.67% Mn, 0.23% Si, 0.20% Ni, 1.01% Cr 0.23% Mo
0.41% C, 0.70% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.80% Cr, 1.80% Ni, 0.25% Mo
0.41% C, 0.73% Mn, 0.42% Si, 4.54% Ni, 0.75% Cr, 0.26% Mo
0.41% C, 0.74% Mn, 0.40% Si, 4.56% Ni, 0.75% Cr, 0.03% Mo
0.41% C, 0.76% Mn, 0.32% Si, 3.59% Ni, 0.77% Cr, 0.03% Mo
0.41% C, 0.76% Mn, 0.32% Si, 3.59% Ni, 0.77% Cr, 0.25% Mo
0.41% C, 0.76% Mn, 0.35% Si, 4.45% Ni, 0.01% Mo
0.41% C, 0.82% Mn, 0.29% Si, 0.022% S, 0.035% P 0.165% Ni, 1.005% Cr, 0.18% Mo
0.41% C, 0.84% Mn, 0.34% Si, 0.35% Cr, 0.77% Mo
0.41% C, 0.84% Mn, 0.35% Si, 0.35% Cr, 0.49% Mo
0.41% C, 0.85% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.50% Cr, 0.55% Ni, 0.20% Mo
0.41% C, 0.86% Mn, 0.26% Si, 1.28% Ni, 0.71% Cr
0.41% C, 0.86% Mn, 0.36% Si, 0.33% Cr, 0.01% Mo
0.41% C, 0.87% Mn, 0.28% Si, 1.83% Ni, 0.72% Cr, 0.20% Mo
0.41% C, 0.87% Mn, 0.28% Si, 1.83% Ni, 0.72% Cr, 0.20% Mo
0.41% C, 0.90% Si, 0.30% Mn, 5.00% Cr, 0.50% V, 1.30% Mo
0.41% C, 0.90% Si, 0.30% Mn, 5.00% Cr, 0.50% V, 1.30% Mo
0.41% C, 1.03% Si, 0.44% Mn, 0.013% P, 0.010% S, 5.08% Cr, 1.22% Mo, 0.49% V
0.41% C, 1.41% Mn, 1.41% Si, 1.36% Ni, 0.78% Cr, 0.26% Mo
0.41% C, 1.41% Mn, 1.51% Si, 0.27% Mo
0.41% C, 1.42% Mn, 1.42% Si, 1.37% Ni, 0.78% Cr, 0.03% Mo
0.41% C, 1.42% Mn, 1.52% Si, 0.02% Mo
0.41% C, 1.44% Mn, 1.50% Si, 0.75% Cr, 0.01% Mo
0.41% C, 1.60% Si, 0.55% Mn, 0.80% Cr, 1.50% Ni, 0.40% Mo, 0.08% V
0.41% C, 1.60% Si, 0.55% Mn, 0.80% Cr, 1.50% Ni, 0.40% Mo, 0.08% V
0.41% C, 0.336% Si, 0.701% Mn, 0.011% P, 0.025% S, 0.998% Cr, 0.380% Cu, 0.171% Mo, 0.191% Ni, 0.029% Al, 0.019% Nb
0.41% C, 0.336% Si, 0.701% Mn, 0.011% P, 0.025% S, 0.998% Cr, 0.380% Cu, 0.171% Mo, 0.191% Ni, 0.029% Al, 0.019% Nb
0.41% C, 0.86% Mn, 0.26% Si, 1.28% Ni, 0.71% Cr
0.41% C, 1.63% Si, 0.83% Mn, 0.83% Cr, 1.91% Ni, 0.41% Mo, 0.08% V, 0.03% Cu
0.41% C, 1.63% Si, 0.83% Mn, 0.83% Cr, 1.91% Ni, 0.41% Mo, 0.08% V, 0.03% Cu
0.41% C, 0.02% Si, 0.38% Mn, 0.013% P, 0.019% S
0.41% C, 0.38% Si, 0.67% Mn, 0.021% P, 0.016% S, 0.16% Cu, 0.13% Cr, 0.05% Ni, 0.05% Mo, 0.010% Al, 0.01% V
0.415% C, 0.34% Mn, 0.52% Si, 1.40% Cr, 0.31% V 2.28% W
0.42-0.5% C, 98.51-98.98% Fe, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.42% C, 0.16% Mn, 0.44% Si, 0.049% S, 0.042% P 0.27% Ni, 13.40% Cr, 0.08% Cu
0.42% C, 0.16% Mn, 0.44% Si, 0.049% S, 0.042% P 0.27% Ni, 13.40% Cr, 0.08% Cu
0.42% C, 0.16% Si, 0.68% Mn, 0.93% Cr, 97.81% Fe
0.42% C, 0.16% Si, 0.68% Mn, 0.93% Cr, 97.81% Fe
0.42% C, 0.16% Si, 0.68% Mn, 0.93% Cr
0.42% C, 0.20% Mn, 0.21% Mo
0.42% C, 0.20% Mn, 0.21% Mo
0.42% C, 0.23% Si, 0.69% Mn, 0.018% P, 0.028% S, 0.05% Ni, 0.94% Cr, 0.18% Mo, 0.025% Al
0.42% C, 0.25% Si, 0.55% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.71% Mo
0.42% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.42% C, 0.25% Si, 0.65% Mn, 1.05% Cr, 0.25% Mo
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S. 41CrS4: 0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.020-0.035% S
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S. 41CrS4: 0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, 0.020-0.035% S
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr, <0.035% S
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.70% Mn, 1.05% Cr
0.42% C, 0.25% Si, 0.71% Mn, 0.030% P, 0.024% S, 1.07% Cr, 0.15% Ni, 0.01% V, 0.34% Cu, 0.03% Mo, 0.031% Al, 0.023% Sn
0.42% C, 0.25% Si, 0.71% Mn, 0.030% P, 0.024% S, 1.07% Cr, 0.15% Ni, 0.01% V, 0.34% Cu, 0.03% Mo, 0.031% Al, 0.023% Sn
0.42% C, 0.25% Si, 0.71% Mn, 0.030% P, 0.024% S, 1.07% Cr, 0.15% Ni, 0.01% V, 0.34% Cu, 0.03% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, <0.035% S, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, <0.035% S, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo, <0.035% S, (Pb). 42CrMoS4: 0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo,0.020-0.035% S, (Pb)
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo, <0.035% S, (Pb). 42CrMoS4: 0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo,0.020-0.035% S, (Pb)
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.75% Mn, 1.10% Cr, 0.22% Mo
0.42% C, 0.25% Si, 0.80% Mn, 1.10% Cr
0.42% C, 0.25% Si, 0.80% Mn, 1.10% Cr
0.42% C, 0.25% Si, 0.80% Mn, 1.10% Cr
0.42% C, 0.25% Si, 0.87% Mn, 0.89% Cr
0.42% C, 0.25% Si, 1.80% Mn, 0.10% V
0.42% C, 0.25% Si, 1.80% Mn, 0.10% V
0.42% C, 0.27% Si, 0.24% Mn, 0.005% P, 0.001% S, 0.98% Cr, 3.17% Ni, 0.14% V, 0.21% Cu, 0.61% Mo
0.42% C, 0.27% Si, 0.24% Mn, 0.006% P, 0.001% S, 0.98% Cr, 3.17% Ni, 0.14% V, 0.21% Cu, 0.61% Mo
0.42% C, 0.27% Si, 0.24% Mn, 0.006% P, 0.001% S, 0.98% Cr, 3.17% Ni, 0.14% V, 0.21% Cu, 0.61% Mo
0.42% C, 0.27% Si, 1.82% Mn, 0.026% P, 0.018% S
0.42% C, 0.28% Si, 0.71% Mn, 1.77% Ni, 0.24% Mo
0.42% C, 0.29% Si, 1.61% Mn, 0.006% P, 0.019% S, 0.004% B
0.42% C, 0.30% Si, 0.60% Mn, 1.10% Cr, 0.20% Mo
0.42% C, 0.30% Si, 0.88% Mn, 0.009% P, 0.019% S, 0.15% Cr, 0.05% Ni, 0.14% Cu, 0.01% Mo, 0.029% Al, 0.008% Sn
0.42% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo. KTW-Ni: 0.42% C, 0.30% Si, 1.50% Mn, 2.00% Cr, 0.20% Mo, 1.00% Ni
0.42% C, 0.31% Si, 0.67% Mn, 0.022% S, 0.029% P, 2.53% Ni, 0.72% Cr, 0.48% Mo
0.42% C, 0.31% Si, 0.67% Mn, 0.029% P, 0.022% S, 2.53% Ni, 0.72% Cr, 0.48% Mo
0.42% C, 0.31% Si, 1.34% Mn, 0.010% P, 0.007% S, 1.99% Cr, 0.96% Ni, 0.22% Cu, 0.24% Mo
0.42% C, 0.39% Si, 0.38% Mn, 0.017% P, 0.010% S, 1.61% Cr, 0.23% Mo, 4.40% Ni, 0.060% V
0.42% C, 0.40% Mn, 0.32% Si, 0.005% S, 0.010% P 4.34% Ni, 1.56% Cr, 0.44% Mo, 0.05% Cu
0.42% C, 0.40% Mn, 0.32% Si, 0.005% S, 0.010% P 4.34% Ni, 1.56% Cr, 0.44% Mo, 0.05% Cu
0.42% C, 0.40% Si, 0.30% Mn, 13.00% Cr
0.42% C, 0.44% Si, 0.16% Mn, 0.042% P, 0.049% S, 13.40% Cr, 0.08% Cu
0.42% C, 0.44% Si, 0.16% Mn, 0.042% P, 0.049% S, 13.40% Cr, 0.27% Ni, 0.08% Cu
0.42% C, 0.50% Mn, 0.18% Si, 0.42% Ni, 0.22% Cr
0.42% C, 0.50% Si, 0.40% Mn, 6.50% Cr, 1.30% Mo, 0.80% V
0.42% C, 0.60% Mn, 0.41% Si, 0.012% S, 0.013% P 4.40% Ni, 1.25% Cr, 0.05% Mo, 0.14% Cu
0.42% C, 0.62% Mn, 1.78% Si, 0.013% S, 0.043% P 0.18% Ni, 0.05% Cr, 0.01% Mo, 0.22% Cu, 0.03% Ti, trace V
0.42% C, 0.65% Mn, 0.30% Si, 0.020% P, 0.020% S, 1.65% Cr, 0.33% Mo, 1.00% Al
0.42% C, 0.67% Mn, 0.31% Si, 0.030% P, 0.022% S, 2.71% Ni, 1.00% Cr, 0.48% Mo
0.42% C, 0.67% Mn, 0.31% Si, 2.53% Ni, 0.72% Cr 0.48% Mo
0.42% C, 0.68% Mn, 0.93% Cr
0.42% C, 0.68% Mn, 0.93% Cr
0.42% C, 0.70% Mn, 1.40% Si, 0.005% S, 0.015% P 0.24% Ni, 0.68% Cr, 0.19% Mo, 0.03% Cu
0.42% C, 0.71% Mn, 0.28% Si, 1.77% Ni, 0.24% Mo
0.42% C, 0.72% Mn, 0.05% Ni, 0.99% Cr, 0.42% Mo
0.42% C, 0.78% Mn, 1.79% Ni, 0.80% Cr, 0.33% Mo
0.42% C, 0.78% Mn, 1.79% Ni, 0.80% Cr, 0.33% Mo
0.42% C, 0.78% Mn, 1.79% Ni, 0.80% Cr, 0.33% Mo
0.42% C, 0.78% Si, 0.018% P, 0.027% S, 0.24% Si, 1.79% Ni, 0.80% Cr, 0.33% Mo
0.42% C, 0.85% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.15% Cr, 0.20% Mo
0.42% C, 0.85% Si, 1.00% Mn, 1.50% Cr, 0.35% V, 0.60% Mo
0.42% C, 0.87% Mn, 0.25% Si, 0.89% Cr
0.42% C, 0.89% Mn, 0.018% P, 0.015% S, 0.30% Si, 0.58% Ni, 0.52% Cr, 0.24% Mo
0.42% C, 0.89% Mn, 0.80% Si, 0.018% P, 0.015% S 0.58% Ni, 0.52% Cr, 0.24% Mo
0.42% C, 1.07% Si, 1.08% Mn, 0.011% P, 0.014% S, 0.20% Cr, 0.09% Ni, 0.09% V, 0.24% Cu, 0.02% Mo, 0.022% Sn
0.42% C, 1.15% Mn, 0.20% Si, 0.020% P, 0.16% S
0.42% C, 1.61% Mn, 0.29% Si, 0.006% P, 0.010% P
0.42% C, 1.61% Mn, 0.29% Si, 0.006% P, 0.019% S, 0.004% B
0.42% C, 1.61% Mn, 0.29% Si, 0.006% P, 0.019% S, 0.004% B
0.42% C, 1.75% Mn, 0.36% Si, 0.031% P, 0.029% S, 0.24% Ni, 0.28% Cr, 0.12% Mo, 0.17% Co, 0.020% Sn, 0.11% Al
0.42% C, 1.78% Si, 0.62% Mn, 0.043% P, 0.013% S, 0.05% Cr, 0.18% Ni, 0.01% Mo, 0.22% Cu, 0.03% Ti, traces V
0.42% C, 13.00% Cr
0.42-0.48% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.42-0.48% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr, max. 0.30% Cu
0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%
0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.045% S, <0.045% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mo+Ni<=063
0.42-0.50% C, <0.40% Si, 0.50-0.80% Mn, <0.045% S, <0.045% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mo+Ni<=063
0.42-0.50% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.42-0.50% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.030% P, max. 0.030% S
0.42-0.50% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.030% P, max. 0.030% S
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.25% Cu
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.25% Cu
0.42-0.50% C, 0.30% Si, 0.50-0.80% Mn, 0.025% P, 0.035% S, 0.25% Cu
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.40-0.60% Cr. 46CrS2: 0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, <0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.42-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.42-0.50% C, 0.40% Si, 0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.40% Si, 0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 1.30-1.70% Si, 0.50-0.80% Mn, 0.030% P, 0.025% S, 0.50-0.75% Cr, 0.15-0.30% Mo
0.42-0.50% C, 1.30-1.70% Si, 0.50-0.80% Mn, 0.030% P, 0.025% S, 0.50-0.75% Cr, 0.15-0.30% Mo
0.42-0.50% C, 1.50-1.80% Si, 0.50-0.80% Mn, 0.050% P, 0.050% S, 0.0070% N
0.42-0.50% C, 1.50-1.80% Si, 0.50-0.80% Mn, max. 0.050% P, max. 0.050% S, max. 0.007% N
0.42-0.50% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.42-0.50% C, max. 0.30% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.40-0.60% Cr
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.035% P, 0.020-0.040% S, 0.40-0.60% Cr
0.42-0.52% C, 1.50-2.00% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S
0.42-9.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-9.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42-9.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.42% C, 0.80% Cr, O.30% Mo, 1.50% Ni
0.42% C, 0.40% Si, 0.40% Mn, 0.030% P, 0.003% S, 13.00% Cr
0.42-0.50% C, 0.40% Si, 0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.030% P, max. 0.035% S
0.42?0.50% C, max. 0.40% Si, 0.50?0.80% Mn, max. 0.025% P, max. 0.010% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni, max. Cr+Ni+Mo=0.63
0.42-0.50% C, 0.40% Si, 0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42-0.50% C, 0.40% Si, 0.80% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.42% C, 1.10% Cr, 0.25% Mo
0.42% C, 1.10% Cr, 0.25% Mo
0.42% C, 0.33% Si, 0.68% Mn, 0.016% P, 0.021% S, 0.93% Cr, 0.19% Mo
0.42-0.5% C, 98.51-98.98% Fe, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.43% , 0.83% Mn, 0.021% P, 0.009% S, 1.55% Si, 1.84% Ni, 0.91% Cr, 0.40% Mo, 0.12% V
0.43% C, 0.14% Si, 0.04% Mn, 0.015% P, 0.012% S, 3.58% Cr, 0.14% Al
0.43% C, 0.23% Si, 0.90% Mn, 0.23% Ni, 0.27% Cr, 0.26% Mo
0.43% C, 0.23% Si, 1.57% Mn, 0.011% P, 0.029% S, 0.20% Ni, 0.12% Cr, 0.07% Mo
0.43% C, 0.24% Si, 0.43% Mn, 0.014% P, 0.014% S, 0.04% Cr, 0.014% Al, 5.00% Ni, <0.00% Ti
0.43% C, 0.25% Si, 0.70% Mn, 1.40% Cr, 0.30% V, 0.70% Mo
0.43% C, 0.25% Si, 0.70% Mn, 1.40% Cr, 0.30% V, 0.70% Mo
0.43% C, 0.27% Si, 0.75% Mn, 0.011% P, 0.011% S, 1.31% Cr, 0.78% Mo, 0.11% Ni, 0.23% V
0.43% C, 0.27% Si, 0.75% Mn, 0.011% P, 0.011% S, 1.31% Cr, 0.78% Mo, 0.11% Ni, 0.23% V
0.43% C, 0.27% Si, 1.43% Mn, 0.015% P, 0.011% S, 2.09% Cr, 0.14% Ni, 0.24% Cu, 0.20% Mo, 0.026% Al
0.43% C, 0.28% Si, 1.67% Mn, 0.021% P, 0.008% S, 0.32% Cr, 0.03% Mo, 0.11% Ni, 0.10% V, 0.06% Cu
0.43% C, 0.28% Si, 1.67% Mn, 0.021% P, 0.008% S, 0.32% Cr, 0.06% Cu, 0.03% Mo, 0.11% Ni, 0.10% V
0.43% C, 0.28% Si, 1.67% Mn, 0.021% P, 0.008% S, 0.32% Cr, 0.06% Cu, 0.03% Mo, 0.11% Ni, 0.10% V
0.43% C, 0.28% Si, 1.70% Mn, 0.011% P, 0.029% S, 0.17% Mo
0.43% C, 0.30% Si, 1.78% Mn, 0.019% P, 0.017% S, 0.10% V
0.43% C, 0.41% Si, 0.82% Mn, 0.041% P, 0.015% S, 1.22% Cr, 0.04% Ni, 0.14% Cu, 0.11% V
0.43% C, 0.41% Si, 0.82% Mn, 0.041% P, 0.015% S, 1.22% Cr, 0.14% Cu, 0.04% Ni, 0.11% V
0.43% C, 0.45% Si, 0.50% Mn, 0.012% P, 0.007% S, 13.60% Cr, 0.10% Mo, 0.30% Ni
0.43% C, 0.49% Mn, 0.33% Si, 0.008% S, 0.02% P 1.51% Ni, 1.10% Cr, 0.33% Mo
0.43% C, 0.52% Mn, 0.025% P, 0.021% S, 0.29% Si, 1.76% Ni, 1.19% Cr, 0.05% Mo, 0.06% Cu
0.43% C, 0.52% Mn, 0.29% Si, 0.025% P, 0.021% S 1.76% Ni, 1.19% Cr, 0.05% Mo, 0.06% Cu
0.43% C, 0.67% Mn, 0.28% Si, 0.32% Cr, 0.10% V
0.43% C, 0.74% Mn, 0.16% V, 0.92% Cr
0.43% C, 0.74% Mn, 0.92% Cr, 0.16% V
0.43% C, 0.75% Mn, 0.27% Si, 0.011% S, 0.011% P, 1.31% Cr, 0.11% Ni, 0.72% Mo, 0.23% V
0.43% C, 0.80% Mn, 0.20% Si, 0.020% P, 0.020% S, 0.85% Ni
0.43% C, 0.83% Mn, 1.55% Si, 0.021% P, 0.009% S 1.84% Ni, 0.91% Cr, 0.40% Mo, 0.12% Cu
0.43% C, 0.83% Mn, 1.55% Si, 0.91% Cr, 2.02% Ni, 0.40% Mo, 0.12% V
0.43% C, 0.83% Mn, 1.55% Si, 1.84% Ni, 0.91% Cr, 0.40% Mo, 0.12% V, 0.083% Al
0.43% C, 0.84% Mn, 0.25% Si, 1.00% Ni, 0.81% Cr, 0.23% Mo
0.43% C, 0.90% Mn, 0.32% Si, 0.30% Cr, 0.10% V, 0.015% Al, 0.015% N
0.43% C, 0.90% Mn, 0.32% Si, 0.30% Cr, 0.10% V, 0.015% Al, 0.015% N
0.43% C, 0.95% Mn, 0.21% Si, 0.018% P, 0.024% S, 0.93% Ni, 0.15% Cr, 0.04% Mo
0.43% C, 0.95% Mn, 1.38% Si, <0.010% S, 0.012% P 0.03% Ni, 1.06% Cr, <0.10% Mo, <0.05% Cu, 0.035% V
0.43% C, 0.95% Mn, 1.38% Si, <0.010% S, 0.012% P 0.03% Ni, 1.06% Cr, <0.10% Mo, <0.05% Cu, 0.035% V
0.43% C, 1.02% Mn, 0.31% Ni, 0.48% Cr, 0.13% Mo, 0.0009% B
0.43% C, 1.02% Mn, 0.31% Ni, 0.48% Cr, 0.13% Mo, 0.0009% B
0.43% C, 1.35% Mn, 0.24% Si, 0.025% P, 0.025% S, 0.45% Cr, 0.75% Ni, 0.20% Mo
0.43% C, 1.45% Mn, 1.00% Al, 0.010% P, 0.004% S, 0.033% Nb, 0.010% Ti
0.43% C, 1.55% Si, 0.83% Mn, 1.84% Ni, 0.91% Cr, 0.40% Mo, 0.12% V, 0.083% Al
0.43% C, 1.58% Mn, 0.42% Si, 0.022% P, 0.042% S, 0.24% Ni, 0.27% Cr, 0.12% Mo, 0.18% Co, 0.033% Sn, 0.005% Al
0.43% C, 1.58% Mn
0.43% C, 1.58% Mn
0.43% C, 1.67% Mn, 0.28% Si, 0.008% S, 0.021% P, 0.32% Cr, 0.11% Ni, 0.03% Mo, 0.10% V, 0.06% Cu
0.43% C, 1.67% Mn, 0.28% Si, 0.008% S, 0.021% P, 0.32% Cr, 0.11% Ni, 0.03% Mo, 0.10% V, 0.06% Cu
0.43% C, 1.67% Mn, 0.28% Si, 0.008% S, 0.021% P, 0.32% Cr, 0.11% Ni, 0.03% Mo, 0.10% V, 0.06% Cu
0.43% C, 13.54% Mn, 0.25% Si, 0.008% P, 0.019% S, 0.17% Ni, 23.23% Cr, 0.46% N
0.43% C, 13.54% Mn, 0.25% Si, 0.008% P, 0.019% S, 0.17% Ni, 23.23% Cr, 0.46% N
0.43% C, 2.00% Cr, 0.50% Mo, 0.40% W, 0.80% V
0.43% C, 2.00% Cr, 0.50% Mo, 0.40% W, 0.80% V
0.43% C, 4.00% Mo
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.43-0.49% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S
0.43-0.50% C, 0.60-0.90% Mn, max. 0.04% P, max. 0.05% S
0.43-0.50% C, 0.60-0.90% Mn, max. 0.04% P, max. 0.05% S
0.43-0.50% C, 0.60-0.90% Mn, max. 0.04% P, max. 0.05% S
0.43% C, 0.28% Si, 1.67% Mn, 0.021% P, 0.008% S, 0.32% Cr, 0.03% Mo, 0.11% Ni, 0.10% V, 0.06% Cu
0.43% C, 0.41% Si, 0.82% Mn, 0.041% P, 0.015% S, 1.22% Cr, 0.14% Cu, 0.04% Ni, 0.11% V
0.43% C, 0.41% Si, 0.82% Mn, 0.041% P, 0.015% S, 1.22% Cr, 0.04% Ni, 0.11% V
0.43% C, 0.33% Si, 0.47% Mn, 0.022% P, 0.015% S, 13.27% Cr, 0.14% Mo, 0.28% Ni, 0.03% W
0.43% C, 0.41% Si, 0.82% Mn, 0.041% P, 0.015% S, 1.22% Cr, 0.04% Ni, 0.14% Cu, 0.11% V
0.43% C, 0.41% Si, 0.82% Mn, 0.041% P, 0.015% S, 1.22% Cr, 0.04% Ni, 0.14% Cu, 0.11% V
0.43% C, 0.28% Si, 1.67% Mn, 0.021% P, 0.008% S, 0.32 Cr, 0.06% Cu, 0.03% Mo, 0.11% Ni, 0.10% V
0.44% C, 0.06% Si, 1.64% Mn, 0.029% P, 0.022% S, 1.84% Ni, 1.64% Cr, 0.40% Mo, 0.15% V
0.44% C, 0.20% Mn, 0.30% Si, 0.010% S, 0.025% P, 12.12% Cr, 0.31% Ni, 0.01% Mo, 0.02% V, 0.09% Cu
0.44% C, 0.22% Si, 0.66% Mn, 0.022% P, 0.029% S, 0.15% Cr, 0.02% V
0.44% C, 0.22% Si, 0.66% Mn, 0.022% P, 0.029% S, 0.15% Cr, 0.02% V
0.44% C, 0.22% Si, 0.66% Mn, 0.022% P, 0.029% S, 0.15% Cr, 0.020% V
0.44% C, 0.22% Si, 0.66% Mn, 0.022% P, 0.029% S, 0.15% Cr
0.44% C, 0.22% Si, 0.80% Mn, 0.030% P, 0.023% S, 1.04% Cr, 0.17% Cu, 0.04% Mo, 0.26% Ni, <0.01% V
0.44% C, 0.22% Si, 0.80% Mn, 0.030% P, 0.023% S, 1.04% Cr, 0.17% Cu, 0.04% Mo, 0.26% Ni, <0.01% V
0.44% C, 0.22% Si, 0.80% Mn, 0.030% P, 0.023% S, 1.04% Cr, 0.17% Cu, 0.04% Mo, 0.26% Ni, max. 0.01% V
0.44% C, 0.22% Si, 0.80% Mn, 0.030% P, 0.023% S, 1.04% Cr, 0.17% Cu, 0.04% Mo, 0.26% Ni, max. 0.01% V
0.44% C, 0.23% Si, 0.58% Mn, 0.004% S, 0.029% P, 1.40% Ni, 1.26% Cr, 0.11% Mo
0.44% C, 0.23% Si, 0.58% Mn, 0.004% S, 0.029% P, 1.40% Ni, 1.26% Cr, 0.11% Mo
0.44% C, 0.23% Si, 0.58% Mn, 0.004% S, 0.029% P, 1.40% Ni, 1.26% Cr, 0.11% Mo
0.44% C, 0.23% Si, 0.58% Mn, 0.004% S, 0.029% P, 1.40% Ni, 1.26% Cr, 0.11% Mo
0.44% C, 0.23% Si, 0.58% Mn, 0.029% P, 0.004% S, 1.40% Ni, 1.26% Cr, 0.11% Mo
0.44% C, 0.25% Si, 0.66% Mn, 0.015% P, 0.024% S, 0.011% Cr, 0.10% Ni, 0.025% Mo, 0.24% Cu, 0.017% Al
0.44% C, 0.26% Si, 0.72% Mn, 0.038% P, 0.028% S, 0.16% Cr, 0.09% Ni, 0.02% Mo
0.44% C, 0.26% Si, 0.75% Mn, 0.016% P, 0.019% S, 1.70% Cr, 0.08% Mo, 0.17% Ni, 0.090% V, 0.18% Cu
0.44% C, 0.26% Si, 0.75% Mn, 0.016% P, 0.019% S, 1.70% Cr, 0.18% Cu, 0.08% Mo, 0.17% Ni, 0.09% V
0.44% C, 0.26% Si, 0.75% Mn, 0.016% P, 0.019% S, 1.70% Cr, 0.18% Cu, 0.08% Mo, 0.17% Ni, 0.09% V
0.44% C, 0.28% Si, 0.60% Mn
0.44% C, 0.28% Si, 0.65% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.15% Mo
0.44% C, 0.29% Si, 1.04% Mn, 1.13% Cr, 0.15% Mo
0.44% C, 0.29% Si, 1.30% Mn, 0.020% P, 0.025% S, 0.08% Cr, 0.02% Ni, 0.14% Cu
0.44% C, 0.29% Si, 1.30% Mn, 0.020% P, 0.025% S, 0.08% Cr, 0.02% Ni, 0.14% Cu
0.44% C, 0.30% Si, 0.20% Mn, 0.025% P, 0.010% S, 13.12% Cr, 0.01% Mo, 0.31% Ni, 0.020% V, 0.09% Cu
0.44% C, 0.30% Si, 0.20% Mn, 0.025% P, 0.010% S, 13.12% Cr, 0.09% Cu, <0.01% Mo, 0.31% Ni, 0.02% V
0.44% C, 0.30% Si, 0.20% Mn, 0.025% P, 0.010% S, 13.12% Cr, 0.09% Cu, <0.01% Mo, 0.31% Ni, 0.02% V
0.44% C, 0.30% Si, 0.20% Mn, max. 0.025% P, max. 0.010% S, 13.12% Cr, 0.01% Mo, 0.31% Ni, 0.020% V, 0.09% Cu
0.44% C, 0.31% Si, 0.80% Mn, 0.013% S, 0.030% P, 0.46% Ni, 0.96% Cr
0.44% C, 0.34% Si, 0.88% Mn, 0.49% Ni, 0.65% Cr, 0.14% Mo, +B
0.44% C, 0.45% Mn, max. 0.005% S, 1.00% Si, 6.00% Cr, 1.90% Mo, 0.80% V
0.44% C, 0.48% Si, 0.30% Mn, 0.023% P, 0.003% S, 14.20% Cr, 0.64% Mo, 0.16% Ni, 0.16% V, 0.03% W, 0.11% Cu, 0.015% Al
0.44% C, 0.50% Mn, 0.18% Si, 0.42% Ni, 0.22% Cr
0.44% C, 0.60% Mn, 0.22% Si, 0.023% P, 0.023% S, 0.24% Ni, 1.19% Cr, 0.37% Mo
0.44% C, 0.66% Mn, 0.22% Si, 0.029% S, 0.022% P, 0.15% Cr, 0.02% V
0.44% C, 0.66% Mn, 0.22% Si, 0.029% S, 0.022% P, 0.15% Cr, 0.02% V
0.44% C, 0.66% Mn. Right diagram: 0.48% C, 2.00% Mn
0.44% C, 0.67% Si, 1.45% Mn, 0.23% Cr, 0.03% Mo, 0.10% Ni, 0.11% V, 0.14% Cu, 0.028% Cu, 0.00% Al, 0.009% N
0.44% C, 0.7% Mn, 0.2% Si, 1.04% Cr, 0.26% Ni, 0.04% Mo, 0.1% V, 0.17% Cu
0.44% C, 0.7% Mn, 0.2% Si, 1.04% Cr, 0.26% Ni, 0.04% Mo, 0.1% V, 0.17% Cu
0.44% C, 0.72% Mn, 0.26% Si, 0.028% S, 0.038% P 0.09% Ni, 0.16% Cr, 0.02% Mo
0.44% C, 0.75% Mn, 0.26% Si, 0.019% S, 0.016% P, 1.70% Cr, 0.17% Ni, 0.08% Mo, 0.09% V, 0.18% Cu
0.44% C, 0.75% Mn, 0.26% Si, 0.019% S, 0.016% P, 1.70% Cr, 0.17% Ni, 0.08% Mo, 0.09% V, 0.18% Cu
0.44% C, 0.79% Mn, 1.63% Si, 2.10% Cr, 0.54% Mo, 0.06% V
0.44% C, 0.80% Mn, 0.31% Si, 0.013% S, 0.030% P 0.46% Ni, 0.96% Cr, 0.05% Mo, 0.18% Cu
0.44% C, 0.80% Mn, 0.31% Si, 0.013% S, 0.030% P 0.46% Ni, 0.96% Cr, 0.05% Mo, 0.18% Cu
0.44% C, 0.88% Mn, 0.34% Si, 0.49% Ni, 0.65% Cr, 0.14% Mo
0.44% C, 0.90% Mn, 0.019% P, 0.031% S, 0.25% Si, 0.45% Ni, 0.54% Cr, 0.22% Mo
0.44% C, 0.90% Mn, 0.45% Ni, 0.54% Cr, 0.22% Mo
0.44% C, 0.90% Mn, 0.45% Ni, 0.54% Cr, 0.22% Mo
0.44% C, 1.04% Mn, 0.29% Si, 1.13% Cr, 0.15% Mo. AISI 4142: 0.40% C, 0.25% Si, 1.00% Mn, 1.00% Cr, 0.20% Mo
0.44% C, 1.04% Mn, 0.29% Si, 1.13% Cr, 0.15% Mo
0.44% C, 1.04% Mn, 0.29% Si, 1.13% Cr, 0.15% Mo
0.44% C, 1.20% Cr. Heat 2: 0.41% C, 1.06% Cr.
