C (diamond) - Dislocation etching

Material Name: C (diamond)
Recipe No.: 10133
Primary Chemical Element in Material: C
Sample Type: Bulk
Uses: Etching
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Dislocation etching
Etchant (Electrolyte) Composition: Fused KNO3.
Procedure (Condition): Use at 500-700 C for 1 h. Pandya and Tolansky.
Note: (111), (110), (100).
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 716.