0.44% C, 1.50% Mn, 0.20% Si, 0.020% P, 0.25% S
0.44% C, 1.63% Si, 0.79% Mn, 2.10% Cr, 0.54% Mo, 0.06% V
0.44% C, 1.64% Mn, 0.06% Si, 0.029% P, 0.022% S, 1.84% Ni, 1.64% Cr, 0.40% Mo, 0.15% Cu
0.44% C, 1.64% Mn, 0.06% Si, 0.029% P, 0.022% S, 1.84% Ni, 1.64% Cr, 0.40% Mo, 0.15% Cu
0.44% C, 1.64% Mn, 0.06% Si, 0.029% P, 0.022% S, 1.84% Ni, 1.64% Cr, 0.40% Mo, 0.15% Cu
0.44% C, 3.17% Si, 0.51% Mn, 0.018% P, 0.004% S, 9.50% Cr
0.44% C, 3.43% Si, 0.44% Mn, 0.038% P, 0.013% S, 9.07% Cr, 0.27% Ni, 0.23% Cu, 0.07% Mo
0.44% C, 0.22% Si, 0.66% Mn, 0.022% P, 0.029% S, 0.15% Cr, 0.02% V
0.44% C, 0.22% Si, 0.66% Mn, 0.15% Cr. Steel b: 0.38% C, 1.05% Si, 1.14% Mn
0.44% C, 0.60% Mn, 0.22% Si, 0.023% P, 0.023% S, 0.24% Ni, 1.19% Cr, 0.37% Mo
0.44% C, 0.22% Si, 0.80% Mn, 0.030% P, 0.023% S, 1.04% Cr, 0.17% Cu, 0.04% Mo, 0.26% Ni, 0.01% V
0.44% C, 0.22% Si, 0.80% Mn, 0.030% P, 0.023% S, 1.04% Cr, 0.17% Cu, 0.04% Mo, 0.26% Ni, 0.01% V
0.44% C, 1.5% Cr, 1.20% Mn, 1.26% Si, 0.08% Ti, 0.15% V, 0.025% P, 0.045% S
0.44% C, 0.02% Si, 0.39% Mn, 0.013% P, 0.019% S
0.44% C, 0.47% Si, 0.58% Mn, 0.019% P, 0.027% S, 0.28% Cu, 0.10% Cr, 0.05% Ni, 0.04% Mo, 0.042% Al, 0.01% V
0.45% C, 0.03-0.50% Si, 1.00% Mn, 0.050% P, 0.050% S
0.45% C, 0.03-0.50% Si, 1.00% Mn, 0.050% P, 0.050% S
0.45% C, 0.20% Si, 0.40% Mn, 1.30% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 0.20% Si, 0.40% Mn, 1.30% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 0.20% Si, 0.40% Mn, 1.30% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 0.20% Si, 0.70% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.45% C, 0.20% Si, 0.70% Mn, max. 0.025% P, max. 0.025% S, max. 0.25% Cu
0.45% C, 0.23% Si, 0.62% Mn, 0.012% P, 0.023% S, 0.17% Cr, 0.06% Ni, 0.01% V, 0.24% Cu, 0.02% Mo
0.45% C, 0.23% Si, 0.62% Mn, 0.012% P, 0.023% S, 0.17% Cr, 0.06% Ni, 0.01% V, 0.24% Cu, 0.02% Mo
0.45% C, 0.25% Si, 0.30% Mn, 0.025% P, 0.003% S, 1.30% Cr, 4.00% Ni, 0.25% Mo
0.45% C, 0.25% Si, 0.35% Mn, 1.40% Cr, 0.20% Mo, 4.0% Ni
0.45% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 4.00% Cr
0.45% C, 0.25% Si, 0.40% Mn, 1.35% Cr, 0.25% Mo, 4.00% Ni
0.45% C, 0.25% Si, 0.65% Mn, <0.03% S
0.45% C, 0.25% Si, 0.65% Mn, <0.03% S
0.45% C, 0.25% Si, 0.65% Mn, <0.030% S, (Pb). C45R: C45E: 0.45% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, (Pb)
0.45% C, 0.25% Si, 0.65% Mn, <0.030% S, (Pb). C45R: C45E: 0.45% C, 0.25% Si, 0.65% Mn, 0.020-0.035% S, (Pb)
0.45% C, 0.25% Si, 0.65% Mn, 0.025% S, 0.008% P, 0.40% Ni, 0.40% Cr, 0.10% Mo, 0.17% Cu, 0.01% Al
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.65% Mn
0.45% C, 0.25% Si, 0.75% Mn, 1.45% Cr, 0.75% Mo, 0.30% V
0.45% C, 0.25% Si, 0.80% Mn, 0.55% Ni, 1.15% Cr, 0.55% Mo, 0.05% V
0.45% C, 0.26% Si, 0.67% Mn, 0.009% P, 0.012% S, 0.06% Ni, 0.009% Mo
0.45% C, 0.26% Si, 0.76% Mn, 0.17% Cr, 0.03% Mo, 0.09% V, 0.11% Cu
0.45% C, 0.27% Si, 0.52% Mn, 0.015% P, 0.025% S, 0.12% Ni, 0.05% Cr, 0.01% Mo, 0.13% Cu
0.45% C, 0.27% Si, 0.52% Mn, 0.025% S, 0.015% P, 0.12% Ni, 0.055% Cr, 0.01% Mo, 0.13% Cu
0.45% C, 0.27% Si, 0.62% Mn, 0.012% P, 0.003% S, 1.04% Cr, 0.80% Mo, 0.035% Nb, 0.052% V, 0.032% Ti, 0.066 Al
0.45% C, 0.27% Si, 0.62% Mn, 1.04% Cr, 0.80% Mo, 0.035% Nb, 0.052% V, 0.032% Ti, 0.003% S, 0.012% P
0.45% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 5.00% Mo, 1.00% V
0.45% C, 0.30% Si, 0.40% Mn, 4.50% Co, 4.5% Cr, 3.00% Mo, 2.00% V
0.45% C, 0.30% Si, 0.40% Mn, 4.50% Cr, 3.00% Mo, 2.00% V, 4.50% Co
0.45% C, 0.30% Si, 0.70% Mn, 1.50% Cr, 0.75% Mo, 0.30% V
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.70% Mn
0.45% C, 0.30% Si, 0.75% Mn, 0.025% P, 0.010% S, 1.50% Cr, 0.50% Mo, 0.30% V
0.45% C, 0.32% Si, 0.44% Mn, 0.030% P, 0.016% S, 13.0% Cr, 0.38% Ni. X30Crl3: 0.27% C, 0.26% Si, 0.40% Mn, 0.015% P, 0.007% S, 13.4% Cr, 0.10% Ni
0.45% C, 0.33% Si, 0.27% Mn, 0.020% P, 0.008% S, 12.73% Cr, 0.02% Mo, 0.09% Ni
0.45% C, 0.33% Si, 0.69% Mn, 0.023% P, 0.020% S, 1.02% Cr, 0.33% Mo, 1.33% Ni, 0.14% Cu, 0.040% Al
0.45% C, 0.34% Mn, 0.20% Si, 0.007% S, 0.019% P 0.44% Ni, 1.25% Cr, <0.01% Mo, 0.14% Cu, 0.36% V, 2.20% W
0.45% C, 0.34% Si, 0.34% Mn, 0.027% P, 0.020% S, 12.80% Cr, 0.33% Ni, 0.18% Cu, 0.05% Mo
0.45% C, 0.34% Si, 0.34% Mn, 0.027% P, 0.020% S, 12.80% Cr, 0.33% Ni, 0.18% Cu, 0.05% Mo
0.45% C, 0.40% Mn, 0.50% Si, 2.10% Cr, 0.80% Mo, 1.10% W, 0.75% V, 1.10% Ni
0.45% C, 0.40% Si, 0.40% Mn, 0.020% P, 0.010% S, 4.50% Cr, 0.50% Mo, 2.00% V, 4.50% W, 4.50% Co
0.45% C, 0.52% Mn, 0.27% Si, 0.025% S, 0.015% P 0.12% Ni, 0.05% Cr, 0.01% Mo, 0.13% Cu
0.45% C, 0.55% Mn, 1.31% Si, 0.005% S, 0.013% P 0.21% Ni, 0.60% Cr, 0.22% Mo, 0.27% Cu, <0.05% V, trace Ti
0.45% C, 0.59% Mn, 0.28% Si, 0.03% S, 0.015% P 0.06% Ni, 0.05% Cr, 0.14% Cu
0.45% C, 0.60% Mn, 3.40% Si, 0.015% P, 0.010% S, 8.50% Cr
0.45% C, 0.60% Si, 0.40% Mn, 1.60% Cr, 0.80% V, 0.50% W
0.45% C, 0.70% Mn, 1.00% Cr, 0.20% V
0.45% C, 0.70% Mn, 1.00% Cr, 0.20% V
0.45% C, 0.70% Mn, 1.00% Cr, 0.20% V
0.45% C, 0.77% Mn, 0.35% Si, 0.015% P, 0.013% S, 0.72% Cr, 0.25% Mo
0.45% C, 0.80% Mn, 0.25% Si, 0.55% Ni, 1.15% Cr, 1.00% Mo, 0.05% V
0.45% C, 0.85% Si, 0.35% Mn, 7.40% Cr, 1.40% Mo, 1.35% V
0.45% C, 0.89% Mn, 0.59% Ni, 0.66% Cr, 0.12% Mo, 0.0015% B
0.45% C, 0.89% Mn, 0.59% Ni, 0.66% Cr, 0.12% Mo, 0.0015% B
0.45% C, 1.00% Si, 0.30% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.45% C, 1.04% Mn, 0.35% Si, 0.012% S, 0.032% P, 1.22% Cr, 0.05% Ni, 0.05% Mo, 0.13% V, 0.16% Cu
0.45% C, 1.34% Mn, 1.45% Si, 0.013% S, 0.022% P, 0.10% V
0.45% C, 1.34% Si, 1.50% Mn, 0.017% P, <0.010% S, 0.03% Cr, 0.03% Ni, <0.01% Mo, 0.09% Cu, 0.040% V
0.45% C, 1.34% Si, 1.50% Mn, 0.017% P, 0.010% S, 0.03% Cr, 0.01% Mo, 0.03% Ni, 0.04% V, 0.09% Cu
0.45% C, 1.34% Si, 1.50% Mn, 0.017% P, 0.010% S, 0.03% Cr, 0.03% Ni, <0.01% Mo, 0.09% Cu, 0.04% V
0.45% C, 1.35% Si, 1.35% Cr, 0.10% V
0.45% C, 1.4% Cr, 0.3% Mo, 4.0% Ni
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 1.40%Cr, 0.25% Mo, 4.00% Ni
0.45% C, 1.50% Mn, 1.34% Si, <0.010% S, 0.017% P 0.03% Ni, 0.03% Cr, <0.01% Mo, 0.09% Cu, 0.040% V
0.45% C, 1.50% Mn, 1.34% Si, <0.010% S, 0.017% P 0.03% Ni, 0.03% Cr, <0.01% Mo, 0.09% Cu, 0.040% V
0.45% C, 3.00% Si, 9.00% Cr
0.45% C, 3.03% Si, 0.32% Mn, 0.57% Cr, 0.051% V, 50 ppm N, 50 ppm O
0.45% C, max. 0.40% Si, 0.65% Mn, max. 0.40% Cr, max. 0.10% Mo, max. 0.10% Mo, 0.45% C
0.45-0.50% C, 0.70-0.90% Si, 0.35-0.45% Mn, max. 0.020% P, max. 0.005% S, 7.30-7.80% Cr, 1.30-1.50% Mo, 1.30-1.50% V
0.45-0.52% C, 1.60-2.00% Si, 0.50-0.80% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.45-0.55% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 3.00-3.50% Ni
0.45-0.55% C, 0.15-0.35% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 3.00-3.50% Ni
0.45-0.55% C, 0.80-1.00% Si, 0.40-0.60% Mn, max. 0.035% P, max. 0.035% S, 8.00-9.00% Cr, 1.10-1.30% Mo, 1.10-1.30% W
0.45-0.60% C, 0.40% Si, 0.60-1.10% Mn, 0.70-1.70% Cr, 1.30-2.50% Ni, 0.40-1.00% Mo
0.45% C, 0.25% Si, 0.30% Mn, 0.025% P, 0.003% S, 1.30% Cr, 4.00% Ni, 0.25% Mo
0.45% C, 0.40% Si, 1.32% Mn, 0.016% P, 0.004% S, 0.11% V, 0.056% RE
0.45% C, 3.5% Cr
0.45-0.60% C, 1.30-1.70% Si, max. 0.80% Mn, 15.00-16.50% Cr, 0.20-0.40% Mo, 0.20-0.40% V, 0.05-0.20% N, max. 0.40% Ni
0.45% C, 0.25% Si, 0.75% Mn, 1.45% Cr, 0.75% Mo, 0.30% V
0.45% C, 1.40% Cr, 0.30% Mo, 4.00% Ni
0.45% C, 0.30% Si, 0.30% Mn, 3.00% Cr, 5.00% Mo, 1.00% V
0.45% C, 1.35% Si, 1.35% Cr, 0.10% V
0.45% C, 0.30% Si, 0.70% Mn, 1.50% Cr, 0.75% Mo, 0.30% V
0.45% C, 0.60% Si, 0.40% Mn, 1.60% Cr, 0.60% Mo, 0.80% V, 0.50% W
0.45% C, 0.05% Si, 0.07% Mn, 0.007% P, 0.020% S
0.456% C, 0.541% Si, 1.36% Mn, 0.014% P, 0.031% S, 0.227% Cr, 0.088% Ni, 0.008% Mo, 0.025% Al, 0.12% Cu, 0.105% V, 0.007% Nb
0.46% C 0.40% Si, 0.40% Mn, 13.00% Cr
0.46% C, 0.22% Si, 0.50% Mn, 0.015% P, 0.014% S, 1.00% Cr, 0.26% Cu, 0.21% Mo, 0.22% Ni, <0.01% V
0.46% C, 0.24% Si, 0.50% Mn, 0.012% P, 0.007% S, 1.53% Cr, 0.20% Cu, 0.07% Mo, 3.96% Ni, 0.59% W
0.46% C, 0.24% Si, 0.50% Mn, 0.018% P, 0.007% S, 1.53% Cr, 0.20% Cu, 0.07% Mo, 3.96% Ni, 0.59% W
0.46% C, 0.25% Si, 0.65% Mn, 0.50% Cr
0.46% C, 0.28% Si, 0.77% Mn, 0.016% P, 0.025% S, 0.15% Ni, 1.06% Cr, 0.22% Mo
0.46% C, 0.29% Si, 0.29% Mn, 0.012% P, 0.013% S, 1.42% Cr, 3.94% Ni, 0.01% V, 0.17% Cu, 0.24% Mo
0.46% C, 0.29% Si, 0.29% Mn, 0.012% P, 0.013% S, 1.42% Cr, 3.94% Ni, 0.01% V, 0.17% Cu, 0.24% Mo
0.46% C, 0.29% Si, 0.29% Mn, 0.012% P, 0.013% S, 1.42% Cr, 3.94% Ni, 0.01% V, 0.17% Cu, 0.24% Mo
0.46% C, 0.31% Si, 0.29% Mn, 0.010% P, 0.005% S, 1.32% Cr, 3.99% Ni, 0.13% Cu, 0.22% Mo
0.46% C, 0.31% Si, 0.29% Mn, 0.010% P, 0.005% S, 1.32% Cr, 3.99% Ni, 0.13% Cu, 0.22% Mo
0.46% C, 0.35% Si, 0.30% Mn, 13.80% Cr
0.46% C, 0.39% Mn, 1.40% Si, 0.30% Ni, 1.41% Cr 0.10% V, 0.0017% B
0.46% C, 0.70% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.50% Cr
0.46% C, 0.75% Mn, 0.02% P, 0.034% S, 0.03% Ni, 0.12% Cr
0.46% C, 0.79% Mn, 0.91% Ni, 0.77% Cr, 0.18% Mo, 0.0021% B
0.46% C, 0.79% Mn, 0.91% Ni, 0.77% Cr, 0.18% Mo, 0.0021% B
0.46% C, 0.85% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.00% Cr, 0.20% Mo
0.46% C, 1.59% Si, 0.68% Mn, 0.75% Cr, 0.43% Mo, 0.08% V, 0.04% Cu
0.46% C, 1.80% Mn, 0.25% Si, 0.020% P, 0.015% S
0.46% C, 1.80% Si, 0.70% Mn
0.46% C, 1.80% Si, 0.70% Mn
0.46% C, 13.50 Cr
0.46% C, 2.83% Si, 0.46% Mn, 0.017% P, 0.008% S, 9.48% Cr, 0.02% Mo, 0.56% Ni, 0.040% V, 0.0290% Nb
0.46-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.50% C, 0.40% Si, 0.50-0.80% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.52% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu
0.46-0.52% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo, max. 0.30% Cu
0.46-0.54% C, <0.40% Si, 0.50-0.80% Mn, <0.035% P, <0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, 1.40-1.80% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.80-1.10% Cr, 0.20-0.35% Mo
0.46-0.54% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46-0.54% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.035% S, 0.90-1.20% Cr, 0.15-0.30% Mo
0.46% C, 1.00% Cr, 1.00% Mo, 0.55% Ni
0.46% C, 0.29% Si, 0.39% Mn, 0.012% P, 0.026% S, 0.003% Al, 0.12% Cr, 0.215% Cu, 0.006% N
0.46% C, 0.29% Si, 0.39% Mn, 0.012% P, 0.026% S, 0.003% Al, 0.12% Cr, 0.215% Cu, 0.006% N
0.46% C, 0.42% Si, 0.54% Mn, 0.033% P, 0.016% S, 0.005% Al, 12.70% Cr, 0.16% Cu, 0.05% Mo, 0.34% Ni
0.46% C, 0.42% Si, 0.54% Mn, 0.033% P, 0.016% S, 0.005% Al, 12.70% Cr, 0.16% Cu, 0.05% Mo, 0.34% Ni
0.47% C, 0.27% Si, 0.90% Mn, 1.10% Cr
0.47% C, 0.29% Si, 0.67% Mn, 0.011% P, 0.002% S, 0.91% Cr, 1.46% Ni, 0.13% V, 0.21% W, 0.22% Cu, 0.017% Sn
0.47% C, 0.29% Si, 0.67% Mn, 0.011% P, 0.002% S, 0.91% Cr, 1.46% Ni, 0.13% V, 0.21% W, 0.22% Cu, 0.017% Sn
0.47% C, 0.36% Mn, 1.37% Mn, 0.015% P, 0.025% S, 0.15% Cr, 0.02% Ni, 0.19% Cu
0.47% C, 0.36% Si, 1.37% Mn, 0.015% P, 0.025% S, 0.15% Cr, 0.02% Ni, 0.19% Cu
0.47% C, 0.67% Mn, 0.06% Cu
0.47% C, 0.82% Mn, 0.35% Si, 0.015% S, 0.035% P, 1.20% Cr, 0.04% Ni, 0.11% V, 0.14% Cu
0.47% C, 0.82% Mn, 0.35% Si, 0.015% S, 0.035% P, 1.20% Cr, 0.04% Ni, 0.11% V, 0.14% Cu
0.47% C, 1.04% Mn, 0.35% Si, 0.012% S, 0.032% P, 1.20% Cr, 0.05% Ni, 0.05% Mo, 0.12% V, 0.16% Cu
0.47% C, 1.04% Mn, 0.35% Si, 0.012% S, 0.032% P, 1.20% Cr, 0.05% Ni, 0.05% Mo, 0.12% V, 0.16% Cu
0.47% C, 1.37% Mn, 0.36% Si, 0.025% S, 0.015% P 0.02% Ni, 0.15% Cr, 0.19% Cu
0.47% C, 1.37% Mn, 0.36% Si, 0.025% S, 0.015% P 0.02% Ni, 0.15% Cr, 0.19% Cu
0.47% C, 1.70% Si, 0.67% Mn, 0.023% P, 0.027% S, 0.20% Cr, 0.11% Ni, 0.01% V, 0.31% Cu, 0.04% Mo, 0.024% Sn
0.47-0.55% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.20% Cr, 0.10-0.20% V
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.47-0.55% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.55% C, 0.70-1.10% Mn, 0.15-0.40% Si, 0.80-1.20% Cr, 0.07-0.12% V
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47-0.55% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.47% C, 0.35% Si, 1.04% Mn, 0.032% P, 0.012% S, 1.20% Cr, 0.05% Ni, 0.05% Mo, 0.16% Cu, 0.12% V
0.47-0.55% C, 0.60-0.90% Mn, max. 0.040% P, max. 0.050% S
0.47-0.55% C, 0.40% Si, 0.70-1.10% Mn, 0.035% P, 0.035% S, 0.90-1.20% Cr, 0.10-0.25% V
0.47-0.53% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.30% Cu, max. 0.20% Ni, max. 0.20% Cr
0.48% C, <0.01% Mn, 0.011% Si, 0.003% P, 0.004% S, 7.64% Ni, <0.01% Cr, <0.01% Al
0.48% C, 0.22% Mn, 0.16% Si, 0.006% P, 0.016% S 7.61% Ni
0.48% C, 0.25% Si, 0.86% Mn, 0.023% P, 0.021% S, 0.18% Ni, 0.98% Cr, 0.04% Mo, 0.09% Cu
0.48% C, 0.27% Mn, 0.67% Si, 0.005% S, 0.010% P 0.14% Ni, 1.20% Cr, 0.02% Mo, 0.21% Cu, 0.013% V, 2.34% W
0.48% C, 0.28% Si, 1.98% Mn, 0.020% P, 0.011% S
0.48% C, 0.35% Si, 0.30% Mn, 14.40% Cr, 0.60% Mo, 0.12% V
0.48% C, 0.57% Mn, 0.20% Si, 0.46% Cu
0.48% C, 0.57% Mn, 0.46% Cu
0.48% C, 0.75% Mn, 0.34% Si, 0.020% P, 0.010% S, 0.58% Cr, 0.60% Ni, 0.20% Mo
0.48% C, 0.80% Mn, 0.30% Si, 0.025% P, 0.020% S, 0.26% Mo
0.48% C, 0.80% Si, 0.40% Mn, 0.020% P, 0.003% S, 8.00% Cr, 1.40% Mo, 1.40% V
0.48% C, 0.83% Mn, 0.28% Si, 0.019% P, 0.015% S, 0.14% Ni, 0.13% Cr, 0.25% Mo
0.48% C, 0.86% Mn, 0.25% Si, 0.18% Ni, 0.98% Cr 0.04% Mo
0.48% C, 0.94% Mn, 0.25% Mo
0.48% C, 0.94% Mn, 0.25% Mo
0.48-0.53% C, 0.80-1.10% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 4.80-5.20% Cr, 1.25-1.45% Mo, 0.80-1.00% V
0.48-0.55% C, 0.15-0.35% Si, 0.75-1.00% Mn, max. 0.035% P, max. 0.035% S, 0.40-0.60% Cr, min. 0.0008% B
0.48-0.56% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% Ni
0.48-0.56% C, 0.40% Si, 0.70-1.10% Mn, 0.025% P, 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% Ni
0.48-0.56% C, max. 0.40% Si, 0.70-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.48-0.56% C, max. 0.40% Si, 0.70-1.10% Mn, max. 0.025% P, max. 0.025% S, 0.90-1.20% Cr, 0.15-0.30% Mo, 0.10-0.20% V
0.48% C, 0.22% Si, 0.88% Mn, 0.013% P, 0.025% S
0.48?0.53% C, 0.70?0.90% Mn, 0.20?0.35% Si, max. 0.040% P, max. 0.40% S, 0.80?1.10% Cr, max. 0.15% V
0.48?0.53% C, 0.70?0.90% Mn, 0.20?0.35% Si, max. 0.040% P, max. 0.40% S, 0.80?1.10% Cr, max. 0.15% V
0.49% C, 0.20% Si, 0.67% Mn, 0.015% P, 0.015% S, 0.98% Cr, 0.14% Ni, 0.25% Cu, 0.18% Mo
0.49% C, 0.20% Si, 0.67% Mn, 0.015% P, 0.015% S, 0.98% Cr, 0.14% Ni, 0.25% Cu, 0.18% Mo
0.49% C, 0.23% Si, 0.90% Mn, 0.016% P, 0.010% S, 1.03% Cr, 0.12% V
0.49% C, 0.23% Si, 0.90% Mn, 0.016% P, 0.010% S, 1.03% Cr, 0.12% V
0.49% C, 0.23% Si, 0.90% Mn, 0.016% P, 0.010% S, 1.03% Cr, 0.12% V
0.49% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.49% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.49% C, 0.26% Si, 0.74% Mn
0.49% C, 0.33% Si, 0.41% Mn, 0.017% P, 0.009% S, 2.97% Ni, 1.87% Cr
0.49% C, 0.52% Mn, 0.007% P, 0.016% S, 0.28% Si, 5.00% Ni, 0.07% Cr, 0.03% Mo
0.49% C, 0.54% Mn, 0.20% Si, 0.00% Cr, 1.49% Cu
0.49% C, 0.54% Mn, 1.49% Cu
0.49% C, 0.57% Mn, 0.26% Si, 0.012% S, 0.011% P 1.62% Ni, 0.83% Cr, 0.24% Mo, 0.13% Cu
0.49% C, 0.57% Mn, 0.26% Si, 0.012% S, 0.011% P 1.62% Ni, 0.83% Cr, 0.24% Mo, 0.13% Cu
0.49% C, 0.57% Mn, 0.97% Cu
0.49% C, 0.77% Mn, 1.35% Si, 0.77% Cr, 0.55% Ni, 0.04% Mo
0.49% C, 0.78% Mn, 0.26% Si, 0.012% S, 0.018% P, 1.04% Cr, 0.50% Ni, 0.96% Mo, 0.09% V
0.49% C, 0.95% Si, 0.41% Mn, 0.018% P, 0.016% S, 4.74% Cr, 1.48% Ni, 1.28% V, 0.07% W, 0.018% Cu, 1.45% Mo
0.49% C, 4.13% Si, 0.58% Mn, 0.012% P, 0.012% S, 2.71% Cr
0.49-0.53% C, 0.20-0.30% Si, 0.85-1.00% Mn, 0.025% P, 0.015-0.030% S, 1.00-1.15% Cr, 0.15-0.25% Ni, 0.05-0.10% Mo, 0.10-0.20% V
0.49-0.56% C, 0.70-0.90% Mn, 1.20-1.50% Si, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49-0.56% C, 1.20-1.50% Si, 0.70-0.90% Mn, 0.035% P, 0.035% S, 0.70-1.00% Cr, 0.50-0.70% Ni
0.49% C, 1.11% Cr, 0.46% Ni, 0.98% Mo, 0.11% V, 0.20% Cu, 0.23% Si, 0.79% Mn, 0.015% S, 0.010% P
0.49% C, 0.26% Si, 0.74% Mn
0.49% C, 0.26% Si, 0.74% Mn
0.49% C, 0.26% Si, 0.74% Mn
0.49% C, 0.26% Si, 0.74% Mn, 0.005% P, 0.018% S, 0.014% Al, 0.16% Cr, 0.0115% N, 0.01% V
0.49% C, 0.46% Si, 0.63% Mn, 0.024% P, 0.025% S, 0.13% Cu, 0.13% Cr, 0.04% Ni, 0.05% Mo, 0.07% Al, 0.01% V
0.491% C, 0.21% Si, 0.647% Mn, 0.005% P, 0.004% S, 1.039% Cr, 0.219% Cu, 0.133% Mo, 0.092% Ni, 0.024% Al, 0.020% Nb
0.5% C, 0.2% Si, 0.5% Mn, 5.0% Cr, 2.3% Mo, 0.5% V
0.5% C, 1.0% Si, 0.5% Mn, 8.0% Cr, 1.5% Mo, 0.5% V
0.5% C, 2% Ni, 0.85% Mo
0.50% C, 0.11% O, 0.0093% S, 0.196% Mn, 0.549% Mo, 1.812% Ni
0.50% C, 0.17% Si, 1.50% Mn, 0.10% Ni, 0.20% Cr, 0.45% Mo
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 3.00% Mo, 0.55% V
0.50% C, 0.23% Mn, 0.53% Si, 0.05% Cr
0.50% C, 0.24% Si, 0.85% Mn, 0.013% P, 0.002% S, 1.05% Cr, 0.15% V
0.50% C, 0.24% Si, 0.85% Mn, 0.013% P, 0.002% S, 1.05% Cr, 0.15% V
0.50% C, 0.25% Si, 0.65% Mn, 1.005% Cr, 0.25% Mo
0.50% C, 0.25% Si, 0.65% Mn, 1.005% Cr, 0.25% Mo
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% Mo
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% P, (Pb)
0.50% C, 0.25% Si, 0.70% Mn, 1.10% Cr, 0.20% P, (Pb)
0.50% C, 0.25% Si, 0.75% Mn, <0.03% S
0.50% C, 0.25% Si, 0.75% Mn, <0.030% S, (Pb)
0.50% C, 0.25% Si, 0.90% Mn, 1.05% Cr, 0.15% V
0.50% C, 0.25% Si, 0.90% Mn, 1.05% Cr, 0.15% V
0.50% C, 0.25% Si, 0.90% Mn, 1.05% Cr, 0.15% V
0.50% C, 0.25% Si, 0.90% Mn, 1.05% Cr, 0.15% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.10% V, 0.25% Mo
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.10% V, 0.25% Mo
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V, (Pb)
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V, (Pb)
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.12% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.25% Si, 0.90% Mn, 1.10% Cr, 0.25% Mo, 0.10% V
0.50% C, 0.30% Si, 0.40% Mn, 5.00% Cr, 1.90% Mo, 0.55% V, +Nb
0.50% C, 0.30% Si, 0.50% Mn, 1.00% Cr, 3.30% Ni
0.50% C, 0.30% Si, 0.50% Mn, 1.00% Cr, 3.30% Ni
0.50% C, 0.31% Si, 1.06% Mn, 0.013% P, 0.003% S, 1.12% Cr, 0.24%Mo, 0.083% V
0.50% C, 0.31% Si, 1.06% Mn, 0.013% P, 0.003% S, 1.12% Cr, 0.24%Mo, 0.083% V
0.50% C, 0.32% Si, 0.80% Mn, 0.017% P, 0.022% S, 1.04% Cr, 0.17% Cu, 0.24% Mo, 0.11% Ni, <0.01% V
0.50% C, 0.32% Si, 0.80% Mn, 0.017% P, 0.022% S, 1.04% Cr, 0.17% Cu, 0.24% Mo, 0.11% Ni, <0.01% V
0.50% C, 0.35% Mn, 1.00% Si, 0.018% P, 0.013% S, 0.19% Ni, 0.11% Cr, 0.50% Mo
0.50% C, 0.38% Si, 0.40% Mn, 0.018% P, 0.003% S, 3.25% Cr, 0.19% Ni, 0.09% V, 0.17% Cu, 1.39% Mo
0.50% C, 0.38% Si, 0.40% Mn, 0.018% P, 0.003% S, 3.25% Cr, 0.19% Ni, 0.09% V, 0.17% Cu, 1.39% Mo
0.50% C, 0.40% Mn, 1.00% Si, 0.50% Mo
0.50% C, 0.40% Si, 0.78% Mn, 0.010% P, 0.027% S, 0.52% Cr, 0.03% Mo, 0.48% Ni, 0.12% Cu
0.50% C, 0.53% Si, 0.23% Mn, 0.005% Cr
0.50% C, 0.67% Mn, 0.24% Si, 0.0022% S, 0.031% P
0.50% C, 0.71% Mn, 0.30% Si, 3.20% Cr, 1.32% Mo
0.50% C, 0.71% Mn, 0.30% Si, 3.20% Cr, 1.32% Mo
0.50% C, 0.73% Mn, 3.92% Ni, 0.04% Cr
0.50% C, 0.75% Mn, 0.25% Si, 0.025% P, 0.025% S, 0.95% Cr, 0.15% Ni, 0.05% Mo, 0.20% V
0.50% C, 0.75% Mn, 0.35% Si, 0.025% P, 0.020% S, 1.20% Cr
0.50% C, 0.77% Mn, 0.60% Ni, 0.51% Cr, 0.22% Mo (0.21% Mo for 86B50, plus 0.0016%B)
0.50% C, 0.77% Si, 0.60% Ni, 0.50% Cr, 0.21% Mo, 0.0016% B
0.50% C, 0.78% Mn, 0.40% Si, 0.027% S, 0.010% P 0.48% Ni, 0.52% Cr, 0.03% Mo, 0.12% Cu
0.50% C, 0.78% Mn, 0.40% Si, 0.027% S, 0.010% P 0.48% Ni, 0.52% Cr, 0.03% Mo, 0.12% Cu
0.50% C, 0.85% Mn, 0.25% Si, 0.020% P, 0.020% S, 1.00% Cr, 0.22% Mo
0.50% C, 0.85% Mn, 0.25% Si, 0.90% Ni, 1.15% Cr, 0.50% Mn
0.50% C, 0.86% Si, 0.74% Mn, 0.023% P, 0.004% S, 7.65% Cr, 0.19% Ni, 1.60% V, 0.07% W, 0.16% Cu, 1.44% Mo, 0.012% Al
0.50% C, 0.86% Si, 0.74% Mn, 0.023% P, 0.004% S, 7.65% Cr, 0.19% Ni, 1.60% V, 0.07% W, 0.16% Cu, 1.44% Mo, 0.012% Al
0.50% C, 0.90% Si, 0.80% Mn, 8.00% Cr, 1.50% Mo, 1.70% V
0.50% C, 0.91 % Mn
0.50% C, 0.91% Mn, 0.00% Mn
0.50% C, 0.91% Mn, 0.046% P, 0.041% S, 0.13% Si
0.50% C, 0.91% Mn
0.50% C, 0.91% Mn
0.50% C, 0.91% Mn
0.50% C, 1.00% Si, 0.35% Mn, 0.018% P, 0.013% S, 0.19% Ni, 0.11% Cr, 0.50% Mo
0.50% C, 1.00% Si, 5.00% Cr, 1.40% Mo
0.50% C, 1.05% Mn, 1.48% Si, 0.044% S, 0.048% P <0.05% Ni, 1.20% Cr, 0.20% Mo, 0.04% Cu
0.50% C, 1.10% Cr, 3.20% Ni
0.50% C, 1.20% Mn
0.50% C, 1.25% Cr, 0.20% V, 2.75% W
0.50% C, 1.25% Cr, 0.20% V, 2.75% W
0.50% C, 1.25% Mn, 0.08% S, 0.65% Cr, 0.18% Mo
0.50% C, 5.00% Cr, 1.30% Mo, 1.30% W, 0.40V
0.50% C, 7.80% Cr, 1.50% Mo
0.50% C, 8.50% Cr, 1.20% Mo, 1.20% W
0.50% C, max. 0.40% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.010% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni, max. Cr+Ni+Mo=0.63
0.50-0.54% C, 0.20-0.30% Si, 0.85-0.95% Mn, 0.012-0.021% S, 0.025% P, 0.80-0.10% Cr, 0.08-0.10% Mo, 0.15% N
0.50-0.55% C, 0.15-0.40% Si, 0.60-0.90% Mn, 0.025% P, 0.001% S, 0.90-1.20% Cr, 0.25% Ni, 0.15-0.25% Mo
0.50-0.57% C, 0.15-0.30% Si, 0.40-0.70% Mn, <0.025% P, <0.035% S
0.50-0.57% C, 0.25-0.50% Si, 0.40-0.70% Mn, 0.045% P, 0.045% S
0.50-0.57% C, 0.80-1.00% Si, 0.80-1.20% Mn, max. 0.035% P, max. 0.035% S
0.50-0.58% C, max. 0.15% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.030% S
0.50-0.58% C, max. 0.15% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.030% S
0.50-0.60% C, <1.00% Mn, 13.00-15.00% Cr, 0.50-0.60% Mo
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.025% P, 0.010% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 0.05-0.15% V, 1.50-1.80% Ni
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.030% S, 0.80-1.20% Cr, 0.35-0.55% Mo, 1.50-1.80% Ni, 0.05-0.15% V
0.50-0.60% C, 0.10-0.40% Si, 0.65-0.95% Mn, max 0.030% P, max. 0.030% S, 0.60-0.80% Cr, 0.25-0.35% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50-0.60% C, 0.15-0.35% Si, 0.50-0.80% Mn, max. 0.025% P, max. 0.025% S, 0.60-0.80% Cr, 0.25-0.35% Mo, 0.070-0.12% V, 1.50-1.80% Ni
0.50-0.60% C, 0.65-0.95% Mn, 0.10-04.0% Si, 1.00-1.20% Cr, 0.45-0.55% Mo, 0.07-0.12% V, 1.50-1.80% Ni
0.50-0.60% C, 0.70-0.90% Mn, 1.70-2.10% Si, 0.30% Cr, 0.25-0.45% Mo
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 0.55% V
0.50% C, 0.20% Si, 0.25% Mn, 4.50% Cr, 0.55% V
0.50% C, 0.30% Si, 0.48% Mn, 0.02% P, 0.02% S
0.50% C, 0.30% Si, 0.48% Mn, 0.02% P, 0.02% S
0.50-0.60% C, 0.10-0.40% Si, 0.65-0.95% Mn, max 0.030% P, max. 0.030% S, 0.60-0.80% Cr, 0.25-0.35% Mo, 1.50-1.80% Ni, 0.07-0.12% V
0.50% C, 0.23% Si, 0.68% Mn, 0.035% S, 0.98% Cr, 0.21% Ni, 0.19% Mo, 8 ppm O, 2 ppm Ca
0.50% C, 0.30% Si, 0.48% Mn, 0.02% P, 0.02% S
0.51% C, 0.17% Si, 0.23% Mn, 0.006% P, 0.017% S, 5.20% Ni, 0.04% Cr, 0.01% Mo
0.51% C, 0.21% Mn, 0.16% Si, 0.005% P, 0.016% S 10.11% Ni
0.51% C, 0.23% Mn, 0.17% Si, 0.006% P, 0.017% S 5.26% Ni
0.51% C, 0.23% Si, 0.35% Mn, 0.012%P, 0.013% S, 1.07% Cr, 0.25% Mo, 3.08% Ni, 0.05% W
0.51% C, 0.23% Si, 0.35% Mn, 0.012%P, 0.013% S, 1.07% Cr, 0.25% Mo, 3.08% Ni, 0.05% W
0.51% C, 0.25% Mn, 3.80% Si, 0.32% Cr
0.51% C, 0.25% Si, 0.81% Mn, 0.26% Mo
0.51% C, 0.27% Si, 0.72% Mn, 0.020% S, 0.021% P, 0.15% Ni, 0.94% Cr, 0.05% Mo, 0.20% V
0.51% C, 0.27% Si, 0.72% Mn, 0.021% P, 0.020% S, 0.15% Ni, 0.94% Cr, 0.05% Mo, 0.20% V, 0.11% W, 0.15% Cu
0.51% C, 0.34% Mn, 0.40% Si, 4.80% Cr, 1.99% Mo, 0.32% Ni
0.51% C, 0.34% Mn, 0.40% Si, 4.80% Cr, 1.99% Mo, 0.32% Ni
0.51% C, 0.34% Si, 0.52% Mn, 0.009% P, 0.016% S, 1.05% Cr, 0.15% Ni, 0.01% V, 0.23% Cu, 0.20% Mo, 0.026% Al, 0.026% Sn
0.51% C, 0.34% Si, 0.52% Mn, 0.009% P, 0.016% S, 1.05% Cr, 0.15% Ni, 0.01% V, 0.23% Cu, 0.20% Mo, 0.026% Al, 0.026% Sn
0.51% C, 0.34% Si, 0.52% Mn, 0.009% P, 0.016% S, 1.05% Cr, 0.15% Ni, 0.01% V, 0.23% Cu, 0.20% Mo, 0.026% Al, 0.026% Sn
0.51% C, 0.34% Si, 0.52% Mn, 0.009% P, 0.016% S, 1.05% Cr, 0.15% Ni, 0.01% V, 0.23% Cu, 0.20% Mo, 0.026% Al, 0.026% Sn
0.51% C, 0.40% Mn, 0.41% Si, 0.023% P, 0.030% S, 3.94% Cr, 2.45% Mo, 1.24% V, 1.50% W
0.51% C, 0.72% Mn, 0.27% Si, 0.020% S, 0.021% P, 0.94% Cr, 0.20% V
0.51% C, 0.72% Mn, 0.27% Si, 0.15% Ni, 0.94% Cr 0.05% Mo
0.51% C, 0.73% Mn, 2.74% Ni, 0.99% Cr, 0.45% Mo
0.51% C, 0.73% Mn, 2.74% Ni, 0.99% Cr, 0.45% Mo
0.51% C, 0.81% Mn, 0.25% Si, 0.26% Mo
0.51% C, 0.85% Si, 0.30% Mn, 4.90% Cr, 1.35% Mo, 0.90% V
0.51% C, 0.91% Si, 0.88% Mn, 0.019% P, 0.017% S, 0.27% Cr, 0.13% Ni, 0.18% Cu, 0.05% Mo
0.51% C, 0.95% Si, 0.31% Mn, 0.014% S, 5.04% Cr, 1.33% Mo, 0.13% Ni, 1.34% V, 0.04% W
0.51% C, 1.17% Si, 0.37% Mn, 0.014% P, 0.010% S, 5.47% Cr, 0.30% Ni, 0.75% V, 0.19% Cu, 1.37% Mo, 0.027% Al
0.51% C, 1.17% Si, 0.37% Mn, 0.014% P, 0.010% S, 5.47% Cr, 0.30% Ni, 0.75% V, 0.19% Cu, 1.37% Mo, 0.027% Al
0.51% C, 1.52% Si, 0.60% Mn, 0.014% P, 0.009% S, 1.41% Cr, 0.14% V
0.51% C, 1.65% Si, 0.65% Mn
0.51% C, 1.65% Si, 0.65% Mn
0.51% C, 1.75% Si, 0.70% Mn
0.51% C, 1.75% Si, 0.70% Mn
0.51% C, 3.80% Si, 0.25% Mn, 0.32% Cr
0.51-0.59% C, 1.20-1.60% Si, 0.50-0.80% Mn, 0.030% P, 0.030% S, 0.50-0.80% Cr
0.51% C, 1.10% Cr, 0.20% V
0.51% C, 1.10% Cr, 0.20% V
0.51% C, 0.32% Si, 0.68% Mn, 0.014% P, 0.009% S, 1.06% Cr, 0.14% Cu, 0.21% Mo, 0.014% N, 0.01% Nb, 0.15% Ni, 0.014% V
0.51% C, 0.32% Si, 0.68% Mn, 0.014% P, 0.009% S, 1.06% Cr, 0.14% Cu, 0.21% Mo, 0.014% N, 0.01% Nb, 0.15% Ni, 0.014% V
0.51% C, 0.02% Si, 0.38% Mn, 0.014% P, 0.017% S
0.52% C, 0.02% Si, 0.38% Mn, 0.014% P, 0.017% S
0.52% C, 0.20% Si, 0.70% Mn, 0.020% P, 0.002% S, 0.75% Cr, 1.75% Ni, 0.30% Mo, 0.10% V
0.52% C, 0.20% Si, 0.70% Mn, 0.020% P, 0.002% S, 0.75% Cr, 1.75% Ni, 0.30% Mo, 0.10% V
0.52% C, 0.25% Si, 0.88% Mn, 0.50% Cr + B
0.52% C, 0.25% Si, 0.88% Mn, 0.50% Cr + B
0.52% C, 0.25% Si, 1.75% Mn, 0.10% V
0.52% C, 0.25% Si, 1.75% Mn, 0.10% V
0.52% C, 0.29% Si, 0.70% Mn, 0.010% P, 0.010% S, 1.09% Cr, 0.43% Mo, 1.72% Ni, 0.14% V
0.52% C, 0.29% Si, 0.70% Mn, 0.010% P, 0.010% S, 1.09% Cr, 0.43% Mo, 1.72% Ni, 0.14% V
0.52% C, 0.30% Si, 0.49% Mn, 0.70% Cr, 2.66% Ni
0.52% C, 0.30% Si, 1.18% Mn, 0.16% Ni, 0.13% Cr, 0.30% Mo
0.52% C, 0.42% Mn, 0.47% Si, 0.028% P, 0.030% S, 3.97% Cr, 3.15% Mo, 1.15% V, 0.99% W
0.52% C, 0.60% Mn, 0.28% Si, 0.017% S, 0.020% P 0.05% Ni, <0.04% Cr, <0.05% Mo
0.52% C, 0.60% Mn, 0.40% Si, 0.011% S, 0.013% P 0.17% Ni, 1.00% Cr, 0.22% Mo, 0.38% Cu, <0.05% V
0.52% C, 0.60% Mn, 0.40% Si, 0.011% S, 0.013% P 0.17% Ni, 1.00% Cr, 0.22% Mo, 0.38% Cu, <0.05% V
0.52% C, 0.7% Mn, 0.29% Si, 1.09% Cr, 1.72% Ni, 0.43% Mo, 0.14% V
0.52% C, 0.7% Mn, 0.29% Si, 1.09% Cr, 1.72% Ni, 0.43% Mo, 0.14% V
0.52% C, 0.70% Mn, 0.29% Si, 0.010% S, 0.010% P, 1.09% Cr, 1.12% Ni, 0.43% Mo, 0.14% V
0.52% C, 0.80% Si, 1.30% Cr, 2.15% W, 0.15% V
0.52-0.59% C, 0.25-0.50% Si, 0.7-1.10% Mn, 0.030% P, 0.030% S, 0.70-1.10% Cr
0.52-0.59% C, max. 0.40% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.70-1.00% Cr
0.52-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%. C55R: 0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.020-0.040% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.030% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, 1.60-2.00% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, max. 0.30% Cu, max. 0.050% Al
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.015% S, max. 0.30% Cu, max. 0.050% Al
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52-0.60% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.52% C, 0.25% Si, 0.80% Mn, 0.025% P, 0.004% S, 1.10% Cr, 1.70% Ni, 0.45% Mo, 0.10% V
0.52% C, 0.29% Si, 0.70% Mn, 0.01% P, 0.01% S, 1.09% Cr, 1.72% Ni, 0.74% V
0.52% C, 0.80% Si, 0.33% Mn, 1.17% Cr, 2.25% W, 0.16% Ni
0.53% C, 0.7% Mn, 0.24% Ni, Cr + Mo + Ni <= 0.63%
0.53% C, 0.24% Mn, 2.32% Ni, 0.32% Cr
0.53% C, 0.25% Si, 0.55% Mn
0.53% C, 0.25% Si, 0.55% Mn
0.53% C, 0.30% Si, 0.50% Mn, 3.20% Cr, 1.50% Mo, max. 0.005% S
0.53% C, 0.30% Si, 0.70% Mn, 3.20% Cr, 1.50% Mo, max. 0.005% S
0.53% C, 0.35% Si, 0.70% Mn, 0.01% S, 0.020% P, 0.24% Ni, 0.09% Cr, <0.1% Mo, 0.52% Cu, 0.049% As, <0.03% Al
0.53% C, 0.62% Mn, 0.25% Si, 0.01% S, 0.015% P 1.23% Cr, 0.27% V
0.53% C, 0.67% Mn, 0.18% V, 0.93% Cr
0.53% C, 0.67% Mn, 0.93% Cr, 0.18% V
0.53% C, 0.67% Mn, 0.93% Cr, 0.18% V
0.53% C, 0.70% Mn, 0.35% Si, 0.010% S, 0.020% P 0.24% Ni, 0.09% Cr, <0.10% Mo, 0.52% Cu, <0.03% V
0.53% C, 0.81% Mn, 0.27% Si, 0.016% S, 0.024% P 0.07% Ni, 1.09% Cr, 0.01% Mo, 0.11% Cu, 0.10% V
0.53% C, 0.81% Mn, 0.27% Si, 0.016% S, 0.024% P 0.07% Ni, 1.09% Cr, 0.01% Mo, 0.11% Cu, 0.10% V
0.53% C, 0.83% Mn, 0.34% Si, 0.92% Cr, 0.21% Mo
0.53% C, 2.32% Si, 0.24% Mn, 0.32% Cr
0.53% C
0.53% C
0.53-0.59% C, 1.60-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.54% C, 0.21% Si, 0.44% Mn, 0.013% P, 0.021% S, 1.25% Cr, 0.59% Ni, 0.16% V, 0.21% Cu, 0.48% Mo, 0.010% Al
0.54% C, 0.23% Mn, 1.27% Si, 0.05% Cr
0.54% C, 0.25% Si, 0.80% Mn, 0.025% P, 0.004% S, 1.10% Cr, 1.70% Ni, 0.50% Mo, 0.10% V
0.54% C, 0.28% Si, 0.90% Mn, 1.05% Cr, 0.20% V, 0.20% Mo
0.54% C, 0.34% Mn, 0.26% Si, 3.92% Ni, 1.28% Cr 0.07% Mo
0.54% C, 0.34% Mn, 0.26% Si, 3.92% Ni, 1.28% Cr 0.07% Mo
0.54% C, 0.44% Mn, 0.33% Si, 0.023% P, 0.023% S, 4.02% Cr, 0.42% Mo, 1.24% V, 7.44% W
0.54% C, 0.45% Si, 0.40% Mn, 17.30% Cr, 1.10% Mo, 0.10% V, +N
0.54% C, 0.46% Mn/ 1.13% C, 0.30% Mn/ 1.13% C, 0.30% Mn Beginning of transformation at left, ending at right
0.54% C, 0.46% Mn
0.54% C, 0.46% Mn
0.54% C, 0.53% Mn, 0.36% Si, 0.005% S, 0.011% P 3.14% Ni, 1.02% Cr, 0.34% Mo
0.54% C, 0.62% Mn, 0.93% Si, 7.83% Cr, 6.90% W
0.54% C, 0.85% Mn, 1.90% Si, 0.030% P, 0.030% S, 0.10% Cr, 0.016% Ni, 0.02% Mo
0.54% C, 0.93% Si, 0.62% Mn, 7.83% Cr, 6.90% W
0.54% C, 1.27% Si, 0.23% Mn, 0.05% Cr
0.54% C, 1.44% Si, 0.74% Mn, 0.03% P, 0.02% S, 0.25% Cr, 0.17% Ni, 0.03% Mo, 0.28% Cu, 0.01% Al, 0.01% Si
0.545% C, 0.46% Mn, 0.26% Si, 4.12% Ni, 1.16% Cr 0.48% Mo, 0.80% W
0.55% C, 0.21% Si, 0.80% Mn, 0.016% P, 0.008% S, 1.01% Cr, 0.11% Ni, 0.12% V, 0.17% Cu, 0.03% Mo, 0.022% Al, 0.012% Sn
0.55% C, 0.21% Si, 0.80% Mn, 0.016% P, 0.008% S, 1.01% Cr, 0.11% Ni, 0.12% V, 0.17% Cu, 0.03% Mo, 0.022% Al, 0.012% Sn
0.55% C, 0.25% Si, 0.45% Mn, 1.00% Cr, 3.10% Ni
0.55% C, 0.25% Si, 0.75% Mn, <0.03% S
0.55% C, 0.25% Si, 0.75% Mn, <0.03% S
0.55% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, (Pb)
0.55% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, (Pb)
0.55% C, 0.25% Si, 0.75% Mn
0.55% C, 0.25% Si, 0.75% Mn
0.55% C, 0.25% Si, 0.95% Mn, 0.015% P, 0.005% S, 1.10% Cr, 2.00% Ni, 0.75% Mo, 0.10% V
0.55% C, 0.30% Si, 0.44% Mn, 0.022% P, 0.014% S, 13.26% Cr, 0.20% Ni, 0.14% V, 0.92% Cu, 1.95% Mo, 0.88% Co
0.55% C, 0.30% Si, 0.70% Mn, 1.10% Cr, 0.80% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.30% Si, 0.80% Mn, 1.10% Cr, 0.45% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.30% Si, 0.80% Mn, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 0.34% Mn, 0.94% Si, 0.012% S, 0.015% P, 1.27% Cr, 0.12% Ni, 0.05% Mo, 0.18% V, 2.10% W
0.55% C, 0.50% Mn, 0.87% Si, 0.035% S, 0.02% P, 0.10% Cr, 0.10% Ni, 0.55% Mo, 0.22% V
0.55% C, 0.52% Mn, 1.96% W
0.55% C, 0.58% Mn, 0.43% Si, 0.021% S, 0.013% P 0.20% Ni, 0.79% Cr, 0.42% Mo, 0.19% Cu
0.55% C, 0.60% Mn, 0.36% Ni, 1.03% Cr, 0.19% Mo
0.55% C, 0.60% Mn, 0.50% Si, 1.55% Ni, 1.00% Cr, 0.80% Mn
0.55% C, 0.60% Mn, 1.03% Cr, 0.19% Mo
0.55% C, 0.61% Mn, 1.68% Si, 0.014% S, 0.012% P 0.19% Ni, 0.05% Cr, 0.01% Mo, 0.20% Cu, trace V
0.55% C, 0.61% Mn, 1.68% Si, 0.014% S, 0.012% P 0.19% Ni, 0.05% Cr, 0.01% Mo, 0.20% Cu, trace V
0.55% C, 0.65% Mn, 0.20% Si, 0.025% P, 0.025% S, 0.65% Ni
0.55% C, 0.68% Mn, 0.30% Si, 0.004% S, 0.014% P 1.65% Ni, 1.00% Cr, 0.35% Mo, 0.11% Cu, 0.22% V, 0.08% W
0.55% C, 0.75% Mn, 1.50% Si, 0.020% P, 0.020% S, 0.70% Cr
0.55% C, 0.78% Mn, 1.62% Si, 0.77% Cr
0.55% C, 0.80% Cr, 0.30% Mo, 1.65% Ni, 0.10% V, 0.00% V
0.55% C, 0.80% Cr, 0.30% Mo, 1.65% Ni, 0.10% V, 0.00% V
0.55% C, 0.83% Mn, 1.15% Ni, 1.01% Cr, 0.48% Mo
0.55% C, 0.83% Mn, 1.15% Ni, 1.01% Cr, 0.48% Mo
0.55% C, 0.87% Mn, 1.74% Si, 0.16% Ni, 0.10% Cr 0.02% Mo
0.55% C, 0.88% Mn, 1.52% Si, 0.005% S, 0.032% P 0.07% Ni, 0.74% Cr, 0.01% Mo, 0.03% Cu
0.55% C, 0.90% Mn, 0.30% Si, 0.020% P, 0.005% S, 1.10% Cr, 1.70% Ni, 0.50% Mo, 0.10% V
0.55% C, 0.90% Mn, 0.30% Si, 0.020% P, 0.005% S, 1.10% Cr, 1.70% Ni, 0.50% Mo, 0.10% V
0.55% C, 0.90% Mn, 1.00% Si, 0.40% Cr, 2.75% Ni, 0.45% Mo, 0.13% V
0.55% C, 0.90% Mn, 1.00% Si, 2.75% Ni, 0.40% Cr 0.45% Mo, 0.13% V
0.55% C, 0.90% Mn, 1.00% Si, 2.75% Ni, 0.40% Cr, 0.45% Mo, 0.13% V
0.55% C, 0.98% Mn, 0.22% Si, 0.013% S, 0.017% P, 1.02% Cr, 0.01% Ni, 0.11% V, 0.07% Cu
0.55% C, 0.98% Mn, 0.22% Si, 0.013% S, 0.017% P, 1.02% Cr, 0.01% Ni, 0.11% V, 0.07% Cu
0.55% C, 0.98% Mn, 0.22% Si, 0.013% S, 0.017% P, 1.02% Cr, 0.01% Ni, 0.11% V, 0.07% Cu
0.55% C, 1.00% Si, 0.75% Mn, 2.60% Cr, 2.25% Mo, 0.85% V
0.55% C, 1.00% Si, 0.90% Mn, 0.40% Cr, 2.70% Ni, 0.13% V, 0.45% Mo
0.55% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.55% C, 1.10% Cr, 1.70% Ni, 0.50% Mo, 0.10% V
0.55% C, 1.62% Si, 0.78% Mn, 0.77% Cr
0.55% C, 1.89% Mn
0.55% C, 3.90% Cr, 0.45% Mo, 0.90% V
0.55-0.62% C, 0.15-0.35% Si, 0.80-1.10% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 0.07-0.12% V
0.55-0.63% C, 1.70-2.00% Si, 0.60-0.90% Mn, max. 0.035% P, max. 0.035% S, 0.35-0.45% Cr
0.55-0.65% C, 0.10-0.40% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.60-0.90% Cr
0.55-0.65% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.035% P, max. 0.035% S
0.55-0.65% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.035% P, max. 0.035% S
0.55-0.65% C, 0.15-0.45% Mn, 0.50-0.70% Si, 0.90-1.20% Cr, 1.80-2.10% W, 0.10-0.20% V
0.55-0.65% C, 0.20-0.40% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 3.70-4.20% Cr, 0.80-1.00% Mo, 8.50-9.50% W, 0.60-0.80% V
0.55-0.65% C, 0.20-0.40% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 3.70-4.20% Cr, 0.80-1.00% Mo, 8.50-9.50% W, 0.60-0.80% V
0.55-0.65% C, 0.70-1.00% Si, 0.15-0.45% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.70-2.20% Mo, 0.10-0.20% V
0.55-0.65% C, 0.70-1.00% Si, 0.15-0.45% Mn, max. 0.035% P, max. 0.035% S, 0.90-1.20% Cr, 1.70-2.20% Mo, 0.10-0.20% V
0.55% C, 1.10% Cr, 1.70% Ni, 0.50% Mo, 0.10% V
0.55% C, 0.25% Si, 0.45% Mn, 1.00% Cr, 3.10% Ni
0.56% C, 0.18% Si, 0.47% Mn, 0.028% S, 0.020% P, 4.25% Ni, 1.16% Cr, 0.18% Mo
0.56% C, 0.18% Si, 0.47% Mn, 0.028% S, 0.020% P, 4.25% Ni, 1.16% Cr, 0.18% Mo
0.56% C, 0.24% Si, 0.47% Mn, 0.025% P, 0.025% S, 1.13% Cr, 0.22% Mo, 4.02% Ni, 0.60% W
0.56% C, 0.25% Si, 0.70% Mn, 0.025% P, 0.003% S, 1.10% Cr, 1.70% Ni, 0.80% Mo, 0.10% V
0.56% C, 0.26% Mn, 1.97% Ni
0.56% C, 0.26% Mn, 1.97% Ni
0.56% C, 0.27% Mn, 0.23% Si, 0.17% Ni, 4.00% Cr 5.00% Mo, 1.80% V, 7.00% W, 0.40% Co
0.56% C, 0.30% Si, 0.70% Mn, 0.024% P, 0.032% S, 3.25% Cr, 0.13% Ni, 0.19% V, 0.23% Cu, 1.36% Mo
0.56% C, 0.30% Si, 0.70% Mn, 0.024% P, 0.032% S, 3.25% Cr, 0.13% Ni, 0.19% V, 0.23% Cu, 1.36% Mo
0.56% C, 0.32% Si, 0.86% Mn, 0.016% P, 0.009% S, 1.17% Cr, 0.11% Ni, 0.26% Cu, 0.21% Mo, 0.022% Al
0.56% C, 0.32% Si, 0.86% Mn, 0.016% P, 0.009% S, 1.17% Cr, 0.11% Ni, 0.26% Cu, 0.21% Mo, 0.022% Al
0.56% C, 0.39% Si, 0.34% Mn, 0.030% P, 0.001% S, 17.21% Cr, 1.06% Mo, 0.41% Ni, 0.09% V, +N
0.56% C, 0.47% Mn, 0.18% Si, 4.25% Ni, 1.16% Cr 0.18% Mo
0.56% C, 0.47% Mn, 0.18% Si, 4.25% Ni, 1.16% Cr 0.18% Mo
0.56% C, 0.47% Mn, 0.35% Si, 0.21% Cr, 0.10% Ni, 0.10% Mo
0.56% C, 0.47% Mn, 0.35% Si, 0.21% Cr, 0.10% Ni, 0.10% Mo
0.56% C, 0.67% Mn, 0.31% Si, 0.023% S, 0.012% P, 0.76% Cr, 1.53% Ni, 0.24% Mo, 0.14% V, 0.06% Cu, sol. 0.010% Al
0.56% C, 0.95% Si, 0.68% Mn, 0.014% P, 0.015% S, 0.56% C, 0.95% Si, 0.68% Mn, 0.014% P, 0.015% S, 0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.56% C, 1.45 Si, 0.70% Mn, max. 0.01% P, max. 0.01% S, 0.65% Cr
0.56% C, 1.54% Si, 0.70% Mn, max. 0.010% P, max. 0.010% S, 0.65% Cr, 0.16% V
0.56% C, 1.90% Si, 0.84% Mn, 0.11% Ni, 0.19% Cr
0.56% C, 1.91% Si, 0.77% Mn, 0.023% P, 0.004% S, 0.26% Cr, 0.11% Ni, 0.16% V, 0.32% Cu, 0.35% Mo
0.56% C, 1.91% Si, 0.77% Mn, 0.023% P, 0.004% S, 0.26% Cr, 0.11% Ni, 0.16% V, 0.32% Cu, 0.35% Mo
0.56-0.64% C, 1.50-1.80% Si, 0.70-1.00% Mn, 0.045% P, 0.045% S
0.56% C, 0.32% Si, 0.70% Mn, 0.016% P, 0.028% S
0.56% C, 0.32% Si, 0.70% Mn, 0.015% P, 0.015% S
0.56% C, 1.10% Cr, 0.50% Mo, 1.70% Ni, 0.10% V
0.57 % C, 2.36 % Ni, 0.75 % Cr , 0.41 % Mo
0.57% C, 0.24% Si, 0.76% Mn, 0.026% P, 0.003% S, 0.96% Cr, 0.22% Ni, 0.21% Cu, 0.17% Mo, 0.015% Al
0.57% C, 0.24% Si, 0.76% Mn, 0.026% P, 0.003% S, 0.96% Cr, 0.22% Ni, 0.21% Cu, 0.17% Mo, 0.015% Al
0.57% C, 0.27% Si, 0.75% Mn, 0.020% P, 0.015% S, 1.07% Cr, 0.83% Mo, 2.15% Ni, 0.10% V
0.57% C, 0.28% Si, 1.10% Mn, 0.012% P, 0.016% S, 0.030% Cr, 0.008% Mo, 0.016% Ni
0.57% C, 0.28% Si, 1.10% Mn, 0.012% P, 0.016% S, 0.030% Cr, 0.008% Mo, 0.016% Ni
0.57% C, 0.30% Si, 0.85% Mn, 0.80% Cr
0.57% C, 0.30% Si, 0.85% Mn
0.57% C, 0.30% Si, 0.85% Mn
0.57% C, 0.65% Mn, 0.31% Si, 0.005% S, 0.010% P 2.35% Ni, 0.75% Cr, 0.41% Mo, 0.13% Cu
0.57% C, 0.65% Mn, 0.31% Si, 0.005% S, 0.010% P 2.35% Ni, 0.75% Cr, 0.41% Mo, 0.13% Cu
0.57% C, 0.82% Mn, 0.30% Si, 0.016% P, 0.019% S, 1.16% Ni, 1.07% Cr, 0.26% Mo
0.57% C, 0.82% Mn, 1.16% Ni, 1.07% Cr, 0.26% Mo
0.57% C, 0.82% Mn, 1.16% Ni, 1.07% Cr, 0.26% Mo
0.57% C, 0.91% Mn, 1.95% Si
0.57-0.63% C, 0.50-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr, 0.07-0.25% V
0.57-0.63% C, 0.50-2.00% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr, 0.07-0.25% V
0.57-0.64% C, 1.60-2.00% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.57-0.64% C, 1.60-2.00% Si, 0.70-1.00% Mn, 0.025% P, 0.025% S, 0.20-0.45% Cr
0.57-0.64% C, 1.70-2.20% Si, 0.70-1.00% Mn, 0.035% P, 0.035% S, 0.40% Cr
0.57-0.65% C, <0.40% Si, 0.60-0.90% Mn, <0.045% S, <0.045% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mo+Ni<=063
0.57-0.65% C, <0.40% Si, 0.60-0.90% Mn, <0.045% S, <0.045% P, 0.40% Ni, <0.40% Cr, <0.10% Mo, Cr+Mo+Ni<=063
0.57-0.65% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.57-0.65% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.035% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%. C60R: 0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, <0.035% P, <0.020-0.040% S, <0.40% Cr, <0.10% Mo, <0.40% Ni, Cr+Mo+Ni=0.63%
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.020-0.040% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, 0.40% Si, 0.60-0.90% Mn, 0.035% P, 0.035% S, 0.40% Cr, 0.10% Mo, 0.40% Ni, Cr+Mo+Ni=0.63
0.57-0.65% C, 0.60-2.00% Si, 0.70-1.00% Mn, max. 0.025% P, max. 0.025% S, 0.20-0.45% Cr
0.57-0.65% C, 1.50-1.80% Si, 0.70-1.00% Mn, max. 0.030% P, max. 0.030% S, 0.20-0.40% Cr
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, 0.020-0.040% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.030% P, max. 0.035% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.57-0.65% C, max. 0.40% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.58% C, 0.25% Si, 0.25% Mn, 4.00% Cr, 0.90% Mo, 0.80% V, 9.00% W
0.58% C, 0.25% Si, 0.25% Mn, 4.00% Cr, 0.90% Mo, 0.80% V, 9.00% W
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V, (Pb)
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V, (Pb)
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.25% Si, 0.95% Mn, 1.10% Cr, 0.12% V
0.58% C, 0.43% Mn, 0.56% Si, 0.003% S, 0.013% P 7.38% Cr, 1.56% Mo, 0.06% V, 1.31% W
0.58% C, 0.62% Mn, 0.39% Si, 0.012% S, 0.015% P 1.68% Ni, 1.35% Cr, 0.40% Mo, 0.01% Cu, 0.10% V
0.58% C, 0.62% Mn, 0.39% Si, 0.012% S, 0.015% P 1.68% Ni, 1.35% Cr, 0.40% Mo, 0.01% Cu, 0.10% V
0.58% C, 0.65% Mn, 0.30% Si, 0.030% S, 0.013% P, 0.12% Cr, 0.05% Ni, 0.50% Mo, 0.03% V, 0.08% Cu, 0.031% Al
0.58% C, 0.81% Mn, 0.89% Si, 0.006% S, 0.013% P, 1.27% Cr, 0.06% Ni, 0.02% Mo, 0.11% V, 0.14% Cu
0.58% C, 0.89% Si, 0.81% Mn, 0.013% P, 0.006% S, 1.21% Cr, 0.11% V, 0.06% Ni, 0.02% Mo, 0.14% Cu
0.58% C, 0.89% Si, 0.81% Mn, 0.013% P, 0.006% S, 1.27% Cr, 0.14% Cu, 0.02% Mo, 0.06% Ni, 0.11% V
0.58% C, 0.89% Si, 0.81% Mn, 0.013% P, 0.006% S, 1.27% Cr, 0.14% Cu, 0.02% Mo, 0.06% Ni, 0.11% V
0.58% C, 0.89% Si, 0.81% Mn, 0.013% P, 0.006% S, 1.27% Cr, 0.14% Cu, 0.02% Mo, 0.06% Ni, 0.11% V
0.58% C, 0.89% Si, 0.81% Mn, 0.013% P, 0.006% S, 1.27% Cr, 0.14% Cu, 0.02% Mo, 0.06% Ni, 0.11% V
0.58% C, 0.90% Si, 1.00% Mn
0.58% C, 0.90% Si, 1.00% Mn
0.58% C, 0.90% Si, 1.00% Mn
0.58% C, 0.90% Si, 1.00% Mn
0.58% C, 0.95% Si, 0.63% Mn, 0.018% P, 0.004% S, 7.96% Cr, 0.15% Ni, 0.13% V, 1.13% W, 0.22% Cu, 1.26% Mo
0.58% C, 0.95% Si, 0.63% Mn, 0.018% P, 0.004% S, 7.96% Cr, 0.15% Ni, 0.13% V, 1.13% W, 0.22% Cu, 1.26% Mo
0.58% C, 1.00% Cr, 0.30% Mo, 3.00% Ni, 0.10% V
0.58% C, 1.00% Cr, 0.30% Mo, 3.00% Ni, 0.10% V
0.58% C, 1.10% Si, 1.07% Mn, 0.020% P, 0.024% S, 0.53% Cr
0.58% C, 1.75% Si, 0.75% Mn, 0.40% Cr
0.58% C, 1.75% Si, 0.75% Mn, 0.40% Cr
0.58% C, 1.75% Si, 0.80% Mn
0.58% C, 1.75% Si, 0.80% Mn
0.58-0.62% C, 0.20-0.50% Si, 0.70-0.90% Mn, max. 0.030% P, max. 0.030% S, 4.30-4.70% Cr, 0.20-0.30% V, 0.40-0.60% Mo
0.58-0.65% C, 0.80-1.00% Si, 0.80-1.20% Mn, max. 0.030% P, max. 0.030% S, 0.20-0.40% Cr
0.58-0.65% C, 0.80-1.00% Si, 0.80-1.20% Mn, max. 0.030% P, max. 0.030% S, 0.20-0.40% Cr
0.58% C, 0.55% Si, 0.32% Mn, 1.27% Cr, 2.25% W, 0.23% Ni
0.59% C, 0.20% Mn/ 0.16% C, 0.19% Mn, 0.94% Ni/ 0.57% C, 0.17% Mn, 1.94% Ni/ 0.55% C, 0.17% Mn, 3.88% Ni Beginning of transformation at left, ending at right
0.59% C, 0.25% Mn, 3.90% Ni
0.59% C, 0.25% Si, 0.95% Mn, 1.05% Cr, 0.10% V
0.59% C, 0.25% Si, 0.95% Mn, 1.05% Cr, 0.10% V
0.59% C, 0.26% Si, 0.34% Mn, 3.20% Ni, 2.26% Cr
0.59% C, 0.28% Si, 0.96% Mn, 1.06% Cr, 0.54% Mo, 0.12% V
0.59% C, 0.30% Mn/ 0.54% C, 0.45% Mn/ 0.50% C, 0.91% Mn./ 0.64% C, 1.13% Mn/ 0.65% C, 1.32 % Mn Beginning of transformation at left, ending at right
0.59% C, 0.30% Mn
0.59% C, 0.60% Mn, 0.25% Si, 0.025% P, 0.025% S, 0.65% Cr, 0.20% Ni
0.59% C, 0.66% Mn, 0.34% Si, 0.17% Ni, 0.65% Cr 0.02% Mo
0.59% C, 0.85% Mn, 1.90% Si, 0.030% P, 0.030% S
0.59% C, 0.89% Mn, 0.017% P, 0.016% S, 0.24% Si, 0.53% Ni, 0.64% Cr, 0.22% Mo
0.59% C, 0.89% Mn, 0.53% Ni, 0.64% Cr, 0.22% Mo
0.59% C, 0.89% Mn, 0.53% Ni, 0.64% Cr, 0.22% Mo
0.59% C, 0.90% Mn, 1.00% Cr, 0.10% V
0.59% C, 0.90% Mn, 1.00% Cr, 0.10% V
0.59% C, 0.96% Mn, 0.28% Si, 0.032% P, 0.022% S, 1.06% Cr, 0.54% Mo, 0.12% V
0.59% C, 1.68% Si, 0.73% Mn, 0.41% Cr, 0.19% Ni, 0.33% Mo
0.59% C, 1.68% Si, 0.73% Mn, 0.41% Cr, 0.19% Ni, 0.33% Mo
0.59% C, 1.97% Si, 0.76% Mn, 0.008% P, 0.004% S, 0.27% Cr, 0.18% Ni, 0.17% V, 0.14% Cu, 0.35% Mo
0.59% C, 1.97% Si, 0.76% Mn, 0.008% P, 0.004% S, 0.27% Cr, 0.18% Ni, 0.17% V, 0.14% Cu, 0.35% Mo
0.59% Ni, 0.25% Mn, 3.90% Ni
0.6% C, 1.8% Ni, 1.6% Cu, 0.55% Mo, Fe is balance
0.6% C, 1.88% Mn
0.60% C, 0.22% Mn, 0.19% Si, 0.20% Ni, 4.65% Cr 1.00% Mo, 1.35% V, 17.80% W, 0.72% Co
0.60% C, 0.25% Si, 0.75% Mn, <0.03% S
0.60% C, 0.25% Si, 0.75% Mn, <0.03% S
0.60% C, 0.25% Si, 0.75% Mn
0.60% C, 0.25% Si, 0.75% Mn
0.60% C, 0.26% Si, 0.39% Mn, 3.29% Ni, 2.22% Cr
0.60% C, 0.37% Mn, 0.24% Si, 3.22% Ni, 2.14% Cr, 0.07% Mo
0.60% C, 0.45% Mn, 0.017% P, 0.009% S, 0.18% Si, 3.33% Ni, 1.52% Cr, 0.03% Mo
0.60% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.60% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.60% C, 0.52% Mn, 0.007% P, 0.016% S, 0.28% Si, 5.00% Ni, 0.07% Cr, 0.03% Mo
0.60% C, 0.52% Mn, 5.00% Ni
0.60% C, 0.52% Mn, 5.00% Ni
0.60% C, 0.60% Mn, 0.30% Si, 0.035% P, 0.024% S, 2.75% Ni, 1.25% Cr, 0.50% Mo, 0.12% V
0.60% C, 0.60% Si, 0.30% Mn, 0.025% P, 0.010% S, 1.10% Cr, 0.60% Mo, 0.15% V, 2.00% W
0.60% C, 0.60% Si, 0.30% Mn, 1.10% Cr, 0.15% V, 2.00% W
0.60% C, 0.60% Si, 0.30% Mn, 1.10% Cr, 0.15% V, 2.00% W
0.60% C, 0.60% Si, 0.35% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.60% Si, 0.35% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.60% Si, 1.10% Cr, 0.20% V, 2.00% W
0.60% C, 0.69% Si, 0.34% Mn, 0.015% P, 0.012% S 1.19% Cr, 0.18% V, 2.00% W
0.60% C, 0.69% Si, 0.34% Mn, 0.015% P, 0.012% S 1.19% Cr, 0.18% V, 2.00% W
0.60% C, 0.75% Mn, 1.90% Si, 0.25% Cr, 0.30% Mo
0.60% C, 0.80% Mn, 0.35% Si, 5.30% Cr, 0.50% Mo, 0.20% V
0.60% C, 0.85% Mn, 0.25% Si, 0.020% P, 0.020% S, 0.80% Cr, 0.30% Mo
0.60% C, 0.85% Mn, 0.25% Si, 0.025% P, 0.025% S, 0.50% Cr, 0.60% Ni, 0.20% Mo
0.60% C, 0.85% Mn, 0.25% Si, 0.025% P, 0.025% S, 0.75% Cr
0.60% C, 0.85% Mn, 1.90% Si, 0.025% P, 0.025% S, 0.30% Cr, 0.25% Mo
0.60% C, 0.90% Si, 0.80% Mn, 1.10% Cr, 0.10% V
0.60% C, 1.00% Si, 1.00% Cr, 2.00% W, 0.20% V
0.60% C, 1.00% Si, 1.00% Mn, 5.00% Cr, 2.10% Mo, 0.50% V
0.60% C, 1.00% Si, 1.10% Mn, 0.30% Cr
0.60% C, 1.50% Si, 0.49% Mn, max. 0.01% P, max. 0.01% S, 0.55% Cr, 0.20% V
0.60% C, 1.80% Si, 0.40% Cr
0.60% C, 1.88% Mn
0.60% C, 2.00% W, 1.00% Cr, 0.15% V
0.60% C, 2.04% Mn, 0.0015% B
0.60% C, 5.00% Cr, plus Mo and V
0.60-0.65% C, 1.00-1.20% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.030% S, 5.00-5.50% Cr, 0.90-1.20% Mo, 0.15-0.35% V
0.60-0.65% C, 1.00-1.20% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.030% S, 5.00-5.50% Cr, 0.90-1.20% Mo, 0.15-0.35% V
0.60-0.65% C, 1.00-1.20% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.030% S, 5.00-5.50% Cr, 1.00-1.30% Mo, 0.25-0.35% V
0.60-0.70% C, 1.50-1.80% Si, 0.70-1.00% Mn, max. 0.035% P, max. 0.035% S
0.60-0.75% C, max. 1.00% Si, max. 1.00% Mn, max. 0.04% P, max. 0.03% S, 16.00-18.00% Cr, max. 0.75% Mo
0.60-0.80% C, 0.10-0.50% Si, 0.80-1.20% Mn, <0.05% P, <0.05% S. Steel THS 11: 0.65-0.75% C, <0.70% Si, 0.80-1.20% Mn, <0.03% P, <0.03% S, 0.80-1.20% Cr, 0.05-0.15% V
0.60-0.80% C, 0.50-1.10% Si, 0.80-1.20% Mn, max. 0.020% P, 0.008-0.025% S, 0.80-1.20% Cr, max. 0.02% Mo, max. 0.10% Ni, max. 0.18% V, max. 0.025% Ti, max. 0.15% Cu, max. 0.004% Al, max. 0.010% Nb
0.60% C, 1.50% Si, 1.25% Mn, 1.50% Cr
0.60% C, 1.50% Si, 0.75% Mn, 2.50% Cr
0.60% C, 1.50% Si, 1.25% Mn, 1.50% Cr, 0.03% Nb
0.60% C, 1.50% Si, 1.25% Mn, 1.50% Cr, 0.10% Mo
0.60% C, 4.50% Cr, 0.50% Mo, 0.20% V
0.60% C, 5.00% Cr, + Mo, + V
0.60% C, 0.90% Si, 0.80% Mn, 0.10% V
0.60% C, 0.60% Si, 0.35% Mn, 1.10% Cr, 0.20% V, 2.00% W
0.61% C, 0.01% Mn, 0.014% Si, 0.003% P, 0.005% S, <0.01% Ni, <0.01% Cr, <0.01% Al
0.61% C, 0.27% Mn, 0.99% Ni
0.61% C, 0.28% Si, 0.75% Mn, 0.028% P, 0.025% S, 0.40% Cr
0.61% C, 0.30% Si, 0.47% Mn, 0.016% P, 0.015% S, 14.1% Cr, 0.17% Ni, 0.52% Mo, 0.19% V. X45CrMoV1: 0.46% C, 0.46% Si, 0.44% Mn, 0.018% P, 0.003% S, 14.3% Cr, 0.16% Ni, 0.51% Mo, 0.13% V
0.61% C, 0.94% Mn, 0.88% Cr, Fe - 0.64% C, 0.88% Mn, 0.83% Cr - 0.0006% B
0.61% C, 0.94% Mn, 0.88% Cr
0.61% C, 0.94% Mn, 0.88% Cr
0.61% C, 1.06% Si, 1.17% Mn, 0.55% Cr
0.61% C, 1% Cr and 0.86% C, 0.5% Mo
0.613% C, 0.204% Si, 0.678% Mn, 0.017% P, 0.001% S, 0.27% Cr, 0.001% Mo, 0.007% Ni
0.62% C, 0.17% Si, 0.30% Mn, 16.59% Cr
0.62% C, 0.30% Mn, 0.17% Si, 16.59% Cr
0.62% C, 0.34% Si, 0.60% Mn, 0.014% P, 0.002% S, 3.05% Cr, 0.20% Ni, 0.13% V, 0.20% Cu, 0.52% Mo
0.62% C, 0.34% Si, 0.60% Mn, 0.014% P, 0.002% S, 3.05% Cr, 0.20% Ni, 0.13% V, 0.20% Cu, 0.52% Mo
0.62% C, 0.35% Mn, 1.11% Si, 0.004% S, 0.017% P 5.19% Cr, 1.02% Mo, 0.28% V
0.62% C, 0.54% Mn, 0.67% Si, 1.79% Ni, 0.60% Cr, 0.32% Mo
0.62% C, 0.64% Mn, 0.67% Si, 1.79% Ni, 0.60% Cr, 0.32% Mo
0.62% C, 0.67% Si, 0.64% Mn, 1.79% Ni, 0.60% Cr, 0.32% Mo
0.62% C, 0.72% Mn, 1.72% Si, 0.46% Mo
0.62% C, 0.82% Mn, 2.01% Si, 0.07% Cr
0.62% C, 0.85% Mn, 1.90% Si, 0.030% P, 0.030% S
0.62% C, 0.86% Mn, 2.13% Si, 0.33% Cr
0.62% C, 0.95% Mn, 2.01% Si, 0.15% Cr
0.62% C, 2.01% Si, 0.82% Mn, 0.07% Cr
0.62% C, 2.01% Si, 0.82% Mn, 0.07% Cr
0.62% C, 2.01% Si, 0.82% Mn, 0.07% Cr
0.62-0.80% C, 0.70-1.20% Mn, 0.15-0.58% Si, max. 0.15% Cr, max. 0.025% P, max. 0.025% S
0.62% C, 0.22% Si, 0.92% Mn, 0.16% Ni, 1.50% Cr, 0.26% Mo, 0.01% P, 0.004% S, 0.076% V
0.625% C, 0.30% Mn, 0.20% Si, 0.015% S, 0.015% P 1.60% Cr, 0.30% Mo
0.63% C, 0.23% Si, 0.86% Mn, 0.83% Cr
0.63% C, 0.29% Si, 0.78% Mn, 0.020% P, 0.004% S, 4.42% Cr, 0.25% Ni, 0.23% V, 0.06% W, 0.18% Cu, 0.44% Mo
0.63% C, 0.29% Si, 0.78% Mn, 0.020% P, 0.004% S, 4.42% Cr, 0.25% Ni, 0.23% V, 0.06% W, 0.18% Cu, 0.44% Mo
0.63% C, 0.54% Si, 0.85% Mn, 0.021% P, 0.026% S, 4.51% Cr, 0.18% Ni, 0.26% V, 0.06% W, 0.08% Cu, 0.61% Mo, 0.05% Ti, 0.032% Al
0.63% C, 0.54% Si, 0.85% Mn, 0.021% P, 0.026% S, 4.51% Cr, 0.18% Ni, 0.26% V, 0.06% W, 0.08% Cu, 0.61% Mo, 0.05% Ti, 0.032% Al
0.63% C, 0.80% Si, 1.10% Mn, 0.30% Cr
0.63% C, 0.80% Si, 1.10% Mn, 0.30% Cr
0.63% C, 0.86% Mn, 0.23% Si, 0.83% Cr
0.63% C, 0.87% Mn, 0.0018% B
0.63% C, 0.87% Mn, none or 0.0018% B
0.63% C, 0.87% Mn
0.63% C, 0.87% Mn
0.63% C, 0.87% Mn
0.63% C, 1.65% Si, 0.82% Mn, 0.011% P, 0.007% S, 0.28% Cr, 0.12% Ni, 0.16% Cu, 0.03% Mo
0.63% C, 1.65% Si, 0.82% Mn, 0.011% P, 0.007% S, 0.28% Cr, 0.12% Ni, 0.16% Cu, 0.03% Mo
0.63-0.70% C, 1.40-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.002% S, 1.00-2.00% Cr, 0.25% Ni, 0.23-0.27% Mo
0.63-0.70% C, 1.40-1.70% Si, 1.35-1.55% Mn, 0.002% S, 0.025% P, 0.25% Ni, 1.00-1.20% Cr, 0.23-0.27% Mo
0.63-0.70% C, 1.40-1.70% Si, 1.35-1.55% Mn, 0.002% S, 0.025% P, 0.25% Ni, 1.00-1.20% Cr, 0.23-0.27% Mo
0.63%C, O.87% Mn, O.22% Si
0.63% C, 0.80% Si, 1.10% Mn, 0.30% Cr
0.63% C, 0.02% Si, 0.38% Mn, 0.013% P, 0.018% S
0.63% C, 0.02% Si, 0.37% Mn, 0.012% P, 0.018% S
0.64% C, 0.22% Si, 0.60% Mn
0.64% C, 0.22% Si, 0.68% Mn
0.64% C, 0.39% Mn, 0.67% Si, 1.20% Cr, 1.68% W
0.64% C, 0.73% Mn, 0.82% Si, 0.011% S, 0.014% P, 1.26% Cr, 0.05% Ni, 0.16% V, 0.03% Cu, 0.006% Al, 0.012% N
0.64% C, 0.74% Mn, 1.61% Si, 0.020% S, 0.016% P 0.07% Ni, 0.61% Cr, 0.10% Cu
0.64% C, 0.88% Mn, 0.83% Cr, 0.0006% B
0.64% C, 1.13% Mn
0.64% C, 1.13% Mn
0.64-0.72% C, 0.15-0.40% Si, 0.60-0.80% Mn, max. 0.035% P, max. 0.035% S
0.65% C, 0.19% Si, 0.39% Mn, 0.011% P, 0.023% S, 0.19% Ni, 0.16% Cr, 0.03% Mo
0.65% C, 0.22% Si, 0.72% Mn, 0.027% P, 0.030% S
0.65% C, 0.23% Si, 1.32% Mn, 0.022% P, 0.041% Si
0.65% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, (Pb)
0.65% C, 0.25% Si, 0.75% Mn, 0.020-0.035% S, (Pb)
0.65% C, 0.40% Si, 1.14% Mn, 1.15% Cr, 0.024% P, 0.015% S, 01.5% V, 0.0054% N
0.65% C, 0.49% Si, 0.50% Mn, max. 1.48% Cr, 0.32% Mo, 0.15% Ni, 0.05% V, 0.13% Cu, 0.017% Al
0.65% C, 0.68% Mn, 0.10% Mo
0.65% C, 0.79% Mn, 0.35% Si, 1.27% Ni, 1.00% Cr, 0.29% Mo
0.65% C, 1.10% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.50% V
0.65% C, 1.10% Si, 1.10% Mn, 0.70% Cr
0.65% C, 1.14% Mn, 0.40% Si, 0.015% S, 0.024% P, 1.15% Cr, 0.15% V, 0.005% N
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65% C, 1.75% Si, 0.80% Mn
0.65-0.70% C, 1.45-1.60% Si, 1.35-1.55% Mn, 0.025% P, 0.002% S, 1.00-1.20% Cr, 0.25% Ni, 0.23-0.27% Mo, 8 ppm O, 30 ppm Ti
0.65-0.72% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.045% P, max. 0.045% S
0.65-0.75% C, 0.15-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S
0.65-0.75% C, 1.50-1.80% Si, 0.60-0.80% Mn, max. 0.030% P, max. 0.030% S
0.65% C, 2.00% Cr, + Mo, + V, + W
0.65% C, 1.10% Si, 1.10% Mn, 0.70% Cr
0.65% C, 1.10% Si, 0.40% Mn, 5.20% Cr, 1.40% Mo, 0.50% V
0.66% C, 0.15% Mn, 0.18% Si, 4.02% Cr, 2.04% Mo, 1.02% V, 0.26% Nb, 2.99% W
0.66% C, 0.20% Si, 0.60% Mn, 0.015% P, 0.024% S
0.67% C, 0.22% Si, 0.75% Mn, max. 0.01% P, max. 0.01% S, 0.23% Cr, 0.03% Al
0.67% C, 0.34% Si, 0.37% Mn, 0.012% P, 0.020% S, 3.13% Cr, 0.85% Ni, 0.09% V, 0.21% Cu, 0.30% Mo, 0.03% W
0.67% C, 0.34% Si, 0.37% Mn, 0.012% P, 0.020% S, 3.13% Cr, 0.85% Ni, 0.09% V, 0.21% Cu, 0.30% Mo, 0.03% W
0.67% C, 0.34% Si, 0.37% Mn, 0.012% P, 0.020% S, 3.13% Cr, 0.85% Ni, 0.09% V, 0.21% Cu, 0.30% Mo.
0.67% C, 0.34% Si, 0.37% Mn, 0.012% P, 0.020% S, 3.13% Cr, 0.85% Ni, 0.09% V, 0.21% Cu, 0.30% Mo
0.67% C, 0.45% Si, 0.98% Cr, 0.23% V
0.67% C, 1.09% Mn, 0.31% Si, 0.016% S, 0.027% P 0.75% Ni, 1.70% Cr, 0.36% Mo, 0.04% Cu
0.67% C, 1.31% Si, 0.49% Mn, 0.016% P, 0.024% S, 0.48% Cr, 0.47% Ni, 0.25% Cu, 0.08% Mo, 0.024% Sn
0.67% C, 1.31% Si, 0.49% Mn, 0.016% P, 0.024% S, 0.48% Cr, 0.47% Ni, 0.25% Cu, 0.08% Mo, 0.024% Sn
0.67% C, 1.39% Mn, 0.75% Si, 0.009% S, 0.015% P, 0.03% Cr, 0.32% Ni, 0.19% V, 0.40% Cu, 0.002% Al, 0.010% N
0.68% C, 0.33% Si, 0.65% Mn, 0.012% P, 0.027% S, 3.18% Cr, 0.13% Ni, 0.14% V, 0.18% Cu, 0.51% Mo, 0.012% Sn
0.68% C, 0.87% Mn, 0.24% Mo
0.68% C, 0.87% Mn, 0.24% Mo
0.68% C, 1.09% Mn, 1.09% Si, 0.72% Cr, 0.04% Mo 0.07% Ni, 0.02% V
0.68% C, 1.23% Si, 0.77% Mn, 0.020% P, 0.008% S, 0.88% Cr, 0.16% Ni, 0.02% V, 0.17% Cu, 0.06% Mo
0.68% C, 1.23% Si, 0.77% Mn, 0.020% P, 0.008% S, 0.88% Cr, 0.16% Ni, 0.02% V, 0.17% Cu, 0.06% Mo
0.68-0.75% C, 0.15-0.35% Si, 0.20-0.35% Mn, max. 0.025% P, max. 0.035% S
0.69% C, 0.12% Si, 0.22% Mn, 0.022% P, 0.011% S, 3.00% Cr
0.69% C, 0.28% Si, 0.63% Mn, 0.016% P, 0.005% S, 12.27% Cr, 0.02% Mo, 0.12% Ni.
0.69% C, 0.42% Mn, 0.80% Ni, 0.20% Cr, 0.13% Mo
0.69% C, 0.42% Mn, 0.80% Ni, 0.20% Cr, 0.13% Mo
0.69% C, 1.41% Mn, 0.70% Si, 0.009% S, 0.030% P, 0.05% Cr, 0.03% Ni, 0.19% V, 0.03% Cu, 0.005% Al, 0.007% N
0.69% C, 0.19% Si, 0.31% Mn, 0.006% P, 0.003% S, 12.7% Cr
0.70% C, 0.16% Si, 0.35% Mn, 0.96% Cr, 3.24% Ni, 0.06% Mo
0.70% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.70% C, 0.20% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 0.50% V
0.70% C, 0.25% Si, 0.25% Mn
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.25% Si, 0.30% Mn
0.70% C, 0.35% Mn, 0.16% Si, 3.24% Ni, 0.96% Cr 0.06% Mo
0.70% C, 0.35% Mn, 0.16% Si, 3.24% Ni, 0.96% Cr 0.06% Mo
0.70% C, 0.50% Si, 1.20% Mn, 0.35% Al
0.70% C, 0.52% Mn, 0.40% Si, 0.021% S and 0.013% P
0.70% C, 1.30% Si, 0.49% Mn, 0.013% P, 0.008% S, 0.55% Cr, 0.54% Mo, 1.14% Ni, 0.23% V
0.70% C, 1.91% Mn, 0.35% Si, 0.009% S, 0.009% P 0.98% Cr, 1.40% Mo
0.70% C, 2.00% Mn, 0.30% Si, 1.00% Cr, 1.35% Mo
0.70-0.77% C, 1.00-1.30% Si, 0.40-0.60% Mn, max. 0.025% P, max. 0.025% S, 0.45-0.65% Mo, 0.15-0.25% V
0.70-0.80% C, 0.15-0.25% Si, 0.60-0.75% Mn, max. 0.025% P, max. 0.005% S, 0.20-0.30% Cr, max. 0.10% Ni, max. 0.08% Mo, max. 0.010% Al
0.70-0.80% C, 0.15-0.30% Si, 0.15-0.35% Mn, max. 0.035% P, max. 0.035% S, 1.40-1.60% Cr, 0.60-0.80% Mo, 0.40-0.60% Ni, 0.20-0.40% W
0.70-0.80% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.045% P, max. 0.045% S
0.70-0.80% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.70-0.80% C, 0.15-0.35% Si, 0.60-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.70-0.80% C, 0.15-0.35% Si, 0.60-0.90% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.70-0.80% C, 0.25-0.50% Si, 0.60-0.80% Mn, max. 0.030% P, max. 0.030% S, 0.30-0.40% Cr
0.70-0.80% C, 0.25-0.50% Si, 0.60-0.80% Mn, max. 0.030% P, max. 0.030% S, 0.30-0.40% Cr
0.70% C, 0.25% Si, 0.25% Mn
0.71% C, 0.29% Si, 0.89% Mn, 0.25% Ni, 0.28% Cr, 0.94% Mo
0.71% C, 0.33% Si, 0.89% Mn, 0.008% P, 0.003% S, 0.09% Cr, 0.11% Ni, 0.01% V, 0.22% Cu, 0.93% Mo
0.71% C, 1.37% Si, 0.49% Mn, 0.57% Cr, 0.58% Mo, 1.15% Ni, 0.18% V, 0.05% Co, 0.04% Cu, 0.010% Al
0.71% C, 1.83% Si, 0.52% Mn, 0.5% Cr, 0.005% P, 0.005% S, 0.19% Mo, 0.13% Cu, 0.02% Ni, 0.009% Al, 46 ppm N, 15 ppm O
0.72% C, 0.72% Mn
0.72% C, 0.23% Mn, 0.43% Si, 4.04% Cr, 1.24% V, 18.38% W, 4.72% Co
0.72% C, 0.23% Si, 0.35% Mn, 0.018% P, 0.010% S, 1.75% Ni, 0.94% Cr
0.72% C, 0.27% Mn, 0.39% Si, 4.09% Cr, 1.25% V, 18.59% W
0.72% C, 0.35% Mn, 0.018% P, 0.010% S, 0.23% Si, 1.75% Ni, 0.94% Cr
0.72% C, 0.35% Mn, 0.20% Si, 0.050% S, 0.011% P 0.06% Ni, 0.28% Cr, 0.049% Cu
0.72% C, 0.35% Mn, 0.23% Si, 0.018% P, 0.010% S 1.75% Ni, 0.94% Cr
0.72% C, 0.39% Si, 0.27% Mn, 4.09% Cr, 1.25% V, 18.59% W
0.72% C, 0.39% Si, 0.27% Mn, 4.09% Cr, 1.25% V, 18.59% W
0.72% C, 0.40% Mn, 0.89% Si, 0.003% S, 0.014% P, 0.88% Ni, 2.94% Cr, 0.97% Mo, 0.20% V, 0.02% W, 0.004% Al, 0.25% Co, 0.06% Cu, 0.007% N, 0.01% Ti
0.72% C, 0.40% Mn, 0.89% Si, 0.003% S, 0.014% P, 0.88% Ni, 2.94% Cr, 0.97% Mo, 0.20% V, 0.02% W, 0.004% Al, 0.25% Co, 0.06% Cu, 0.007% N, 0.01% Ti
0.72% C, 0.40% Mn, 0.89% Si, 0.003% S, 0.014% P, 0.88% Ni, 2.94% Cr, 0.97% Mo, 0.20% V, 0.02% W, 0.004% Al, 0.25% Co, 0.06% Cu, 0.007% N, 0.01% Ti
0.72% C, 0.43% Si, 0.23% Mn, 4.04% Cr, 18.38% W, 1.24% V, 4.72% Co
0.72% C, 0.72% Mn, 0.34% Si, 0.026% S, 0.031% P
0.72-0.80% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 0.50-0.80% Mo, 17.50-18.50% W, 1.40-1.70% V, 9.00-10.00% Co
0.72-0.82% C, 0.15-0.40% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S
0.72% C, 0.72% Mn. Steel b: 0.47% C, 1.37% Mn, 0.36% Si, 0.15% Cr, 0.02% Ni, 0.19% Cu, 0.025% S, 0.015% P.
0.728% C, 0.96% Mn, 0.329% Si, 0.024% P, 0.019% S, 0.06% Cr
0.728% C, 0.96% Mn, 0.329% Si, 0.024% P, 0.019% S, 0.06% Cr
0.73% C, 0.26% Si, 0.56% Mn, 0.019% P, 0.027% S, 0.07% Cr, 0.20% Cu, <0.01% Mo, 0.05% Ni, <0.01% V
0.73% C, 0.42% Si, 0.65% Mn, 0.010% P, 0.029% S, 3.14% Cr, 0.12% Ni, 0.16% V, 0.19% Cu, 0.54% Mo, 0.010% Sn
0.73% C, 0.77% Mn, 0.27% Si, 0.010% S, 0.012% P, 1.58% Cr, 0.01% Ni, 0.46% Mo, 0.05% V, 0.05% Cu, sol. 0.010% Al
0.73% C, 0.77% Mn, 0.27% Si, 1.58% Mo, 1.46% Cr, 0.01% Ni, 0.01% Al, 0.05% Cu, 0.05% V
0.73% C, 1.00% Si, 0.52% Mn, 0.017% P, 0.006% S, 5.28% Cr, 0.33% Ni, 0.64% V, 1.15% W, 0.25% Cu, 1.28% Mo, 0.020% Sn
0.73% C, 1.00% Si, 0.52% Mn, 0.017% P, 0.006% S, 5.28% Cr, 0.33% Ni, 0.64% V, 1.15% W, 0.25% Cu, 1.28% Mo, 0.020% Sn
0.73% C, 1.20% Si, 0.50% Mn, 0.55% Mo, 0.20% V
0.73% C, 1.62% Si, 0.73% Mn, 0.019% P, 0.012% S, 0.10% Cr, 0.12% Ni, 0.010% V, 0.19% Cu
0.73% C, 1.62% Si, 0.73% Mn, 0.019% P, 0.012% S, 0.10% Cr, 0.12% Ni, 0.010% V, 0.19% Cu
0.73% C, 1.62% Si, 0.73% Mn, 0.019% P, 0.012% S, 0.10% Cr, 0.19% Cu, 0.12% Ni, 0.01% V
0.73% C, 1.62% Si, 0.73% Mn, 0.019% P, 0.018% S, 0.10% Cr, 0.19% Cu, 0.12% Ni, 0.01% V
0.73% C, 4.00% Cr, 2.00% V, 14.00% W
0.73% C, 4.00% Cr, 2.00% V, 14.00% W
0.73-0.78% C, 0.10-0.30% Si, 0.50-0.80% Mn, max. 0.035% P, max. 0.035% S, max. 0.25% Cu, max. 0.010% Al
0.73% C, 1.20% Si, 0.50% Mn, 0.55% Mo, 0.20% V
0.73% C, 0.02% Si, 0.40% Mn, 0.014% P, 0.018% S
0.74% C, 0.25% Si, 0.34% Mn, 0.21% Ni, 1.43% Cr, 0.23% Mo
0.74-0.78% C, 0.10-0.30% Si, 0.50-0.70% Mn, max. 0.020% P, max. 0.025% S, max. 0.10% Cr, max. 0.02% Mo, max. 0.10% Ni, max. 0.15% Cu, max. 0.010% Al
0.74-0.88% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.74-0.88% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.74-0.88% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.74-0.88% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.74-0.88% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.75% C, 0.22% Si, 0.27% Mn, 0.10% P, 0.025% S
0.75% C, 0.24% Si, 0.75% Mn, 0.010% S, 0.012% P, 0.43% Ni, 0.06% Cr
0.75% C, 0.25% Si, 0.70% Mn, <0.035% S
0.75% C, 0.25% Si, 0.70% Mn, <0.035% S
0.75% C, 0.27% Si, 0.50% Mn, 0.007% P, 0.020% S
0.75% C, 0.31% Mn, 0.22% Si, 0.019% S, 0.025% P, 4.25% Cr, 0.20% Ni, 1.45% V, 17.65% W
0.75% C, 0.33% Si, 0.70% Mn, 0.017% P, 0.016% S, 0.20% Ni, 0.17% Cr
0.75% C, 0.40% Mn, 1.50% Ni, 1.00% Cr
0.75% C, 0.57% Mn, 0.17% Si, 0.013% P, 0.015% S, 0.012% Ni, 0.014% Cr
0.75% C, 0.61% Mn, 0.27% Si, 0.02% P, 0.02% S, 0.004% Cr, 0.10% Mo, 0.003-0.01% Al
0.75% C, 0.70% Mn, 0.25% Si, 1.35% Ni, 0.75% Cr 0.30% Mo, 0.15% V
0.75% C, 0.70% Mn, 0.25% Si, 1.35% Ni, 0.75% Cr, 0.30% Mo, 0.15% V
0.75% C, 0.70% Mn, 0.33% Si, 0.20% Ni, 0.17% Cr 0.02% Mo
0.75% C, 0.70% Mn, 0.75% Cr, 1.35% Ni, 0.30% Mo, 0.15% V
0.75% C, 0.70% Mn, 1.50% Ni, 0.75% Cr, 0.30% Mo
0.75% C, 0.70% Si, 1.30% Mn, max. 0.015% P, max. 0.065% S, 0.50% Cr, 0.07% V, 0.012% N
0.75% C, 0.75% Mn, 0.24% Si, 0.010% S, 0.012% P 0.43% Ni, 0.06% Cr, <0.10% Mo, 0.56% Cu, <0.03% V
0.75% C, 0.75% Si, 0.35% Mn, 0.017% P, 0.016% S, 0.24% Cr, 0.19% Ni, 0.14% V, 0.64% W, 0.25% Cu, 0.35% Mo, 0.021% Al
0.75% C, 0.75% Si, 0.35% Mn, 0.017% P, 0.016% S, 0.24% Cr, 0.19% Ni, 0.14% V, 0.64% W, 0.25% Cu, 0.35% Mo, 0.021% Al
0.75% C, 0.85% Mn, 0.50% Cr
0.75% C, 1.00 Mn, Grade 1100: 0.75% C, 1.00 Mn, 0.90% Cr
0.75% C, 1.63% Si, 1.95% Mn, 0.003% P, 0.003% S, 1.48% Cr, 0.28% Mo, 0.10% V, 0.01% Al
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.35% Mn, max. 0.030% P, max. 0.030% S
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S
0.75-0.88% C, 0.60-0.90% Mn, max. 0.04% P, max. 0.05% S
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S
0.75-0.85% C, 0.10-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S
0.76% C, 0.20% Si, 0.41% Mn, 0.012% P, 0.023% S, 2.50% Ni, 0.13% Cr, 0.08% Mo, 0.12% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.008% P, 0.008% S, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.008% P, 0.008% S, 0.11% Cr, 0.17% Cu, 0.019% Mo, 0.07% Ni, 0.02% V
0.76% C, 0.22% Si, 0.29% Mn, 0.008% P, 0.008% S, 0.11% Cr, 0.17% Cu, 0.019% Mo, 0.07% Ni, 0.02% V
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.22% Si, 0.29% Mn, 0.11% Cr, 0.02% Mo, 0.07% Ni, 0.020% V, 0.17% Cu
0.76% C, 0.24% Si, 0.22% Mn, 0.013% P, 0.003% S, 1.44% Cr, 0.48% Ni, 0.27% W, 0.20% Cu, 0.69% Mo, 0.018% Al
0.76% C, 0.24% Si, 0.22% Mn, 0.013% P, 0.003% S, 1.44% Cr, 0.48% Ni, 0.27% W, 0.20% Cu, 0.69% Mo, 0.018% Al
0.76% C, 0.25% Mn, 0.35% Si, 0.031% S, 0.025% P 4.54% Cr, 5.75% Mo, 2.05% V, 6.50% W, 0.86% Co
0.76% C, 0.26% Si, 0.42% Mn, 0.006% P, 0.026% S
0.76% C, 0.27% Si, 2.06% Cr, 0.25% Mo
0.76% C, 0.29% Mn, 0.22% Si, 0.008% S, 0.008% P, 0.11% Cr, 0.07% Ni, 0.02% Mo, 0.02% V, 0.17% Cu
0.76% C, 0.41% Mn, 0.012% P, 0.023% S, 0.20% Si, 2.50% Ni, 0.13% Cr, 0.08% Mo, 0.12% Cu
0.76% C, 0.41% Mn, 0.20% Si, 0.012% P, 0.023% S 2.50% Ni, 0.13% Cr, 0.08% Mo. 0.12% Cu
0.76% C, 0.60% Mn, 0.27% Si, 0.02% P, 0.02% S, 0.58% Cr, 0.30% Mo, 0.003-0.01% Al
0.76% C, 0.61% Mn, 0.25% Si, 0.02% P, 0.02% S, 0.017% Cr, 0.006% Mo, 0.003-0.01% Al
0.76% C, 0.82% Mn, 0.25% Si, 0.02% P, 0.02% S, 0.60% Cr, 0.16% Mo, 0.003-0.01% Al
0.76% C, 0.84% Si, 1.24% Mn, 0.023% P, 0.009% S, 0.006% Nb. NS-II steel: 0.76% C, 0.82% Si, 0.82% Mn, 0.020% P, 0.006% S, 0.49% Nb, 0.005% Nb
0.762% C, 0.89% Mn, 0.371% Si, 0.05% Cr
0.77% C, 0.20% Mn, 0.22% Si, 0.006% P, 0.019% S 10.01% Ni
0.77% C, 0.28% Si, 0.72% Mn, 0.011% P, 0.029% S, 0.52% Mo
0.77% C, 0.29% Si, 0.70% Mn, 0.011% P, 0.029% S, 0.15% Mo
0.77% C, 0.29% Si, 0.71% Mn, 0.011% P, 0.029% S, 0.017% Mo
0.77% C, 0.39% Si, 1.06% Mn, 1.07% Al
0.77% C, 0.55% Si, 0.48% Mn, 0.010% P, 0.015% S, 1.19% Cr, 2.00% W, 0.32% V
0.77% C, 0.78% Mn, 0.16% Si, 0.021% S, 0.013% P
0.77% C, 0.88% Mn, 0.11% Si
0.77% C, 0.95% Mn, 0.22% Si, 0.014% P, 0.017% S, 0.10% Cr
0.77% C, 0.95% Mn, 0.22% Si, 0.10% Mo
0.77-0.85% C, max. 0.40% Si, 0.15-0.35% Mn, max. 0.025% P, max. 0.015% S, 3.90-4.30% Cr, 4.00-4.50% Mo, max. 0.25% W, 0.90-1.10% V, max. 0.30% Cu
0.77% C, 0.21% Si, 0.27% Mn, 0.019% P, 0.010% S, 4.11% Cr, 0.53% Mo, 1.04% V, 17.93% W
0.77% C, 0.21% Si, 0.27% Mn, 0.019% P, 0.010% S, 4.11% Cr, 0.53% Mo, 1.04% V, 17.93% W
0.78% C, 0.23% Si, 0.24% Mn, 0.026% P, 0.009% S, 3.94% Cr, 0.19% Ni, 0.99% V, 0.19% Cu, 4.30% Mo
0.78% C, 0.26% Si, 0.47% Mn, 0.019% P, 0.005% S, 0.49% Cr, 0.06% Ni, 0.23% V, 0.61% W, 0.13% Cu, 0.29% Mo, 0.036% Al
0.78% C, 0.26% Si, 0.47% Mn, 0.019% P, 0.005% S, 0.49% Cr, 0.06% Ni, 0.23% V, 0.61% W, 0.13% Cu, 0.29% Mo, 0.036% Al
0.78% C, 0.28% Si, 0.58% Mn, 0.022% P, 0.023% S, 0.02% Cu, 0.03% Cr
0.78% C, 0.28% Si, 0.58% Mn, 0.022% P, 0.023% S, 0.03% Cu, 0.03% Cu
0.78% C, 0.28% Si, 0.73% Mn, 0.011% P, 0.029% S, 0.32% Mo
0.78% C, 0.35% Si, 0.72% Mn, 0.024% P, 0.015% S, 17.77% Cr, 2.49% Mo, 0.12% Ni, 0.52% V
0.78% C, 0.45% Si, 0.42% Mn, 0.010% P, 0.035% S, 1.10% Cr, 0.12% Ni, 0.27% V, 2.00% W, 0.19% Cu, 0.53% Mo, 0.018% Al
0.78% C, 0.86% Mn, 0.59% Ni, 0.49% Cr, 0.21% Mo, 0.0025% B
0.78% C, 1.61% Mn, 0.48% Si, 0.018% Al, 0.18% Cu, 0.26% V
0.78% C, 1.61% Mn, 0.48% Si, 0.018% Al, 0.18% Cu, 0.26% V
0.78% C, 1.61% Mn, 0.48% Si, 0.028% S, 0.014% P, 0.16% V, 0.18% Cu, 0.018% Al, 0.018% N
0.78% C, 5.6% Cr, 2.1% W, 3.4% Mo and 2.2% V
0.78-0.86% C, max. 0.40% Si, max. 0.40% Mn, max. 0.015% P, max. 0.015% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 6.00-6.70% W, 1.70-2.00% V
0.78-0.86% C, max. 0.40% Si, max. 0.40% Mn, max. 0.025% P, max. 0.015% S, 3.90-4.30% Cr, 4.70-5.20% Mo, 6.00-6.70% W, 1.70-2.00% W, max. 0.30% Cu
0.78-0.86% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.50-4.20% Cr, 8.00-9.00% Mo, 1.50-2.00% W, 1.00-1.30% V
0.79% C, 0.17% Mn, 0.18% Si, 0.026% S, 0.035% P 0.08% Ni, 4.00% Cr, 0.20% Mo, 2.11% V, 18.15% W, 0.17% Co
0.79% C, 0.21% Mn, 0.22% Si, 0.008% P, 0.016% S 7.53% Ni
0.79% C, 0.21% Si, 0.76% Mn, 0.030% S, 0.026% P
0.79% C, 0.22% Si, 0.23% Mn, 0.007% P, 0.015% S, 5.25% Ni, 0.04% Cr, 0.01% Mo
0.79% C, 0.23% Mn, 0.22% Si, 0.007% P, 0.015% S 5.25% Ni
0.79% C, 0.27% Si, 0.76% Mn, 0.011% P, 0.029% S, 0.77% Mo
0.79% C, 0.38% Si, 1.12% Mn, 0.037% P, 0.036% S, 0.28% Cr, 0.98% Cu, 0.27% Mo, 0.79% Ni
0.79% C, 0.76% Mn
0.79% C, 0.76% Mn
0.79% C, 0.76% Mn
0.79% C, 0.76% Mn
0.79% C, 0.77% Mn, 0.58% Ni, 0.50% Cr, 0.21% Mo/0.78% C, 0.86% Mn, 0.59% Ni, 0.49% Cr, 0.21% Mo, 0.0025% B
0.79% C, 1.59% Si, 1.94% Mn, 1.33% Cr, 0.30% Mo, 0.11% V. Steel B: 0.98% C, 1.46% Si, 1.89% Mn, 1.26% Cr, 0.26% Mo, 0.09% V
0.79% C, 1.59% Si, 1.94% Mn, 1.33% Cr, 0.30% Mo, 0.11% V. Steel B: 0.98% C, 1.46% Si, 1.89% Mn, 1.26% Cr, 0.26% Mo, 0.09% V
0.79% C, 15.8% Mn, 0.05% S, <0.05% Al, 0.03% P, 0.002% Ti, 0.022% Nb, 0.036% N, 0.03% Cr
0.79% C, 0.65% Mn, 0.24% Si
0.8% C, 0.1% Mn, 1.8% Ni, 0.5% Mo, 2% Cu
0.80% C, 0.25% Mn, 0.015% P, 0.015% S, 0.25% Si, 4.00% Cr, 0.10% Ni, 4.50% Mo, 1.00% V
0.80% C, 0.27% Si, 0.61% Mn, 0.007% P, 0.005% S, 0.01% Al, 0.15% V
0.80% C, 0.28% Si, 0.52% Mn, 5.00% Ni, 0.07% Cr, 0.03% Mo
0.80% C, 0.29% Mn, 0.28% Si, 0.026% S, 0.018% P 4.40% Cr, 0.37% Mo, 1.60% V, 19.20% W, 9.30% Co
0.80% C, 0.30% Mn, 0.23% Si, 0.005% S, 0.019% P, 4.34% Cr, 0.30% Ni, 0.78% Mo, 1.52% V, 17.89% W, 4.52% Co
0.80% C, 0.43% Si, 0.63% Mn, 0.010% P, 0.027% S, 3.14% Cr, 0.12% Ni, 0.12% V, 0.19% Cu, 0.50% Mo, 0.013% Sn
0.80% C, 0.45% Mn, 0.017% P, 0.009% S, 0.18% Si, 3.33% Ni, 1.52% Cr, 0.03% Mo
0.80% C, 0.45% Mn, 3.33% Ni, 0.00% Cr, 1.52% Mo
0.80% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
0.80% C, 0.52% Mn, 0.007% P, 0.016% S, 0.28% Si, 5.00% Ni, 0.07% Cr, 0.03% Mo
0.80% C, 0.52% Mn, 5.00% Ni
0.80% C, 0.52% Si, 0.26% Mn, 0.018% P, 0.004% S, 8.40% Cr, 0.19% Ni, 2.60% V, 0.24% Cu, 1.55% Mo
0.80% C, 0.52% Si, 0.26% Mn, 0.018% P, 0.004% S, 8.40% Cr, 0.19% Ni, 2.60% V, 0.24% Cu, 1.55% Mo
0.80% C, 0.53% Mn, 0.28% Si, 3.80% Cr, 1.05% V 17.40% W, 4.62% Co
0.80% C, 0.59% Si, 0.41% Mn, 0.009% P, 0.035% S, 1.20% Cr, 0.10% Ni, 0.35% V, 1.02% W, 0.12% Cu, 0.50% Mo, 0.016% Al, 0.010% Sn
0.80% C, 0.60% Cr, 0.20% V
0.80% C, 1.88% Mn
0.80% C, 1.88% Mn
0.80% C, 1.90% Si, 0.75% Mn, 0.25% Cr, 0.30% Mo
0.80% C, 12.70% Cr, 0.90% V, 1.10% Mo, 0.70% Nb
0.80% C, 12.70% Cr, 1.10% Mo, 0.90% V, 0.70% Co
0.80% C, 4.0% Cr, 3.0% Mo, 3.0% W, 8.0% Co, 1.0% V, 1.0% Nb
0.80% C, 4.00% Cr, 0.70% Mo, 19.00% W, 1.60% V, 5.00% Co
0.80% C, 4.00% Cr, 0.75% Mo, 14.00% W, 2.00% W, 5.00% Co
0.80% C, 4.00% Cr, 0.75% Mo, 5.00% Co, 2.00% V, 14.00% W
0.80% C, 4.00% Cr, 1.00% V, 4.25% Mo
0.80% C, 4.00% Cr, 4.25% Mo, 1.00% V
0.80-0.90% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.80-0.90% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.80-0.90% C, 0.20-0.40% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 1.60-1.90% Cr, 0.20-0.35% Mo
0.80-0.90% C, 0.25-0.40% Si, 0.50-0.70% Mn, max. 0.025% P, max. 0.020% S
0.80C-2.76Cr
0.80% C, 1.50% Si, 0.75% Mn, 0.50% Cr
0.80% C, 0.60% Cr, 0.20% V
0.80% C, 0.20% Si, 0.30% Mn, 4.00% Cr, 4.30% Mo, 1.00% V
0.81% C, 0.15% Si, 0.33% Mn, 0.024% P, 0.003% S, 3.77% Cr, 0.44% Mo, 0.12% Ni, 1.07% V, 18.25% W
0.81% C, 0.17% Mn, 0.23% Si, 0.019% S, 0.018% P 0.08% Ni, 4.25% Cr, 0.09% Mo, 1.08% V, 17.60% W, 0.05% Co
0.81% C, 0.19% Si, 0.32% Mn, 0.023% P, 0.010% S, 3.80% Cr, 0.29% Ni, 1.20% V, 1.68% W, 0.23% Cu, 8.55% Mo, 0.15% Co, 0.047% Al
0.81% C, 0.24% Mn, 0.26% Si, 0.016% P, 0.007% S, 4.10% Cr, 4.69% Mo, 1.64% V, 5.95% W
0.81% C, 0.26% Mn, 0.21% Si, 0.002% S, 0.021% P 4.28% Cr, 3.98% Mo, 1.08% V
0.81% C, 0.26% Si, 0.24% Mn, 0.016% P, 0.007% S, 4.10% Cr, 4.69% Mo, 5.95% W, 1.64% V
0.81% C, 0.31% Si, 0.41% Mn, 4.11% Cr, 4.27% Mo, 5.46% W, 1.51% V, 5.22% Co
0.81% C, 0.33% Mn, 0.15% Si, 0.003% S, 0.024% P, 3.77% Cr, 0.12% Ni, 0.44% Mo, 1.07% V, 18.25% W
0.81% C, 0.73% Mn, 0.45% Si, 6.10% Cr, 1.05% Mo
0.81% C, 0.76% Mn, 0.50% Si, 6.04% Cr, 0.035% Mo
0.81% C, 2.10% Mn, 0.29% Si, 0.003% S, 0.016% P 0.06% Ni, 0.02% Cr, 0.01% Mo, 0.04% Cu, 0.17% V
0.81% C, 2.10% Mn, 0.29% Si, 0.003% S, 0.016% P 0.06% Ni, 0.02% Cr, 0.01% Mo, 0.04% Cu, 0.17% V
0.81% C, 2.15% Si, 0.55% Mn, 1.63% Ni, 19.40% Cr
0.81% C, 2.23% Si, 0.47% Mn, 0.018% P, 0.013% S, 20.27% Cr, 0.08% Mo, 1.27% Ni
0.82% C, 0.17% Si, 0.50% Mn, 0.32% Cr, 0.03% Mo, 2.52% Ni, 0.82% C, 0.29% Mn, 0.25% Si, 0.010% S, 0.032% P 0.20% Ni, 4.10% Cr, 1.60% Mo, 2.06% V, 12.10% W
0.82% C, 0.30% Mn, 0.25% Si, 4.25% Cr, 5.00% Mo, 1.80% V, 6.25% W
0.82% C, 0.79% Si, 0.29% Mn, 0.012% P, 0.005% S, 5.10% Cr, 0.10% Ni, 0.28% Mo, 0.03% V, 0.15% Cu, 0.04% W, 0.02% Co, 0.011% Sn, 0.012% Al
0.82% C, 0.70% Si, 0.40% Mn, 8.00% Cr, 1.60% Mo, 0.60% V, +Al
0.83% C, <0.25% Si, <0.35% Mn, 4.10% Cr, 1.00% V, 4.25% Mo
0.83% C, <0.25% Si, <0.35% Mn, 4.10% Cr, 1.00% V, 4.25% Mo
0.83% C, 0.25% Si, 0.32% Mn, 3.89% Cr, 4.30% Mo, 5.79% W, 1.30% V
0.83% C, 0.28% Si, 0.28% Mn, 0.10% Cr, 0.04% Mo, 0.80% Ni, 0.09% Cu, 0.053% Al
0.83% C, 0.28% Si, 0.82% Mn, 0.34% Ni, 1.13% Cr, 0.05% Mo
0.83% C, 0.32% Mn, 0.25% Si, 3.89% Cr, 4.30% Mo, 1.30% V, 5.79% W
0.83% C, 0.35% Si, 0.41% Mn, 0.012% P, 0.016% S, 1.15% Cr, 0.13% Ni, 0.20% V, 1.90% W, 0.12% Cu, 0.06% Mo, 0.014% Al
0.83% C, 0.45% Si, 0.40% Mn, 1.90% Cr, 0.30% Mn
0.83% C, 0.45% Si, 0.40% Mn, 1.90% Cr, 0.30% Mo
0.84% C, 0.22% Mn, 0.23% Si, 0.014% S, 0.025% P 4.36% Cr, 4.95% Mo, 1.83% V, 6.48% W, 4.85% Co
0.84% C, 0.22% Si, 0.53% Mn, 0.033% P, 0.049% S, 0.12% Ni, 0.09% Cr, 0.12% Cu
0.84% C, 0.32% Si, 0.41% Mn, 0.012% P, 0.016% S, 1.11% Cr, 0.13% Ni, 0.19% V, 1.90% W, 0.12% Cu, 0.06% Mo, 0.014% Al
0.84% C, 0.32% Si, 0.41% Mn, 0.012% P, 0.016% S, 1.11% Cr, 0.13% Ni, 0.19% V, 1.90% W, 0.12% Cu, 0.06% Mo, 0.014% Al
0.84% C, 0.72% Mn, 0.44% Si, 12.10% Cr, 1.05% Mo
0.84, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.50% Mo, 1.20% V, 1.80% W
0.85-0.98% C, 0.6-0.9% Mn, max. 0.04% P, max. 0.05% S
0.85% C, 0.21% Si, 0.38% Mn, 0.011% P, 0.016% S, 1.71% Cr, 0.16% Ni, 0.09% V, 0.22% Cu, 0.25% Mo
0.85% C, 0.25% Si, 0.65% Mn, <0.035% S
0.85% C, 0.25% Si, 0.65% Mn, <0.035% S
0.85% C, 0.25% Si, 0.65% Mn
0.85% C, 0.25% Si, 0.65% Mn
0.85% C, 0.26% Si, 1.18% Mn, 0.50% Cr, 0.44% W
0.85% C, 0.27% Mn, 0.24% Si, 0.023% S, 0.024% P 4.03% Cr, 8.00% Mo, 1.38% V, 1.43% W, 0.19% Co
0.85% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 1.85% Ni, 5.00% Mo, 6.40% W
0.85% C, 0.30% Si, 0.30% Mn, 4.25% Cr, 1.85% Ni, 5.00% Mo, 6.40% W
0.85% C, 0.30% Si, 0.31% Mn, 0.015% P, 0.010% S, 4.15% Cr, 4.79% Mo, 0.18% Ni, 2.01% V, 6.34% W
0.85% C, 0.30% Si, 2.00% Mn, max. 0.030% P, max. 0.030% S, 1.00% Cr, max. 0.25% Ni, 1.40% Mo, max. 0.25% Cu
0.85% C, 0.30% Si, 2.00% Mn, max. 0.030% P, max. 0.030% S, 1.00% Cr, max. 0.25% Ni, 1.40% Mo, max. 0.25% Cu
0.85% C, 0.31% Mn, 0.30% Si, 0.010% S, 0.015% P, 4.15% Cr, 0.18% Ni, 4.79% Mo, 2.01% V, 6.34% Cu
0.85% C, 0.31% Si, 0.27% Mn, 0.024% S, 0.025% P, 4.26% Cr, 0.50% Mo, 17.00% W, 1.26% V
0.85% C, 0.31% Si, 0.30% Mn, 4.14% Cr, 4.61% Mo, 6.55% W, 1.94% V, 0.025% P, 0.021% S
0.85% C, 0.32% Si, 0.38% Mn, max. 0.012% P, max. 0.008% S, 1.75% Cr, 0.26% Mo, 0.090% V
0.85% C, 0.34% Si, 0.29% Mn, 0.023% P, 0.007% S, 16.25% Cr, 0.55% Mo, 0.27% V, 1.39% Co
0.85% C, 0.55% Si, 4.35% Cr, 2.80% Mo, 2.10% V, 2.55% W, 4.50% Co
0.85% C, 0.65% Mn, 0.30% Si, 0.030% S, 0.013% P, 0.12% Cr, 0.05% Ni, 0.50% Mo, 0.03% V, 0.08% Cu, 0.051% Al
0.85% C, 0.71% Mn, 0.43% Si, 12.10% Cr, 3.07% Mo
0.85% C, 0.75% Mn, 0.45% Si, 12.00% Cr, 0.068% Mo
0.85% C, 1.18% Mn, 0.26% Si, 0.50% Cr, 0.44% W
0.85% C, 1.18% Mn, 0.26% Si, 0.50% Cr, 0.44% W
0.85% C, 1.98% Mn, 0.40% Si, 0.46% Cr, 0.14% V
0.85% C, 4.00% Cr, 0.75% Mo, 18.50% W, 2.10% V
0.85% C, 4.00% Cr, 0.75% Mo, 2.10% V, 18.50% W
0.85% C, 4.00% Cr, 8.00% Mo, 0.00% P, 1.90% V
0.85% C, 4.00% Cr, 8.00% Mo, 1.90% V
0.85-0.95% C, 0.10-0.50% Si, 1.40-2.00% Mn, max. 0.03% P, max. 0.03% S, 0.20-0.50% Cr, max. 0.30% Ni, 0.25-0.45% Mo, max. 0.25% Cu
0.85-0.95% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.70-0.90% Cr
0.85-0.95% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.70-0.90% Cr
0.85-0.95% C, 0.15-0.35% Si, 0.40-0.70% Mn, max. 0.025% P, max. 0.025% S, max. 0.40% Cr, max. 0.10% Mo, max. 0.40% Ni
0.85-0.95% C, 0.15-0.35% Si, 0.70-0.90% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.85% C, 0.02% Si, 0.38% Mn, 0.013% P, 0.016% S
0.86% C, 0.18% Si, 0.22% Mn, 0.012% P, 0.018% S, 0.08% Cr, 0.02% Ni, 0.23% Cu
0.86% C, 0.30% Si, 1.20% Mn, max. 0.030% P, max. 0.030% S, 0.50% Cr, max. 0.25% Ni, 0.13% Mo, 0.50% V, + special elements
0.86% C, 0.30% Si, 1.20% Mn, max. 0.030% P, max. 0.030% S, 0.50% Cr, max. 0.25% Ni, 0.13% Mo, 0.50% V, + special elements
0.86% C, 0.35% Mn, 0.34% Si, 0.012% S, 0.005% P 0.58% Ni, 1.62% Cr, <0.01% Mo, 0.05% Cu, 0.174% V
0.86% C, 0.38% Si, 0.66% Mn, 2.47% Ni, 1.21% Cr, 0.50% Mo
0.86% C, 0.66% Mn, 0.38% Si, 0.040% P, 0.024% S, 2.47% Ni, 1.21% Cr, 0.50% Mo
0.86-0.94% C, 0.40% Mn, 0.45% Si, 0.03% S, 0.03% P, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.10% V, 5.90-6.70
0.86-0.94% C, 0.40% Mn, 0.45% Si, 0.03% S, 0.03% P, 3.80-4.50% Cr, 4.70-5.20% Mo, 1.70-2.10% V, 5.90-6.70
0.86-0.94% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.10% V
0.86-0.94% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.10% V
0.86-0.94% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% W, 1.70-2.10% V
0.87% C, 0.21% Si, 2.04% Mn, 0.012% P, 0.015% S, 0.27% Cr, 0.15% Ni, 0.09% V, 0.32% Cu, 0.05% Mo, 0.005% Al
0.87% C, 0.22% Si, 2.04% Mn, 0.013% P, 0.017% S, 0.27% Cr, 0.14% Ni, 0.09% V, 0.32% Cu, 0.05% Mo, 0.005% Al
0.87% C, 0.22% Si, 2.04% Mn, 0.013% P, 0.017% S, 0.27% Cr, 0.14% Ni, 0.09% V, 0.32% Cu, 0.05% Mo, 0.005% Al
0.87% C, 0.22% Si, 2.04% Mn, 0.013% P, 0.017% S, 0.27% Cr, 0.14% Ni, 0.09% V, 0.32% Cu, 0.05% Mo, 0.005% Al
0.87% C, 0.27% Si, 0.32% Mn, 0.020% P, 0.005% S, 3.99% Cr, 0.80% Mo, 0.11% Ni, 2.52% V, 11.91% W
0.87% C, 0.29% Si, 1.78% Mn, 0.027% P, 0.010% S, 0.15% Ni, 0.20% Cr, 0.03% Mo
0.87% C, 0.30% Mn, 0.27% V
0.87% C, 0.30% Mn, 0.27% V
0.87% C, 0.30% Mn, 0.27% V
0.87% C, 0.32% Mn, 0.27% Si, 0.005% S, 0.020% P, 3.99% Cr, 0.11% Ni, 0.80% Mo, 2.52% V, 11.91% W
0.87% C, 0.39% Mn, 0.19% Si, 4.00% Ni, 1.58% Cr
0.87% C, 1.21% Mn, 0.28% Si, 0.52% Cr, 0.58% W
0.87% C, 1.78% Mn, 0.29% Si, 0.027% P, 0.010% S, 0.15% Ni, 0.20% Cr, 0.03% Mo
0.87-0.95% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 4.70-5.20% Mo, 5.90-6.70% Ni, 1.70-2.10% V, 4.50-5.00% Co
0.88% C, 0.21% Si, 2.03% Mn, 0.014% P, 0.014% S, 0.27% Cr, 0.15% Ni, 0.09% V, 0.30% Cu, 0.05% Mo, 0.005% Al
0.88% C, 0.22% Si, 0.35% Mn, 0.021% P, 0.011% S, 4.12% Cr, 4.97% Mo, 1.77% V, 6.50% W
0.88% C, 0.22% Si, 0.35% Mn, 0.021% P, 0.011% S, 4.12% Cr, 4.97% Mo, 1.77% V, 6.50% W
0.88% C, 0.24% Si, 0.41% Mn, 0.010% S, 0.010% P, 0.10% Ni, 0.78% Cr
0.88% C, 0.30% Si, 0.66% Mn, 0.018% P, 0.011% S, 0.049% Al, max. 0.0005% B, 0.56% Cr, 0.18% Cu, 0.44% Mo, 0.020% N, 0.15% Ni
0.88% C, 0.31% Si, 0.35% Mn, 0.009% P, 0.01% S, 1.80% Cr, 0.13% Ni, 0.13% V, 0.24% Cu, 0.21% Mo
0.88% C, 0.31% Si, 0.35% Mn, 0.009% P, 0.01% S, 1.80% Cr, 0.13% Ni, 0.13% V, 0.24% Cu, 0.21% Mo
0.88% C, 0.35% Mn, 0.021% P, 0.011% S, 4.12% Cr, 4.97% Mo, 1.77% V, 6.50% W
0.88% C, 0.40% Si, 0.39% Mn, 0.026% P, 0.004% S, 17.48% Cr, 0.30% Ni, 0.10% V, 0.14% W, 0.12% Cu, 0.94% Mo
0.88% C, 0.40% Si, 0.39% Mn, 0.026% P, 0.004% S, 17.48% Cr, 0.30% Ni, 0.10% V, 0.14% W, 0.12% Cu, 0.94% Mo
0.88% C, 0.41% Mn, 0.24% Si, 0.010% S, 0.010% P 0.10% Ni, 0.78% Cr, 0.05% Mo, 0.12% Cu
0.88% C, 0.41% Mn/ 0.90% C, 0.47% Mn, 0.20% V Beginning of transformation at left, ending at right
0.88% C, 0.41% Si, 0.41% Mn
0.88, 0.22% Si, 0.35% Mn, 0.021% P, 0.011% S, 4.12% Cr, 4.97% Mo, 1.77% V, 6.50% W
0.88, 0.22% Si, 0.35% Mn, 0.021% P, 0.011% S, 4.12% Cr, 4.97% Mo, 1.77% V, 6.50% W
0.88% C, 0.30% Si, 0.66% Mn, 0.018% P, 0.011% S, 0.049% Al, 0.0005% B, 0.56% Cr, 0.18% Cu, 0.44% Mo, 0.020% N, 0.15% Ni
0.88% C, 0.43% Si, 0.38% Mn, 0.024% P, 0.014% S, 17.64% Cr, 1.10% Mo, 0.44% Ni, 0.09% V, 0.03% W
0.89% C, 0.19% Si, 0.39% Mn, 4.00% Ni, 1.58% Cr
0.89% C, 0.25% Si, 0.25% Mn, 0.019% P, 0.010% S, 4.13% Cr, 4.75% Mo, 1.82% V, 6.12% W, 4.62% Co
0.89% C, 0.25% Si, 0.25% Mn, 0.019% P, 0.010% S, 4.13% Cr, 4.75% Mo, 1.82% V, 6.12% W, 4.62% Co
0.89% C, 0.25% Si, 0.25% Mn, 0.019% P, 0.010% S, 4.13% Cr, 4.75% Mo, 6.12% W, 1.82% V, 4.62% Co
0.89% C, 0.26% Si, 0.59% Mn, 0.021% P, 0.015% S, 0.40% Cr, 0.13% V, 0.08% Cu
0.89% C, 0.29% Mn
0.89% C, 0.29% Mn
0.89% C, 0.39% Mn, 0.19% Si, 4.00% Ni, 1.58% Cr
0.89% C, 0.42% Si, 0.31% Mn, 0.005% S, 0.002% P, 0.03% Ni, 1.80% Cr, 0.27% Mo, 0.10% V
0.89% C, 0.42% Si, 0.31% Mn, 0.005% S, 0.002% P, 0.03% Ni, 1.80% Cr, 0.27% Mo, 0.10% V
0.89% C, 0.42% Si, 0.31% Mn, 0.005% S, 0.002% P, 0.03% Ni, 1.80% Cr, 0.27% Mo, 0.10% V
0.89% C, 0.42% Si, 0.31% Mn, 0.005% S, 0.002% P, 0.03% Ni, 1.80% Cr, 0.27% Mo, 0.10% V
0.89% C, 0.50% Mn, 0.18% Si, 3.90% Cr, 1.03% V 19.10% W, 9.66% Co
0.89% C, 0.28% Si, 1.88% Mn, 0.027% P, 0.009% S, 0.40% Cr, 0.10% Cu, 0.18% Ni, 0.08% V
0.89% C, 0.28% Si, 1.88% Mn, 0.027% P, 0.009% S, 0.40% Cr, 0.10% Cu, 0.18% Ni, 0.08% V
0.89% C, 0.29% Si, 2.43% Mn, 0.028% P, 0.008% S, 0.0020% Al, 0.27% Cr, 0.03% Cu, 0.011% N, 0.22% Ni, 0.09% V
0.9% C, 0.9% Si, 0.5% Mn, 7.8% Cr, 2.5% Mo, 0.5% V
0.9% C, 0.9% Si, 0.5% Mn, 7.8% Cr, 2.5% Mo, 0.5% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 0.25% Si, 2.00% Mn, 0.30% Cr, 0.10% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.12% V
0.90% C, 0.25% Si, 2.00% Mn, 0.35% Cr, 0.12% V
0.90% C, 0.30% Mn, 0.30% Si, 0.020% P, 0.020% S, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 0.30% Mn, 0.30% Si, 0.020% P, 0.020% S, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 0.30% Si, 0.30% Mn, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 0.30% Si, 2.00% Mn, 0.025% P, 0.015% S, 0.40% Cr, 0.10% V
0.90% C, 0.33% Si, 0.30% Mn, 0.019% P, 0.009% S, 1.98% Cr, 0.11% Ni, 0.15% V, 0.16% Cu, 0.25% Mo
0.90% C, 1.07% Mn, 0.30% Si, 0.49% Cr, 0.63% W
0.90% C, 1.20% Mn, 0.50% Cr, 0.20% V, 0.50% W, Fe is balance
0.90% C, 1.25% Mn, 0.50% Cr, 0.50% W, 0.20% V
0.90% C, 1.97% Mn, 0.20% Si, 0.43% Cr, 0.03% Mo 0.13% Ni, 0.08% V
0.90% C, 18.00% Cr, 1.10% Mo, 0.10% V
0.90% C, 18.00% Cr, 1.20% Mo, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.10% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.20% V
0.90% C, 2.00% Mn, 0.40% Cr, 0.20% V
0.90% C, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, max. 1.00% Si, max. 1.00% Mn, 18.00% Cr, 1.10% Mo, 0.10% V
0.90% C, max. 1.00% Si, max. 1.00% Mn, 18.00% Cr, 1.10% Mo, 0.10% V
0.90, 0.29% Si, 0.30% Mn, 0.019% P, 0.007% S, 3.97% Cr, 4.27% Mo, 0.13% Ni, 1.83% V, 1.12% W, 0.15% Cu, 0.027% Co
0.90-1.00% C, 0.15-0.40% Si, 0.20-0.40% Mn, 0.020% P, 0.002% S, 1.40-1.60% Cr, 0.25% Ni, 0.10% Mo
0.90-1.05% C, 0.15-0.35% Si, 0.25-0.45% Mn, max. 0.030% P, max. 0.025% S, 0.40-0.60% Cr, max. 0.30% Ni, max. 0.30% Cu
0.90-1.05% C, 0.15-0.35% Si, 1.00-1.20% Mn, max. 0.035% P, max. 0.035% S, 0.50-0.70% Cr, 0.50-0.70% W, 0.050-0.15% V
0.90-1.05% C, 0.15-0.35% Si, 1.00-1.20% Mn, max. 0.035% P, max. 0.035% S, 0.50-0.70% Cr, 0.50-0.70% W, 0.050-0.15% V
0.90% C, 0.30% Si, 2.00% Mn, 0.025% P, 0.015% S, 0.40% Cr, 0.10% V
0.90% C, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W
0.90% C, 0.20% Si, 2.00% Mn, 0.40% Cr, 0.10% V
0.91% C, 0.32% Mn, 0.37% Si, 0.006% S, 0.016% P 5.20% Ni, 1.07% Cr, 0.09% Cu, 0.42% V
0.91% C, 0.65% Mn, 0.013% P, 0.026% S, 0.23% Si, 1.35% Ni, 0.60% Cr, 0.03% Cu
0.91% C, 0.65% Mn, 0.23% Si, 0.013% P, 0.026% S 1.35% Ni, 0.60% Cr, 0.03% Cu
0.92% C, 0.18% Si, 0.30% Mn, 0.20% Cr
0.92% C, 0.18% Si, 0.30% Mn, 0.20% Cr
0.92% C, 0.31% Mn, 0.35% Si, 0.019% S, 0.025% P, 4.10% Cr, 4.90% Mo, 1.88% V, 6.20% W
0.92% C, 0.37% Si, 0.29% Mn, 0.025% P, 0.008% S, 17.97% Cr, 1.18% Mo, 0.34% Ni, 0.12% V, 0.12% Cu
0.92% C, 0.93% Mn, 0.30% Si, 0.90% Ni, 0.57% Cr 0.03% Mo
0.92% C, 0.93% Mn, 0.30% Si, 0.90% Ni, 0.57% Cr 0.03% Mo
0.92-1.02% C, 0.25-0.40% Si, 0.25-0.40% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.25% Ni, 0.15-0.25% Mo
0.92-1.02% C, 0.25-0.40% Si, 0.25-0.40% Mn, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.25% Ni, 0.15-0.25% Mo
0.92-1.05% C, 0.25-0.40% Si, 0.60-0.80% Mn, 0.025% P, 0.015% S, 1.65-1.95% Cr, 0.25% Ni, 0.40-0.50% Mo
0.92-1.05% C, 0.40-0.60% Si, 0.80-1.00% Mn, 0.025% P, 0.015% S, 1.80-2.05% Cr, 0.25% Ni, 0.50-0.60% Mo
0.92% C, 4.10% Cr, 5.00% Mo, 1.90% V, 6.40% W, 4.80% Co
0.93 % C, 0.31 % Mn, 0.20 % Ni, 0.12 % Cr
0.93% C, 0.11% Si, 0.31% Mn, 0.010% S, 0.012% P, 0.20% Ni, 0.12% Cr
0.93% C, 0.20% Si, 1.25% Mn, 0.020% P, 0.007% S, 0.50% Cr, 0.24% Ni, 0.15% Cu
0.93% C, 0.23% Si, 1.00% Mn, 0.013% P, 0.005% S, 0.51% Cr, 0.14% Ni, 0.08% V, 0.51% W, 0.09% Cu, 0.011% Mo, 0.04% Al
0.93% C, 0.23% Si, 1.00% Mn, 0.013% P, 0.005% S, 0.51% Cr, 0.14% Ni, 0.08% V, 0.51% W, 0.09% Cu, 0.011% Mo, 0.04% Al
0.93% C, 0.23% Si, 1.00% Mn, 0.013% P, 0.005% S, 0.51% Cr, 0.14% Ni, 0.08% V, 0.51% W, 0.09% Cu, 0.011% Mo
0.93% C, 0.23% Si, 1.00% Mn, 0.013% P, 0.005% S, 0.51% Cr, 0.14% Ni, 0.08% V, 0.51% W, 0.09% Cu, 0.011% Mo
0.93% C, 0.25% Si, 1.99% Mn, 0.016% P, 0.005% S, 0.35% Cr, 0.09% Ni, 0.09% V, 0.24% Cu, 0.03% Mo, 0.021% Sn
0.93% C, 0.25% Si, 1.99% Mn, 0.016% P, 0.005% S, 0.35% Cr, 0.09% Ni, 0.09% V, 0.24% Cu, 0.03% Mo, 0.021% Sn
0.93% C, 0.28% Mn, 0.28% Si, 0.009% P, 0.001% S, 1.47% Cr, 0.10% Ni, 0.02% Mo, 0.10 Cu, 12 ppm Ti, 3.9 ppm O
0.93% C, 0.28% Mn, 0.28% Si, 0.009% P, 0.001% S, 1.47% Cr, 0.10% Ni, 0.02% Mo, 0.10 Cu, 12 ppm Ti, 3.9 ppm O
0.93% C, 0.29% Si, 0.30% Mn, 0.021% P, 0.026% S, 4.12% Cr, 0.29% Ni, 2.02% V, 6.57% W, 0.20% Cu, 5.06% Mo, 0.28% Co
0.93% C, 0.29% Si, 0.30% Mn, 0.021% P, 0.026% S, 4.12% Cr, 0.29% Ni, 2.02% V, 6.57% W, 0.20% Cu, 5.06% Mo, 0.28% Co
0.93% C, 0.31% Mn, 0.11% Si, 0.010% S, 0.012% P 0.20% Ni, 0.12% Cr, 0.1<0% Mo, 0.62% Cu, 0.03% V
0.93% C, 0.39% Si, 0.50% Mn, 0.017% S, 0.026% P, 4.25% Ni, 1.18% Cr, 0.16% Mo
0.93% C, 0.39% Si, 0.50% Mn, 0.017% S, 0.026% P, 4.25% Ni, 1.18% Cr, 0.16% Mo
0.93% C, 0.43% Si, 0.49% Mn, 18.40% Cr, 0.55% Mo
0.93% C, 0.49% Mn, 0.43% Si, 18.40% Cr, 0.55% Mo
0.93% C, 0.50% Mn, 0.26% Si, 0.01% P, 0.02% S, 0.16% Ni, 3.65% Cr
0.93% C, 0.50% Mn, 0.30% Si, 4.25% Ni, 1.18% Cr 0.16% Mo
0.93% C, 0.50% Mn, 0.30% Si, 4.25% Ni, 1.18% Cr 0.16% Mo
0.93% C, 0.71% Mn, 0.38% Si, 2.10% Ni, 1.70% Cr 0.20% Mo
0.93% C, 0.71% Mn, 0.38% Si, 2.10% Ni, 1.70% Cr 0.20% Mo
0.93% C, 1.25% Mn, 0.20% Si, 0.007% S, 0.020% P 0.24% Ni, 0.60% Cr, 0.15% Cu
0.93% C, 1.25% Mn, 0.20% Si, 0.007% S, 0.020% P 0.24% Ni, 0.60% Cr, 0.15% Cu
0.93-1.05% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, max. 0.30% Cu, max. 0.050% Al
0.93-1.05% C, 0.15-0.35% Si, 0.60-0.80% Mn, max. 0.025% P, max. 0.015% S, 1.65-1.95% Cr, 0.20-0.35% Mo, max. 0.30% Cu, max. 0.050% Al
0.93-1.05% C, 0.45-0.75% Si, 1.00-1.20% Mn, max. 0.025% P, max. 0.015% S, 1.45-1.65% Cr, max. 0.10% Mo, max. 0.30% Ni, max. 0.050% Al
0.93-1.05% C, 0.45-0.75% Si, 1.00-1.20% Mn, max. 0.025% P, max. 0.015% S, 1.45-1.65% Cr, max. 0.10% Mo, max. 0.30% Ni, max. 0.050% Al
0.93% C, 0.28% Si, 0.42% Mn, 0.04% Ni, 1.54% Cr, 0.03% Mo
0.94% C
0.94% C
0.94% C, 1.20% Mn, 0.30% Si, 0.50% Cr, 0.50% W
0.94% C, 0.02% Si, 0.40% Mn, 0.012% P, 0.017% S
0.95% C, 0.15% Si, 0.25% Mn, 1.35% Cr
0.95% C, 0.15% Si, 0.25% Mn, 1.35% Cr
0.95% C, 0.15% Si, 0.25% Mn, 1.35% Cr
0.95% C, 0.15% Si, 0.25% Mn, 1.35% Cr
0.95% C, 0.19% Si, 0.45% Mn, 0.084% P, 0.027% S
0.95% C, 0.20% Si, 0.25% Mn
0.95% C, 0.20% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 0.20% V
0.95% C, 0.20% V
0.95% C, 0.24% Mn, 0.28% Si, 0.018% S, 0.006% P 4.64% Cr, 4.80% Mo, 2.45% V, 7.12% W
0.95% C, 0.25% Mn, 0.20% Si, 0.20% V
0.95% C, 0.26% Si, 0.40% Mn, 0.015% S, 0.028% P, 2.95% Ni, 0.36% Cr, 0.08% Mo
0.95% C, 0.30% Si, 0.84% Mn, 0.55% Ni, 0.66% Cr, 0.11% Mo
0.95% C, 0.30% Si, 1.10% Mn, 0.50% Cr, 0.10% V, 0.50% W
0.95% C, 0.30% Si, 1.10% Mn, 0.50% Cr, 0.10% V, 0.50% W
0.95% C, 0.40% Mn, 0.26% Si, 2.95% Ni, 0.36% Cr 0.08% Mo
0.95% C, 0.40% Mn, 0.26% Si, 2.95% Ni, 0.36% Cr 0.08% Mo
0.95% C, 0.45% Mn/ 0.95% C, 0.48% Mn, 0.95% Co/ 0.98% C, 0.49% Mn, 1.98% Co Beginning of transformation at left, ending at right
0.95% C, 0.50% Mn, 0.24% Si, 0.011% S, 0.018% P 0.26% Ni, 4.90% Cr, 1.03% Mo, 0.22% Cu, 0.02% Al
0.95% C, 0.58% Mn, 0.24% Si, 1.79% Ni, 0.25% Mo
0.95% C, 0.58% Mn, 0.24% Si, 1.79% Ni, 0.25% Mo
0.95% C, 0.60% Mn, 0.22% Si, 3.27% Ni, 1.23% Cr 0.13% Mo
0.95% C, 0.60% Mn, 0.22% Si, 3.27% Ni, 1.23% Cr, 0.13% Mo
0.95% C, 0.82% Mn, 0.23% Si, 0.56% Ni, 0.52% Cr 0.19% Mo
0.95% C, 0.82% Mn, 0.23% Si, 0.56% Ni, 0.52% Cr, 0.19% Cu
0.95% C, 0.98% Si, 0.34% Mn, 0.015% P, 0.005% S, 7.34% Cr, 0.09% Ni, 2.01% V, 0.87% W, 0.08% Cu, 1.40% Mo, 0.015% Al
0.95% C, 0.98% Si, 0.34% Mn, 0.015% P, 0.005% S, 7.34% Cr, 0.09% Ni, 2.01% V, 0.87% W, 0.08% Cu, 1.40% Mo, 0.015% Al
0.95% C, 1.1% Mn, 0.6% Cr, 0.1% V, 0.6% W
0.95% C, 1.1% Mn, 0.6% Cr, 0.1% V, 0.6% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 1.10% Mn, 0.60% Cr, 0.60% W, 0.10% V
0.95-1.00% C, 0.20-0.35% Si, 0.20-0.40% Mn, 0.025% P, 0.015% S, 1.35-1.60% Cr, 0.25% Ni, 0.08% Mo
0.95-1.00% C, 0.20-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.25% Ni, max. 0.08% Mo
0.95-1.05% C, 0.15-0.25% Si, 0.15-0.30% Mn, max. 0.025% P, max. 0.025% S, 0.10-0.15% V
0.95-1.05% C, 0.15-0.35% Si, 0.60% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.95-1.05% C, 0.15-0.35% Si, 0.60% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
0.95-1.10% C, <1.00% Si, <1.00% Mn, 16.00-17.00% Cr, 0.40-0.60% Mo
0.95-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, 0.025% P, 0.025% S, 1.35-1.60% Cr, 0.10% Mo, 0.40% Ni
0.95-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, 0.025% P, 0.025% S, 1.35-1.60% Cr, 0.10% Mo, 0.40% Ni
0.95-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.025% S, 1.35-1.60% Cr, max. 0.10% Mo, max. 0.40% Ni
0.95-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.025% S, 1.35-1.60% Cr, max. 0.10% Mo, max. 0.40% Ni
0.95-1.10% C, 0.25-0.40% Mn, 0.20-0.40% Si, 1.65-1.95% Cr, 0.30-0.40% Mo
0.95-1.10% C, 0.25-0.45% Mn, 0.15-0.35% Si, 1.40-1.60% Cr
0.95-1.10% C, 0.25-0.45% Mn, 0.20-0.40% Si, 1.65-1.95% Cr, 0.30-0.40% Mo
0.95-1.10% C, 0.40-0.70% Si, 0.90-1.15% Mn, <0.025% P, <0.025% S, 0.90-1.20% Cr
0.95-1.00% C, 0.20-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.25% Ni, max. 0.08% Mo
0.95-1.00% C, 0.20-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.25% Ni, max. 0.08% Mo
0.95% C, 0.20% Si, 0.25% Mn
0.95-1.00% C, 0.28-0.50% Mn, 0.15-0.35% Si, max. 0.025% P, max. 0.025% S, 1.35-1.60% Cr, max. 0.40% Ni
0.95-1.00% C, 0.20-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.25% Ni, max. 0.08% Mo
0.95-1.00% C, 0.20-0.35% Si, 0.20-0.40% Mn, max. 0.025% P, max. 0.015% S, 1.35-1.60% Cr, max. 0.25% Ni, max. 0.08% Mo
0.95% C, 0.20% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
0.95% C, 0.32% Mn, 0.26% Si, 0.009% P, 0.001% S, 1.42% Cr
0.96% C, 0.23% Si, 1.08% Mn, 0.014% P, 0.003% S, 0.57% Cr, 0.13% Ni, 0.08% V, 0.56% W, 0.20% Cu, 0.12% Mo
0.96% C, 0.32% Si, 0.55% Mn, 0.013% P, 0.012% S, 0.11% Cr
0.96% C, 0.55% Mn, 0.32% Si, 0.08% Ni, 0.11% Cr 0.01% Mo
0.96% C, 0.74% Mn, 0.26% Si, 1.19% Ni, 0.84% Cr 0.09% Mo
0.96% C, 0.74% Mn, 0.26% Si, 1.19% Ni, 0.84% Cr 0.09% Mo
0.97% C, 0.18% Mn, 0.31% Si, 0.006% S, 0.035% P, 4.11% Cr, 0.25% Ni, 2.61% Mo, 2.51% V, 3.23% W
0.97% C, 0.20% Si, 0.40% Mn, 1.78% Ni, 0.18% Cr, 0.27% Mo
0.97% C, 0.27% Mn, 0.26% Si, 0.006% S, 0.010% P 0.05% Ni, 0.77% Cr, <0.01% Mo, 0.04% Cu
0.97% C, 0.31% Si, 0.18% Mn, 0.035% P, 0.008% S, 4.11% Cr, 2.61% Mo, 0.25% Ni, 2.52% V, 3.23% W
0.97% C, 0.32% Si, 0.72% Mn, 0.012% P, 0.020% S, 1.54% Ni, 0.80% Cr, 0.26% Mo, 0.06% Cu, 0.027% V, 0.025% Al, 0.005% N, 0.0006% B
0.97% C, 0.39% Mn, 0.25% Si, 0.020% P, 0.013% S, 1.04% Cr
0.97% C, 0.40% Si, 0.48% Mn, 4.58% Cr, 1.04% Mo, 0.25% V
0.97% C, 0.41% Si, 0.18% Mn, 0.035% P, 0.006% S, 4.11% Cr, 2.61% Mo, 0.25% Ni, 3.23% W, 2.51% V
0.97% C, 0.48% Mn, 0.40% Si, 4.58% Cr, 1.04% Mo, 0.205% V
0.97% C, 0.52% Mn, 3.36% Ni, 0.19% Mo
0.97% C, 0.52% Mn, 3.36% Ni, 0.19% Mo
0.97% C, 0.93% Si, 0.36% Mn, 0.015% P, 0.003% S, 7.36% Cr, 0.14% Ni, 2.08% V, 0.86% W, 0.16% Cu, 1.39% Mo, 0.012% Al
0.97% C, 1.00% Mn, 0.33% Si, 1.93% Ni, 1.13% Cr 0.23% Mo
0.97% C, 1.00% Mn, 0.33% Si, 1.93% Ni, 1.13% Cr 0.23% Mo
0.97% C, 1.04% Mn, 0.32% Mo
0.97% C, 1.04% Mn, 0.32% Mo
0.97% C, 1.04% Mn, 0.32% Mo
0.97C-0.14Ni-0.14Cr-O.13Cu-0.13Si-0.16Mn
0.97% C, 0.40% Si, 0.48% Mn, 4.58% Cr, 1.04% Mo, 0.25% V
0.98% C, 0.08% Si, 1.84% Mn, 0.023% P, 0.011% S
0.98% C, 0.17% Si, 0.24% Mn, 0.023% P, 0.026% S, 11.30% Cr, 0.15% Ni, 0.92% V, 0.13% Cu, 0.98% Mo
0.98% C, 0.20% Si, 0.70% Mn, 0.60% Ni, 0.68% Cr, 0.12% Mo
0.98% C, 0.30% Mn, 0.16% Si, 0.003% S, 0.015% P 0.17% Ni, 0.63% Cr, 0.28% Mo, 0.11% Cu, 0.28% V, 3.66% W
0.98% C, 0.30% Mn, 0.16% Si, 0.003% S, 0.015% P 0.17% Ni, 0.63% Cr, 0.28% Mo, 0.11% Cu, 0.28% V, 3.66% W
0.98% C, 0.32% Si, 0.29% Mn, 3.80% Cr, 2.48% Mo, 2.60% Ni, 2.77% W, 2.56% V
0.98% C, 0.35% Si, 0.31% Mn, 3.85% Cr, 2.50% Mo, 1.28% Ni, 2.92% W, 2.66% V
0.98-1.10% C, 0.15-0.30% Si, 0.25-0.45% Mn, max. 0.025% P, max. 0.025% S, 1.3-1.6% Cr
0.98-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.025% S, 1.30-1.60% Cr
0.98-1.10% C, 0.15-0.35% Si, 0.25-0.45% Mn, 0.025% P, 0.025% S, 1.30-1.60% Cr
0.99% C, 0.17% Si, 0.57% Mn, 0.018% P, 0.017% S, 5.25% Cr, 1.02% Mo, 0.16% V
0.99% C, 0.17% Si, 0.57% Mn, 0.018% P, 0.017% S, 5.25% Cr, 1.02% Mo, 0.16% V
0.99% C, 0.21% Si, 0.30% Mn, 0.016% P, 0.013% S, 1.00% Cr, 0.09% Ni, 0.01% V, 0.05% Cu, 0.20% Mo, 0.003% Sn
0.99% C, 0.21% Si, 0.30% Mn, 0.016% P, 0.013% S, 1.00% Cr, 0.09% Ni, 0.01% V, 0.05% Cu, 0.20% Mo, 0.003% Sn
0.99% C, 0.21% Si, 0.30% Mn, 0.016% P, 0.013% S, 1.00% Cr, 0.09% Ni, 0.01% V, 0.05% Cu, 0.20% Mo, 0.003% Sn
0.99% C, 0.37% Mn, 0.24% Si, 0.011% P, 0.022% S, 0.07% Ni, 1.50% Cr, 0.01% Mo, 0.11% Cu
0.99% C, 0.52% Mn, 0.009% P, 0.010% S, 0.27% Si, 3.36% Ni, 0.09% Cr, 0.19% Mo, 0.04% Cu
0.99% C, 0.56% Mn, 0.29% Si, 1.61% Ni, 0.32% Cr 0.29% Mo
0.99% C, 0.56% Mn, 0.29% Si, 1.61% Ni, 0.32% Cr 0.29% Mo
0.99% C, 0.57% Si, 0.80% Mn, 0.011% P, 0.056% S, 3.97% Cr, 0.13% Ni, 0.10% V, 0.30% Cu, 0.22% Mo
0.99% C, 0.57% Si, 0.80% Mn, 0.011% P, 0.056% S, 3.97% Cr, 0.13% Ni, 0.10% V, 0.30% Cu, 0.22% Mo
0.99% C, 0.22% Si, 0.25% Mn, 0.011% P, 0.008% S
0.996% C, 0.236% Si, 0.468% Mn, 0.005% S, 0.008% P, 0.107% Ni, 1.580% Cr, 0.11% Cu
1.0% C, 0.90% Si, 8.00% Cr, 1.60% Cr, 0.10% V
1.0% C, 5.3% Cr, 1.1% Mo, 0.2% V
1.00% C, 0.20% Si, 0.20% Mn, 0.10% V
1.00% C, 0.20% Si, 0.20% Mn
1.00% C, 0.20% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.20% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.24% Mn, 0.32% Si, 1.48% Cr, 0.16% Ni, 0.06% Mo, 0.11% Cu
1.00% C, 0.25% Si, 0.30% Mn, 0.025% P, 0.010% S, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 0.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 0.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.25% Si, 1.10% Mn, 0.025% P, 0.010% S, 0.60% Cr, 0.10% V, 0.60% W
1.00% C, 0.28% Si, 0.31% Mn, 0.003% S, 0.013% P, 0.21% Ni, 1.71% Cr
1.00% C, 0.28% Si, 0.31% Mn, 0.003% S, 0.013% P, 0.21% Ni, 1.71% Cr
1.00% C, 0.28% Si, 0.31% Mn, 0.003% S, 0.013% P, 0.21% Ni, 1.71% Cr
1.00% C, 0.30% Mn, 0.12% Si, 3.27% Ni, 0.90% Cr 0.07% Mo
1.00% C, 0.30% Mn, 0.12% Si, 3.27% Ni, 0.90% Cr 0.07% Mo
1.00% C, 0.30% Mn, 0.27% Si, 0.030% S, 0.013% P 0.21% Ni, 1.71% Cr, 0.04% Mo, 0.14% Cu, 0.010% V
1.00% C, 0.30% Mn, 0.27% Si, 0.030% S, 0.013% P 0.21% Ni, 1.71% Cr, 0.04% Mo, 0.14% Cu, 0.010% V
1.00% C, 0.30% Si, 0.60% Mn, 5.25% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.60% Mn, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.30% Si, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.35% Mn, 7.50% Cr, 0.005% S, 2.60% Mo, 0.30% V, +Ti
1.00% C, 0.35% Mn, 7.50% Cr, 0.005% S, 2.60% Mo, 0.30% V, +Ti
1.00% C, 0.45% Mn, 0.017% P, 0.009% S, 0.18% Si, 3.33% Ni, 1.52% Cr, 0.03% Mo
1.00% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
1.00% C, 0.45% Mn, 3.33% Ni, 1.52% Cr
1.00% C, 0.50% Si, 0.40% Mn, 5.00% Cr, 0.95% Mo, 0.20% V
1.00% C, 0.52% Mn, 0.007% P, 0.016% S, 0.28% Si, 5.00% Ni, 0.07% Cr, 0.03% Mo
1.00% C, 0.52% Mn, 5.00% Ni
1.00% C, 0.52% Mn, 5.00% Ni
1.00% C, 0.60% Mn, 0.30% Si, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.60% Mn, 5.00% Cr, 1.00% Mo, 0.25% V
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.60% Si, 1.10% Mn, 1.50% Cr
1.00% C, 0.70% Mn, 1.80% Cr, 0.30% Mo
1.00% C, 0.80 % Mn, 0.30% Si, 5.25% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.80 % Mn, 0.30% Si, 5.25% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.90% Si, 0.41% Mn, 0.016% P, 0.001% S, 8.08% Cr, 0.15% Ni, 0.25% V, 0.07% W, 0.16% Cu, 2.04% Mo, 0.66% Nb
1.00% C, 0.90% Si, 8.00% Cr, 1.60% Mo, 1.60% V
1.00% C, 0.99% Mn, 0.28% Si, 1.42% Ni, 1.12% Cr 0.11% Mo
1.00% C, 0.99% Mn, 0.28% Si, 1.42% Ni, 1.12% Cr 0.11% Mo
1.00% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 0.30% V, 2.00% Mo
1.00% C, 1.10% Mn, 1.50% Cr
1.00% C, 1.50% Cr
1.00% C, 1.50% Cr
1.00% C, 1.88% Mn
1.00% C, 1.88% Mn
1.00% C, 4.00% Cr, 0.70% Mo, 19.00% W, 1.10% V
1.00% C, 4.00% Cr, 9.00% Mo, 1.75% W, 2.00% V
1.00% C, 4.00% Mo
1.00% C, 5.00% Cr, 0.95% Mo, 0.20% V
1.00% C, 5.20% Cr, 1.20% Mo, 0.30% V
1.00% C, 5.30% Cr, 1.10% Mo, 0.20% V
1.00% C, 5.40% Cr, 1.10% Mo, 0.25% V
1.00% C
1.00-1.10% C, 0.10-0.30% Si, 0.10-0.35% Mn, max. 0.030% P, max. 0.030% S
1.00-1.10% C, 0.10-0.30% Si, 0.10-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.10-0.20% V
1.00-1.10% C, 0.10-0.40% Si, 0.80-1.10% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.10% Cr, 1.00-1.30% W
1.00-1.10% C, 0.10-0.40% Si, 0.80-1.10% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.10% Cr, 1.00-1.30% W
1.00-1.10% C, 0.15-0.35% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.90-1.10% Cr
1.00-1.10% C, 0.15-0.35% Si, 0.25-0.40% Mn, max. 0.030% P, max. 0.025% S, 0.90-1.15% Cr
1.00% C, 1.45% Cr
1.00% C, 1.50% Si, 0.75% Mn, 0.50% Cr
1.00% C, 1.50% Si, 0.75% Mn, 0.50% Cr, 0.03% Nb
1.00% C, 1.50% Si, 0.75% Mn, 0.50% Cr, 0.10% Mo
1.00% C, 2.50% Si, 0.75% Mn, 1.00% Cr, 0.03% Mo
1.00% C, 4.00% Cr, 5.00% Mo, 1.90% V, 6.40% W
1.0% C, 1.1% Mn, 1.5% Cr
1.00% C, 0.20% Si, 0.35% Mn, 1.50% Cr
1.00% C, 0.30% Si, 0.50% Mn, 5.00% Cr, 0.95% Mo, 0.20% V
1.00% C, 0.20% Si, 0.20% Mn, 0.10% V
1.00% C, 0.90% Si, 8.00% Cr, 1.10% Mo, 1.60% V
1.00% C, 0.30% Si, 0.60% Mn, 5.25% Cr, 1.10% Mo, 0.20% V
1.00% C, 0.30% Si, 1.10% Mn, 0.60% Cr, 0.10% V, 0.60% W
1.00% C, 0.22% Si, 0.34% Mn, 0.010% P, 0.006% S, 1.52% Cr, 0.16% Cu, 0.01% Mo, 0.10% Ni, 0.01% V
1.00% C, 0.22% Si, 0.34% Mn, 0.010% P, 0.006% S, 1.52% Cr, 0.16% Cu, 0.01% Mo, 0.10% Ni, 0.01% V
1.01% C, 0.20% Si, 0.48% Mn, 0.004% P, 0.002% S, 0.01% Cu, 0.49% Co. Steel B: 1.15% C, 0.23% Si, 0.52% Mn, 0.008% P, 0.003% S, 0.01% Cu, 0.98% Co
1.01% C, 0.30% Si, 0.50% Mn, 1.21% Cr
1.01% C, 0.36% Si, 0.38% Mn, 0.029% P, 0.008% S, 3.99% Cr, 0.20% Ni, 2.05% V, 1.75% W, 0.25% Cu, 8.99% Mo, 0.019% Al
1.01% C, 0.36% Si, 0.38% Mn, 0.029% P, 0.008% S, 3.99% Cr, 0.20% Ni, 2.05% V, 1.75% W, 0.25% Cu, 8.99% Mo, 0.019% Al
1.01% C, 0.50% Mn, 0.30% Si, 1.21% Cr
1.01% C, 0.76% Si, 0.58% Mn, 0.015% P, 0.033% S, 16.80% Cr, 1.69% Ni, 0.17% Cu, 0.69% Mo, 0.015% Sn
1.01% C, 0.37% Mn, 0.27% Si, 1.5% Cr, 0.02% P, 0.007% S, 0.027% Al
1.02% C, 0.21% Si, 0.29% Mn, 0.020% P, 0.016% S, 4.20% Cr, 0.25% Ni, 2.54% V, 6.22% W, 0.20% Cu, 4.93% Mo, 0.24% Co
1.02% C, 0.33% Mn, 0.35% Si, 0.016% P, 0.011% S, 8.80% Cr
1.02% C, 0.33% Mn, 0.35% Si, 0.020% P, 0.012% S, 2.90% Cr
1.02% C, 0.35% Si, 0.33% Mn, 0.016% P, 0.011% S, 8.80% Cr
1.02% C, 0.35% Si, 0.33% Mn, 0.020% P, 0.012% S, 2.90% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.36% Mn, 0.20% Ni, 1.41% Cr
1.02% C, 0.40% Si, 0.30% Mn, 17.00% Cr, 0.50% Mo
1.02% C, 0.40% Si, 0.30% Mn, 17.00% Cr, 0.50% Mo
1.02% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
1.02% C, 0.47% Mn, 0.27% Si, 4.15% Ni, 1.22% Cr 0.05% Mo
1.02% C, 0.47% Mn, 0.27% Si, 4.15% Ni, 1.22% Cr 0.05% Mo
1.02% C, 0.73% Mn, 0.46% Si, 6.08% Cr, 1.03% Mo
1.02% C, 2.41% Mn
1.02% C, 0.40% Si, 0.30% Mn, 3.80% Cr, 8.60% Mo, 1.90% V, 1.80% W
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.007% Cr, 0.10% Ni, 0.14% Cu, 0.01% Mo
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.007% Cr, 0.10% Ni, 0.14% Cu, 0.01% Mo
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.07% Cr, 0.01% Mo, 0.10% Ni, 0.14% Cu
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.07% Cr, 0.01% Mo, 0.10% Ni, 0.14% V
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.07% Cr, 0.14% Cu, 0.01% Mo, 0.10% Ni
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.07% Cr, 0.14% Cu, 0.01% Mo, 0.10% Ni
1.03% C, 0.17% Si, 0.22% Mn, 0.014% P, 0.012% S, 0.07% Cr, 0.14% Cu, 0.01% Mo, 0.10% Ni
1.03% C, 0.21% Si, 0.53% Mn, 0.030% P, 0.002% S, 5.17% Cr, 0.25% Ni, 0.24% V, 0.23% Cu, 1.12% Mo
1.03% C, 0.21% Si, 0.53% Mn, 0.030% P, 0.002% S, 5.17% Cr, 0.25% Ni, 0.24% V, 0.23% Cu, 1.12% Mo
1.03% C, 0.28% Si, 0.97% Mn, 0.018% P, 0.018% S, 1.05% Cr, 0.25% Cu, 0.03% Mo, 0.13% Ni, 1.15% W
1.03% C, 0.28% Si, 0.97% Mn, 0.018% P, 0.018% S, 1.05% Cr, 0.25% Cu, 0.03% Mo, 0.13% Ni, 1.15% W
1.03% C, 0.76% Mn, 0.50% Si, 6.03% Cr, 0.038% Mo
1.03% C, 0.30% Si, 0.29% Mn, 0.016% P, 0.007% S, 1.47% Cr
1.04% C, 0.18% Mn, 0.35% Si, <0.01% P, <0.01% S, 4.00% Cr
1.04% C, 0.26% Si, 0.33% Mn, 0.023% P, 0.006% S, 1.53% Cr, 0.20% Cu, <0.01% Mo, 0.31% Ni, <0.01% V
1.04% C, 0.26% Si, 0.33% Mn, 0.023% P, 0.006% S, 1.53% Cr, 0.20% Cu, <0.01% Mo, 0.31% Ni, <0.01% V
1.04% C, 0.35% Si, 0.18% Mn, <0.01% P, <0.01% S, 4.00% Cr
1.04% C, 0.38% Si, 0.45% Mn, 0.031% P, 0.004% S, 16.84% Cr, 0.50% Mo, 0.08% Ni, 0.11% Cu
1.04% C, 0.39% Si, 0.42% Mn, 0.028% P, 0.014% S, 16.39% Cr, 0.40% Ni, 0.11% Cu, 0.45% Mo
1.04% C, 0.48% Si, 0.48% Mn, 0.027% P, 0.005% S, 16.70% Cr, 0.46% Ni, 0.07% V, 0.13% Cu, 0.47% Mo
1.04% C, 0.48% Si, 0.48% Mn, 0.027% P, 0.005% S, 16.70% Cr, 0.46% Ni, 0.07% V, 0.13% Cu, 0.47% Mo
1.04% C, 0.26% Si, 0.33% Mn, 0.023% P, 0.006% S, 1.53% Cr, 0.20% Cu, 0.31% Ni, 0.01% Mo, 0.01% V
1.05% C, 0.20% Si, 1.08% Mn, 0.94% Cr
1.05% C, 0.31% Mn, 0.35% Si, 0.017% P, 0.012% S, 5.70% Cr
1.05% C, 0.35% Si, 0.31% Mn, 0.017% P, 0.012% S, 5.70% Cr
1.05% C, 0.40% Si, 0.40% Mn, 16.70% Cr, 0.50% Mo
1.05% C, 0.50% Cr
1.05% C, 1.00% Cr
1.05-1.12% C, 1.20-1.80% W, 9.00-10.00% Mo, 3.60-4.40% Cr, 1.00-1.30% V, 7.50-8.50 Co
1.05-1.15% C, 0.30% Mn, 0.50% Si, 0.25% Cr
1.05-1.15% C, 0.50% Si, 0.30% Mn, 0.25% Cr
1.05-1.15% C, max. 0.70% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.50-4.50% Cr, 9.00-10.00% Mo, 1.20-1.90% W, 0.90-1.30% V, 7.50-9.50% Co
1.05% C, 0.25% Si, 1.00% Mn, 1.00% Cr, 1.10% W
1.06% C, 0.19% Si, 0.28% Mn, 0.018% P, 0.012% S, 3.78% Cr, 3.16% Mo, 1.65% W, 1.24% W, 7.59% Co
1.06% C, 0.19% Si, 0.28% Mn, 0.018% P, 0.012% S, 3.78%Cr, 9.16% Mo, 1.24% V, 1.65% W, 7.59% Co
1.06% C, 0.19% Si, 0.28% Mn, 0.018% P, 0.012% S, 3.78%Cr, 9.16% Mo, 1.24% V, 1.65% W, 7.59% Co
1.06% C, 0.32% Si, 0.33% Mn, 1.44% Cr
1.06% C, 0.33% Mn, 0.32% Si, 1.44% Cr
1.06% C, 4.43% Cr, 0.44% Mo, 2.32% V, 10.32% W, 3.92% Co
1.07% C, 0.01% Mn, 0.32% Mo, 0.29% V
1.07% C, 0.32% Mn, 0.31% Si, 0.016% S, 0.012% P 0.17% Ni, 2.05% Cr, 0.18% Mo, 0.13% Cu
1.07% C, 0.32% Mn, 0.31% Si, 0.016% S, 0.012% P 0.17% Ni, 2.05% Cr, 0.18% Mo, 0.13% Cu
1.08% C, 0.25% Mn, 0.25% Si, 0.01% P, 0.01% S, 4.00% Cr, 9.50% Mo, 1.20% V, 1.50% W, 8.00% Co
1.08% C, 0.53% Mn, 0.25% Si, 0.33% Ni, 1.46% Cr 0.06% Mo
1.08% C, 0.77% Si, 0.73% Mn, 0.027% P, 0.031% S, 0.113% Cr, 0.042% Al
1.09% C, 0.37% Si, 0.209% Mn, 0.016% S, 0.0039% P, 0.05% Ni, 0.077% Cr, 0.013% Mo, 0.132% Cu, 0.0023% V
1.1% C, 1.8% N, 0.5% Si, 0.4% Mn, 4.5% Cr, 3.2% Mo, 3.7% W, 8.5% V
1.1% C, 1.8% N, 0.5% Si, 0.4% Mn, 4.5% Cr, 3.2% Mo, 3.7% W, 8.5% V
1.1% C, 1.8% N, 0.5% Si, 0.4% Mn, 4.5% Cr, 3.2% Mo, 8.5% V, 3.7% W
1.1% C, 1.8% N, 0.5% Si, 0.4% Mn, 4.5% Cr, 3.2% Mo, 8.5% V, 3.7% W
1.10% C, 0.060% S, 3.75% Cr, 9.50% Mo, 8.25% Co, 1.15% V, 1.50% W
1.10% C, 0.19% Si, 0.81% Mn, 0.55% Ni, 0.63% Cr, 0.11% Mo
1.10% C, 0.70% Si, 0.40% Mn, 8.20% Cr, 2.10% Mo, 0.50% V, +Al, Nb
1.10% C, 0.70% Si, 0.40% Mn, 8.20% Cr, 2.10% Mo, 0.50% V, +Al, Nb
1.10% C, 0.90% Si, 0.40% Mn, 0.005% S, 8.25% Cr, 2.15% Mo, 0.30% V
1.10% C, 0.90% Si, 0.40% Mn, 8.30% Cr, 2.10% Mo, 0.50% V + additions
1.10% C, 17.00% Cr, 0.10% V, 1.00% Mo
1.10% C, 7.50% Cr, 1.50% Mo, 2.10% V, 1.10% W
1.10-1.25% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.50-0.80% Cr, 0.070-0.12% V
1.10-1.25% C, 0.15-0.30% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 0.50-0.80% Cr, 0.070-0.12% V
1.10% C, 4.10% Cr, 9.50% Mo, 1.20% V, 1.50% W, 8.00% Co
1.11% C, 0.24% Mn, 0.27% Si, 0.007% S, 0.023% P 3.91% Cr, 9.50% Mo, 1.21% V, 1.47% W, 8.35% Co
1.11% C, 0.65% Mn, 0.30% Si, 0.030% S, 0.013% P, 0.12% Cr, 0.05% Ni, 0.50% Mo, 0.03% V, 0.08% Cu, 0.051% Al
1.11% C, 0.70% Si, 0.39% Mn, 0.016% P, 0.002% S, 4.58% Cr, 1.39% W, 9.46% Mo, 1.37% V, 8.04% Co
1.11% C, 1.00% Si, 0.41% Mn, 0.011% P, 0.002% S, 8.43% Cr, 2.12% Mo, 0.19% Ni, 0.45% V, 0.04% W, 0.05% Cu
1.11% C, 0.7% Si, 0.39% Mn, 0.016% P, 0.002% S, 4.58% Cr, 1.39% W, 9.46% Mo, 1.37% V, 8.04% Co
1.12% C, 0.24% Si, 0.51% Mn, 0.009% P, 0.016% S, 5.36% Ni
1.12% C, 0.28% Si, 0.55% Mn, 0.007% P, 0.014% S, 3.56% Ni
1.12% C, 0.48% Mn, 0.24% Si, 0.004% S, 0.012% P, 14.55% Cr, 0.20% Ni, 4.01% Mo, 1.25% V
1.12% C, 0.55% Mn, 0.007% P, 0.014% S, 0.28% Si, 3.56% Ni
1.13% C, 0.24% Si, 0.59% Mn, 0.006% P, 0.018% S
1.13% C, 0.30% Mn/ 1.17% C, 0.30% Mn, 0.26% Cr Beginning of transformation at left, ending at right
1.13% C, 0.30% Mn
1.13% C, 0.30% Mn
1.13% C, 0.30% Mn
1.13% C, 0.51% Mn, 0.50% Si, 0.022% S, 0.025% P, 4.02% Cr, 8.80% Mo, 1.24% V, 7.90% Co
1.13% C, 0.85% Si, 0.35% Mn, 7.70% Cr, 1.50% Mo, 2.45% V, 1.10% W
1.14% C (total), 0.066% P, 0.068% S
1.14% C, 0.16% Si, 0.22% Mn
1.14% C, 0.22% Mn, 0.16% Si
1.15% C, 0.28% Si, 0.76% Mn, 0.011% P, 0.029% S, 0.53% Mo
1.15% C, 0.37% Si, 0.32% Mn, 0.026% P, 0.024% S, 11.46% Cr, 0.20% Ni, 1.60% V, 2.40% W, 0.23% Cu, 1.36% Mo, 0.020% Al
1.15% C, 0.37% Si, 0.32% Mn, 0.026% P, 0.024% S, 11.46% Cr, 0.20% Ni, 1.60% V, 2.40% W, 0.23% Cu, 1.36% Mo, 0.020% Al
1.15% C, 0.38% Mn, 0.38% Si, 0.008% S, 0.018% P 0.21% Ni, 0.74% Cr, 0.02% Mo, 0.12% Cu, 1.20% W
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, max. 0.035% P, max. 0.035% S, 0.15-0.25% Cr, 0.90-1.10% W, 0.070-0.12% V
1.15-1.25% C, 0.15-0.30% Si, 0.20-0.35% Mn, max. 0.035% P, max. 0.035% S, 0.15-0.25% Cr, 0.90-1.10% W, 0.070-0.12% V
1.16% C, 0.29% Si, 0.75% Mn, 0.011% P, 0.029% S, 0.15% Mo
1.16% C, 0.30% Mn, 0.57% Si, 0.009% S, 0.006% P 0.71% Ni, 1.79% Cr, 0.27% Mo, 1.30% W
1.17% C, 0.21% Mn, 0.22% Si, 0.009% P, 0.019% S 10.30% Ni
1.17% C, 0.75% Mn, 2.00% Si, 0.30% Mo, 0.60% Cu
1.18% C, 0.22% Mn, 0.22% Si, 0.008% P, 0.016% S 7.64% Ni
1.18% C, 0.28% Si, 0.75% Mn, 0.011% P, 0.029% S, 0.78% Mo
1.18% C, 0.29% Si, 0.76% Mn, 0.011% P, 0.029% S, 0.009% Mo
1.18% C, 0.63% Mn, 0.28% Si, 0.011% S, 0.022% P 1.13% Ni, 0.49% Cr, 0.13% Mo, 0.10% Cu
1.19% C, 0.28% Si, 0.77% Mn, 0.011% P, 0.029% S, 0.33% Mo
1.19% C, 0.31% Mn, 0.29% Si, 0.0021% S, 0.01% P 4.54% Cr, 5.10% Mo, 3.29% V, 7.92% W, 12.27% Co
1.20% C, 0.20% Cr, 0.10% V, 1.00% W
1.20% C, 0.28% Si, 0.52% Mn, 5.00% Ni, 0.07% Cr, 0.03% Mo
1.20% C, 0.52% Mn, 0.007% P, 0.016% S, 0.28% Si, 5.00% Ni, 0.07% Cr, 0.03% Mo, 0.10% Cu
1.20% C, 0.52% Mn, 5.00% Ni
1.20% C, 0.70% Cr, 0.10% V
1.20% C, 0.70% Si, 0.10% V
1.20% C, 0.91% Mn, 0.23% Si, <0.003% P, 0.002% S
1.20% C, 1.88% Mn
1.20% C, 1.88% Mn
1.20% C, 12.00% Cr, 1.40% Mo, 1.70% V, 2.50% W
1.20-1.30% C, 0.15-0.35% Si, 0.25-0.40% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.60% Cr, max. 0.10% Mo, max. 0.40% Ni
1.20-1.30% C, 0.15-0.35% Si, 0.25-0.40% Mn, max. 0.025% P, max. 0.025% S, 0.40-0.60% Cr, max. 0.10% Mo, max. 0.40% Ni
1.20-1.30% C, 0.15-0.35% Si, 0.30-0.60% Mn, 0.025% P, 0.025% S, 0.40% Cr, 0.10% Mo, 0.40% Ni
1.20-1.35% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 0.70-1.00% Mo, 11.50-12.50% W, 3.50-4.00% V
1.20-1.35% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 3.20-3.90% Mo, 9.00-10.00% W, 3.00-3.50% V, 9.50-10.50% Co
1.20-1.35% C, max. 0.45% Si, max. 0.40% Mn, max. 0.030% P, max. 0.030% S, 3.80-4.50% Cr, 3.20-3.90% Mo, 9.00-10.00% W, 3.00-3.50% V, 9.50-10.50% Co
1.20% C, 0.70% Cr, 0.10% V
1.20% C, 0.20% Cr, 0.10% V, 1.00% W
1.22% C, 0.19% Si, 1.93% Mn, 0.020% S, 0.020% P, 1.52% Cr, 0.36% Mo, 0.17% V, 0.04% Al
1.22% C, 1.22% Si, 0.78% Mn, 0.008% P, 0.008% S, 1.25% Cr
1.22% C, 0.21% Si, 0.27% Mn, 4.09% Cr, 5.04% Mo, 2.88% V, 6.80% W
1.22% C, 0.21% Si, 0.27% Mn, 4.09% Cr, 5.04% Mo, 2.88% V, 6.80% W
1.23% C, 0.25% Mn, 0.25% Si, 0.01% P, 0.01% S, 4.00% Cr, 3.80% Mo, 3.30% V, 10.0% W, 10.50% Co
1.23% C, 0.25% Si, 0.26% Mn, max. 0.015% P, max. 0.010% S, 0.13% Cr, 0.98% W
1.24% C, 0.27% Si, 0.27% Mn, 0.011% P, 0.011% S, 0.24% Cr, 0.09% Ni, 0.12% V, 1.10% W, 0.23% Cu, 0.03% Mo
1.24% C, 0.42% Si, 0.46% Mn, 0.021% P, 0.005% S, 1.24% Cr, 0.60% Ni, 0.15% Cu, 0.38% Mo
1.25% C, 0.27% Si, 0.38% Mn, 0.021% P, 0.024% S, 4.03% Cr, 0.19% Ni, 3.68% V, 12.60% W, 0.17% Cu, 0.83% Mo
1.25% C, 0.27% Si, 0.38% Mn, 0.021% P, 0.024% S, 4.03% Cr, 0.19% Ni, 3.68% V, 12.60% W, 0.17% Cu, 0.83% Mo
1.25% C, 0.70% Si, 0.50% Mn, 4.12% Cr, 0.50% Ni, 2.95% V, 6.32% W, 5.00% Mo, 8.38% Co
1.25% C, 0.70% Si, 0.50% Mn, 4.15% Cr, 0.50% Ni, 2.95% V, 6.30% W, 5.00% Mo, 1.00% Co
1.25% C, 0.90% Si, 0.35% Mn, 8.75% Cr, 2.70% Mo, 1.18% Mo, + Additions
1.26% C, 0.21% Mn, 0.23% Si, 0.009% P, 0.019% S 5.30% Ni
1.26% C, 0.23% Si, 0.21% Mn, 0.009% P, 0.019% S, 5.30% Ni, 0.04% Cr, 0.01% Mo
1.27% C, 0.30% Mn, max. 0.030% P, max. 0.030% S, 0.55% Si, 4.20% Cr, 5.00% Mo, 8.50% Co, 3.10% V, 6.25% W
1.28% C, 0.37% Si, 0.29% Mn, 0.019% P, 0.017% S, 2.90% Cr
1.28% C, 12.35% Mn, 0.35% Si, 0.009% S, 0.031% P 0.28% Ni, 0.01% Mo, 0.23% Cu
1.28% C, 4.00% Cr, 5.00% Mo, 6.40% W, 3.10% V
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V, 8.50% Co
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V, 8.50% Co
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 8.50% Co, 3.10% V
1.28% C, 4.2% Cr, 5.0% Mo, 6.4% W, 3.1% V
1.28% C, 4.20% Cr, 5.00% Mo, 6.40% W, 3.10% V, 8.50% Co
1.29% C, 0.08%Cr, 12.50% Mn
1.29% C, 0.20% Mn, 0.27% Si, 0.005% S, 0.015% P 0.09% Ni, 0.04% Cr, 0.01% Mo, 0.08% Cu
1.29% C, 0.20% Mn, 0.27% Si, 0.005% S, 0.015% P 0.09% Ni, 0.04% Cr, 0.01% Mo, 0.08% Cu
1.29% C, 0.26% Mn, 0.43% Si, 0.006% S, 0.025% P 4.42% Cr, 4.10% Mo, 4.00% V, 5.54% W, 0.37% Co
1.29% C, 0.40% Mn, 0.03% P, 0.02% S, 4.03% Cr, 4.43% Mo, 5.26% W, 3.82% V
1.29% C, 0.40% Mn, 0.03% P, 0.02% S, 4.03% Cr, 4.43% Mo, 5.26% W, 3.82% V
1.29% C, 0.40% Mn, 0.03% P, 0.02% S, 4.03% Cr, 4.43% Mo, 5.26% W, 3.82% V
1.29% C, 0.50% Si, 0.30% Mn, 0.024% P, 0.020% S, 4.20% Cr, 5.00% Mo, 0.15% Ni, 3.00% V, 6.30% W, 0.15% Cu, 0.25% Co
1.29% C, 0.50% Si, 0.30% Mn, 0.024% P, 0.020% S, 4.20% Cr, 5.00% Mo, 0.15% Ni, 6.30% W, 3.00% V, 0.25% Co, 0.15% Cu
1.29% C, 1.21% Si, 0.70% Mn, 0.017% P, 0.009% S, 1.20% Cr
1.30% C, 0.25% Cr, 0.25% Si, 0.30% Mn
1.30% C, 4.20% Cr, 6.40% W, 5.00% Mo, 3.10% V, 8.50% Co
1.30% C, 4.20% Cr, 6.40% W, 5.00% Mo, 3.10% V
1.30% C, 0.25% Cr, 0.25% Si, 0.30% Mn
1.30% C, 0.22% Si, 0.30% Mn, 0.017% P, 0.010% S, 4.13% Cr, 3.58% Mo, 0.16% Ni, 3.07% V, 9.70% W, 10.10% Co
1.30% C, 0.22% Si, 0.30% Mn, 0.017% P, 0.010% S, 4.13% Cr, 3.58% Mo, 0.16% Ni, 3.07% V, 9.70% W, 10.10% Co
1.31% C, 0.22% Si, 0.28% Mn, 0.024% P, 0.005% S, 3.86% Cr, 0.24% Ni, 3.30% V, 10.05% W, 0.15% Cu, 3.76% Mo, 10.70% Co, 0.013% Al
1.32% C, 0.28% Mn, 0.50% Si, 0.22% Cr, 3.51% W
1.32% C, 0.44% Si, 0.14% Mn, 0.027% P, 0.026% S, 4.13% Cr, 4.94% Mo, 0.26% Ni, 3.09% V, 6.25% W, 0.16% Cu, 8.38% Co
1.32% C, 0.50% Si, 0.28% Mn, 0.22% Cr, 3.51% W
1.35% C, 0.28% Si, 0.52% Mn, 0.006% P, 0.017% S
1.35% C, 0.73% Mn, 0.45% Si, 6.00% Cr, 0.98% Mo
1.35% C, 4.20% Cr, 4.50% Mo, 5.80% W, 4.00% V
1.35% C, 4.25% Cr, 4.50% Mo, 4.0% V, 5.75% W
1.36% C, 0.70% Mn, 0.43% Si, 11.90% Cr, 3.06% Mo
1.36% C, 0.72% Mn, 0.44% Si, 12.00% Cr, 1.00% Mo
1.36% C, 0.77% Mn, 0.50% Si, 5.99% Cr, 0.041% Mo
1.36% C, 1.84% Mn, 1.14% Si, 1.81% Ni, 0.15% Cr, 1.41% Mo
1.36% C, 1.84% Mn, 1.14% Si, 1.81% Ni, 0.15% S 1.41% Mo, 0.38% Graphite
1.37% C
1.37% C
1.38% C, 0.74% Mn, 0.46% Si, 11.80% Cr, 0.078% Mo
1.4% C, 1.0% Si, 0.6% Mn, 4.6% Cr, 3.2% Mo, 3.7% V
1.4% C, 1.0% Si, 0.6% Mn, 4.6% Cr, 3.2% Mo, 3.7% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.40% C, 0.90% Si, 0.80% Mn, 0.25 Mo
1.40-1.50% C, 0.20-0.35% Si, 0.30-0.50% Mn, max. 0.030% P, max. 0.030% S, 3.00-3.50% V
1.40% C, 6.40% Cr, 1.50% Mo, 3.70% V, 3.50% W, +Nb
1.40% C, 0.40% Si, 0.40% Mn, 4.70% Cr, 3.50% Mo, 3.70% V
1.42% C, 0.37% Si, 0.61% Mn, 0.024% P, 0.015% S, 1.37% Cr, 0.04% Cu, 0.18% V
1.42% C, 0.37% Si, 0.61% Mn, 0.024% P, 0.015% S, 1.37% Cr, 0.04% Cu, 0.18% V
1.42% C, 0.43% Mn, 0.38% Si, 0.025% S, 0.005% P 4.42% Cr, 0.70% Mo, 4.55% V, 12.99% W, 4.97% Co
1.43% C, 0.17% Mn, 0.29% Si, 0.045% S, 0.023% P 0.15% Ni, 4.18% Cr, 0.87% Mo, 11.00% W, 4.35% V
1.43% C, 0.22% Mn, 0.21% Si, 0.013% S, 0.020% P 0.11% Ni, 2.55% Cr, 0.08% Mo, 0.05% Cu, 0.015% V
1.43% C, 0.22% Si, 0.71% Mn, 0.014% P, 0.060% S, 1.45% Cr, 0.03% Ni
1.43% C, Fe-1.49% C-4.90% Cu
1.44% C, 0.38% Mn, 0.17% Cr, 0.02% Ni
1.45% C, 0.30% Si, 0.40% V, 3.25% V
1.45% C, 4.00% Cr, 1.00% Mo, 13.00% W, 4.50% V, 5.00% Co
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.20-0.60% Mn, 0.10-0.60% Si, 0.03% S, 0.03% P, 11.0-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.20-0.60% Mn, 0.10-0.60% Si, 0.03% S, 0.03% P, 11.0-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.45-1.60% C, 0.20-0.60% Mn, 0.10-0.60% Si, 0.03% S, 0.03% P, 11.0-13.00% Cr, 0.70-1.00% Mo, 0.70-1.00% V
1.46% C, 0.10% Mn, 0.27% Si, 0.033% S, 0.031% P 3.72% Cr, 0.47% Mo, 0.09% Cu, 4.10% V, 13.70% W, 5.00% Co
1.48% C, 0.21% Si, 0.45% Mn, 0.015% P, 0.017% S, 0.29% Cr, 0.12% Ni, 3.50% V, 0.11% Cu, 0.01% Mo, 0.013% Sn
1.48% C, 0.90% Mn, 0.24% Si, 0.002% P, 0.0039% S
1.485% C, 0.80% Mn, 0.46% Si, 0.028% S, 0.028% P 0.40% Ni, 1.24% Cr, 0.55% Mo
1.49% C, 0.27% Si, 0.26% Mn, 11.65% Cr, 0.48% Mo, 0.22% V
1.49% C, 0.60% Si, 0.67% Mn, 0.020% P, 0.020% S, 14.39% Cr, 0.33% Ni, 0.11% V, 0.05% W, 0.17% Cu, 0.49% Mo
1.49% C, 0.60% Si, 0.67% Mn, 0.020% P, 0.020% S, 14.39% Cr, 0.33% Ni, 0.11% V, 0.05% W, 0.17% Cu, 0.49% Mo
1.49% C, 0.26% Si, 0.33% Mn, 12.32% Cr, 1.01% Mo, 0.37% V
1.49% C, 0.26% Si, 0.33% Mn, 12.32% Cr, 1.01% Mo, 0.37% V
1.50% C, 0.25% Si, 0.25% Mn, 11.25% Cr, 0.80% Mo, 0.85% V
1.50% C, 0.40% Si, 0.40% Mn, 12.00% Cr, 0.95% Mo, 1.00% V
1.50% C, 0.50% Mn, 0.30% Si, 12.00% Cr, 0.80% Mo, 0.90% V
1.50% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 1.50% Mo, 4.00% V
1.50% C, 1.00% Si, 0.40% Mn, 8.00% Cr, 1.50% Mo, 4.00% V
1.50% C, 11.50% Cr, 0.80% Mo, 0.20% V
1.50% C, 11.50% Cr, 0.80% Mo, 0.20% V
1.50% C, 12.00% Cr, 0.90% Mo, 0.90% V
1.50% C, 22.59% Cr
1.50-1.60% C, 0.15-0.45% Mn, 0.10-0.40% Si, 11.00-12.00% Cr, 0.60-0.80% Mo, 0.90-1.10% V
1.50-2.00% C, 0.75-1.50% Si, 0.40-1.00% Mn, 4.00-9.00% Cr, 0.60-1.50% Ni, 3.00-8.00% Mo, 2.00-7.00% V, 1.00-4.00% W, 1.00-1.50% other MC elements
1.50% C, 8.00% Cr, 1.50% Mo, 4.00% V
1.50-1.60% C, 0.40-0.60% Mn, 0.50-0.80% Si, 11.00-12.00% Cr, 0.70-0.90% Mo, 0.90-1.10% V
1.50% C, max. 0.60% Si, max. 0.60% Mn, max. 0.030% P, max. 0.30% S, 12.0% Cr, 0.80% V, 0.95% Mo, max. 0.30% Cu, max. 0.55% Ni+Cu
1.51% C, 0.32% Si, 0.27% Mn, 0.019% P, 0.016% S, 11.60% Cr, 0.63% Mo, 0.20% Ni, 0.91% V, 0.02% W
1.52% C, 0.30% Si, 0.32% Mn, 0.019% P, 0.016% S, 11.50% Cr, 0.29% Ni, 0.11% W, 0.18% Cu, 0.68% Mo, 0.03% Co
1.52% C, 0.30% Si, 0.32% Mn, 0.019% P, 0.016% S, 11.50% Cr, 0.29% Ni, 0.11% W, 0.18% Cu, 0.68% Mo, 0.03% Co
1.52% C, 0.34% Si, 0.27% Mn, 0.020% P, 0.013% S, 11.37% Cr, 0.75% Mo, 0.19% Ni, 0.88% V, 0.19% W
1.52% C, 0.34% Si, 0.27% Mn, 0.020% P, 0.013% S, 11.37% Cr, 0.75% Mo, 0.19% Ni, 0.88% V, 0.19% W
1.52% C, 6.27% Cr
1.52% C, 0.52% Si, 1.48% Mn, 1.49% Ni, 1.50% Cr, 0.51% Mo, 0.005% P, 0.002% S
1.53% C, 0.37% Mn, 0.39% Si, 0.008% S, 0.009% P 12.30% Cr, 0.79% Mo, 1.13% V, 0.005% Nb
1.53% C, 12.00% Cr, 0.70% Mn, 1.00% V
1.54% C, 0.37% Mn, 0.41% Si, 0.009% S, 0.011% P 11.99% Cr, 0.75% Mo, 0.50% V, 0.65% Nb
1.55% C, 0.20% Si, 0.30% Mn, 0.030% P, 0.005% S, 12.00% Cr, 0.80% Mo, 1.00% V
1.55% C, 0.30% Mn, 0.30% Si, 12.00% Cr, 0.70% Mo, 1.00% V
1.55% C, 0.30% Si, 0.30% Mn, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.70% Mo, 1.00% V
1.55% C, 0.35% Mn, 0.30% Si, 0.020% P, 0.005% S, 11.75% Cr, 0.75% Mo, 0.75% V
1.55% C, 0.35% Mn, 0.30% Si, 0.020% P, 0.005% S, 11.75% Cr, 0.75% Mo, 0.75% V
1.55% C, 12.0% Cr, 0.70% Mo, 1.0% V
1.55% C, 12.00% Cr, 0.70% Mo, 1.00% V
1.55% C, 12.00% Cr, 0.70% Mo, 1.00% V
1.55% C, 12.00% Cr, 0.70% Mo, 1.00% V
1.55% C, 12.00% Cr, 0.70% Mo, 1.00% V
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 11.00-12.00% Cr, 0.50-0.70% Mo, 0.40-0.60% W, 0.10-0.50% V
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, max. 0.030% P, max. 0.030% S, 11.00-12.00% Cr, 0.50-0.70% Mo, 0.40-0.60% W, 0.10-0.50% V
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 11.00-12.00% Cr, 0.50-0.60% Mo, 0.00% Ni, 1.20-1.40% Co
1.55-1.75% C, 0.25-0.40% Si, 0.20-0.40% Mn, max. 0.035% P, max. 0.035% S, 11.00-12.00% Cr, 0.50-0.60% Mo, 0.00% Ni, 1.20-1.40% Co
1.55% C, 0.20% Si, 0.30% Mn, 0.030% P, 0.005% S, 12.00% Cr, 0.80% Mo, 1.00% V
1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 12.00% Cr, 0.80% Mo, 0.90% V
1.55% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.75% Mo, 0.90% V
1.55% C, 0.30% Si, 0.40% Mn, 11.50% Cr, 0.70% Mo, 1.00% V
1.56% C, 0.35% Mn, 0.30% Si, 0.020% P, 0.005% S, 11.75% Cr, 0.85% Mo, 0.30% V
1.56% C, 0.35% Mn, 0.30% Si, 0.020% P, 0.005% S, 11.75% Cr, 0.85% Mo, 0.30% V
1.56% C, 0.36% Mn, 0.35% Si, 0.009% S, 0.011% P 11.99% Cr, 0.72% Mo, 0.06% V, 1.01% Nb
1.56% C, 0.37% Mn, 0.20% Si, 0.001% S, 0.020% P 0.26% Ni, 12.46% Cr, 0.54% Mo, 0.10% Cu, 0.65% V, 0.28% W
1.57% C, 11.20% Cr
1.58% C, 0.29% Si, 0.37% Mn, 0.020% P, 0.017% S, 11.50% Cr, 0.19% Ni, 0.94% V, 0.11% Cu, 0.69% Mo
1.58% C, 0.29% Si, 0.37% Mn, 0.020% P, 0.017% S, 11.50% Cr, 0.19% Ni, 0.94% V, 0.11% Cu, 0.69% Mo
1.59% C, 0.42% Si, 0.42% Mn, 0.024% P, 0.019% S, 11.80% Cr, 0.22% Ni, 0.15% V, 0.51% W, 0.16% Cu, 0.61% Mo
1.59% C, 0.42% Si, 0.42% Mn, 0.024% P, 0.019% S, 11.80% Cr, 0.22% Ni, 0.15% V, 0.51% W, 0.16% Cu, 0.61% Mo
1.6% C, 0.3% Si, 0.35% Mn, 12% Cr, 0.6% Mo, 0.9% V, 0.12% Al
1.60% C, 0.070% S, 4.25% Cr, 5.00% Co, 5.00% V, 12.25% W
1.60% C, 0.30% Si, 0.35% Mn, 12.00% Cr, 0.60% Mo, 0.90% V, 0.12% Al
1.60% C, 0.31% Si, 0.27% Mn, 0.024% P, 0.003% S, 11.47% Cr, 0.15% Ni, 0.09% V, 0.13% Cu, 0.02% Mo
1.60% C, 0.31% Si, 0.27% Mn, 0.024% P, 0.003% S, 11.47% Cr, 0.15% Ni, 0.09% V, 0.13% Cu, 0.02% Mo
1.60% C, 0.40% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 7.20% V
1.60% C, 0.40% Si, 0.50% Mn, 5.00% Cr, 2.30% Mo, 7.20% V
1.60%C, 0.50% Mn, 0.40% Si, 16.00% Cr, 0.35% Ni, 0.80% Mo, 0.45% V, 79.90% Fe
1.62% C, 0.40% Mn, 0.48% Si, 0.01% S, 0.024% P 12.44% Cr, 0.80% Mo, 0.83% V
1.64% C, 0.21% Mn, 0.31% Si, 0.005% S, 0.021% P 4.50% Cr, 0.66% Mo, 5.50% V, 11.64% W, 11.35% Co
1.65% C, 0.27% Si, 0.39% Mn, 0.025% P, 0.019% S, 11.17% Cr, 0.50% Mo, 0.20% Ni, 0.16% V, 0.59% W
1.65% C, 0.30% Si, 0.30% Mn, 0.025% P, 0.010% S, 12.00% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 12.00% Cr, 0.50% W, 0.25% V
1.65% C, 12.00% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.65% C, 0.27% Si, 0.39% Mn, 0.025% P, 0.019% S, 11.17% Cr, 0.50% Mo, 0.20% Ni, 0.16% V, 0.59% W
1.65% C, 0.27% Si, 0.39% Mn, 0.025% P, 0.019% S, 11.17% Cr, 0.50% Mo, 0.20% Ni, 0.16% V, 0.59% W
1.65 C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.60% Mo, 0.30% V, 0.50% W
1.7% C, 0.8% Si, 0.3% Mn, 18.0% Cr, 1.0% Mo, 3.0% V
1.7% C, 0.8% Si, 0.3% Mn, 18.0% Cr, 1.0% Mo, 3.0% V
1.70% C, 0.80% Si, 0.30% Mn, 18.00% Cr, 1.00% Mo, 3.00% V
1.70% C, 0.80% Si, 0.30% Mn, 18.00% Cr, 1.00% Mo, 3.00% V
1.70% C, 1.20% Si, 1.00% Mn, 1.00% Cr, 1.50% Ni, 0.75% Mo
1.72% C, 0.26% Si, 0.34% Mn, 0.033% P, 0.014% S, 11.50% Cr, 0.19% Ni, 0.12% V, 0.66% W, 0.18% Cu, 0.68% Mo
1.72% C, 0.26% Si, 0.34% Mn, 0.033% P, 0.014% S, 11.50% Cr, 0.19% Ni, 0.12% V, 0.66% W, 0.18% Cu, 0.68% Mo
1.72% C, 0.37% Si, 0.26% Mn, 0.022% P, 0.002% S, 11.53% Cr, 0.25% Ni, 1.03% V, 0.11% W, 0.19% Cu, 0.84% Mo
1.72% C, 0.38% Si, 0.43% Mn, 0.022% P, 0.005% S, 11.44% Cr, 0.24% Ni, 1.03% V, 0.19% W, 0.17% Cu, 0.78% Mo
1.72% C, 0.38% Si, 0.43% Mn, 0.022% P, 0.005% S, 11.44% Cr, 0.24% Ni, 1.03% V, 0.19% W, 0.17% Cu, 0.78% Mo
1.72% C, 0.90% Mn, 0.25% Si, <0.003% P, 0.003% S
1.78% C, 0.27% Mn, 0.25% Si, 0.010% S, 0.025% P 0.35% Ni, 11.70% Cr, 0.61% Mo, 0.09% V, 0.63% W
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.020% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.10-0.60% Si, 0.20-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr
1.90-2.20% C, 0.15-0.45% Mn, 0.10-0.40% Si, 11.00-12.00% Cr
1.90-2.20% C, 0.15-0.45% Mn, 0.10-0.40% Si, 11.00-12.00% Cr
1.95% C, 10.80% Cr, 3.80% Mo
1.95% C, 10.80% Cr, 3.80% Mo
1.96% C, 15.40% Cr, 2.20% Mo
1.96% C, 15.40% Cr, 2.20% Mo
1.98% C (total), 0.148% P, 0.071% S
1.98% C, 0.19% Si, 0.32% Mn, 11.84% Cr, 0.18% Ni, 0.05% W
1.98% C, 0.19% Si, 0.32% Mn, 11.84% Cr, 0.18% Ni, 0.05% W
1.98% C, 20.25% Cr, 2.14% Mo
1.99% C, 0.23% Si, 0.27% Mn, 0.016% P, 0.013% S, 11.18% Cr, 0.16% Ni, 0.12% Cu, 0.02% Mo, 0.021% Al
1.99% C, 0.23% Si, 0.27% Mn, 0.016% P, 0.013% S, 11.18% Cr, 0.16% Ni, 0.12% Cu, 0.02% Mo, 0.021% Al
2.00% C, 0.30% Si, 0.30% Mn, 12.00% Cr
2.00% C, 0.35% Si, 0.30% Mn, 11.50% Cr
2.00% C, 0.40% Si, 0.35% Mn, 15.70% Cr, 0.60% Ni, 0.70% Mo, 1.38% W, 0.025% P, 0.040% S
2.00% C, 0.43% Si, 0.30% Mn, 0.021% P, 0.018% S, 3.77% Cr, 2.49% Mo, 4.83% V, 14.27% W, 11.00% Co
2.00% C, 0.65% Mn, 0.30% Si, 0.030% S, 0.013% P, 0.12% Cr, 0.05% Ni, 0.50% Mo, 0.03% V, 0.08% Cu, 0.051% Al
2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
2.00-2.30% C, 0.10-0.40% Si, 0.30-0.60% Mn, max. 0.030% P, max. 0.030% S, 11.00-13.00% Cr, 0.60-0.80% W
2.0% C, 5% Cr, 5% Mo, 5% W, 5% V, 5% Co
2.00% C, 0.30% Si, 0.30% Mn, 12.00% Cr
2.03% C, 0.39% Si, 0.32% Mn, 11.49% Cr, 0.11% V, 0.78% W
2.03% C, 0.39% Si, 0.32% Mn, 11.49% Cr, 0.11% V, 0.78% W
2.04% C, 20.55% Cr, 0.61% Mo
2.04% C, 20.55% Cr, 0.61% Mo
2.05% C, 0.30% Si, 0.30% Mn, 11.50% Cr
2.05% C, 0.30% Si, 0.30% Mn, 11.50% Cr
2.05% C, 15.60% Cr, 0.81% Mo
2.05% C, 15.60% Cr, 0.81% Mo
2.07% C (total), 2.19% C (graphite), 0.78% C (combined), 2.00% Si
2.07% C, 0.25% Si, 0.38% Mn, 0.017% P, 0.012% S, 11.50% Cr, 0.20% Ni, 0.07% V, 0.15% Cu
2.08% C, 0.28% Si, 0.39% Mn, 0.017% P, 0.012% S, 11.48% Cr, 0.15% Cu, 0.02% Mo, 0.31% Ni, 0.04% V
2.08% C, 0.28% Si, 0.39% Mn, 0.017% P, 0.012% S, 11.48% Cr, 0.15% Cu, 0.02% Mo, 0.31% Ni, 0.04% V
2.08% C, 0.39% Mn, 0.28% Si, 0.012% S, 0.017% P, 11.48% Cr, 0.31% Ni, 0.02% Mo, 0.04% V, 0.15% Cu
2.08% C, 15.85% Cr, trace level Mo
2.08% C, 15.85% Cr, trace level Mo
2.08% C, 20.55% Cr, <0.01% Mo
2.08% C, 20.55% Cr, <0.01% Mo
2.08% C, 0.28% Si, 0.39% Mn, 0.017% P, 0.012% S, 11.48% Cr, 0.31% Ni; 0.02% Mo, 0.15% Cu, 0.04% V
2.09% C, 0.26% Si, 0.30% Mn, 0.014% P, 0.022% S, 11.74% Cr, 0.18% Ni, 0.55% W, 0.13% Cu, 0.07% Mo, 0.10% Al
2.09% C, 0.26% Si, 0.30% Mn, 0.014% P, 0.022% S, 11.74% Cr, 0.18% Ni, 0.55% W, 0.13% Cu, 0.07% Mo, 0.10% Al
2.09% C, 0.52% Mn, 0.33% Si, 12.76% Cr
2.10% C, 0.18% Si, 0.30% Mn, 0.020% P, 0.022% S, 11.80% Cr, 0.15% Ni, 0.19% Cu, 0.06% Mo
2.10% C, 0.30% Si, 0.30% Mn, 0.030% P, 0.005% S, 12.00% Cr, 0.70% W
2.10% C, 0.30% Si, 0.30% Mn, 12.00% Cr
2.10% C, 0.35% Si, 0.35% Mn, 12.00% Cr, 0.70% W
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 1.00% Si, 0.40% Mn, 6.80% Cr, 1.50% Mo, 5.40% V
2.10% C, 12.00% Cr, 0.70% W
2.10% C, 12.00% Cr, 0.70% W
2.10% C, 12.00% Cr, 0.80% W
2.10% C, 12.00% Cr
2.10% C, 12.00% Cr
2.10% C, 12.50% Cr
2.10% C, 0.35% Si, 0.35% Mn, 12.00% Cr, 0.70% W
2.10% C, 0.25% Si, 0.30% Mn, 12.50% Cr, 0.90% Mo, 2.10% V
2.10% C, 0.30% Si, 0.30% Mn, 11.50% Cr, 0.70% W
2.12% C, 12.12% Cr, 0.81% W, 0.33% Mn, 0.21% Si
2.13% C, 11.30% Cr, 1.41% Mo
2.13% C, 11.30% Cr, 1.41% Mo
2.15-2.30% C, 0.15-0.30% Si, 0.25-0.40% Mn, max. 0.035% P, max. 0.035% S, 12.00-13.00% Cr, 0.80-1.00% Mo, 2.00-2.30% V
2.15-2.30% C, 0.15-0.30% Si, 0.25-0.40% Mn, max. 0.035% P, max. 0.035% S, 12.00-13.00% Cr, 0.80-1.00% Mo, 2.00-2.30% V
2.16% C (total), 0.113% P, 0.071% S
2.19% C, 0.32% Mn, 0.26% Si, 0.008% S, 0.027% P, 11.75% Cr, 0.31% Ni, 0.12% Mo, 0.08% V, 0.12% Cu, 0.84% W
2.19% C, 11.65% Cr, 0.02% Mo
2.20% C, 13.00% Cr, 1.00% Mo, 4.00% V
2.25% C, 0.29% Si, 0.32% Mn, max. 0.011% S, 12.34% Cr, 0.98% Mo, 3.94% V
2.25% C, 11.50% Cr, 0.80% Mo, 0.20% V
2.25% C, 11.50% Cr, 0.80% Mo, 0.20% V
2.25% Cr, 1% Mo
2.30% C, 0.40% Si, 0.40% Mn, 26.00% Cr, 4.00% V, 1.10% Mo
2.30% C, 0.40% Si, 0.40% Mn, 26.00% Cr, 4.00% V, 1.10% Mo
2.30% C, 0.40% Si, 0.40% Mn, 4.80% Cr, 3.60% Mo, 8.00% V
2.30% C, 0.60% Si, 0.30% Mn, 12.50% Cr, 1.10% Mo, 4.00% V
2.30% C, 4.00% Cr, 7.00% Mo, 6.50% W, 6.50% V, 10.50% Co
2.30% C, 4.20% Cr, 6.50% W, 7.00% Mo, 6.50% V, 10.50% Co
2.30% C, 4.20% Cr, 7.00% Mo, 6.50% W, 10.50% Co, 6.50% V
2.30% C, 4.20% Cr, 7.00% Mo, 6.50% W, 6.5% V, 10.50% Co
2.30% C, 0.40% Si, 0.40% Mn, 4.80% Cr, 3.80% Mo, 8.00% V
2.30% C, 4.20% Cr, 7.00% Mo, 6.50% W, 6.50% V, 10.50% Co
2.40% C, 0.35% Si, 0.73% Mn, 17.50% Cr, 1.00% Ni, 1.00% Mo, 0.028% P, 0.034% S
2.41% C, 12.15% Cr, 2.45% Mo
2.41% C, 12.15% Cr, 2.45% Mo
2.45% C, 0.55% Si, 4.15% Cr, 3.75% Mo, 9.00% V, 1.00% W, 2.00% Co
2.45% C, 0.55% Si, 4.15% Cr, 3.75% Mo, 9.00% V, 1.00% W, 2.00% Co
2.45% C, 19.82% Cr, 2.94% Mo
2.45% C, 19.82% Cr, 2.94% Mo
2.48% C, 4.2% Cr, 3.1% Mo, 4.2% W, 8.0% W
2.5% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 1.00% Ni, 0.10% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 1.00% Ni, 0.50% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 1.00% Ni, 1.00% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 2.00% Ni, 0.50% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 2.00% Ni, 1.00% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 3.00% Ni, 0.5% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 3.00% Ni, 1.00% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 4.00% Ni, 0.50% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 4.00% Ni, 1.00% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 5.00% Ni, 0.50% Mo
2.50% C (total), 2.50% Si, 0.85% Mn, 0.10% P, 0.10% S, 5.00% Ni, 1.00% Mo
2.50% C, 2.00% Cr, 0.60% Ni, 5.20% Mo, 7.20% V
2.54% C, 20.22% Cr, 1.52% Mo
2.54% C, 20.22% Cr, 1.52% Mo
2.55% C, 12.40% Cr, 1.25% Mo
2.55% C, 12.40% Cr, 1.25% Mo
2.57% C, 0.48% Mn, 1.44% Si, 0.27% P, 0.11% S, 0.05% Cr, 0.008% Al, 0.0028% B
2.58% C, 0.40% Mn, 1.44% Si, 0.32% Mo, 0.001% B
2.58% C, 0.42% Mn, 1.37% Si, 0.15% Mo, 0.001% B
2.60% C, 0.42% Mn, 1.43% Si, 0.017% Mo, 0.002% B
2.60% C, 0.80% Si, 0.60% Mn, 27.80% Cr
2.60% C, 15.20% Cr, 1.95% Mo
2.60% C, 15.20% Cr, 1.95% Mo
2.65% C, 12.65% Cr, 0.02% Mo
2.65% C, 12.65% Cr, 0.02% Mo
2.67% C, 14.95% Cr, trace level Mo
2.67% C, 14.95% Cr, trace level Mo
2.67% C, 15.20% Cr, 1.09% Mo
2.67% C, 15.20% Cr, 1.09% Mo
2.67% C, 20.75% Cr, <0.01% Mo
2.67% C, 20.75% Cr, <0.01% Mo
2.72% C, 25.15% Cr, 2.52% Mo
2.72% C, 25.15% Cr, 2.52% Mo
2.73% C, 0.03% Mn, 1.25% Si, 0.015% S. B5: 2.73% C, 0.02% Mn, 1.23% Si, 0.064% S. B6: 2.83% C, 0.03% Mn, 1.23% Si, 0.123% S. B7: 2.71% C, 0.02% Mn, 1.20% Si, 0.275% S
2.75% C, 0.13% Mn, 1.21% Si, 0.008% S. A2: 2.71% C, 0.44% Mn, 1.22% Si, 0.008% S. A3: 2.70% C, 0.72% Mn, 1.24% Si, 0.007% S
2.80% C, 0.80% Si, 0.70% Mn, 7.00% Cr, 2.30% Mo, 8.90% V
2.80% C, 0.80% Si, 0.70% Mn, 7.00% Cr, 2.30% Mo, 8.90% V
2.80% C, 15.25% Cr, 9.00% V, 3.00% Nb, 2.25% Mo, 2.50% Co
2.80-3.00% C, 0.15-0.25% Si, 0.20-0.40% Mn, max. 0.020% P, max. 0.020% S, 11.50-12.50% Cr
2.87% C, 25.50% Cr, 1.22% Mo
2.87% C, 25.50% Cr, 1.22% Mo
2.88% C, 0.78% Mn, 0.60% Si, 16.90% Cr, 1.52% Mo, 1.74% Cu
2.89% C, 1.56% Mn, 0.60% Si, 17.40% Cr, 1.49% Mo
2.89% C, 19.35% Cr, 2.08% Mo, 1.02% Cu, 0.73% Mn, 0.55% Si
2.89% C, 3.08% Mn, 0.61% Si, 17.00% Cr, 1.49% Mo
2.90% C, 0.50% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 9.80% V
2.90% C, 0.50% Si, 0.50% Mn, 8.00% Cr, 1.50% Mo, 9.80% V
2.90% C, 0.60% Si, 0.70% Mn, 19.40% Cr, 2.10% Mo, 1.00% Cu
2.90% C, 0.75% Mn, 0.56% Si, 17.60% Cr, 0.48% Mo
2.90% C, 0.76% Mn, 0.55% Si, 0.61% Ni, 17.40% Cr, 1.43% Mo
2.91% C, 0.76% Mn, 0.59% Si, 17.50% Cr, 2.89% Mo
2.91% C, 0.77% Mn, 0.58% Si, 17.40% Cr, 0.56% Mo, 1.02% Cu
2.93% C, 0.60%Si, 0.78% Mn, 17.4% Cr, 0.04% Mo
2.93% C, 0.76% Mn, 0.55% Si, 1.10% Ni, 17.40% Cr, 2.43% Mo
2.93% C, 0.76% Mn, 0.56% Si, 2.07% Ni, 17.50% Cr, 0.45% Mo
2.93% C, 0.76% Mn, 0.59% Si, 17.50% Cr, 1.59% Mo
2.93% C, 0.78% Mn, 0.60% Si, 17.40% Cr, 0.04% Mo
2.93% C, 1.89% Si, 0.74% Mn, 0.218% P, 0.062% S, 0.513% Mo
2.94% C, 0.78% Mn, 0.58% Si, 1.16% Ni, 17.60% Cr, 0.54% Mo
2.95% C, 0.77% Mn, 0.55% Si, 17.50% Cr, 0.56% Mo, 1.95% Cu
2.95% C, 25.82% Cr, 0.02% Mo
2.95% C, 25.82% Cr, 0.02% Mo
2.96% C, 0.52% Si,0.79% Mn, 17.5% Cr, 0.98% Cu, 1.55% Mo
2.96% C, 0.79% Mn, 0.52% Si, 17.50% Cr, 1.55% Mo, 0.98% Cu
2.96% C, 0.79% Mn, 0.93% Si, 17.50% Cr, 1.55% Mo, 0.98% Cu
2.96% C, 0.93% Si, 0.79% Mn, 17.5% Cr, 0.98% Cu, 1.55% Mo
2.97% C (total), 2.02% Si, 0.82% Mn, 0.30% P, 0.08% S
2.97% C (total), 2.11% C (graphite), 0.86% C (combined), 2.00% Si, 0.02-0.02% Al
3.00% C, 1.85% Si, 0.73% Mn, 0.216% P, 0.072% S, 0.249% Mo
3.04% C, 1.83% Si, 0.72% Mn, 0.212% P, 0.072% S, 0.149% Mo
3.08% C, 0.52% Si, 0.54% Mn, 2.3% Cr, 4.03% Ni
3.08% C, 0.52% Si, 0.54% Mn, 2.3% Cr, 4.03% Ni
3.11% C, 1.22% Si, 0.60% Mn, 8.32% Cr, 5.39% Ni
3.12% C, 1.91% Si, 0.76% Mn, 0.210% P, 0.068% S, 0.086% Mo
3.14% C, 2.15% Si, 0.81% Mn, 0.219% P, 0.064% S
3.2% C, 1.95% Si, 0.50% Mn, 8.5% Cr, 5.0% Ni
3.20% C, 2.40% Si, 0.21% Mn, 0.59% Ni, 0.62% Cu, 0.13% Mo
3.2% C, 2.4% Si, 0.21% Mn, 0.59% Ni, 0.62% Cu and 0.13% Mo [10]. Ductile iron 2 contains: 3.6% C, 0.27% Mn and 1.72% Si [11].
3.24% C, 0.31% Mn, 2.36% Si, 0.024% P, 0.008% S, 4.82% Ni, 0.49% Mo, 0.034% Mg
3.25% C, 11.80% Cr, 2.60% Mo
3.25% C, 11.80% Cr, 2.60% Mo
3.25Cr-0.5Mo steel: 0.69-0.75% C, 0.40-0.50% Si, 0.69-0.50% Mn, 3.00-3.50% Cr, 0.45-0.55% Mo, 0.04-0.08% V. 5Cr-0.5Mo steel: 0.79-0.85% C, 0.40-0.50% Si, 0.40-0.50% Mn, 4.75-5.25% Cr, 0.45-0.55% Mo, 0.04-0.08% V.
3.29% C, 2.35% Si, 0.07% Mn, 1.90% Mo, 0.94% Ni
3.29% C, 2.35% Si, 0.07% Mn, 1.90% Mo, 0.94% Ni
3.3% C, 0.32% Mn, 2.40% Si, 0.024% P, 0.008% S, 2.37% Ni, 0.50% Mo, 0.038% Mg
3.32% C, 0.31% Mn, 2.58% Si, 0.024% P, 0.008% S, 0.49% Mo
3.32% C, 0.31% Mn, 2.58% Si, 0.49% Mo
3.32% C, 14.63% Cr, 2.05% Mo, 1.02% Cu, 0.72% Mn, 0.58% Si
3.33% C, 0.31% Mn, 2.57% Si, 0.024% P, 0.008% S, 0.75% Mo
3.33% C, 0.32% Mn, 2.69% Si, 0.022% P, 0.008% S, 0.25% Mo
3.33% C, 0.32% Mn, 2.69% Si, 0.25% Mo
3.34% C, 0.32% Mn, 2.65% Si, 0.022% P, 0.008% S, 0.20% Mo
3.36% C, 0.32% Mn, 2.46% Si, 0.023% P, 0.011% S, 1.17% Ni, 0.49% Mo, 0.044% Mg
3.37% C, 0.31% Mn, 2.62% Si, 0.022% P, 0.009% S
3.37% C, 2.62% Si, 0.31% Mn
3.39% C, 0.32% Mn, 2.45% Si, 0.023% P, 0.011% S, 0.61% Ni, 0.50% Mo, 0.041% Mg
3.39% C, 0.32% Mn, 2.45% Si, 0.61% Ni, 0.50% Mo
3.39% C, 11.95% Cr, 1.36% Mo
3.39% C, 11.95% Cr, 1.36% Mo
3.40% C, 19.85% Cr, 3.40% Mo
3.40% C, 19.85% Cr, 3.40% Mo
3.47% C, 0.33% Mn, 2.47% Si, 0.022% P, 0.011% S, 0.05% Ni, 0.50% Mo, 0.044% Mg
3.47% C, 0.33% Mn, 2.47% Si, 0.05% Ni, 0.50% Mo
3.51% C, 12.20% Cr, 0.02% Mo
3.51% C, 12.20% Cr, 0.02% Mo
3.51% C, 20.10% Cr, 1.37% Mo
3.51% C, 20.10% Cr, 1.37% Mo
3.52% C, 24.65% Cr, 2.67% Mo
3.52% C, 24.65% Cr, 2.67% Mo
3.54% C, 0.31% Mn, 3.45% Si, 0.024% P, 0.005% S, 0.04% Cr, 0.04% Ni, 0.02% Mo, 0.023% Mg
3.56% C, 14.60% Cr, 0.47% Mo
3.56% C, 14.60% Cr, 0.47% Mo
3.58% C, 0.32% Mn, 2.69% Si, 0.004% S, 0.02% Cr, 0.46% Mo, 0.06% Cu, 0.017% Al, 0.040% Mg
3.58% C, 14.45% Cr, trace level Mo
3.58% C, 14.45% Cr, trace level Mo
3.58% C, 14.65% Cr, 0.52% Mo
3.58% C, 14.65% Cr, 0.52% Mo
3.59% C, 0.29% Mn, 2.71% Si, 0.024% P, 0.007% S, 0.04% Cr, 0.03% Ni, 0.02% Mo, 0.024% Mg
3.60% C, 0.37% Mn, 3.68% Si, 0.022% P, 0.007% S, 0.04% Cr, 0.03% Ni, 0.03% Mo, 0.027% Mg
3.60% C, 0.38% Mn, 2.61% Si, 0.005% S, 0.02% Cr, 0.01% Mo, 0.01% Cu, 0.025% Al, 0.041% Mg
3.60% C, 0.40% Si, 0.90% Mn, 15.00% Cr, 2.60% Mo
3.61% C, 0.20% Mn, 2.83% Si, 0.022% P, 0.009% S, 0.04% Cr, 0.04% Ni, 0.02% Mo, 0.025% Mg
3.61% C, 0.35% Mn, 2.75% Si, 0.003% S, 0.07% Cr, 0.24% Mo, 0.07% Cu, 0.020% Al, 0.040% Mg, 0.0024% B
3.62% C, 0.32% Mn, 2.46% Si, 1.17% Ni, 0.49% Mo
3.62% C, 0.37% Mn, 2.70% Si, 0.005% S, 0.02% Cr, 0.08% Mo, 0.08% Cu, 0.021% Al, 0.043% Mg
3.62% C, 20.35% Cr, <0.01% Mo
3.62% C, 20.35% Cr, <0.01% Mo
3.63% C (total), 2.92% C (graphite), 0.71% C (combined), 1.75% Si, 0.53% Mn, 0.56% P, 0.10% S
3.63% C, 2.92% GC, 0.71% CC, 0.53% Mn, 1.75% Si, 0.56% P, 0.10% S. GC=Graphite carbon, CC=Combined carbon
3.66% C, 24.95% Cr, 1.53% Mo
3.66% C, 24.95% Cr, 1.53% Mo
3.66% C, 2.38% Si, 0.85% Ni, 0.53% Cu, 0.21% Mn, 0.16% Mo, 0.07% Mg, 0.05% Cr, 0.013% Al, 0.042% P, 0.032% S
3.66% C, 2.38% Si, 0.85% Ni, 0.53% Cu, 0.21% Mn, 0.16% Mo, 0.07% Mg, 0.05% Cr, 0.013% Al, 0.042% P, 0.032% S
3.68% C (total), 2.56% C (graphite), 1.12% C (combined), 2.03% Si, 0.37% Mn, 0.28% P, 0.11% S
3.68% C, 2.56% GC, 1.12% CC, 0.37% Mn, 1.20% Si, 0.28% P, 0.11% S, 2.03% Ni. GC=Graphite carbon, CC=Combined carbon
3.70% C, 25.32% Cr, 0.02% Mo
3.70% C, 25.32% Cr, 0.02% Mo
3.72% C, 2.32% Si, 0.31% Mn, 0.50% Cr, 3.85% Ni, 1.03% Cu
3.72% C, 2.32% Si, 0.31% Mn, 0.50% Cr, 3.85% Ni, 1.03% Cu
3.75% C, 2.40% Si, 0.33% Mn, 0.51% Cr, 1.41% Mo, 1.03% Cu
3.75% C, 2.40% Si, 0.33% Mn, 0.51% Cr, 1.41% Mo, 1.03% Cu
3.77% C, 0.42% Mn, 2.74% Si, 0.038% P, 0.011% S, 0.02% Cr, 0.43% Mo, 0.047% Mg
3.78% C, 2.26% Si, 0.24% Mn, 0.89% Cr, 0.78% Ni, 1.50% Cu
3.78% C, 2.26% Si, 0.24% Mn, 0.89% Cr, 0.78% Ni, 1.50% Cu
3.79% C, 0.42% Mn, 2.75% Si, 0.039% P, 0.010% S, 0.02% Cr, 0.04% Mo, 0.050% Mg
3.81% C, 14.75% Cr, 2.50% Mo
3.81% C, 14.75% Cr, 2.50% Mo
3.83% C, 2.36% Si, 0.06% Mn, 2.00% Mo, 1.62% Ni
3.83% C, 2.36% Si, 0.06% Mn, 2.00% Mo, 1.62% Ni
3.86% C, 0.43% Mn, 2.31% Si, 0.039% P, 0.012% S, 0.02% Cr, 0.37% Mo, 0.042% Mg
3.87% C, 0.44% Mn, 2.32% Si, 0.040% P, 0.011% S, 0.02% Cr, 0.01% Mo, 0.094% Mg
3.94% C, 23.45% Cr, 2.94% Mo
3.94% C, 23.45% Cr, 2.94% Mo
3.96% C, 14.80% Cr, 1.45% Mo
3.96% C, 14.80% Cr, 1.45% Mo
3.96% C, 17.55% Cr, 2.53% Mo
3.96% C, 17.55% Cr, 2.53% Mo
4.08% C, 18.00% Cr, 1.14% Mo
4.08% C, 18.00% Cr, 1.14% Mo
4.10% C, 15.10% Cr, trace level Mo
4.10% C, 15.10% Cr, trace level Mo
4.10% C, 23.67% Cr, 1.32% Mo
4.10% C, 23.67% Cr, 1.32% Mo
4.13% C, 18.22% Cr, 0.05% Mo
4.13% C, 18.22% Cr, 0.05% Mo
4.31% C, 24.80% Cr, 0.02% Mo
4.31% C, 24.80% Cr, 0.02% Mo
8% Cr steel
9% Cr steel
11.00% Ni, 18.50% Cr
13.45 Ni%, 24.70% Co, 3.00% Cu, 7.95% Al, 0.80% Nb + (dashed line) 0% Si; (light line) 0.2% Si; (heavy line) 0.4% Si
13.60 Ni%, 24.00% Co, 3.00% Cu, 7.85% Al. b.) 13.75 Ni%, 23.70% Co, 2.90% Cu, 8.00% Al, 1.80% Nb. c.) 14.30 Ni%, 24.10% Co, 3.60% Cu, 7.55% Al, 5.30% Nb
15.00% Cr, 25.00% Ni
18.7% Cr, 9.0% Ni, 1.73% Mn, 0.6% Si, 0.05% C
24.62 wt.% Mn, 13.18 wt.% Cr, 3.23 wt.% Ni, 0.62 wt.% N, 0.051 wt.% C, balance Fe
25Cr-6.9Ni-3.8Mo-0.3N
26% Cr, 1-4% Mo, 0-4% Ni
46.60% Al, 1.80% Cr, 1.80% Nb, 0.90% Mo, 420 ppm O, balance is Ti
47.90% Al, 1.90% Cr, 1.80% Nb, 0.90% Mo, 0.20% B, 420 ppm O, balance is Ti
CTC-08 as deposited weld metal (MIL-120S) with 0.04% C
CTC03-L as deposited weld metal with 0.009% C
CTC03-L as deposited weld metal with 0.009% C
CTC03-R as deposited weld metal with 0.035% C
CTC03-R as deposited weld metal with 0.035% C
Fe-0.005C
Fe-0.22% C-2% Mn
Fe-0.22% C-2% Mn
Fe-0.22% C
Fe-0.22% C
Fe-0.22% C
Fe-0.24C-0.27Mn-0.37Si-0.32Ni-13.3Cr-0.06Mo
Fe-0.42C-0.68Mn-0.16Si-0.93Cr
Fe-0.72C-0.27Mn-0.39Si-4.09Cr-1.25V-18.59W
Fe-0.7C-0.35Mn-0.16Si-3.24Ni-0.96Cr-0.06Mo
Fe-0.95C-0.36Mn-0.28Si-1.84Cr
Fe-0.95C-0.44Mn-0.21Si-1.42C
Fe-1.04C-0.32Mn-0.19Si-1.35Cr
Fe-3%Cr-0.5%Mo+0.4% C
Fe-3.62Mn-23.2Ni
Fe-O.11C
Fe-O.75C
Fe-O.81C
Fe-28 wt% Cr-Mo system with curves for 0, 2, 3.5 and 5 wt% Mo.